• 제목/요약/키워드: Dentin surface treatment

검색결과 112건 처리시간 0.02초

다양한 치은 연하 수복물에 대한 치은 섬유아 세포 부착 연구 (Attachment of Human Gingival Fibroblast to Various Subgingival Restorations;A Comparative Study in Vitro)

  • 이은숙;송인택;임정수;김형섭
    • Journal of Periodontal and Implant Science
    • /
    • 제29권3호
    • /
    • pp.621-636
    • /
    • 1999
  • When mucoperiosteal flaps are positioned and sutured to desirable position, the wound contains several interface between tissues which differ fundamentally in composition & biological reaction. Thus the C-T surface of the flap will, on one hand, oppose another vascularized surface, and on the other, the avascular dental material for example, when root resoptions, fractured root, endodontic perforation, deep root carious lesions were filled with amalgam, glass ionomer, resin etc. Recently, a number of case report described the successful treatment of a subgingival root lesion with restorative material & free gingival graft, open flap surgery, but more objective research was needed . Most of study on restorative materials were concerned for cytotoxicity not for actual healing event on that materials and its influencing factors such as biocompatibility, surface wettability, surface topography . The aim of this in vitro study was to evaluate the effect of amalgam, resin modified glass ionomer, composite resin per se, and their surface roughness on the growth of human gingival fibroblast. The cells were obtained and placed on culture flask and incubated for 3 days with the prepared test materials. Then count the attached cell number with hemocytometer,(n=12) and 2 samples were examined with SEM about attachment cell morphology . Another 4 samples were evaluated on their surface roughness with Talysurf and average surface roughness value(Ra) were obtained. Statistical difference in attached cell number, roughness value were analyzed using ANOVA. The number of attached cell was as follows, for root dentin specimen 16.7${\pm}$4.41, resin modified glass ionomer 14.0${\pm}$4.15, resin 8.13${\pm}$3.63, amalgam 0.72${\pm}$3.33(${\times}10^3$). Between root dentin and resin-modified glass ionomer, no significant difference was observed, but resin, amalgam showed a significant less cell numbers than for root dentin, resin modified glass ionomer cement. SEM examination expressed many cell surface attachment apparatus in root dentin and resin modified glass ionomer specimens. For resin specimen, cell attachment was observed but exposed less appratus. The average surface roughness value are following results. Dentin specimen 0.6972${\pm}$ 0.104, resin modified glass ionomer 0.0822${\pm}$0.009, resin 0.0875${\pm}$0.005, amalgam 4.2145${\pm}$0.985(${\mu}m$). Between root dentin, resin-modified glass ionomer, and resin, no significant difference was observed, but amalgam showed a significant more rough surface than other groups. When evlauated the interrelationship between cell attachment and surface roughness, therefore, there was weak reverse correlation.(pearson correlation : - 0.593) These results suggest that resin modified glass ionomer have the favorable healing potential when used for subgingival restoration. And for relationship between cell attachment and surface characteristics, further investigations were needed.

  • PDF

염산테트라싸이클린으로 처리한 치근면의 치은상피세포부착에 관한 연구 (Effect of tetracycline-HCl root conditioning on gingival epithelial cell attachment to root surface)

  • 황나영;박병기;김상목;국중기;박주철;김병옥
    • Journal of Periodontal and Implant Science
    • /
    • 제32권1호
    • /
    • pp.13-23
    • /
    • 2002
  • The ultimate goal of periodontal therapy is directed to arresting the progression of the disease, and regenerating the fibrous attachment. In order to achieve such treatment aim, the plaque and calculus must be eliminated and the physiological conditions of the root surface must be changed to facilitate the attachment and migration of the new fibroblasts, The method of changing the proper root surface conditions to promote the healing of periodontal tissue involves mechanical procedures, such as scaling and root planing, and chemical procedures such as tetracycline-HCl. However, the formation of a long junctional epithelium was most frequently observed type of healing. Thus, the aim of this study was to examine in vitro the influence of surface conditioning of dentin by TC-HCl on human gingival epithelial cell attachment. Human gingival epithelial cells were obtained from healthy retromolar pad area(under the age 23 years). Seventy two teeth extracted from severe periodontitis were used as study material. To evaluate the epithelial cell attachment to dentin, the prepared specimen was divided to four groups. For the control group, only scaling and root planing were carried out, and for the test group, 1 to 3, the concentration of the TC-HCl was 50, 125 and 250mg/ml respectively. After cell cultivation time of 1-, 3-. 24 hour, for the indirect quantitative assessment of gingival epithelial cell attached to dentin sample, the absorbance of epithelial cell unattached to dentin was measured. The results were as follows; 1. There was no statistically significant difference between scaling and root planing group and TC-HCl 50mg/ml 125mg/ml and 250mg/ml group about absorbance of unattached epithelial cell to dentin sample(p>0.5). 2. As time passes, the absorbance of unattached gingival epithelial cell to dentin sample was decreased statistically significant(p<0.05). 3. There was no statistically significant difference among the TC-HCl group(p>0.05) We concluded that there was similar effect on gingival epithelial cell attachment between TC-HCl conditioning on root surface and only scaling and root planing treatment

