• 제목/요약/키워드: Drawbead friction test

검색결과 9건 처리시간 0.025초

드로우비드 성형시 박판재 마찰계수 영향인자 해석 (Analysis on Parameters Affecting the Friction Coefficient in Drawbead Forming of Sheet Metal)

  • 김원태;이동활;서만석;문영훈
    • 소성∙가공
    • /
    • 제14권8호통권80호
    • /
    • pp.668-674
    • /
    • 2005
  • In sheet metal forming, drawbeads are often used to control uneven material flow which may cause deffets such as wrinkles, fractures, surface distortion and springback. Appropriate setting and adjusting of the drawbead force is one of the most important parameters in sheet forming process control. Therefore in this study, drawbead friction test with circular shape bead was performed at various sheets, lubricants(dry, three kinds of lubricants having different viscosities), bead materials and surface treatments of bead surface. The results obtained by drawbead friction test show that the friction and drawing characteristics of deforming panels were mainly influenced by strength of sheet, viscosity of lubricant and hardness of bead surface.

자동차용 냉간압연재의 드로우비드 성형시 비드 재질별 마찰특성에 관한 연구 (Study on the Friction Characteristics of Various Bead Materials in Drawbead Forming of Cold Rolled Steels for Automotive Parts)

  • 이동활;김원태;문영훈
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 제5회 압연심포지엄 신 시장 개척을 위한 압연기술
    • /
    • pp.91-97
    • /
    • 2004
  • The drawbead is one of the most important factors in sheet metal forming for automotive parts. So clarifying the friction characteristics between sheets and drawbead is essential to improve the formability of sheet metal. Therefore in this study, drawbead friction test was performed at various bead materials(FC300, HC891, FCD550, HD700, HK600, HK700, SKD11) and surface treatment of beads(Base, induction hardening, Cr plating, ion nitriding, Toyoda diffusion process, TiCN, TiN, CrN). Circular shape bead has been used for the test. The results show that friction and drawing characteristics were mainly influenced by surface treatment.

  • PDF

자동차용 냉간압연재의 드로우비드 성형시 비드 형상별 마찰특성에 관한 연구 (Study on the Friction Characteristics of Circular bead and rectangular bead in Drawbead Forming of Cold Rolled Steels for Automotive Parts)

  • 김동우;김원태;이동활;문영훈
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 제5회 압연심포지엄 신 시장 개척을 위한 압연기술
    • /
    • pp.137-144
    • /
    • 2004
  • The drawbead is one of the most important factors in sheet metal forming for automotive parts. So clarifying the friction characteristics between sheets and drawbead is essential to improve the formability of sheet metal. Therefore in this study, drawbead friction test was performed at circular shape bead and rectangular shape bead. The results show that the tendency of drawing force for rectangular bead is nearly similar with circular bead and the drawing force is nearly proportional to friction coefficient.

  • PDF

박판성형공정의 유한요소해석을 위한 드로우비드 전문모델 개발(1부: 실험) (Development of Drawbead Expert Models for Finite Element Analysis of Sheet Metal Forming Processes (Part1:Experiment))

  • 이재우;금영탁
    • 소성∙가공
    • /
    • 제7권1호
    • /
    • pp.3-11
    • /
    • 1998
  • During the forming process of sheet metals, the drawbead in the die face controls a restraining force so that the sheet flows into the die cavity with tension. In order to investigate a drawgbead restraining force and a pre-strain just after drawbeads which are essential in the finite element analysis of form-ing processes, the friction test and drawing test are employed. The experiments performed with a cir-cular bead stepped bead double circular bead and circular-and-stepped bead in the various forming conditions and bead sizes show that the restraining force varies linearly with the blank holding force. bead radius blank thickness and friction but the pre-strain nonlinearly does with them.

  • PDF

자동차용 냉간압연재의 원형 드로우비드 성형시 강판 재질별 마찰특성에 관한 연구 (Study on the Friction Characteristics of Various Panels in Circular Drawbead Forming of Cold Rolled Steels for Automotive Parts)

  • 김대현;이동활;김원태;문영훈
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 제5회 압연심포지엄 신 시장 개척을 위한 압연기술
    • /
    • pp.83-90
    • /
    • 2004
  • The drawbead is one of the most important factors in sheet metal forming for automotive parts. So clarifying the friction characteristics between sheets and drawbead is essential to improve the formability of sheet metal. Therefore in this study, drawbead friction test was performed at various panels(cold rolled steel sheets, galvanized steel sheets, electrogalvanized coating steel sheets, electrogalvanized Zn-Fe alloy steel sheets and aluminum alloy steel sheets). Circular shape bead has been used for the test. The results show that friction and drawing characteristics were mainly influenced by the nature of zinc coating.

