Lee, Han Saem;Park, Da So Mi;Hwang, Yuhoon;Ha, Jong Gil;Shin, Hyung Sang
Environmental Engineering Research
/
제25권3호
/
pp.335-344
/
2020
This work describes highly efficient recovery and selective leaching of Zn from electric arc furnace dust (EAFD) with different physicochemical properties, induced by acid leaching at ambient conditions. The chemical compositions, mineralogical phases, and particle sizes of the EAFDs were analyzed and compared. The effects of leaching time, liquid/solid ratio, acid type, and acid concentration on the selective leaching of Zn were also studied. The EAFD with high Fe/Zn ratio (> 1, EAFD3) was richer in ZnFe2O4 and exhibited larger particle size than samples with low Fe/Zn ratio (< 1, EAFD1,2). ANOVA analysis revealed that the Fe/Zn ratios of the EAFDs also have a significant effect on Zn extraction (p < 0.005). Selective leaching of Zn with minimum Fe dissolution was obtained at pH > 4.5, regardless of other parameters or sample properties. The maximum Zn extraction rate obtained by the pH control was over 97% for EAFD1 and EAFD2, 76% for EAFD3, and 80% for EAFD4. The present results confirm that the Fe/Zn ratio can be used to identify EAFDs that permits facile and high-yield Zn recovery, and pH can be used as a process control factor for selective leaching of Zn regardless of any differences in the properties of the EAFD sample.
In general, when scrap is dissolved in an electric arc furnace, the amount of electric furnace steel dust (EAFD) generated is about 1.5% of the scrap charge amount, and the electric furnace steel dust collected by the bag filter is charged into the Rotary Kiln or Rotary Hearth Furnace (RHF), and the zinc component is recovered as crude zinc oxide, at which time a clinker of Fe-Base is generated. In this research, first, for the efficient resource conversion of electric furnace steel dust, a reduction and roasting experiment was conducted and the reaction kinetics was examined. As a result of the experiment, it was observed that the reduction and roasting reaction was actively conducted in the range of 1100~1150℃, and melting occurred in the range of 1250℃. In the past, this clinker was widely used as a roadbed material for road construction and an Fe-Source for cement production, but in recent years, it has been mainly reclaimed due to strengthening environmental standards. However, landfill treatment is by no means a desirable treatment method due to environmental pollution caused by leachate, expensive landfill costs, and waste of Fe resources. Therefore, in order to more actively recycle the Fe component in the clinker, first of all the clinker was pulverized into an optimal particle size, and anthracite and binder (starch) were added to the magnetic material obtained by specific gravity and magnetic separation for briquet. As a experimental results, it was possible to efficiently separate clinker as Fe component and other slag component by specific gravity and magnetic force. As a results of loading and dissolving the manufactured briquet clinker in an electric arc furnace, it was observed that the unit of power and production yield were clearly improved and the carbon addition effect in molten metal was also somewhat.
Essentially, when electrical current flows easily in concrete that has large pores filled with highly connective pore water, this is an indication of a low resistivity concrete. In concrete, the flow of current between anodic and cathodic sites on a steel reinforcing bar surface is regulated by the concrete electrical resistance. Therefore, deterioration of any existing reinforced concrete structure due to corrosion of reinforcement steel bar is governed, to some extent, by resistivity of concrete. Resistivity of concrete can be improved by using SCMs and thus increases the concrete electrical resistance and the ability of concrete to resist chloride ingress and/or oxygen penetration resulting in prolonging the onset of corrosion. After depassivation it may slow down the corrosion rate of the steel bar. This indicates the need for further study of the effect of electric arc furnace dust (EAFD) addition on the concrete resistivity. In this study, concrete specimens rather than mortars were cast with different additions of EAFD to verify the electrochemical results obtained and to try to understand the role of EAFD addition in influencing the corrosion behaviour of reinforcing steel bar embedded in concrete and its relation to the resistivity of concrete. The results of these investigations indicated that the corrosion resistance of steel bars embedded in concrete containing EAFD was improved, which may link to the high resistivity found in EAFD-concrete. In this paper, potential measurements, corrosion rates, gravimetric corrosion weight results and resistivity measurements will be presented and their relationships will also be discussed in details.
Electric arc furnace dust (EAFD) is a solid waste generated by the steel-scrap recycling process. It mainly consists of zinc oxides (ZnO), alumina ($Al_2O_3$), iron oxides ($Fe_2O_3$), and silica ($SiO_2$). Here we report the preparation and characterization of blue ceramic pigments using EAFD powder as a starting material. $(Zn(EAFD),Co)Al_2O_4$ blue ceramic pigment was prepared by the solid-state reaction method. The color characteristics of the pigment obtained were compared with those of pure $CoAl_2O_4$. The new pigment was characterized using XRD, CIE-$L^*a^*b^*$ color-measurements, SEM, and EDX. The XRD analysis revealed that the $(Zn(EAFD),Co)Al_2O_4$ pigment was composed of mainly the spinel phase of $(Zn,Co)Al_2O_4$. The $Zn(EAFD)_{0.25}Co_{0.75}Al_2O_4$ pigments showed a vivid blue color with a $b^*$ value of -28.64 and a good glaze stability with a transparent glaze.