Dentin permeability change according to the process of compomer restoration treatment

  • Cho, Hye-Jin;Lee, Kwang-Won;Lee, Se-Jun
    • 대한치과보존학회:학술대회논문집
    • /
    • 대한치과보존학회 2001년도 추계학술대회(제116회) 및 13회 Workshop 제3회 한ㆍ일 치과보존학회 공동학술대회 초록집
    • /
    • pp.591.2-591
    • /
    • 2001
  • Microleakage of restorative materials has been investigated mostly by dye penetration method. Dye penetration method was not quantitative and not measured repeatedly. Fluid filtration method was used to research purpose to understand the effects of various restorative treatments on dentin permeability. The purpose of this study was to evaluate of dentin permeability according to the process of compomer restoration treatment. In this study, C1 V cavities were prepared on buccal surface of thirty extracted human molars. The prepared cavities were etched by 37% phosphoric acid.(omitted)

  • PDF

경화된 상아질의 접합 양상에 관한 주사전자현미경적 연구 (A SCANNING ELECTRON MICROSCOPIC STUDY OF BONDING ASPECTS TO THE SCLEROTIC DENTIN)

  • 이린;이형일;이광원;손호현
    • Restorative Dentistry and Endodontics
    • /
    • 제22권1호
    • /
    • pp.228-243
    • /
    • 1997
  • The changes of microstructures, morphology of sclerotic dentin and bonding aspects generated by an adhesive resin was investigated. Incisors and premolars showing natural cervical abrasions were collected and conditioned with 10 % phosphoric acid or 10 % maleic acid. The sclerotic dentin specimens were then rinsed and blot-dried and applied with dentin adhesive (All Bond 2) to the conditioned dentin surface. To examine the morphologic change of the sclerotic dentin specimen after etching and bonding procedure, the treated specimens were examined by SEM. To analyze the chemical composition of sclerotic dentin and crystals occluding dentinal tubules, the sclerotic dentin specimen was powdered and examined with X-ray Diffractometer. To investigate the Ca/P weight percent ratio within the dentinal tubules, the sclerotic dentin specimen was fractured perpendicularly to the long axis of the tooth from the center of cervical abrasion lesion and then examined with EDX(Energy Dispersive X-ray) microanalyzer. The results were as follows : 1. The increased width of peritubular dentin and the depositions of the irregular amorphous materials within the dentinal tubules were showed in the sclerotic dentin specimens. 2. After the treatment of sclerotic dentin specimen with 10 % phosphoric acid or 10 % maleic acid, the lateral side of tubules rather than cross-sectional tubule openings was showed exclusively at the incisal and gingival incline of the specimens. 3. After the treatment of sclerotic dentin specimen with 10 % phosphoric acid or 10 % maleic acid, the hybrid layer was not formed evidently and the resin tag was not formed or shortly penetrated into the tubules with the thinner diameter. 4. According to the results of XRD analysis of the sclerotic dentin specimen, Hydroxyapatite and Octacalcium phosphate were predominent, however, Whitlockite crystals were rare. 5. The mean Ca/P weight percent ratio analysed from 5 fractured sclerotic dentin specimens was $2.322{\pm}0.170$ at the intertubular dentin, $1.826{\pm}0.051$ within the dentinal tubule.

