Effect of Al2O3 Addition and WO3 Modification on Catalytic Activity of NiO/Al2O3-TiO2/WO3 for Ethylene Dimerization

  • Pae, Young-Il;Sohn, Jong-Rack
    • Bulletin of the Korean Chemical Society
    • /
    • 제28권10호
    • /
    • pp.1763-1770
    • /
    • 2007
  • Strong solid acid catalysts, NiO/Al2O3-TiO2/WO3 for ethylene dimerization were prepared by the addition of Al2O3 and the modification with WO3. The acid sites and acid strength were increased by the inductive effect of WO3 species bonded to the surface of catalysts. The larger the dispersed WO3 amount, the higher both the acidity and catalytic activity for ethylene dimerization. The addition of Al2O3 to TiO2 up to 5 mol% enhanced acidity and catalytic activity gradually due to the interaction between Al2O3 and TiO2 and consequent formation of Al-O-Ti bond.

Highly Active Catalyst of Nickel Sulfate Supported on Titania for Ethylene Dimerization

  • 손종락;박원천
    • Bulletin of the Korean Chemical Society
    • /
    • 제22권12호
    • /
    • pp.1303-1308
    • /
    • 2001
  • A series of catalysts, NiSO4/TiO2, for ethylene dimerization was prepared by the impregnation method using aqueous solution of nickel sulfate. On the basis of the results obtained from X-ray diffraction, the addition of NiSO4 shifted the transition of TiO2 from the anatase to the rutile phase toward higher temperatures due to the interaction between NiSO4 and TiO2. Nickel sulfate supported on titania was found to be very active even at room temperature. The high catalytic activity of NiSO4/TiO2 closely correlated with the increase of acidity and acid strength due to the addition of NiSO4. It is suggested that the active sites responsible for ethylene dimerization consist of low valent nickel, Ni+, with an acid.

Characterization of NiSO4 Supported on Fe2O3 and Catalytic Properties for Ethylene Dimerization

  • Pae, Young-Il;Sohn, Jong-Rack
    • Bulletin of the Korean Chemical Society
    • /
    • 제28권8호
    • /
    • pp.1273-1279
    • /
    • 2007
  • The NiSO4 supported on Fe2O3 catalysts were prepared by the impregnation method. No diffraction line of nickel sulfate was observed up to 30 wt %, indicating good dispersion of nickel sulfate on the surface of Fe2O3. The addition of nickel sulfate to Fe2O3 shifted the phase transition of Fe2O3 (from amorphous to hematite) to higher temperatures because of the interaction between nickel sulfate and Fe2O3. 20-NiSO4/Fe2O3 containing 20 wt % of NiSO4 and calcined at 500 oC exhibited a maximum catalytic activity for ethylene dimerization. The initial product of ethylene dimerization was found to be 1-butene and the initially produced 1-butene was also isomerized to 2-butene during the reaction. The catalytic activities were correlated with the acidity of catalysts measured by the ammonia chemisorption method.

Preparation and Characterization of NiO/CeO2-ZrO2/WO3 Catalyst for Ethylene Dimerization: Effect of CeO2 Doping and WO3 Modifying on Catalytic Activity

  • Sohn, Jong-Rack;Han, Jong-Soo;Kim, Hae-Won;Pae, Young-Il
    • Bulletin of the Korean Chemical Society
    • /
    • 제26권5호
    • /
    • pp.755-762
    • /
    • 2005
  • A series of catalysts, NiO/$CeO_2-ZrO_2/WO_3$, for ethylene dimerization was prepared by the precipitation and impregnation methods. For NiO/$CeO_2-ZrO_2/WO_3$ sample, no diffraction line of nickel oxide was observed up to 40 wt%, indicating good dispersion of nickel oxide on the surface of catalyst. The hexagonal and monoclinic phases of $WO_3$ up to the calcination temperature of 500 ${^{\circ}C}$ were observed, whereas the hexagonal phase of WO3 completely was transformed into monoclinic phase of $WO_3$ at 600 ${^{\circ}C}$ and above. The role of $CeO_2$ in the catalysts was to form a thermally stable solid solution with zirconia and consequently to give high surface area and acidity. The catalytic activities for ethylene dimerization were correlated with the acidity of catalysts measured by the ammonia chemisorption method. 25-NiO/5-$CeO_2-ZrO_2/15-WO_3$ containing 25 wt% NiO, 15 wt% $WO_3$ and 5 mol% $CeO_2$, and calcined at 400 ${^{\circ}C}$ exhibited a maximum catalytic activity due to the effects of $WO_3$ modifying and $CeO_2$ doping.

NiSO4 Supported on FeO-promoted ZrO2 Catalyst for Ethylene Dimerization

  • Sohn, Jong-Rack;Kim, Young-Tae;Shin, Dong-Cheol
    • Bulletin of the Korean Chemical Society
    • /
    • 제26권11호
    • /
    • pp.1749-1756
    • /
    • 2005
  • The $NiSO_4$ supported on FeO-promoted $ZrO_2$ catalysts were prepared by the impregnation method. FeOpromoted $ZrO_2$ was prepared by the coprecipitation method using a mixed aqueous solution of zirconium oxychloride and iron nitrate solution followed by adding an aqueous ammonia solution. The addition of nickel sulfate (or FeO) to $ZrO_2$ shifted the phase transition of $ZrO_2$ (from amorphous to tetragonal) to higher temperatures because of the interaction between nickel sulfate (or FeO) and $ZrO_2$. 10-$NiSO_4$/5-FeO-$ZrO_2$ containing 10 wt % $NiSO_4$ and 5 mol % FeO, and calcined at 500 ${^{\circ}C}$ exhibited a maximum catalytic activity for ethylene dimerization. $NiSO_4$/FeO-$ZrO_2$ catalysts was very effective for ethylene dimerization even at room temperature, but FeO-$ZrO_2$ without $NiSO_4$ did not exhibit any catalytic activity at all. The catalytic activities were correlated with the acidity of catalysts measured by the ammonia chemisorption method. The addition of FeO up to 5 mol % enhanced the acidity, surface area, thermal property, and catalytic activities of catalysts gradually, due to the interaction between FeO and $ZrO_2$ and due to consequent formation of Fe-O-Zr bond.