• Title/Summary/Keyword: Dielectric mixing rule

Search Result 17, Processing Time 0.455 seconds

Evaluation of Microwave Dielectric Properties in $(Pb_{0.5}Ca_{0.5})(Fe_{0.5}Ta_{0.5})O_3$ Ceramics by the Dielectric Mixing Rule (유전체 혼합 법칙을 이용한 $(Pb_{0.5}Ca_{0.5})(Fe_{0.5}Ta_{0.5})O_3$세라믹스의 마이크로파 유전특성 평가)

  • 박흥수;윤기현;김응수
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.3
    • /
    • pp.240-246
    • /
    • 2000
  • The microwave dielectric properties of the complex perovskite (Pb0.5Ca0.5)(Fe0.5Ta0.5)O3 ceramics were investigated with the porosity and the dielectric mixing rule. Assuming that the specimens were mixtures of real dielectrics and pores, with 3-0 connectivity, the ionic polarizabilities modified by Maxwell's equation were more close to the theoretical values rather than those modified by Wiener's equation in porous specimens. The theoretical dielectirc loss were obtained with the infrared reflectivity spectra from 50 to 4000cm-1, which were calculated by Kramers-Kronig analysis and classical osciallator model. The relative tendency of dielectric loss calculated from the theoretical value and Maxwell's equation in the specimens with different porosities was in good agreement with the one by the post resonant method.

  • PDF

Microwave dielectric properties of $(1-x)CaWO_4-xYNbO_4$ ceramics ($(1-x)CaWO_4-xYNbO_4$계 세라믹스의 마이크로파 유전특성)

  • Kim, Su-Jung;Kim, Eung-Soo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.17 no.5
    • /
    • pp.217-222
    • /
    • 2007
  • Microwave dielectric properties of $(1-x)CaWO_4-xYNbO_4$ ceramics have been investigated as a function of $YNbO_4$ content($0.05{\leq}x{\leq}0.4$). A single phase with tetragonal scheelite structure was obtained up to x=0.10 and then the secondary phase with fergusonite structure was increased. With the increase of $YNbO_4$ content, apparent densities of the specimens were decreased. This results were due to the lower theoretical density of $YNbO_4(5.581g/cm^3)$ than that of $CaWO_4(6.117g/cm^3)$. Dielectric constant(K) and quality factor(Qf) were decreased with $YNbO_4$ content which could be attribute to the decrease of density and the increase of secondary phase. Temperature coefficient of resonant frequency (TCF) of the specimens with the $YNbO_4$ content was depended on dielectric mixing rule.

Microwave Dielectric Characteristics of Aluminum Magnesium Tantalate Solid Solutions with Variations of Ionic Polarizability and Crystal Structure (이온 분극률과 결정구조에 따른 Aluminum Magnesium Tantalate 고용체의 마이크로파 유전특성)

  • 최지원;하종윤;강종윤;윤석진;윤기현;김현재
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.07a
    • /
    • pp.119-122
    • /
    • 2002
  • The calculated and measured dielectric constant of (1-x)(Al$\sub$1/2/Ta$\sub$1/2/)O$_2$-x(Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$(O$\leq$x$\leq$1.0) solid solutions were investigated by variations of ionic polarizability and crystal structure. (Al$\sub$1/2/Ta$\sub$1/2/)O$_2$ and (Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$were orthorhombic and tetragonal trirutile structure, respectively. When (Al$\sub$1/2/Ta$\sub$1/2/)O$_2$ was substituted by (Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$, the phase transformed to tetragonal structure over 60 mole%. Because the ionic radius of (Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$was slightly bigger than one of (A1$\sub$1/2/Ta$\sub$1/2)O$_2$, the cell parameters increased with an increase of (Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$ substitution. The measured dielectric constant increased with an increase of (Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$ substitution and coincided with dielectric mixing rule and the calculated dielectric constant with the molecular additivity rule. There were some differences between the measured and the calculated dielectric constant. The reason of the lowered dielectric constant comparing with the calculated one was compressed stress due to the electronic structure of tantalum.

