• Title/Summary/Keyword: Double L-shape

Search Result 33, Processing Time 0.018 seconds

Observation of Dynamic Movement of Probing Pin on PCB Pad Using Electrical Reliability Test (인쇄회로 기판의 전기검사에서의 미세 탐침과 패드의 동적 거동 현상 관측)

  • Song, Seongmin;Cha, Gangil;Kim, Myungkyu;Jeon, Seungho;Yu, SangSeok
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.39 no.3
    • /
    • pp.245-251
    • /
    • 2015
  • In an electrical reliability test of a printed circuit board (PCB), the impact of the micro probing pins on the PCB needs to be checked to ascertain the quality of the circuit. In this study, the impact of the dynamic movement of the probing pin on the pad was observed. As a misaligned pin can exert horizontal force on the pad of the PCB, this study focused on the behavior of a misaligned probing pin. The parameters of observation were the circular and flat edges of the probing pin. The effects of the speed of movement, diameter, and the length of projection of the probing pin were also investigated. The results demonstrated that slippage angle is strongly affected by the shape of the edge of the probing pin, and that projection length is an important factor affecting pin slippage. In contrast, the speed of movement of the probing pin was able to double the slippage angle.

Effect of F$e_2$P Addition on Microstructures of Sintered 4600 Steel (4600계 소결강의 조직에 미치는 F$e_2$P첨가의 영향)

  • Kim, Dong-Uk;Lee, Wan-Jae
    • Korean Journal of Materials Research
    • /
    • v.2 no.6
    • /
    • pp.428-435
    • /
    • 1992
  • AISI 4600 Iron powder was mixed with 0~1.0% phosphor as F$e_2$P powder and/or 0~0.8% carbon as graphite powder in rotating mixer. Mixed powder was pressed 800MPa in double-punch mould. Compacts were sintered at 115$0^{\circ}C$for 30 min. in vacuum or mixed hydrogen and nitrogen gas. Sintered compacts were ground and polished, and etched by 2% nital etchant. The microstructure was observed by image analyzer and optical microscope. Density and microhardness were tested by ASTM B3l2 and Microvickers hardness tester. The results obtained were as follows : (1) As the amount of F$e_2$P powder increased, sintered microstructure showed more densified effect and the grain size was larger. (2) The shape of pore was rounded and the number of pore was decreased by F$e_2$P addition. But mean pore size was larger with F$e_2$P content. (3) Simultaneous alloying addition of F$e_2$P and graphite brought about larger grain growth than respective addition. (4) Sintering atmosphere did not affect the microstructure. (5) Hardness of sintered compact increased with phosphrous and carbon content.

  • PDF

Characteristics of New Microsporidia S80 Isolated from Silkworm, Bombyx mori L. in Korea (가잠(家蠶)으로부터 분리(分離)된 새로운 Microsporidia S80의 특성(特性))

  • Lim, Jong Sung;Cho, Sae Yun
    • Current Research on Agriculture and Life Sciences
    • /
    • v.1
    • /
    • pp.67-83
    • /
    • 1983
  • The new microsporidia S80 isolated from, Bombyx mori L. in Korea showed ovoid in the morphology of the spores and the size were measured $2.9{\pm}0.28{\mu}$ in length and $1.7{\pm}0.29{\mu}$ width. No other microsporidian spore like this has not been so far isolated from Silkworm. The length of the polar filament extruded in hydrogen peroxide ($H_2O_2$) at $30^{\circ}C$ was $26{\mu}$ of a round cytoplasm on the top. The spores were partly stained with Giemsa, Safranin-O and Gram as the same staining properties as Nosema bombycis, Microsporidia K 79 and other microsporidian spores. The fine structures were observed under scanning eleceron microscope through ultrathin sectioning. The spore wall was composed of three layers ; the thin exospore of an electron dense rippled layer, the thick electron lucent endospore which was thinning considerably at the polar filament insertion point, and the inner limiting membrane. Polar cap present at the sporeapex, with a long polar filament of 12-13 coils, subtending angle of $60^{\circ}$ to spore axis, which is tubular made up of a multilayered and are a benes core, light ring structure enclosing the dance core, the dark ring structure enclosing the inner light ring structure and the other than and light ring structure bounded from cytoplasm. Lamellate polaroplast occupied the anterior part of the spore, and the two neclei with dense nucleoplasm bounded by a double nuclear envelope were cited in the slight downer middle portion of spore. From the characteristics of the shape, size and fine structures, it is certain to reason the Microsporidia S80 belong to the phylum Microspora, class Microspora, order Microsporida, order Microsporida. The shape of two nuclei cited seems to be genus Nosema, but in the classification for the suborder it should be defined wheather pansporoblasts be formed or not and for the genis especial attempts have been made to define the characters which distinguish the disporous genera in the life cycle. Survey through the infection of the bad cocoons during 1980 to 1982 in South Korea the areas contaminated with new microsporidia were revealed 5 provinces of Kyung-Gi, Kang-Won, Chung-Nam and Chun-Nam. Pathological effects inoculated per os at second instar larvae of silkworm, the LD 50 was $7.1{\times}10^7/ml$ as lower pathogenecity than that of Nosema bombycis Naegeli of $1.2{\times}10_7/ml$. While on the other hand the inoculation of the microsporidia at fourth instar larvae lowerd the whole cocoon weight and cocoon shell weight and significant at 1% level. The microsporidia S80 defined it can not be transmitted transovarially from the result of predictive and collective examination of 21 egg batches from the infected female moth.

  • PDF