The Dyeing Properties and Antibacterial Function of Perilla frutescens var. acuta Extract on Cotton (차조기 추출물의 면직물에 대한 염색성과 항균기능성 평가)

  • Kim, Seongsuk;Park, Youngmi
    • Textile Coloration and Finishing
    • /
    • v.33 no.3
    • /
    • pp.105-112
    • /
    • 2021
  • This study investigated the proper dyeing conditions, fastness and functionality of cotton fabrics dyed with Perilla frutescens var. acuta extract. Repeat dyeing, combination dyeing of persimmon juice and fermentation dyeing were conducted as dyeing conditions. It was confirmed that the ΔE and the K/S value of cotton fabrics dyed with Perilla frutescens var. acuta extracts depending on repeat dyeing and combination dyeing slightly increased. Furthermore, the fastness to washing of persimmon combination dyeing and fermentation dyeing was very good. The fastness to rubbing was shown to be above grade 4 in all methods, and the fastness to light was not as good as grade 3 or lower. The persimmon juice dyeing, Perilla frutescens var. acuta extract repeat dyeing 4 times and combination fermentation dyeing showed very good antimicrobial abilities. Thereafter, additional studies are needed to improve the fastness to light and alternatives to further improve the dyeing properties.

Reduction Cleaning and Thermomigration Effects on Micro Polyester SUEDE (극세 폴리에스테르 스웨드의 환원세정과 열이행의 영향)

  • Choi, Kyung-Yeon;Han, Sam-Sook;Lee, Mun-Cheul
    • Textile Coloration and Finishing
    • /
    • v.21 no.6
    • /
    • pp.12-21
    • /
    • 2009
  • The dyeing property of direct-spinning type and seaisland type 0.2D micro polyester nonwoven fabrics was characterized by three disperse dyes (Dorosperse Red KFFB, Blue KGBR, Yellow KRL) at $120^{\circ}C$ and $130^{\circ}C$. Before and after reduction cleaning, dyeing fastness was evaluated and the thermomigaration after heat setting at $180^{\circ}C$ for 60 min were also evaluated. Direct-spinning type fabric showed better dyeing property, wash fastness, and light fastness, but worse rub fastness than seaisland type fabric. The dyeing property and fastness of direct-spinning type fabric increased at higher dyeing temperature, whereas seaisland type fabric exhibited lower dyeing fastness and the increase of thermomigration at higher dyeing temperature. Non-fixed dye in fiber surface was removed by reduction cleaning process, then dyeing fastness was improved and thermomigration decreased. The higher dye uptake of direct-spinning type non-woven fabric caused the increase of dye molecule migration from fiber internal to fiber surface, so this fabric showed larger thermomigration than seaisland type non-woven fabric.

Combination Dyeing of Juniperus Chinensis Heartwood and Alnus Japonica Heartwood Extracts

  • Sa, A-Na;Lee, Jung Soon
    • Fashion & Textile Research Journal
    • /
    • v.17 no.1
    • /
    • pp.127-136
    • /
    • 2015
  • The purpose of this study was to examine improvements in dye uptake, expression of various colors, and color fastness when washed or exposed to light. We examined these improvements by doing the combination dyeing of Juniperus chinensis heartwood and Alnus japonica heartwood extracts. In this study, two combination dyeing methods were used. One-bath dyeing involves combining Juniperus chinensis heartwood extract and Alnus japonica heartwood extract. Two-bath dyeing involves dyeing by sequence, which means that we dyed the Juniperus chinensis heartwood extract first and then dyed Alnus japonica heartwood extract sequentially (or in the opposite order). In terms of improving dye uptake, two-bath dyeing was more effective than one-bath dyeing. For cotton, dyeing Juniperus chinensis heartwood extract first and then dyeing Alnus japonica heartwood extract sequentially showed higher dye uptake in the two-bath method, while for silk, there wasn't much difference in the dyeing order. Through combination dyeing, red-violet color from Juniperus chinensis heartwood and brown color from Alnus japonica heartwood made various Y, YR, R series of color as a result. Moreover, combination dyeing improved fabric's fastness when washed or exposed to light. In the case of cotton, fabric dyed using two-bath dyeing, with Juniperus chinensis heartwood extract being the first dye, showed improvement in fastness to washing and light. And in the case of silk, fastness to washing and light improved regardless of dyeing order in two-bath dyeing.

