Synergistic Effect on the Photocatalytic Degradation of 2-Chlorophenol Using $TiO_2$Thin Films Doped with Some Transition Metals in Water

  • 정오진
    • Bulletin of the Korean Chemical Society
    • /
    • 제22권11호
    • /
    • pp.1183-1191
    • /
    • 2001
  • The metallorganic chemical vapor deposition (MOCVD) method has been used to prepare TiO2 thin films for the degradation of hazardous organic compounds, such as 2-chlorophenol (2-CP). The effect of supporting materials and metal doping on the photocatalytic activity of TiO2 thin films also has been studied. TiO2 thin films were coated onto various supporting materials, including stainless steel cloth(SS), quartz glass tube (QGT), and silica gel (SG). Transition metals, such as Pd(II), Pt(IV), Nd(III) and Fe(III), were doped onto TiO2 thin film. The results indicate that Nd(Ⅲ) doping improves the photodegradation of 2-CP. Among all supporting materials studied, SS(37 ${\mu}m)$ appears to be the best support. An optimal amount of doping material at 1.0 percent (w/w) of TiO2-substrate thin film gives the best photodegration of 2-CP.

광전기 화학변환에 미치는 $TiO_2$ 전극의 두께와 첨가제의 영향 (Effects of the Thickness and Dopant on the Photoelectro- chemical Conversion in the Polycrystalline $TiO_2$ Electrodes)

  • 윤기현;강동헌
    • 한국세라믹학회지
    • /
    • 제21권3호
    • /
    • pp.266-270
    • /
    • 1984
  • The photoelectrochemical properties of the reduced $TiO_2$ceramic electrodes are investigated varying the thickness of the electrodes and the amounts of $Sb_2O_3$ as dopant. As the thickness of the undoped. $TiO_2$ceramic electrode increases the photocurrent tends to decrease. However for the R-F sputtered $TiO_2$ thin film electrodes the photocurrent tends to increase to about 1$\mu\textrm{m}$ thick and then decreases with increasing thickness. For the $TiO_2$ ceramic electrodes doped with $Sb_2O_3$ the photocurrent decreases with inreasing the amounts of dopant and in the case of rapid cooling in air without reduction treatment the photocurrent shows lower value. Also visible light excitation is observed at 500~550(nm) wavelength for the $TiO_2$ ceramic electrodes doped with $Sb_2O_3$comparing wtih the $TiO_2$ ceramic electrodes (~420nm)

  • PDF

Pt-and $TiO_2-doped\; Nb_2O_5$ Thin Film by Ion-Beam-Enhanced Deposition

  • Zhu, Jianzhong;Ren, Congxin
    • 한국진공학회지
    • /
    • 제7권s1호
    • /
    • pp.100-105
    • /
    • 1998
  • This paper describes the preparation of Pt-and $TiO_2$-doped $Nb_2O_5$ thin film by Ion-Beam-Enhanced Deposition. Platinum and titanium doping, and Nb2O5 deposition were carried out in situ. The dependence of oxygen sensing properties on the amounts of Pt and Ti dopant in the $Nb_2O_5$ film was investigated. There were the highist sensitivity, the lowest temperature coefficient and the shortest responce time at doping of 5 mol% $TiO_2$ and 0.3 mol%Pt

  • PDF

Sol-gel 법으로 제작된 BST 박막의 Bi 첨가에 따른 구조적, 유전적 특성 (Fabrication of BST thin films with Bi addition by Sol-gel method and their Structure and Dielectric properties)

  • 김경태;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 춘계학술대회 논문집 반도체 재료 센서 박막재료 전자세라믹스
    • /
    • pp.18-21
    • /
    • 2004
  • An alkoxide-based sol-gel method was used to fabricate $Ba_{0.6}Sr_{0.4}TiO_3$ thin films doped by Bi from 5 to 20 mol% on a $Pt/Ti/SiO_2/Si$ substrate. The structural and dielectric properties of BST thin films were investigated as a function of Bi dopant concentration. The dielectric properties of the Bi doped BST films were strongly dependent on the Bi contents. The dielectric constant and dielectric loss of the films decreased with increasing Bi content. However, the leakage current density of the 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin film showed the lowest value of $5.13{\times}10^{-7}\;A/cm^2$ at 5 V. The figure of merit (FOM) reached a maximum value of 32.42 at a 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin films. The dielectric constant, loss factor, and tunability of the 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin films were 333, 0.0095, and 31.1%, respectively.