제강분진(Electric Arc Furnace Dusts)은 유해폐기물로 지정되어있는 유해한 환경오염물질이다. 이 분진은 철강산업의 부산물로써 철, 아연, 니켈, 구리 등 많은 유가금속을 포함하고 있어 적절한 처리를 거치면 폐기물이 아닌 자원으로 재활용이 가능하다. 본 연구에서는 국내 전기로에서 발생하는 제강분진을 대상으로 가장 높은 함유량을 가진 아연의 회수를 위한 최적조건을 도출하기 위해 습식침출법을 적용하였다. 분진과 황산의 고액비, 침출시간, $MnO_2$ 투입량 등의 조건을 종합하여 실험을 진행하여 최적 아연회수조건을 도출하였다. 황산농도 3 M, 고액비 1:2, 철 제거를 위한 폭기 1.8 L/min 강도로 2시간에서 95%의 아연 회수율이 관찰되었다. 그러나, 현장 적용의 현실성을 고려한 다른 최적의 조건은 저농도 황산과 $MnO_2$ 3.5 g을 투입했을 경우 약 80 %의 아연 회수율을 나타내었다.
제강분진(Electric arc furnace dust)은 제강공정에서 발생하는 분진폐기물로서 중금속을 다량 포함하고 있어 관리가 매우 중요하다. 제강분진은 아연, 철 등의 유가금속을 다량 함유하고 있기 때문에 최근 이를 재활용하는 연구가 활발하게 진행 중이며, 본 연구에서는 전처리 과정 없이 제강분진을 청색 계열의 세라믹 안료의 코발트를 대체할 수 있는 원료로 사용하였다. 또한 합성된 청색 세라믹 안료를 잉크젯 프린팅용 세라믹 잉크로 개발하기 위해 미립화 과정에서의 입도 분포, 결정 구조 및 발색 특성 변화에 대해 고찰하였다. 제강분진이 첨가된 $Co_{0.75}Zn(EAFD)_{0.25}Al_2O_4$ 세라믹 안료는 우수한 청색 발색 특성을 보이며, 어트리션 밀링(Attrition Milling)을 이용한 미립화 공정을 통하여 단정(monomodal) 분포의 입도를 확보할 수 있었다. 3시간 밀링 후 $Co_{0.75}Zn(EAFD)_{0.25}Al_2O_4$ 세라믹 안료의 평균 입도는 $0.271{\mu}m$로 제강분진이 첨가되지 않은 $CoAl_2O_4$ 세라믹 안료의 5시간 밀링 후의 평균 입도인 $0.303{\mu}m$보다 더욱 작은 것을 확인하였다. 특히, $Co_{0.75}Zn(EAFD)_{0.25}Al_2O_4$ 세라믹 안료는 미립화 공정 중 발색 변화(${\Delta}E{^*}_{ab}$) 값이 5.67로 $CoAl_2O_4$ 보다 작아서 더 우수한 발색 특성을 보이는 것으로 확인되었다. 이러한 결과는 분진폐기물인 제강분진을 어떠한 전처리 과정 없이 고가의 코발트를 대체하여 청색 계열의 세라믹 안료의 원료로 사용할 수 있다는 것을 보여주고 있다.
Cement acts as the most important component of concrete as it binds and holds the concrete together. But it is one of the major $CO_2$ emitters all over the world, during manufacturing (900 kg of $CO_2$ per 1000 kg). Some of the modern construction methods aim at reducing the amount of usage of cement and came out with numerous solutions for replacement of the same. One such supplement in current trend is the Steel dust or the Electric Arc Furnace Dust (EAFD), which is a waste product from the electric arc furnace when the scrap metal is melted. When the concrete containing steel dust is exposed to atmosphere, the environmental oxygen and moisture play role to form rust and ultimately the member becomes harder. As Cement is the binder of conventional concrete, only certain percentage of the same could be replaced by the new material, steel dust. Tests were conducted for the 28 days cube strength of M45 grade (suitable for prestressing) concrete which has 0%, 10%, 20%, 30%, 40% and 50% steel dust instead cement. From the test, the optimum percentage replacement of steel dust was obtained, for which the beams and overhead poles were cast, prestressed and tested for the failure load and deflections. A conventional concrete beam and overhead pole were also cast, prestressed and tested to compare the results with those of the beam and pole that contained steel dust. The load vs. deflection plot and other results from the test is also discussed.