  • PDF

PDGF-BB 적용시간이 decalcified dentin에서의 치은섬유아세포의 증식에 대한 효과 (The Influence of PDGF-BB Application Time on the Proliferation of HGF Using Decalcifed Dentin)

  • 박진우;이재목;서조영
    • Journal of Periodontal and Implant Science
    • /
    • 제26권4호
    • /
    • pp.873-887
    • /
    • 1996
  • Platelet-derived growth factor(PDGF) is one of the polypeptide growth fators. PDGF has been reported as a biological mediator which regulates activities of wound healing process including the cell proliferation, migration and metabolism. Recent studies indicated that demineralized root surface as the primary site for growth factor application has advantages over other application method, especially due to binding capacity of growth factor for exposed matrix component of deminera1ized dentin surface. The purpose of this study is to evaluate optimal application time of PDGF-BB on proliferation of human gingival fibroblasts using deminera1ized dentin surface as primary application site. Human gingival fibroblasts and dentin slabs were prepared from the first premolar tooth extracted for the orthodontic treatment, cells were cultured in DMEM/I0% FBS at the $37^{\circ}C$, 5% CO2 incubator. All of the dentin slabs were preconditioned with Tetracycline HCI(100mg/ml) solution and rinsed in PBS. In the cell proliferation experiment, experimental group was immersed in DMEM containing 10% FBS, 50ng/rnl PDGF-BB during different time(30sec, 1, 2, 4, 8 minutes) and dried. Cells at concentration of $1{\times}10^5$cells/ml were seeded in each culture well which contained dentin slabs and incubated for 6 hours. Then, all of the dentin slabs were moved into new 24 well culture dish and incubated for 24, 48, 72 hours. The cell counting was done by hemocytometer with inverted phase contrast microscope after trypsinization. The results were as follows : The application of PDGF-BB for 1, 2 min slightly increased the number of gingival fibroblasts, and the application of PDGF-BB for 4, 8 min prominently increased the number of gingival fibroblasts. The application of PDGF-BB for 4 min showed maximum proliferation rate of gingival fibroblasts at 24, 48, 72 hours, and the application of PDGF-BB for 8 min showed less proliferation rate of gingival fibroblasts compared to the application of PDGF-BB for 4 min at 24, 48, 72 hours. In conclusion, the application of PDGF-BB for 4 min appeared to be optimal to obtain maximum proliferation of gingival fibroblasts using demineralized dentin surface as primary applicaton site of PDGF-BB.

  • PDF

수종 상아질 표면처리제에 의한 레진 침투 및 전단결합강도에 관한 연구 (A STUDY ON THE RESIN IMPREGNATION AND SHEAR BOND STRENGTH BY VARIOUS DENTIN CONDITIONERS)

  • 이광원;이명종
    • Restorative Dentistry and Endodontics
    • /
    • 제15권1호
    • /
    • pp.201-216
    • /
    • 1990
  • A variety of surface pre-treatments have been advocated to prepare the dentin prior to placement of a bonding agent. The purpose of this study was to evaluate the effect of various dentin conditioners upon the degree of resin impregnation to the dentinal tubules and the shear bond strength of a new dentinal bonding agent (Scotchbond 2) used in conjunction with a visible light cured composite (Silux). The healthy eighty human molars extracted due to periodontal or orthodontic reasons were used and randomly divided into five groups. All the grinded dentin surfaces were conditioned with 3% $H_2O_2$, Cavity Cleanser (Columbus/Bayer), Dentin Conditioner (GC Inter. Corp.), Scotchprep (3M Co.) according to the manufacturer's directions. The specimens were then demineralized in 10% HCl for 20 sec. and 24 hrs. in order to observe the resin tags in Hitachi X-450 scanning electron microscope at 25KV. Also, shear strengths were obtained using an Instron Testing Machine with a cross head speed of 1 mm/min. The following results were obtained ; 1. In group treating with Dentin Conditioner and Scotchprep, the resin strings were formed on most of the surfaces and penetrated more than $50{\mu}m$ into the tubules. 2. The inner surface of resin treated with Cavity Cleanser, indicating the resin strings formed partly and penetrated about in depth of $30{\mu}m$. 3. In control and experimental group treated with 3% $H_2O_2$, the resin tags were not formed, if any, penetrated shortly. 4. Shear bond strengths in groups treating with Dentin Conditioner and Scotchprep were statistically significant increase than with 3% $H_2O_2$. (P<0.01). 5. The Scotchprep treatment group was significantly higher in shear strength than groups treated with no conditioning and Cavity Cleanser.(P<0.01) 6. Shear bond strengths evaluated were gradually increase in proportion to the tag length of resin impregnation.