  • PDF

Sol-gel 법으로 제작된 BST 박막의 Bi 첨가에 따른 구조적, 유전적 특성 (Fabrication of BST Thin films with Bi Addition by Sol-gel Method and their Structural and Dielectric Properties)

  • 김경태;김창일
    • 한국전기전자재료학회논문지
    • /
    • 제17권8호
    • /
    • pp.852-858
    • /
    • 2004
  • An alkoxide-based sol-gel method was used to fabricate $Ba_{0.6}Sr_{0.4}TiO_{3}$thin films doped by Bi from 5 to 20 mol% on a Pt/Ti/$SiO_2$/Sisubstrate. The structural and dielectric properties of BST thin films were investigated as a function of Bi dopant concentration. The dielectric properties of the Bi doped BST films were strongly dependent on the Bi contents. The dielectric constant and dielectric loss of the films decreased with increasing Bi content. However, the leakage current density of the 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_{3}$ thin film showed the lowest value of 5.13$\times 10^{-7} A/{cm}^2$ at 5 V. The figure of merit (FOM) reached a maximum value of 32.42 at a 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_{3}$thin films. The dielectric constant, loss factor, and tunability of the 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}Tio_{3}$ thin films were 333, 0.0095, and 31.1%, respectively.

Sm이 첨가된 PZT 박막의 강유전 특성 (Ferroelectirc Properties of Sm-doped PZT Thin films)

  • 손영훈;김경태;김창일;이병기;장의구
    • 한국전기전자재료학회논문지
    • /
    • 제17권2호
    • /
    • pp.178-183
    • /
    • 2004
  • PBT thin film was known to be a representative for the FeRAM devices because of its good ferroelectric proporties and the ease in fabricating the thin film. However, there have been several problems such as polarization fatigue and leakage current in memory devices with a PZT thin film. In this study, Sm-dolled PZT thin films were fabricated by the so1-gel method, and their ferroelectric and dielectric proportrics were compared as a function of Sm content. We investigated the effect of the Sm dopant on structural and electrical properties of PZT film. Sm-doped PZT thin films on the Pt/Ti/SiO$_2$/Si substrates have been prepared by a sol-gel method. The remanent polarization and coercive field decreased with increasing the concentration of Sm. The dielectric constant and dielectric loss decreased with Increasing Sm content. Sm-doped PZT thin films showed improved fatigue characteristics compared to the undoped PZT thin film.

Tunable 소자 응용을 위한 Sol-gel 법으로 제작된 BST 박막의 Bi 첨가에 따른 구조적, 유전적 특성 (Structure and Dielectric properties of BST Thin Films prepared by Sol-gel method for Tunable element application)

  • 김태형;김경태;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 하계학술대회 논문집 Vol.5 No.2
    • /
    • pp.565-568
    • /
    • 2004
  • An alkoxide-based sol-gel method was used to fabricate $Ba_{0.6}Sr_{0.4}TiO_3$ thin films doped by Bi from 5 to 20 mol% on a Pt/Ti/SiO2/Si substrate. The structural and dielectric properties of BST thin films were investigated as a function of Bi dopant concentration. The dielectric properties of the Bi doped BST films were strongly dependent on the Bi contents. The dielectric constant and dielectric loss of the films decreased with increasing Bi content. However, the leakage current density of the 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin film showed the lowest value of 5.13 10-7 at 5 V. The figure of merit (FOM) reached a maximum value of 32.42 at a 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin films. The dielectric constant, loss factor, and tunability of the 10 mol% Bi doped $BBa_{0.6}Sr_{0.4}TiO_3$ thin films were 333,0.0095, and 31.1%, respectively.

  • PDF

BST 축전박막의 누설전류 평가 (Leakage Current of Capacitive BST Thin Films)