본 연구에서는 전기 제강로 분진(EAFD)으로부터 고 순도의 아연회수를 위한 산 습식법 중 알칼리 금속 및 염화물(Na, K, Cl) 제거를 위한 적정 수 세척공정의 운영조건에 대해 조사하였다. 서로 다른 성상을 가지는 두 종류의 EAFD 시료를 대상으로 원소분석, XRD, 입도 분석 등의 물리화학적 특성을 분석하였고, 세척액의 pH, 세척시간, 고액비(mL/g) 및 세척반복횟수 등에 따른 알칼리 금속 및 염화물의 세척효율(%)을 비교하였다. 연구 결과, EAFD 내 알칼리 금속과 염화물은 고액비 3, 세척시간>30, pH 10~11의 조건에서 아연과 철의 손실을 최소화하면서(<~0.1%) 효과적으로 제거할 수 있었으며, 1회 세척시 Na-78%, K-76%, Cl >99%의 세척효율을 보였다. Na와 K는 3회 반복 세척 시 각각 97%, 89%까지 제거 가능하였다. 두 종류의 EAFD 혼합(1:1)시료를 대상으로 시료 용량을 늘려(10배) 수행한 실험 결과에서도 세척액의 최종 pH 10~11에서 Zn의 손실 없이 Na, K, Cl 등을 효과적으로 제거 가능함을 확인하였다.
전기로 제강분진(EAFD : Electric Arc Furnace Dust) 중에 다량 함유되어있는 아연을 회수하기 위한 재활용 기술로서, 현재 세계적으로 가장 많이 상용화된 기술은 Wealz Kiln Process이다. Wealz Kiln Process에서는, 제강분진 중의 Zn, Pb 등과 같은 성분들을 고온의 Kiln에서 환원/휘발(흡열반응)시킨 후에 다시 기체상에서 재산화(발열반응)시켜 후단에 설치된 Bag Filter에서 조산화아연(60wt%Zn)의 형태로 회수하는 프로세스이다. 본 연구에서는, 상업용 규모의 대형 kiln의 재활용 공정에 실제로 적용하기 위한 최적의 공정변수 값을 조사하기 위해서, 실험용 Wealz kiln을 제작하였다. 그리고, 전기로 제강분진과 환원제, 석회석을 혼합한 Pellet을 연속적으로 Kiln에 장입하면서, 조산화아연 회수율을 얻기 위한 최적의 장입량과 가열온도, 체류시간 등을 조사하였다. 또한 Pellet의 최적의 제조조건( Drum 경사각, 수분의 첨가량, 혼합시간 등)도 조사하였다. 또한, SiO2-CaO-FeO 3성분계 상태도를 참고하여, Pellet의 염기도(basicity)의 변화에 따른 Kiln 내부에서의 저융점 화합물의 생성거동과 Kiln내벽에 시공된 Castable과의 반응성(부착성)을 평가하여 보았다. 그리고, 환원제인 Coke의 대체제로서 무연탄의 사용 가능성을 실질적으로 평가하기 위하여, 무연탄의 첨가량 증가에 따라서 산화/환원반응이 일어나는 Kiln 내부의 온도분포변화, 조산화아연의 품위, 무연탄 중의 타르(Tar)의 거동에 대해서도 조사하였다.
전기로 제강분진 중에는 아연(Zn), 납(Pb)등과 같은 유가금속들이, 다양한 화합물(산화물 또는 염화물 등)의 형태로 다량 함유되어 있다. 전기로 제강분진 내에 함유되어 있는 이들 유용금속원소들을, 가장 효율적이며 안정적으로 회수할 수 있는 대표적인 방법으로서는 Rotary Kiln Process가 있다. Rotary Kiln Process는 전기로 제강분진에 환원제(Coke, 무연탄)와 석회석(염기도 제어용)을 첨가하여 성형한 후에 가열함으로서, 아연성분을 조산화아연(Crude Zinc Oxide : 60% Zn)의 형태로 회수하는 방법으로 오래전에 이미 상용화되었으며, 지금도 공정 및 설비의 단점을 개선하기 위한 연구개발을 지속적으로 수행하고 있다. 현재 국내에서도 전기로 제강분진을 재활용하여 조산화아연을 생산하는 다수의 상용화공장들이 가동되고 있다. 조산화아연 중에는, 아연성분 외에도 다양한 기타의 성분원소들(Pb, Cd, Sn, In, Fe, Cl, F 등)이 산화물, 염화물, 알칼리 화합물 등의 형태로 함께 혼재되어 있다. 그러므로 조산화아연을 건식 또는 습식아연제련용 원료로서 그대로 사용하게 되면 조산화아연에 함유된 이들 불순물 성분들이 미치는 악영향으로 인하여, 아연제련과정에서 많은 문제점들이 발생하므로. 따라서 이들 불순물 성분원소들을 가능하면 모두 제거하기 위한 건식 또는 습식정제공정이 추가로 필요하다. 따라서 본 연구에서는 조산화아연의 건식휘발 정제공정에서 발생되어 백필터에 포집된 아연(Zn) 및 납(Pb)을 함유한 2차분진(2nd Dust)으로부터 아연(Zn)과 납(Pb)을 효율적으로 분리하고, 더욱 부가가치를 높이기 위하여 Zn-cementation법으로 이들 성분원소들을 금속탄산염의 형태로 분리회수할 수 있는 공정기술에 대하여 기초적인 연구를 수행하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.