  • PDF

Microwave Dielectric constant characteristics or (Al,Mg,Ta)O2 Solid Solutions with Crystal Structure and Ionic Polarizability (결정구조와 이온 분극률에 따른 (Al,Mg,Ta)O2고용체의 마이크로파 유전상수 특성)

  • 최지원;하종윤;안병국;박용욱;윤석진;김현재
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.16 no.2
    • /
    • pp.108-112
    • /
    • 2003
  • The calculated and measured dielectric constants of (1-x)(A $l_{1}$2/ T $a_{1}$2/) $O_2$-x(M $g_{1}$3/ T $a_{2}$3/) $O_2$ (0$\leq$x$\leq$1.0) solid solutions were investigated by variations of ionic polarizability and crystal structure. (A $l_{1}$2/ T $a_{1}$2/) $O_2$ and (M $g_{1}$3/ T $a_{2}$3/) $O_2$ were orthorhombic and tetragonal trirutile structure, respectively. When (A $l_{1}$2/ T $a_{1}$2/) $O_2$ was substituted by (M $g_{1}$3/ T $a_{2}$3/) $O_2$, the phase transformed to tetragonal structure over 60 mole. Because the total ionic radius of [(Mg+2Ta)/3]$^{4+}$ was slightly bigger than one of [(Al+Ta)/2]$^{4+}$, the lattice parameters increased with an increase of (M $g_{1}$3/ T $a_{2}$3/) $O_2$ substitution. The measured dielectric constant increased with an increase of (M $g_{1}$3/ T $a_{2}$3/) $O_2$ substitution and coincided with dielectric mixing rule and the calculated dielectric constant with the molecular additivity rule. There were some differences between the measured and the calculated dielectric constant. The reason of the lowered dielectric constant comparing with the calculated one was compressed stress due to the electronic structure of tantalum.

Dielectric characteristics of PMMA-PZT coated Ni Composites (PMMA-PZT coated Ni 복합체의 유전특성)

  • Jeong, Won-Chae;Lee, Hee Young;Kim, Jeong-Joo;Im, Eun-Seop
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.349-349
    • /
    • 2005
  • 수동소자를 PCB(Printed Circuit Board) 안으로 집적하기 위한 방법의 일환으로 polymer-metal, polymer-ceramic composite에 연구가 국내외 연구 국내외 연구기관에서 광범위하게 진행되고 있다. 본 연구에서는 polymer-metal-ceramic composite 에서 PZT-coated Ni의 volume fraction에 따른 유전율 변화에 대하여 조사하였다. 원료로는 PZT(52/48) solution. 니켈금속분말, PMMA(polymethyl methacrylate)를 사용하였다. 전기적 특성은 임피던스분석기를 이용하여 측정하였으며 mixing rule과 percolation theory를 이용하여 결과를 해석하였다.

  • PDF

Microwave Dielectric Characteristics of the $xMgTiO_3$(1-x) ($Na_{1/2}Ln_{1/2}$) $TiO_3$(Ln = La, Pr, Nd, Sm)Systems ($xMgTiO_3$(1-x) ($Na_{1/2}Ln_{1/2}$) $TiO_3$(Ln = La, Pr, Nd, Sm)의 초고주파 유전특성에 관한 연구)

  • Kim, Duck-Hwan;Lim, Sang-Kyu;An, Chul
    • Journal of the Korean Institute of Telematics and Electronics D
    • /
    • v.35D no.10
    • /
    • pp.51-59
    • /
    • 1998
  • ($Na_{1/2}Ln_{1/2}$)$TiO_3$ceramics have a high relative dielectric constant and a positive temperature coefficient of resonant frequency ($\tau_f$)(where Ln represents a lanthanide: $La^{+3}$, $Pr^{+3}$, $Nd^{+3}$ and $Sm^{+3}$). On the other hand, $MgTiO_3$ ceramic has a high Qf value and a negative temperature coefficient. So We have investigated the microwave dielectric properties of $xMgTiO_3$-(1-x) ($Na_{1/2}Ln_{1/2}$)$TiO_3$. In these systems, there are no clues on solid-solution and secondary phase. There are mixed phases with $MgTiO_3$and ($Na_{1/2}Ln_{1/2}$)$TiO_3$ phases. Its dielectric characteristics (Qf, temperature coefficient and dielectric constant) are intermediate between ($Na_{1/2}Ln_{1/2}$)$TiO_3$ and $MgTiO_3$ and are predictable by the logarithmic mixing rule. The dielectric ceramic compositions temperature coefficient each approximates to zero at Ln=La, x=0.9, Ln=Pr, x=0.87, and Ln=Nd, x=0.84. At this time, there are Qf values in the range of 55,000 to 28,00GHz and relative dielectric constants in the range of 22 to 25.