  • 인태경;안건호;백성기
    • 한국세라믹학회지
    • /
    • 제34권8호
    • /
    • pp.803-810
    • /
    • 1997
  • Ba0.5Sr0.5TiO3박막을 RF 마그네트론 스퍼터링법을 이용하여 Pt/Ti/SiO2/Si(100) 기판에 증착하였다 .누설전류에 영향을 주는 것으로 알려진 열처리 조건, dopant 효과 등을 평가하고자 이온반경이Ti와 유사하고 대부분이 Ti 자리를 치환하는 것으로 알려진 Nb와 Al을 각각 danor와 acceptor로 선택하여 BST 박막에 첨가한 후 누설전류를 측정하였다. 고온에서 in-situ 증착된 BST 박막은 거친 표면 형상을 보이며 낮은 전압에서 파괴가 발생하고, Nb 첨가로 누설전류가 증가하였다. 삼온 증착후 후열처리된 박막은 표면 형상도 평할도가 증가하였으며 in-situ로 제조된 박막에 비해 높은 파괴전압과 낮은 누설전류를 나타내었다. 특히 Al이 첨가된 BST 박막의 누설전류밀도는 ~10A/cm2로 도핑을 하지 않은 박막이나 Nb가 첨가된 박막에 비해 매우 낮은 누설전류밀도를 나타내었으며, 이는 산화로 인한 산소공공의 감소, 이동 가능한 hole의 감소와 후열처리과정중 계면 및 입계의 산화로 Schottky 장벽에 높아진 결과로 판단된다.

  • PDF

$BCl_3$/Ar 플라즈마에서 $Cl_2$ 첨가에 따른 TiN 박막의 식각 특성 (Etch characteristics of TiN thin film adding $Cl_2$ in $BCl_3$/Ar Plasma)

  • 엄두승;강찬민;양설;김동표;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 하계학술대회 논문집 Vol.9
    • /
    • pp.168-168
    • /
    • 2008
  • Dimension of a transistor has rapidly shrunk to increase the speed of device and to reduce the power consumption. However, it is accompanied with several problems like direct tunneling through the gate dioxide layer and low conductivity characteristic of poly-Si gate in nano-region. To cover these faults, study of new materials is urgently needed. Recently, high dielectric materials like $Al_2O_3$, $ZrO_2$, and $HfO_2$ are being studied for equivalent oxide thickness (EOT). However, poly-Si gate is not compatible with high-k materials for gate-insulator. Poly Si gate with high-k material has some problems such as gate depletion and dopant penetration problems. Therefore, new gate structure or materials that are compatible with high-k materials are also needed. TiN for metal/high-k gate stack is conductive enough to allow a good electrical connection and compatible with high-k materials. According to this trend, the study on dry etching of TiN for metal/high-k gate stack is needed. In this study, the investigations of the TiN etching characteristics were carried out using the inductively coupled $BCl_3$-based plasma system and adding $Cl_2$ gas. Dry etching of the TiN was studied by varying the etching parameters including $BCl_3$/Ar gas mixing ratio, RF power, DC-bias voltage to substrate, and $Cl_2$ gas addition. The plasmas were characterized by optical emission spectroscopy analysis. Scanning electron microscopy was used to investigate the etching profile.

  • PDF

Interface Control to get Higher Efficiency in a-Si:H Solar Cell

  • Han, Seung-Hee;Kim, En-Kyeom;Park, Won-Woong;Moon, Sun-Woo;Kim, Kyung-Hun;Kim, Sung-Min
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.193-193
    • /
    • 2012
  • In thin film silicon solar cells, p-i-n structure is adopted instead of p/n junction structure as in wafer-based Si solar cells. PECVD is the most widely used thin film deposition process for a-Si:H or ${\mu}c$-Si:H solar cells. Single-chamber PECVD system for a-Si:H solar cell manufacturing has the advantage of lower initial investment and maintenance cost for the equipment. However, in single-chamber PECVD system, doped and intrinsic layers are deposited in one plasma chamber, which inevitably impedes sharp dopant profiles at the interfaces due to the contamination from previous deposition process. The cross-contamination between layers is a serious drawback of single-chamber PECVD system. In this study, a new plasma process to solve the cross-contamination problem in a single-chamber PECVD system was suggested. In order to remove the deposited B inside of the plasma chamber during p-layer deposition, a high RF power was applied right after p-layer deposition with SiH4 gas off, which is then followed by i-layer, n-layer, and Ag top-electrode deposition without vacuum break. In addition to the p-i interface control, various interface control techniques such as FTO-glass pre-annealing in O2 environment to further reduce sheet resistance of FTO-glass, thin layer of TiO2 deposition to prevent H2 plasma reduction of FTO layer, and hydrogen plasma treatment prior to n-layer deposition, etc. were developed. The best initial solar cell efficiency using single-chamber PECVD system of 10.5% for test cell area of 0.2 $cm^2$ could be achieved by adopting various interface control methods.

  • PDF