Combination Dyeing of Silk Fabrics with Dansam and Sappan Wood (단삼과 소목을 이용한 견직물의 복합염색)

  • Nam, Jeongran;Lee, Jeongsook
    • Textile Coloration and Finishing
    • /
    • v.25 no.4
    • /
    • pp.314-326
    • /
    • 2013
  • The purpose of this research is to analyze the effects of Dansam and Sappan wood extract to perform combination dyeing on silk fabrics, with respect to color changes, fastness (washing, dry cleaning, perspiration, rubbing and light fastness), and functionality (antibacterial activity and deodorization). Combination dyeing was performed by first combining Dansam with Sappan wood, then Sappan wood with Dansam, in these orders. Given the changes in the combination ratio, pre-mordant treatment was performed. Looking at the surface colors of each dye, Dansam generally produces YR color series, while Sappan wood produces YR, R, and RP color series. The effects of changing the order in which combination dying was performed on the surface colors were as follows. First, combination dyeing (A) was performed by using Dansam before Sappan wood, to produce YR and R color series. Then combination dyeing (B) was performed by using Sappan wood before Dansam, to produce YR, R, and RP color series. By visual inspections, more similar color changes of the combination dyeing were noticed with the post-dyeing material rather than the pre-dyeing material. Therefore, it was presumably confirmed that surface color changes of combination dyeing were greatly influenced by the post-dyeing color. Individual dyeing tests for fastness showed that Dansam was comparatively superior to Sappan wood, which demonstrated lower fastness to washing, dry cleaning, perspiration, and light, relatively. The fastness of combination dyed samples was shown middle, but similar fastness to the post-dye material, The fastness of (B) method was higher than (A) method in the washing and light fastness. This confirms that color fastness from combination dyeing was considerably influenced by the post-dye material. It was found that all dyed samples had a very high bacterial reduction rate of 99.9% and high deodorization rate of 95%.

Dyeing Properties of Silk Fabric with Alnus Firma Extracts (오리나무 열매 추출물에 의한 견직물의 염색성 연구)

  • 손보현;장지혜
    • Journal of the Korean Home Economics Association
    • /
    • v.40 no.12
    • /
    • pp.109-118
    • /
    • 2002
  • The Purpose of this study was to investigate dyeing properties and color fastness of Ainus firma sieb. et Zucc. Fruit, according to dyeing temperature, dyeing time, dyeing concentrations and various mordants. The results were as follows ; 1. The dyeabilities of the natural colorants extracted from Alnus firma fruit were investigated under various dyeing temperature, dyeing time and dyeing concentration. As a result, the optimum dyeing temperature, time and concentration of silk fabric with Alnus firma fruit were $60^{\circ}C$, 60min and 100%(o.w.f.) respectively. 2. Alnus firma fruit extract dyed reddish purple (RP hue) on the Fe-mordanted silk fabric. In the case of other mordants, silk fabrics dyed yellow (Y hue). 3. Generally, the light color fastness was relatively fair in the silk fabric dyed with the Alnus firma fruit and Fe mordant. The washing color fastness of color change of silk dyeings mordanted with Al, Sn showed 4 grade. However, the dry cleaning color fastness of the silk fabric was fastness was excellent. The rubbing color fastness showed 4 grade at the most of mordants except Cu.

The Dyeing Properties of Silk Fabrics of Glycyrrhizae Radix Extract (감초 추출물에 의한 견직물의 염색성)

  • 이영숙;장정대
    • Textile Coloration and Finishing
    • /
    • v.16 no.1
    • /
    • pp.34-39
    • /
    • 2004
  • Dyeing properties of Glycyrrhizae Radix was investigated with silk fabrics. Dyeing water is a type of chalcone, it showed yellow in IR spectrum. K/S value showed high in following conditions; Glycyrrhizae Radix $200g/1\ell4 water, $80^{\circ}$ of dyeing temperature, 90 minute of dyeing time. Glycyrrhizae Radix dyeing water has higher K/S value in alkalinity(pH9) than in neutrality(pH7) or acidity(pH3) conditions. K/S value showed highest in pH5 premordant method of alkalinity dyeing water condition. The color of silk fabric dyed with Glycyrrhizae Radix is yellow. The change of color did not show by mordant treatment. K/S value showed higher in mordant treatment than nonmordant. Light fastness showed over 3 degree in nonmordant, premordant, simmordant(Al,Cu,Fe) and postmordant(Cu). Water fastness showed over 3 degree in dyeing water(pH3, pH5, pH7). Dry cleaning fastness showed over 3 degree in all dyeing methods. Washing fastness is showed in 2-3 degree; Al in nonmordant, premordant, simmordant and Cu in simmordant are 2-3 degree. Perspiration fastness is nearly 3-4 degree in premordant and simmordant. Perspiration fastness shows high in premordant, simmordant than postmordant. The fastness of light, water, dry cleaning, washing, perspiration shows better nonmordant, premordant, simmordant than postmordant method.

