Microscopic fracture criterion of crack growth initiation (연성 균열성장 개시의 미시적 파괴조건)

  • 구인회
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.11 no.5
    • /
    • pp.740-745
    • /
    • 1987
  • For the prediction of the crack growth initiation from a blunt notch or a precrack in a prestrained material under plane strain tension and small-scale yielding conditions, a microscopic fracture criterion is proposed in terms of the crack tip opening displacement(COD) needed for the attainment of fracture strain at a microstructural distance. Smooth blunting of a crack tip with an initial root radius is assumed, and strain distributions on the crack-line axis are calculated at each deformation stage until the distributions against an original distance normalized to the COD are insensitive to an initial root radius. This case of no initial-root-radius effect is taken as for a sharp crack tip, on which the criterion is applied to determine the characteristic length of material from a critical COD for a fatigue-precracked specimen. The predicted COD at the fracture initiation from a crack with an initial root radius or a prestraining shows reasonable agreement with experimental values.

Simulation of fracture in plain concrete modeled as a composite material

  • Bui, Thanh T.;Attard, Mario M.
    • Computers and Concrete
    • /
    • v.2 no.6
    • /
    • pp.499-516
    • /
    • 2005
  • A composite model is used to represent the heterogeneity of plain concrete consisting of coarse aggregates, mortar matrix and the mortar-aggregate interface. The composite elements of plain concrete are modeled using triangular finite element units which have six interface nodes along the sides. Fracture is captured through a constitutive single branch softening-fracture law at the interface nodes, which bounds the elastic domain inside each triangular unit. The inelastic displacement at an interface node represents the crack opening or sliding displacement and is conjugate to the internodal force. The path-dependent softening behaviour is developed within a quasi-prescribed displacement control formulation. The crack profile is restricted to the interface boundaries of the defined mesh. No re-meshing is carried out. Solutions to the rate formulation are obtained using a mathematical programming procedure in the form of a linear complementary problem. An event by event solution strategy is adopted to eliminate solutions with simultaneous formation of softening zones in symmetric problems. The composite plain concrete model is compared to experimental results for the tensile crack growth in a Brazilian test and three-point bending tests on different sized specimens. The model is also used to simulate wedge-type shear-compression failure directly under the loading platen of a Brazilian test.

Evaluation of the Crack Initiation of Curved Compact Tension Specimens of a Zr-2.5Nb Pressure Tube Using the Unloading Compliance and Direct Current Potential Drop Methods (제하 컴플라이언스법 및 직류전위차법을 이용한 Zr-2.5Nb 압력관 휘어진 CT 시편의 균열시작 평가)

  • Jeong, Hyeon-Cheol;Ahn, Sang-Bok;Kim, Young-Suk
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.29 no.8 s.239
    • /
    • pp.1118-1122
    • /
    • 2005
  • The direct current potential drop (DCPD) method and the unloading compliance (UC) method with a crack opening displacement gauge were applied simultaneously to the Zr-2.5Nb curved compact tension (CCT) specimens to determine which of the two methods can precisely determine the crack initiation point and hence the crack length for evaluation of their fracture toughness. The DCPD method detected the crack initiation at a smaller load-line displacement compared to the UC method. As a verification, a direct observation of the fracture surfaces on the curved compact tension specimens was made on the CCT specimens experiencing either 0.8 to 1.0 mm load line displacement or various loads from $50\%\;to\;80\%$ of the maximum peak load, or $P_{max}$. The DCPD method is concluded to be more precise in determining the crack initiation and fracture toughness, J in Zr-2.5Nb CCT specimens than the UC method.

A Study of the Influence of Roughness on fracture Shear Behaviour and Permeability (거칠기가 절리의 전단거동 및 투수성에 미치는 영향에 관한 연구)

    • Tunnel and Underground Space
    • /
    • v.12 no.4
    • /
    • pp.312-320
    • /
    • 2002
  • It is well-known that when single rock fractures undergo shear displacement, they are influenced by the boundary conditions and fracture roughness. In this case, aperture geometry will change by means of dilation due to the shear displacement. As fractures become the flow paths, fluid flow through rock fractures is affected by the void geometry. In this study, therefore, the influence of roughness on shear behavior of fractures has been investigated, and the resulting hydraulic behavior has been analyzed. In order for this study, a statistical method has been used to generate rough fractures, and they have been adopted into new conceptual models fur fracture shearing and flow calculations. The main contributions of this study are as follows: firstly, fracture shear behavior becomes less brittle with decreasing fracture roughness and increasing normal stress. Then, the characteristics of aperture distribution becomes those of roughness of fractures indicating its hydraulic significance. Finally, it is observed that with decreasing fracture roughness the breakdown of channel flow occurs more slowly.

