• 제목/요약/키워드: Diamond wear

검색결과 259건 처리시간 0.025초

저순도 알루미나 예비소결체의 절삭유제에 따른 세라믹, CBN, 다이아몬드공구의 가공 특성 평가 (Evaluation of Wet Machining Characteristics of the Presintered Low Purity Alumina with the Ceramic, CBN and Diamond Tools)

  • 이재우
    • 한국정밀공학회지
    • /
    • 제24권2호
    • /
    • pp.33-40
    • /
    • 2007
  • In this study, presintered and full sintered low purity alumina ceramics were machined with various tools to clarify the effect of cutting fluid in machinability. The main conclusions obtained were as follows. When the presintered ceramics were wet machined with sintered diamond tool, the tool wear becomes extremely large, and higher cutting speed can be used than in the case of full sintered ceramics. The productivity of wet cutting with the sintered diamond tool is much higher than that of dry cutting. In the case of the CBN and ceramic tools, the tool wear were smaller at wet cutting than at dry cutting, especially exhibiting considerably larger grooved tool wear in wet cutting with ceramic tool.

표면거칠기 측정용 다이아몬드 촉침의 마모에 관한 연구 (A Study on the Wear of Diamond Stylus for Surface Roughness Measurement)

  • 한응교;노병옥;박두원;김종억
    • 한국정밀공학회지
    • /
    • 제8권3호
    • /
    • pp.105-113
    • /
    • 1991
  • The practicability of Ion-Sputter machining renders it possible to make diamond stylus for surface roughness measurement with micro stylus tip radius less than 2${\mu}mR$, and to measure surface roughness of fine-machined surface. In this study, we researched the wear or Ion-Sputtered stylus with 0.1${\mu}mR$ and 0.5${\mu}mR$ for micro-figure measurement and polished stylus with 0.5${\mu}mR$ according to measurement distance. As a result, we know that the case of Ion-Sputtered stylus is worn down easilier the case of polished stylus. And we know that in the evaluation of stylus wear, it is more useful method that examine the wear by measuring the variation of stylus tip radius than by evaluating the variation of Ra values.

  • PDF

PCD 초경 복합 원형 톱 개발과 공구마모 비교 (Development of Polycrystalline Diamond Tungsten Carbide Combination Circular Saw and Comparison of Tool Wear)

  • 주창민;박윤옥;김수진
    • 한국기계가공학회지
    • /
    • 제20권9호
    • /
    • pp.48-56
    • /
    • 2021
  • Tungsten carbide (WC) circular saws have been widely used to cut plywood. Recently, expensive polycrystalline diamond (PCD) were adopted to extend the tool life of circular saws. This study developed a PCD-WC combination circular saw and compared its performance with that of existing WC and PCD saws. Flank wear of WC saw blades and edge chipping of rectangular PCD was observed during the experiments. The PCD-WC saw replaced half of the chamfered teeth with PCD and applied tough WC for all rectangular teeth. In the experiments, edge chipping was not observed in rectangular WC teeth and the flank wear of chamfered teeth was decreased compared with that of conventional circular saws.

티타늄 코팅 된 다이아몬드 지립이 다이아몬드 공구의 성능에 미치는 영향 (Effect of Ti Coated Diamond Grit on Performance of Diamond Tool)

  • 임동필;임대순;민언기;임종관
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1997년도 제25회 춘계학술대회
    • /
    • pp.242-246
    • /
    • 1997
  • Diamond grit was coated with Ti by RF Sputtering to investigate the effect of coated diamond particles on performance of diamond impregnated saw. Coated and uncoated powders were separately mixed with 70Co-30W(wt %) powders by conventional milling technique. Hot pressing was carried out to make specimens. The wear test were carried out with these two types of diamond impregnated specimens. It was demonstrated that Ti coating was effective in improving the ability of grit retention and thus enhanced the tribological performance of diamond tool.

  • PDF

티타늄 코팅된 다이아몬드 지립이 다이아몬드 공구의 성능에 미치는 영향 (Effect of Ti Coated Diamond Grit on Performance of Diamond Tool)

  • 임동필;임대순;민언기;임종관
    • Tribology and Lubricants
    • /
    • 제13권3호
    • /
    • pp.102-107
    • /
    • 1997
  • Diamond grit was coated with Ti by RF Sputtering to investigate the effect of coated diamond particles on performance of diamond impregnated saw. Coated and uncoated powders were separately mixed with 70Co-30W powders by conventional milling technique. Hot pressing was carried out to make specimens. The wear test were carried out with these two types of diamond impregnated specimens. It was demonstrated that Ti coating was effective in improving the ability of grit retention and thus enhanced the tribological performance of diamond tool.