A Study on the Dyeing according to Kinds of Loess (황토 종류에 따른 염색성 연구)

  • 강영의;박순옥
    • Textile Coloration and Finishing
    • /
    • v.15 no.6
    • /
    • pp.39-46
    • /
    • 2003
  • The experiments about dyeing concentration, temperature and time were done using yellow, red and purple loess as natural inorganic dyes in order to verify a degree of dyeing, characteristics of color and fastness. The results were as following; 1. As a result of analyzing components of loess, purple loess was much than other loess in quartz component and coarse particles contained. This affected to the degree of dyeing. 2. The stronger dyeing concentration was, the more the degree of dyeing was improved, and yellow loess containing fine particles was the best in the degree of dyeing. 3. When it was dyed with raising up to $100^\circ{C}$ for 10 minutes after stirring for 20 minutes at $60^\circ{C}$, was better than on starting at $40^\circ{C}$ or $80^\circ{C}$ in the degree of dyeing. Also yellow loess was the best in these experiments. 4. Washing fastness of loess was low such as other natural dyes, but dyeing wasn't transferred to other textiles. On the other hand, light fastness of it was very excellent and rubbing fastness was relatively good as 3~3.5.

A Study on the Dyeing Properties of Silk and Cotton Fabrics with Chestnut Bur Extract(2) (밤송이 추출액을 이용한 견과 면직물 염색 (2))

  • Kim, Ae Sun;Jang, Jae Cheol
    • Textile Coloration and Finishing
    • /
    • v.13 no.2
    • /
    • pp.7-7
    • /
    • 2001
  • This paper investigated the dyeability and surface color of silk and cotton fabrics dyed with chustnut bur extract. Some experiments were performed under the various dyeing conditions such as dyeing temperature, dyeing time, repetition of dyeing, dyeing pH, mordanting condition, washing fastness and light fastness with silk and cotton fabrics. The results obtained were as follows 1. △E value was increased when dyeing temperature and time was higher, value of munsell was shifted from Yellow to Yellow-Red at hither dyeing temperature and time in silk and cotton fabrics. 2. Optimal dyeing pH was increased with acidity of dyeing solution in silk and cotton fabrics, and repetition of dyeing did not change the dye-uptake. 3. When mordanting time and temperature was higher, △E value was larger in silk and cotton fabrics. Silk and cotton fabrics with Fe-premordanting treatment had best dyeability, but treatment with Sn-mordanting was worst. 4. Washing fastness and light fastness was excellent in various dyeing condition at silk fabric but cotton was without practical use.

A Study on the Dyeing Properties of Silk and Cotton Fabrics with Chestnut Bur Extract(2) (밤송이 추출액을 이용한 견과 면직물 염색 (2))

  • 김애순;장재철
    • Textile Coloration and Finishing
    • /
    • v.13 no.2
    • /
    • pp.93-103
    • /
    • 2001
  • This paper investigated the dyeability and surface color of silk and cotton fabrics deed with chustnut bur extract. Some experiments were performed under the various dyeing conditions such as dyeing temperature, dyeing time, repetition of dyeing, dyeing pH, mordanting condition, washing fastness and light fastness with silk and cotton fabrics. The results obtained were as follows 1. $\Delta{E}$ value was increased when dyeing temperature and time was higher, value of munsell was shifted from Yellow to Yellow-Red at hither dyeing temperature and time In silk and cotton fabrics. 2. Optimal dyeing pH was increased with acidity of dyeing solution in silk and cotton fabrics, and repetition of dyeing did not change the dye-uptake. 3. When mordanting time and temperature was higher, $\Delta{E}$ value was larger in silk and cotton fabrics. Silk and cotton fabrics with Fe-premordanting treatment had best dyeability, but treatment with Sn-mordanting was worst. 4. Washing fastness and light fastness was excellent in various dyeing condition at silk fabric but cotton was without practical use.

  • PDF

Washing Fastness of PET Fibers according to Supercritical CO2 and Aqueous Dyeing Methods (초임계 CO2 및 수계 염색방법이 적용된 PET 섬유의 세탁견뢰도)

  • Oh, Jiyeon;Park, Changpyo;Kim, Sam Soo;Lee, Jaewoong
    • Textile Coloration and Finishing
    • /
    • v.32 no.4
    • /
    • pp.208-216
    • /
    • 2020
  • In this study, C.I. Disperse Red 60 (DR60), C.I. Disperse Yellow 54 (DY54) dyes were used to investigate the washing fastness characteristics of PET fibers according to supercritical CO2 and aqueous dyeing process. The changes in K/S values and L⁎ values before and after washing of dyed PET fibers were observed according to the KS K ISO 105 washing fastness measurement method. In addition, it was confirmed by changing the ΔE⁎ and ΔL⁎ values of control PET fibers. Overall, it was confirmed that both the supercritical CO2 and aqueous dyeing process had excellent washing fastness ratings of 4-5 for DR60 and DY54 dyes. Comparatively, the K/S and L⁎ values for before and after washing of PET fibers with supercritical CO2 dyeing process was higher than that of the aqueous dyeing process and the ΔE⁎ and ΔL⁎ values of the control PET fibers were low. From the results, we observed that the supercritical CO2 dyeing process of PET fibers has better washing fastness characteristics than the aqueous dyeing process.