Pitting Corrosion of Inconel Alloy 600 at Elevated Solution Temperatures

  • Park, Jin-Ju;Pyun, Su-Il
    • Journal of the Korean Electrochemical Society
    • /
    • v.6 no.4
    • /
    • pp.271-281
    • /
    • 2003
  • The present article is concerned with pitting corrosion of Inconel alloy 600 at elevated solution temperatures. This article first summarized the previous works on the characteristics and the growth models of oxide film grown on alloy 600 at elevated solution temperatures. Thereafter, this article reviewed previous works on the morphological study on pitting corrosion of alloy 600 as functions of solution temperature and such anion additives as thiosulphate, sulphate, nitrate and bicarbonate ions in terms of pit morphology and its fractal dimension.

The Thermal Stability and Elevated Temperature Mechanical Properties of Spray-Deposited $SiC_P$/Al-11.7Fe-1.3V-1.7Si Composite

  • Hao, L.;He, Y.Q.;Wang, Na;Chen, Z.H.;Chen, Z.G.;Yan, H.G.;Xu, Z.K.
    • Advanced Composite Materials
    • /
    • v.18 no.4
    • /
    • pp.351-364
    • /
    • 2009
  • The thermal stability and elevated temperature mechanical properties of $SiC_P$/Al-11.7Fe-1.3V-1.7Si (Al-11.7Fe-1.3V-1.7Si reinforced with SiC particulates) composites sheets prepared by spray deposition (SD) $\rightarrow$ hot pressing $\rightarrow$ rolling process were investigated. The experimental results showed that the composite possessed high ${\sigma}_b$ (elevated temperature tensile strength), for instance, ${\sigma}_b$ was 315.8 MPa, which was tested at $315^{\circ}C$, meanwhile the figure was 232.6 MPa tested at $400^{\circ}C$, and the elongations were 2.5% and 1.4%, respectively. Furthermore, the composite sheets exhibited excellent thermal stability: the hardness showed no significant decline after annealing at $550^{\circ}C$ for 200 h or at $600^{\circ}C$ for 10 h. The good elevated temperature mechanical properties and excellent thermal stability should mainly be attributed to the formation of spherical ${\alpha}-Al_{12}(Fe,\;V)_3Si$ dispersed phase particulates in the aluminum matrix. Furthermore, the addition of SiC particles into the alloy is another important factor, which the following properties are responsible for. The resultant Si of the reaction between Al matrix and SiC particles diffused into Al matrix can stabilize ${\alpha}-Al_{12}(Fe,\;V)_3Si$ dispersed phase; in addition, the interface (Si layer) improved the wettability of Al/$SiC_P$, hence, elevated the bonding between them. Furthermore, the fine $Al_4C_3$ phase also strengthened the matrix as a dispersion-strengthened phase. Meanwhile, load is transferred from Al matrix to SiC particles, which increased the cooling rate of the melt droplets and improved the solution strengthening and dispersion strengthening.

Study on the optimum hot forming temperature and solution heat treatment temperature for the super duplex stainless steel weld (수퍼 이상 스테인리스강 용접부의 최적 열간 성형온도 및 용체화 열처리 온도에 관한 연구)

  • Ji Chun-Ho;Choi Jun-Tae;Kim Dae-Sun
    • Proceedings of the KWS Conference
    • /
    • 2006.05a
    • /
    • pp.137-139
    • /
    • 2006
  • In order to establish the optimum hot forming temperature and solution heat treatment temperature for 25% chromium super duplex stainless steel weld, a commercial 25%Cr-10%Ni-4%Mo weld metal for super duplex stainless steel(UNS S32750) with different solution heat treatment conditions at $1100^{\circ}C,\;1050^{\circ}C,\;1025^{\circ}C\;and\;1000^{\circ}C$ for 1.5 hours has been investigated by means of optical metallography, and estimated mechanical properties. It is found that exposure to elevated temperatures at $1050^{\circ}C,\;1025^{\circ}C\;and\;1000^{\circ}C$ except $1100^{\circ}C$ brings partial decomposition of ferrite to austenite and sigma phase, which deteriorates their properties and heat treatment at $1100^{\circ}C$ shows acceptable mechanical properties.