다이아몬드 코어드릴 공정의 구멍가공 특성과 모델링 (Drilling Characteristics and Modeling of Diamond Core Drilling Processes)

  • 윤관우;정성종
    • 한국공작기계학회논문집
    • /
    • 제17권4호
    • /
    • pp.95-103
    • /
    • 2008
  • Diamond core drills are applied to drill difficult-to-cut materials. This paper proposes basic understanding of ceramic drilling mechanics and characteristics of main factors affecting tool life, tool wear, cutting force, and chipping thickness. In contrast to conventional drilling, the core drilling process make deep grooves on the workpiece. One difficulty of it is the evacuation of chips from the drilled groove. As the drilling depth increases, an increased amount of chips tend to cluster together and clog the groove. Eventually severe wear develops and diamond grits are separated from the drill body. To relieve the clogging problem and to evacuate chips from the groove easily, the helical drilling process is applied for the core drilling process. To analyze drilling characteristics and derive optimal drilling conditions, tool life, tool wear, cutting force, and chipping thickness are quantified through the monitoring system and the Taguchi method. Mathematical models for the tool life and chipping thickness are derived from the response surface method. Optimal drilling database has been constructed through the experimental models.

무전해 니켈도금과 무전해복합도금(Ni-P-X, X: SiC, $Al_2$O$_3$, Diamond)의 내마모성 비교 (The Wear Resistance of Electroless Nickel and Electroless Composite(Ni-P-X, X: SiC, $Al_2$O$_3$, Diamond) Coating Layers)

  • 김만;장도연;정용수;노병호;이규환
    • 한국표면공학회지
    • /
    • 제27권4호
    • /
    • pp.193-206
    • /
    • 1994
  • A wear behavior of electroless (Ni-P-X, X: SiC, $Al_2O_3$, Diamond) composite coating layers, formed under various conditions on commerical grade low carbon steel, has been investigated using Taber abrasion tester and scanning electron microscope. Several factors, which are type of particles, co-deposited content, particle size, distribution of particles and heat-treatment, influenced the wear resistance. The wear resistance of the composited coating layers after heat-treatment at $400^{\circ}C$ for 1 hr was increased 70 times with diamond, 15 times with SiC and 8 times with $Al_2O_3$, compared with the electroless nickel plating layer without heat-treatment.

  • PDF

상대 마찰재에 따른 DLC 코팅의 트라이볼로지적 특성평가 (Influence of counter-bodies on the tribological behavior of diamond-like carbon coatings)

  • 이동춘;이진우;김석삼
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2003년도 학술대회지
    • /
    • pp.360-367
    • /
    • 2003
  • Diamond-like carbon(DLC) films are considerable research interest because of their widespread applications as protective coatings in areas such as optical windows, magnetic storage disks, car parts, biomedical coatings and as micro-electromechanical devices(MEMs). DLC films were deposited on WC-Co by PECVD using Ar, $C_2H_4$ gas. Tribological tests were conducted using a ball-on-disk type tribometer in dry air. Three kinds of counter-bodies balls were used. The counter-bodies balls are SM45C, SUJ2 and $ZrO_2$(3.17mm in diameter). Wear rate of the samples were calculated after measuring the worn-out volume of the wear track. As results wear test, the higher hardness of counter-bodies, friction coefficient low. As result of XPS estimation, wear debris generated as an oxide lower the friction coefficient.

  • PDF

초경합금상에 합성된 다이아몬드 박막의 부착력 특성 (Adhesion Characteristics of Diamond Thin Film on WC-Co Substrate)

  • 이상희;박상현;이덕출
    • 한국전기전자재료학회논문지
    • /
    • 제14권7호
    • /
    • pp.584-589
    • /
    • 2001
  • Diamond thin films were synthesized on WC-Co substrate by RF PACVD(radio frequency plasma-assisted chemical vapor deposition) technique with H$_2$-CH$_4$-O$_2$ gas mixture. WC-Co substrate was pre-treated in HNO$_3$solution, scratched with 3$\mu\textrm{m}$ diamond paste and exposed in the O$_2$ plasma before deposition. The diamond thin film prepared at 11% oxygen concentration showed the best quality of good adhesion and wear resistance at various oxygen concentration with the fixed 5% CH$_4$ concentration.

  • PDF

강 표면의 다이아몬드/몰리브데늄/니켈 복합층의 생성 (Formation of Diamond/Mo/Ni Multi-Layer on Steel Substrate)

  • Lee, H.J.;J.I. Choe;Park, Y.
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2002년도 춘계학술발표회 초록집
    • /
    • pp.37-37
    • /
    • 2002
  • Diamoncl/Mo/Ni multi-layers on SKH-51 steel substrate was prepared to improve the abrasive wear resistance of a tool and die by a commercial chemical vapor deposition unit and electro-plating. The diamond after 7 hour deposition had cuba-octahedral structure with 2~5$\mu\textrm{m}$ grains. The existence of non-ferrous metals such as chromium, nickel and molybdenum between diamond and SKH-51 substrate results in forming higher quality of diamond layer by retarding carbon diffusion in the diamond layer during deposition, and also improving hardness and wear resistance. Surface cracks on the film was sometimes observed by the difference of by the thermal expansion coefficients between the steel substrate and the deposited layers during cooling.

  • PDF