The basic study about streaming potential generated by specimen fracture (시료 파괴 시 발생하는 SP에 관한 기초 연구)

  • Kim, Jong-Wook;Cho, Sung-Jun;Park, Sam-Gyu;Sung, Nark-Hoon;Song, Young-Soo
    • 한국지구물리탐사학회:학술대회논문집
    • /
    • 2007.06a
    • /
    • pp.291-296
    • /
    • 2007
  • We measured potential waveform of load, displacement, micro electric signal generated by rock and mortar fracture using PXI A/D Converter. The rock type used for measurement was used granite, limestone and sandstone, and mortar specimen. we made measuring equipment of physical properties to confirm basic information of physical properties, measured physical properties of rock engineering, electric resistivity and seismic velocity. Potential waveform system was built using PXI A/D Converter and measured potential waveform of load, displacement, micro-electric signal generated using this during uniaxial compressive test by the specimen finished such test of physical properties. Using the saturated rock and mortar specimen, micro electric signal increased, and It didn't increase a signal in dried rock and mortar specimen according as load and strain rate increases. But signal also increased in saturated or dried specimen in case of sandstone. It was possible to check the close correlation relationship the signal and fracture behavior by a compressive load as the signal of fracture position was increased bigger than the other position. It was also possible to check the correlation relationship between physical properties and micro geo-electric signal.

  • PDF

Behavior Analysis Using FEM for Earth Retaining Wall of Soft Rock Fracture Zone (FEM을 이용한 연암 파쇄대 지반의 흙막이 벽체 거동 분석)

  • Jang, Gi-Soo;Park, Min-Chul;Shin, Hyo-Hee;Lee, Song
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.17 no.4
    • /
    • pp.30-37
    • /
    • 2013
  • A soft rock fracture zone is an important element for rock slope or earth retaining, however stability studies of earth retaining wall have been lack. Therefore, this study is analyzed for a behavior of earth retaining wall with condition of fracture zone or no fracture zone and then a numerical analysis (Finite Element Method) was performed considering interaction with field monitoring data between ground and structures. As a result, applied horizontal displacement on retaining wall is correspond between result of numerical analysis and field monitoring data and displacement point stress distribution with fracture zone condition analyzed to be stable side but no fracture zone condition is expressed to be unstable side. The results of this study is purpose for applying safety construction as a top priority at field when designing for future.

Long-term outcomes of initially conservatively treated midshaft clavicle fractures

  • Lee, Gwan Bum;Kim, Hyojune;Jeon, In-Ho;Koh, Kyoung Hwan
    • Clinics in Shoulder and Elbow
    • /
    • v.24 no.1
    • /
    • pp.9-14
    • /
    • 2021
  • Background: Recent studies about completely displaced midshaft clavicle fractures have reported that their nonunion/malunion rates were significantly higher in conservatively treated patients compared to surgically treated patients. The purpose of this study was to evaluate the factors associated with treatment decisions for midshaft clavicle fractures and also the factors that affect patient satisfaction with their treatment choice. Methods: We retrospectively reviewed the records of 75 patients who had been diagnosed with a midshaft clavicle fracture and were treated conservatively at a single institution between March 1, 2013, and December 31, 2014. Their medical records were reviewed to investigate the severity of the initial vertical displacement. A telephone survey was carried out to identify the presence of any patient-perceived deformity and determine if the patient eventually underwent surgery and whether the patient would prefer surgery if the injury recurred. Results: Significantly more patients with vertical displacement ≥100% (9/28) eventually underwent surgery compared to patients with vertical displacement <100% (3/32, p=0.028). Patients with vertical displacement ≥100% (13/28) were significantly more likely to prefer surgery compared to patients with vertical displacement <100% (7/32, p=0.044). Among the conservatively treated patients, nine of 32 participants with a patient-perceived deformity and one of 16 without a patient-perceived deformity responded that they would prefer to receive surgery in same situation in the future (p=0.079). Conclusions: Patients with a midshaft clavicle fracture with vertical displacement of ≥100% may eventually require surgical treatment. When conservative treatment is carried out, the long-term patient results may be unsatisfactory due to perceived residual deformities.

