Proceedings of the Korean Society for Technology of Plasticity Conference
/
2003.10a
/
pp.261-264
/
2003
Semi-solid processing is now becoming of great interest for the production of various parts by pressure die casting. Many advantages are associated with this forming process at the condition that the forming operation is performed under appropriate conditions. The thixoforming process, which needs a suspension of a globular, non-dendritic solid phase in the liquid phase, is characterized by three major steps. The first step is casting of billets with a microstructure suited for thixoforming. The second step is reheating of slugs cut from these billets. The third step is injection of the semi-solid slugs into a die. In this paper, the horizontal reheating machine to obtain the optimal conditions suitable for semiu-solid die casting process was used and applied to extrusion material. It is estimated the possibility of application on semi-solid die casting with extrusion material through various results.
Proceedings of the Korean Society of Precision Engineering Conference
/
2002.05a
/
pp.711-714
/
2002
Although recent research of metallic materials in high temperature fatigue have been much accomplished, many studies about brittle material as a die steel in high temperature fatigue does not have been reported. Especially, the study on the fatigue behavior over the transformation temperature is not studied sufficiently because of its difficult analysis and experiment. Therefore, reliable results of brittle material in high temperature fatigue behavior are needed. In this paper, stress-strain curves and stress-life curves in die STD61 steel at 700 and 900 are carefully examined, as the basic experimental data are used to predict from fatigue life over 700.
Journal of the Korean Society for Precision Engineering
/
v.17
no.6
/
pp.96-102
/
2000
The finishing process for dies and molds is an important process because it has influence on final quality of products. And it is difficult to automatize finishing process so that the process has depended on expert's skill until now. However, recently a study on development of die automatic finishing machine has been progressed, and actually this machine is applied to fabrication of die. But the research about tooling system is not enough and finishing tool must have high machining efficiency and adaptability of curved surface. So, this study investigated the application of conductive elastic tool which is composed of metal-resin bonded pellet and elastic backing material. The metal-resin bonded pellet is used to finish the surface by conventional mechanical grinding or electro-chemial grinding method. And elastic backing material is used to follow the curved surface. So conductive elastic tool has long lifetime, uniform removal rate and adaptability of curved surface.
Journal of the Korean Society for Precision Engineering
/
v.14
no.3
/
pp.130-136
/
1997
The velocity distrubution at the exit of extrusion die depends on the width of bearing land very much. When uniform bearing land without flow guide is used, the material which is extended through the same die does not, deflect to the constant direction, but when the flow guide is equipped and then the volume compensation is done accurately, the material deflects to one constant direction. Therfore, the part of problem can be known exactly, and extrusion products of straight shape can be produced by the corrected bearing land width.
Proceedings of the International Microelectronics And Packaging Society Conference
/
2002.09a
/
pp.79-94
/
2002
Root cause -Thermal expansion coefficient mismatch -Tape warpage -Initial die crack (die roughness) Guideline for failure prevention -Optimized tape/Substrate design for minimizing the warpage -Fine surface of die backside Root cause -Thermal expansion coefficient mismatch - Repetitive bending of a signal trace during TC cycle - Solder mask damage Guideline for failure prevention - Increase of trace width - Don't make signal trace passing the die edge - Proper material selection with thick substrate core Root cause -Thermal expansion coefficient mismatch -Creep deformation of solder joint(shear/normal) -Material degradation Guideline for failure Prevention -Increase of solder ball size -Proper selection of the PCB/Substrate thickness -Optimal design of the ball array -Solder mask opening type : NSMD -In some case, LGA type is better
Proceedings of the Korean Society of Precision Engineering Conference
/
2000.11a
/
pp.846-849
/
2000
In this paper backward extrusion process with lower die rotation was studied to improve the conventional backward extrusion problems ; requirement of large forming machine, the difficulty to selecting of die material caused by high surface pressure, high cost of forming machine caused by improvement of noise and vibration, and etc. In this experiment, model material, plasticine, was used of specimen. The result values of torsional and conventional backward extrusions were analyzed and compared. FE-simulation is used for analysis with DEFPRM-3D. These results show that the torsional backward extrusion is very useful process because this process can obtain the homogeneous deformation, low forming load. Decreasing forming load improves die life and makes it possible to use press of relatively low capacity. Also this process can reduce corner cavity, improve the initial cast-structure, owing to the high deformation and uniform starin distribution.
Proceedings of the Korean Powder Metallurgy Institute Conference
/
2006.09a
/
pp.97-98
/
2006
Gas-permeable metal die materials are developed using tool steel powder, packed in a mold having the insertion of orthogonally arrayed polymer wires. Linear gas-permeable channels in orthogonal array are thus developed by the burning out of the polymer wires, which yield a microstructure with wear resistance value and air permeability much larger than those of the conventional gas-permeable die material.
Most of automobile parts manufactured through sheet metal forming are mass-produced by using press mold. In recent years, automation and speeding up of press lines have been expanding to maximize product productivity using a press die. The proportion of the moving time in the press line is high, and therefore requires high-speed and automated equipment for the moving process. In this paper, to provide the double-moving system can be the moving time reduction and increased productivity. Developed transport system consists of the material supply, the material feeding device and the PLC controller and the devices are positioned between each of the pressing process. In this paper, the double-moving system including developed units using a multi-axial single-acting through this reduced the C/T(cycle time) and improved the productivity.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2007.11a
/
pp.390-391
/
2007
LED Packaging 과정 중 Die bond 재료로 Silver epoxy를 사용하여 Packaging 한 후 T3Ster 장비로 열 저항 값(Rth)을 측정하였다. Silver epoxy 의 접착 두께를 조절하여 열 저항 값을 측정하였고, 열전도도 값이 다른 Silver epoxy를 사용하여 열 저항 값을 측정하였다. Silver epoxy 접착 두께가 충분하여 Chip 전면에 고루 분포되었을 경우 그렇지 않은 경우보다 평균 4.8K/W 낮은 13.23K/W의 열 저항 값을 나타내었고, 열전도도가 높은 Silver epoxy 일수록 열전도도가 낮은 재료보다 평균 4.1K/W 낮은 12K/W의 열 저항 값을 나타내었다.
Nowadays there has been great interest in using heat treated cast material for press dies due to several advantages like reduction in die production costs. However, in hot press forming processes H13 forged tool steel is mostly used. Cooling performance of dies in hot press forming processes is considered as an important factor of study and also the IHTC parameter between cast material die and sheet metal should be considered as an essential. In the present study, the IHTC was calculated for the sheet metal in the hot press forming process with cast and forged material dies. The temperature measurements were performed for the sheet metal, casting and forged material dies by applying various contact pressure in hot press forming. IHTC was calculated and studied by adopting the inverse heat convection method in DEFORM-2D. Each IHTC was considered as a function of contact time and contact pressure. The experimental data were compared with calculated data obtained from the proposed equation and references.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.