  • PDF

Nd : YAG 레이저가 상아질 및 도재와 복합레진간의 결합강도에 미치는 영향 (AN EFFECT OF ND : YAG LASER ON THE BONDING STRENGTH OF COMPOSITE RESIN TO DENTIN AND PORCELAIN)

  • 우금진;양홍서
    • 대한치과보철학회지
    • /
    • 제35권2호
    • /
    • pp.385-399
    • /
    • 1997
  • The purpose of this experiment was to determine the effects of etching with a Nd : YAG Laser on dentin, or porcelain surface on the bond strength with composite resin. The dentin specimens were devided into the following 4 groups. D1 : No treatment D2 : Etched with 10% phosphoric acid D3 : Laser etchded with 1W, 20PPs D4 : Laser etched with 2W, 20PPS The procelain specimens were devided into the following 4 groups. P1 : diamond roughened P2 : etched with HF acid P3 : Laser etched with 2W, 20PPS P4 : Laser etched with 3W, 20PPS All specimens were veneered with resin. One half of the specimens were stored in $37^{\circ}C$ water for one day and the other half were thermocycled 1000 times at temperature of $5^{\circ}C\;to\;55^{\circ}C$ at 20 seconds intervals. After that, the bonding strength of composite resin to the dentin and porcelain was measured. The surface treated state and fractured state were observed with SEM. The following results were obtained. 1. In the dentin specimens, the bond strength of group D2 was highter than that of groups D1 and D3 in the case of the specimens stored in $37^{\circ}C$ water for one day, there was a statistically significant difference between group D2 and D1, D3 (P<0.05). The bonding strength of the specimens that were thermocycled decreased in the following order : group D2,D4,D3 and then D1. 2. In the porcelain specimens, the bonding strength of groups P1,P2 were higher than that of group P3 in the case of the specimens stored in $37^{\circ}C$ water for one day (P<0.05). The bonding strength of the specimens of being thermocycled decreased in the following order : group P2,P1,P4 and then P3. 3. The groups of high bond strength had a rougher surface and a high level of microporosity with SEM findings.

  • PDF

타액에 오염된 상아질에 대한 콤포머의 접합양상 (THE ADHESIVE PATTERNS OF COMPOMER TO SALIVA-CONTAMINATED DENTIN)

  • 조영곤;김병태;이석종
    • Restorative Dentistry and Endodontics
    • /
    • 제25권4호
    • /
    • pp.575-586
    • /
    • 2000
  • In this study, adaptation of compomer to saliva contaminated dentin was evaluated with scanning electron microscope(SEM) and confocal laser scanning microscope(CLSM). For the SEM study, the occulusal surfaces of thirty two molar teeth were grounded to exposure dentin surfaces. The specimen were randomly assigned to control and three experimental groups with four samples in each group. In control group, Dyract and F-2000 compomer were bonded on the specimens according to the manufactures direction. Experimental groups were subdivided into three groups. They were contaminated with saliva on dentin surfaces ; Experimental group 1 : Saliva was dried with compressed air. Experimental group 2 : Saliva was rinsed with air-water spray and dried. Experimental group 3 : After polymerization of an adhesive, they were contaminated with saliva, and then saliva was rinsed with air-water spray and dried. Dyract and F-2000 compomer were bonded on saliva-treated dentin surfaces. The interfaces between dentin and compomer were observed with SEM. For the CLSM study, Class V cavities were prepared in buccal and ligual surfacess of thirty two molars. The specimens were divided into control and experimental groups. Class V cavities in experimental group were contaminated with saliva and those surfaces in each experimental groups received the same treatments as for the SEM study. Cavities were applied Prime & Bond 2.1 and F-2000 compomer primer/adhesive that were mixed with fluorescein, and then were filled with Dyract and F-2000 compomer. Specimens were embedded in transparent acrylic resin and sectioned buccolingual1y with diamond wheel saw, and then mounted on cover slide for CLSM study. The interface between cavity and compomer was observed by fluoresence imaging with a CLSM. The results were as follows : 1. In SEM exammination of Dyract group, control group, experimental group 2, 3 showed close adaptation to dentin and hybrid layer of $3{\sim}4{\mu}m$ diameter. Interfacial gap between compomer and dentin in experimental group 1 was wider than in control group. 2. In SEM examination of F-2000 group, adaptation to dentin of control group was closer than Dytact control group, but hybrid-like layer was not observed. Interfacial gap between compomer and dentin in experimental group 1 was wider than in Dyract experimental group 1. 3. In dissolution specimens of Dyract and F-2000 group, resin tags penetrated through dentinal tubules in control group and experimental group 1 and 3, but the penetration of resin tag was irregular and partial in experimental group 1. 4. In CLSM exammination of Dyract and F-2000 group, adhesive patterns of control and experimental groups showed same as in SEM. This result suggests the treatment methods, rinsing & drying, repeating all adhesive procedures, will produce good effect on adaptation of compomer to dentin if the dentin surface or polymerized adhesive is contaminated by saliva.