Evaluation of fracture toughness of dynamic interlaminar for CFRP laminate plates inserted interleaf (인터리브가 삽입된 CFRP 적층판의 인성평가)

  • 김지훈;강태식;한길영;김재열;심재기
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.10 no.4
    • /
    • pp.91-96
    • /
    • 2001
  • In this paper, an investigation was performed on the dynamic interlaminar fracture toughness of CFRP(carbon filber rein-forcement plastics). Specimens used in this experiments are CF/PEEK laminated plates. In this experiments, Split Hopkin-sons Bar(SHPE) tes was apply to dynamic and notched flexure test. The model II fracture toughness of each unidirectional CFRP was estimated by the analyzed deflection of the specimen and J-integral with the measured impulsive load and reac-tions at the supported points. As an experimental results the vibration amplitude of [$0^{\circ}_10 /F_4 0^{\circ}_10 $] j-aminates appear more than that of [$0^{\circ}_10 /F_2 0^{\circ}_10 $ laminates for the j-integral and displacement velocity at a measuring point. Also, it is thought that the dynamic fracture toughness of two kind specimen(CF/PEEK) with the crease of displacement velocity becomes great at a measuring point with in the range of measurement.

  • PDF

A study on the fracture toughness of dynamic interlaminar for CFRP composite laminates (선진복합재료 적층판의 동적 층간 파괴 인성평가)

  • 김지훈;김영남;양인영;심재기
    • Journal of the Korean Society of Safety
    • /
    • v.13 no.4
    • /
    • pp.41-48
    • /
    • 1998
  • In this paper, an investigation was performed on the dynamic interlaminar fracture toughness of CFRP(carbon fiber reinforcement plastics) composite laminates. Composite laminates used in this experimentation are CF/EPOXY and CF/PEEK laminated plates. In the experiments, Split Hopkinson's Bar(SHPE) test was applied to dynamic and notched flexure test. The mode Ⅱ fracture toughness of each unidirectional CFRP was estimated by the analyzed deflection of the specimen and J-integral with the measured impulsive load and reactions at the supported points. As an experimental result, the vibration amplitude of CF/PEEK laminates appear more than that of CF/EPOXY laminates for the J-integral and displacement velocity at a measuring point. Also, it is thought that the dynamic fracture toughness of two kind specimens(CFRP/EPOXY and CF/PEEK) with the in crease of displacement velocity becomes a little greater at a measuring point within the range of measurement.

  • PDF

Evaluation on The Fracture Toughness of Chopped Strand Reinforced ALS Matrix Composites (촙트 스트랜드 강화 ALS계 복합재료의 파괴인성 평가)

  • 차용훈;김덕중;이연신;성백섭;채경수
    • Journal of the Korean Society of Safety
    • /
    • v.13 no.1
    • /
    • pp.13-18
    • /
    • 1998
  • It is well known in the fracture mechanics community that the fracture toughness of brittle materials, such as ceramics, can be improved improves significantly when fibers are added into the material. This is because in presence of fibers the cracks cannot propagate as freely as it can in absence of them. Fibers bridge the gap between two adjacent surfaces of the crack and reduce the crack tip opening displacement, thus make it harder to propagate. Several investigators have experimentally studied how the length, diameter and volume fraction of fibers affect the fracture toughness of chopped strand reinforced matrix composite materials. In this paper, matrix used ALS, Arizona Lunar Simulant, types of fiber used carbon steels and stainless steels. To analyze quantitatively fiber reinforced ALS composites, experimental and analytical methods was progressed. Load-displacement curve is used to experimental method, and FEM analysis program using ABAQUS is used analytical method.

  • PDF