  • PDF

Effect of the Heating Temperature on the Alkali-activation Reaction of Calcined Kaolin Powder (열처리 카올린 분말의 알칼리활성화 반응에 미치는 가열온도의 영향)

  • Kim, Sung Gon;Song, Tae Woong
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.6
    • /
    • pp.601-607
    • /
    • 2012
  • The alkali-activation reaction of two types of typical kaolin calcined at various lower temperatures was investigated at room temperature and at elevated temperatures. For the assessment of the reactivity, the temperature increase and the setting time of pastes prepared with calcined kaolin and sodium/potassium hydroxide solution were measured. Unlike raw kaolin, calcined kaolin samples prepared at various temperature showed an alkali-activation reaction according to the different aspects of the changes in the mineral phases. The reactivity with alkaline solutions was exceedingly activated in the samples calcined at $600-650^{\circ}C$, but the reactivity gradually decreased as the temperature increased in a higher temperature range, most likely due to the changes in the crystal structure of the dehydrated kaolin. The activation effect of the calcination treatment was achieved at reaction temperatures that exceeded $60^{\circ}C$ and was enhanced as the temperature increased. The reactivity of the calcined kaolin with an alkaline solution was more enhanced with the solution of a higher concentration and with a solution prepared from sodium hydroxide rather than potassium hydroxide.

Effect of hydrofluoric acid-based etchant at an elevated temperature on the bond strength and surface topography of Y-TZP ceramics

  • Yu, Mi-Kyung;Lim, Myung-Jin;Na, Noo-Ri;Lee, Kwang-Won
    • Restorative Dentistry and Endodontics
    • /
    • v.45 no.1
    • /
    • pp.6.1-6.8
    • /
    • 2020
  • Objectives: This study investigated the effects of a hydrofluoric acid (HA; solution of hydrogen fluoride [HF] in water)-based smart etching (SE) solution at an elevated temperature on yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) ceramics in terms of bond strength and morphological changes. Materials and Methods: Eighty sintered Y-TZP specimens were prepared for shear bond strength (SBS) testing. The bonding surface of the Y-TZP specimens was treated with 37% phosphoric acid etching at 20℃-25℃, 4% HA etching at 20℃-25℃, or HA-based SE at 70℃-80℃. In all groups, zirconia primers were applied to the bonding surface of Y-TZP. For each group, 2 types of resin cement (with or without methacryloyloxydecyl dihydrogen phosphate [MDP]) were used. SBS testing was performed. Topographic changes of the etched Y-TZP surface were analyzed using scanning electron microscopy and atomic force microscopy. The results were analyzed and compared using 2-way analysis of variance. Results: Regardless of the type of resin cement, the highest bond strength was measured in the SE group, with significant differences compared to the other groups (p < 0.05). In all groups, MDP-containing resin cement yielded significantly higher bond strength values than MDP-free resin cement (p < 0.05). It was also shown that the Y-TZP surface was etched by the SE solution, causing a large change in the surface topography. Conclusions: Bond strength significantly improved when a heated HA-based SE solution was applied to the Y-TZP surface, and the etched Y-TZP surface was more irregular and had higher surface roughness.

An Experimental Study on Anisotropic Tensile Properties of AZ31 Mg Alloy (AZ31B 마그네슘 합금의 인장특성 및 이방성의 실험적 연구)

  • Kim, S.H.;Lee, H.W.;Lee, G.A.;Kim, G.T.;Choi, S.W.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2007.10a
    • /
    • pp.254-257
    • /
    • 2007
  • In this paper, anisotropic tensile properties of the AZ31B Mg-alloy sheet are obtained with the tensile test at elevated temperatures. Change of microscopic structures and the hardness is inspected after the solution heat treatment process in order to confirm the micro-structural stability of the used sheet metal. Results obtained from tensile tests show that it is very difficult to apply the conventional modeling scheme with the assumption of strain hardening to the forming analysis of the magnesium alloy sheet which shows the strain-softening behavior at the elevated temperature.

  • PDF

Preliminary Study on the Total Dissolved Organics Measurement and Their Contribution to Conductivities at Elevated Temperature

  • Kim, Kwang-Rag;Kang, Hee-Suk;Park, Seung-Woo;Lee, Sung-Ho;Ahn, Do-Hee;Lee, Han-Soo;Hongsuk Chung;Sung, Ki-Woung
    • Proceedings of the Korean Nuclear Society Conference
    • /
    • 1996.11a
    • /
    • pp.127-132
    • /
    • 1996
  • Total organic carbon (TOC) derived from organics is one of tile possible contamination in the reactor water system and causes of pH change and high conductivity levels. Measurements of total dissolved oxidizable carbon were carried out and its contribution to conductivities at elevated temperature was studied by using tile thermodynamic equilibrium analysis in carbonic acid system. The calculated conductivities were in good agreement with tile levels observed for tile formation of carbonic acid from salicylic acid solution.