  • PDF

Low Temperature Sintering and Microwave Dielectric Properties of Zn1-x(Li1/2La1/2)xTiO3 Ceramics (Zn1-x(Li1/2La1/2)xTiOM3계 세라믹스의 저온 소결 및 마이크로파 유전특성)

  • 김응수;한기문
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.2
    • /
    • pp.165-169
    • /
    • 2004
  • Microwave dielectric properties and the behavior of low-temperature sintering of $Zn_{1-x}(Li_{1/2}La_{1/2})_xTiO_3$ ($0.01{\leq}x{\leq}0.05$) with 4 wt% $H_3BO_3$ were investigated as a function of $(Li_{1/2}La_{1/2})^{2+}$ content. The sintering temperature of the specimens can be reduced from $1150^{\circ}C$ to $875^{\circ}C$ with the addition of 4 wt% $H_3BO_3$ as a sintering agent. Dielectric constant (K) and Temperature Coefficient of resonant Frequency (TCF) with the substitution of ($(Li_{1/2}La_{1/2})^{2+}$ ion depended on dielectric mixing rule. Quality factor (Qf) depended on density and microstructure. Typically, K of 26.5, Qf of 19,030 GHz and TCF of 7.5 ppm$/^{\circ}C$ were obtained for the specimens with x=0.03 sintered at $875^{\circ}C$ for 3 h.

Microwave Dielectric Properties of the 0.7Mg4Ta2O9-0.3SrTiO3 Ceramics with Sintering Temperature (소결온도에 따른 0.7Mg4Ta2O9-0.3SrTiO3 세라믹스의 마이크로파 유전특성)

  • Kim, Jae-Sik;Choi, Eui-Sun;Lee, Moon-Kee;Lee, Young-Hie;Bae, Seon-Gi
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.18 no.6
    • /
    • pp.538-542
    • /
    • 2005
  • The structural and microwave dielectric properties of $0.7Mg_4Ta_2O_9-0.3SrTiO_3$ ceramics with sintering temperature were investigated. All the sample of the $0.7Mg_4Ta_2O_9-0.3SrTiO_3$ ceramics were prepared by conventional miked oxide method and the sintering temperature was $1425\~1500^{\circ}C$. The hexagonal phase of $Mg_4Ta_2O_9$ and the cubic phase of $SrTiO_3$ were coexisted. The porosity of $0.7Mg_4Ta_2O_9-0.3SrTiO_3$ ceramics were reduced with increasing sintering temperature. In the case of $0.7Mg_4Ta_2O_9-0.3SrTiO_3$ ceramics sintered at $1475^{\circ}C$, dielectric constant, quality factor and temperature coefficient of resonant frequency were 14.51, 82,596 GHz and $-3.14\;ppm/^{\circ}C$, respectively.

Microwave dielectric properties of (1-x)$CaTiO_3-xLa(Zn_{1/2}Ti_{1/2})O_3$ System ($(1-x)CaTiO_3$-xLa$(Zn_{1/2}Ti_{1/2})O_3$ 계의 마이크로파 유전 특성)

  • Yeo, Dong-Hun;Kim, Jae-Beom;Yun, Seok-Jin;Kim, Hyeon-Jae;Yun, Sang-Ok;Song, Jun-Tae
    • Proceedings of the KIEE Conference
    • /
    • 1994.07b
    • /
    • pp.1257-1261
    • /
    • 1994
  • Phsysical and dielectric properties of $(1-x)CaTiO_3-xLa(Zn_{1/2}Ti_{1/2})O_3$ ceramics were investigated at the temperature range of $25^{\circ}C$ to $80^{\circ}C$ at the frequency of 6 GHz. As increasing addition of the amount of $La(Zn_{1/2}Ti_{1/2})O_3$ to x = 5 mol,Q value was increased due to grain growth and increase of density. For more addition, Q value decreased due to electrical defect. Temperature coefficient of resonant frequency could be controlled by the amount of $La(Zn_{1/2}Ti_{1/2})O_3$, which could be explained by volume mixing rule.

  • PDF

High Dielectric Constant Ni-Coated $BaTiO_3$-PMMA Composites for Embedded Passive Device (내장형 수동소자용 고유전율 Ni코팅된 $BaTiO_3$-PMMA 복합체)

  • Park, Jung-Min;Lee, Hee-Young;Kim, Jeong-Joo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.06a
    • /
    • pp.315-316
    • /
    • 2007
  • 최근 전자제품의 경박단소화와 고성능화에 대한 관심이 증가하면서 내장형 수동소자 (Embedded Passive Device)에 대한 연구가 활발히 진행되고 있다. 본 연구에서는 Ni-coated $BaTiO_3$와 PMMA의 함량 변화에 따른 복합체의 유전적 특성을 연구하였다. Ni-coated $BaTiO_3$첨가량을 0~50%까지 증가시키며 유전율을 측정하였으며, 코팅되지 않은 $BaTiO_3$-PMMA복합체의 유전율과 결과를 비교하였다. 본 연구결과 Ni 코팅에 의한 유전율 증가를 관찰할 수 있었으며, 코팅 상태는 코팅공정시의 시간과 온도 등에 의존한다는 것을 확인하였다. 본 논문에서는 이러한 실험결과를 개선된 혼합법칙을 바탕으로 해석하고자 한다.

  • PDF