  • PDF

비교원성 단백질이 상아질 접착제의 결합강도와 교원질의 형태에 미치는 영향 (THE EFFECT OF THE REMOVAL OF CHONDROITIN SULFATE ON BOND STRENGTH OF DENTIN ADHESIVES AND COLLAGEN ARCHITECTURE)

  • 김종률;박상진;최기운;최경규
    • Restorative Dentistry and Endodontics
    • /
    • 제35권3호
    • /
    • pp.211-221
    • /
    • 2010
  • 본 연구는 상아질의 비교원성 단백질을 chondroitinase ABC (C-ABC)를 이용하여 제거함으로써 비교원성 단백질의 제거가 상아질 접착제의 미세인장결합강도와 교원질망의 형태에 미치는 영향을 상아질의 다양한 습윤상태에 따라 평가하고자 시행하였다. 비교원성 단백질의 상아질접착제의 미세인장강도에 대한 영향을 평가하기 위해 제 3대구치의 상아질을 노출시키고, 두 군으로 나누고 한 군은 C-ABC, 다른 군은 증류수를 $37^{\circ}C$에서 48시간 동안 적용한 후, 상아질의 습윤상태(wet, dry 및 re-wet)와 상아질 접착제(Single Bond 2, One Step Plus)를 다르게 이용하여 복합레진을 수복하였다. 24시간 후 가로 1 mm, 세로 1mm의 시편을 제작하고 미세인장강도를 측정하였다. 상아질 교원질의 형태변화를 관찰하기 위하여 상아질 시편에 산부식을 시행하고 C-ABC 적용 후, 시편을 제작하였고 미세인장강도 측정후 파괴된 접착면의 파괴양상과 각 접착제의 접착계면 관찰을 위하여 FE-SEM 관찰하였다. C-ABC 처리여부와 관계없이 습윤한 상아질면에 접착한 군은 모든 접착제에서 통계학적으로 유의성있는 미세인장결합강도의 차이를 나타나지 않았다(p > 0.05). C-ABC를 적용하였을 경우, Single Bond 2에서는 재수화한 상아질면에 접착한 군이 습윤한 상아질면에 접착한 군에 비해 미세인장결합강도가 감소하였다(p < 0.05). FE-SEM 관찰결과, C-ABC를 적용후에는 접착성 파괴가 주로 일어났으며, 교원질 섬유간 거리가 증가하였으며 부분적으로 교원질 섬유들간에 응집된 양상이 관찰되었다.

Microshear bond strength according to dentin cleansing methods before recementation

  • Tasar, Simge;Ulusoy, Mutahhar Muhammed;Meric, Gokce
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권2호
    • /
    • pp.79-87
    • /
    • 2014
  • PURPOSE. The aim of this study was to determine the efficiency of Erbium, Chromium: Yttrium-Scandium-Gallium-Garnet laser in different output powers for removing permanent resin cement residues and therefore its influence on microshear bond strength compared to other cleaning methods. MATERIALS AND METHODS. 90 extracted human molars were sectioned in 1 mm thickness. Resin cement was applied to surface of sliced teeth. After the removal of initial cement, 6 test groups were prepared by various dentin surface treatment methods as follows: no treatment (Group 1), ethylene diamine tetra acetic acid application (Group 2), Endosolv R application (Group 3), 1.25 W Erbium, Chromium:Yttrium-Scandium-Gallium-Garnet laser irradiation (Group 4), 2 W Erbium, Chromium:Yttrium-Scandium-Gallium-Garnet laser irradiation (Group 5) and 3.5 W Erbium, Chromium:Yttrium-Scandium-Gallium-Garnet laser irradiation (Group 6). The topography and morphology of the treated dentin surfaces were investigated by scanning electron microscopy (n=2 for each group). Following the repetitive cementation, microshear bond strength between dentin and cement (n=26 in per group) were measured with universal testing machine and the data were analyzed by Kruskal Wallis H Test with Bonferroni correction (P<.05). Fracture patterns were investigated by light microscope. RESULTS. Mean microshear bond strength ${\pm}$ SD (MPa) for each group was $34.9{\pm}17.7$, $32.1{\pm}15.8$, $37.8{\pm}19.3$, $31.3{\pm}12.7$, $44.4{\pm}13.6$, $40.2{\pm}13.2$ respectively. Group 5 showed significantly difference from Group 1, Group 2 and Group 4. Also, Group 6 was found statistically different from Group 4. CONCLUSION. 2 W and 3.5 W Erbium, Chromium: Yttrium-Scandium-Gallium-Garnet laser application were found efficient in removing resin residues.