  • PDF

Elevared Temperature Mechanical Properties of Mechanically Alloyed Al-4Mg Alloys (기계적합금화로 제조된 Al-4Mg기 합금의 고온 기계적성질)

  • Lee, Yong Gak;Jeon, Chae Hong;Kwun, S.I.;Yeon, Yun Mo
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.11 no.3
    • /
    • pp.168-176
    • /
    • 1998
  • The mechanical properties of mechanically alloyed Al-4wt%Mg alloys dispersed with $MgAl_2O_4$ dispersoilds at room and elevated temperatures were investigated. The powders in steady state during mechanical alloying consisted of Mg-supersatu rated Al solid solution and $Al_4C_3$ which resulted from the reaction of Al with C in process control agent (methanol). The hot-extruded materials consisted of uniformly dispersed fine $MgAl_2O_4$, ${\gamma}-Al_2O_3$, $Al_2O_3$ and matrix with extremly fine substructure. Tensile specimens prepared from the extruded bars were tested at room temperature to $400^{\circ}C$ under different strain rates. The tensile strength of alloys at room temperature ranged from 500 to 594MPa. At elevated temperatures, the tensile strengths and elongations decreased with increasing temperature. Adding 3% $MgAl_2O_4$ to Al-4wt%Mg increased the tensile strength of 50MPa at rowan temperature and 20MPa at $400^{\circ}C$.

  • PDF

Experimental Study About Properties of Limestone-calcined-clay Cement (LC3) Concrete Under High Temperature (석회석 소성 점토 시멘트(LC3) 페이스트의 고온 내화성능에 관한 연구)

  • Wang, Xiao-Yong
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2021.11a
    • /
    • pp.133-134
    • /
    • 2021
  • Limestone-calcined clay-Cement (LC3) concrete provides a solution for sustainability, durability, and profitability of concrete industry. This study shows experimental studies of the macro properties (residual compressive strength), the meso properties (mesoscopic images), and micro properties (thermogravimetric (TG) analysis, X-ray powder diffraction (XRD), FTIR spectra, Raman spectra, Mercury intrusion porosimetry, and SEM) of LC3 paste with various mixtures and at high elevated temperatures (20 ℃, 300 ℃, 550 ℃ and 900 ℃). We find (1) Regarding to macro properties, LC3 cementitious materials are at a disadvantage in compressive strength when the temperature is higher than 300 ℃. (2) Regarding to meso properties, when the temperature reached 550 ℃, all samples generated more meso cracks. (3) Regarding to micro properties, first, as the substitution amount increases, its CH content decreases significantly; second, at 900 ℃, for samples with calcined clay, a large amount of gehlenite crystalline phase was found; third, at elevated temperatures (20 ℃, 300 ℃, 550 ℃ and 900 ℃), there is a linear relationship between the residual compressive strength and the cumulative pore volume; fourth, at 900 ℃, a large amount of dicalcium silicate was generated, and damage cracks were more pronounced. The experimental results of this study are valuable of material design of fire resistance of LC3 concrete.

  • PDF

Effect of Cr Addition on the High Temperature Deformation Behavior of Fe-Al Intermetallics (Fe-Al 금속간 화합물의 고온변형거동에 미치는 Cr 첨가의 효과)

  • Bang W.;Lim H. T.;Ha T. K.;Song J. H.;Chang Y. W.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2001.05a
    • /
    • pp.167-171
    • /
    • 2001
  • High temperature deformation behavior of Fe-28Al-5Cr alloy has been investigated known to show anomalous temperature dependence of yield strength. Specifically, the effect of Cr addition has been examined. A series of tensile and load relaxation tests have been carried out to obtain the flow behavior of Fe-28Al-5Cr alloy at the elevated temperatures. The flow curves have then been analyzed using the inelastic deformation theory recently proposed. Firstly, high temperature flow stress of iron aluminides can be resolved into internal stress and frictional stress. Secondly, the temperature corresponding to peak strength gets higher level at faster strain rate, which presumably due to the increased contribution of internal stress in observed flow stress. And thirdly, the alloying of Cr seems to cause solid-solution strengthening of frictional stress level and the elevation of 2nd order transition temperature. In this analogy, Fe-28Al-5Cr exhibits better strength especially at relatively higher temperature and lower strain rate than Fe-28Al.

  • PDF