  • PDF

3차원 박판형성 공정 유한요소해석용 드로우비드 모델 (Drawbead Model for 3-Dimensional Finite Element Analysis of Sheet Metal Forming Processess)

  • 금영탁;김준환;차지혜
    • 소성∙가공
    • /
    • 제11권5호
    • /
    • pp.394-404
    • /
    • 2002
  • The drawbead model for a three-dimensional a finite element analysis of sheet metal forming processes is developed. The mathematical models of the basic drawbeads like circular drawbead, stepped drawbead, and squared drawbaed are first derived using the bending theory, belt-pulley equation, and Coulomb friction law. Next, the experiments for finding the drawing characteristics of the drawbead are performed. Based on mathematical models and drawing test results, expert models of basic drawbeads are then developed employing a linear multiple regression method. For the expert models of combined drawbeads such as the double circular drawbead, double stepped drawbead, circular-and-stepped drawbead, etc., those of the basic drawbeads are summed. Finally, in order to verify the expert models developed, the drawing characteristics calculated by the expert models of the double circular drawbead and circular-and-stepped drawbead are compared with those obtained from the experiments. The predictions by expert models agree well with the measurements by experiments.

자동차용 판재 성형시 드로우비드 공정인자별 인출특성에 대한 연구 (Effect of drawbead process parameters on the drawing characteristics of sheet metals for automotive parts)

  • 김원태;이동활;강우순;서만석;문영훈
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 추계학술대회논문집
    • /
    • pp.140-143
    • /
    • 2003
  • The drawbead is an important part in sheet metal forming for automotive part and its effect is affected by various process parameters. Therefore in this study, drawbead friction test was performed at various process parameters - panels (cold rolled and galvanized sheet steel), lubricants (having three different viscosities), bead materials(steel, iron) and surface treatment of bead (Cr plating). Circular shape bead has been used for the test. The results show that friction and drawing characteristics were mainly influenced by the nature of zinc coating, viscosity of lubricants, surface treatment of a bead and hardness of coated layer.

  • PDF

자동차용 합금화 용융아연도금강판의 도금층 미소물성 및 파괴 거동 (Microproperties and Fracture Behavior of Galvannealed Coating Layer of Automobiles)

  • 박춘달;고대철;김병민
    • 한국정밀공학회지
    • /
    • 제24권3호
    • /
    • pp.91-99
    • /
    • 2007
  • Fractures of galvannealed coating layer during actual press forming in automotive applications were observed by scanning electron microscopy in order to understand fracture mechanism. Fracture behaviors of galvannealed coating layer in extra deep drawing quality steels and high strength steels have been studied by performing the tests describing the representative plastic deformation in sheet metal forming such as uni-axial tensile test, compression test, bi-axial test and plane strain test. Growth and direction of cracks were deeply related to the plastic deformation modes and history. The material properties of galvannealed coating layer were investigated by nano-indentation test equipped with Berkovich diamond indentor for the specimens. Hardness and elastic modulus of the coating layer were higher than bared steels and that was the reason for crack of coating layer. Flat friction test and drawbead friction test were performed to observe the effect of the surface morphology on the frictional characteristics. The micro-plasto hydrodynamic lubrication were appeared and played an important role in reducing the coefficient of friction.

판재의 드로우비드 성형시 비드표면처리와 비드형상이 인출 및 마찰특성에 미치는 효과 (Effect of Bead Surface Treatments and Bead Shapes on the Drawing and Friction Characteristics in Drawbead Forming of Sheet Metal)

  • 이동활;류종수;정우창;문영훈
    • 열처리공학회지
    • /
    • 제18권2호
    • /
    • pp.105-111
    • /
    • 2005
  • In sheet metal forming, drawbeads are often used to control uneven material flow, which may cause defects such as wrinkles, fractures, surface distortion and springback. Appropriate setting and adjusting of the drawbead force is one of the most important parameters in sheet forming process control. Therefore in this study, drawbead test was performed at various bead surface treatment conditions to clarify the frictional characteristics between sheet and drawbead. Furthermore, the differences in drawing force between circular and rectangular shape beads have also been measured to estimate the effectiveness of bead shape on the material flow control. The results show that drawing and friction characteristic were strongly influenced by surface treatments of bead and bead shapes.