• 제목/요약/키워드: Dental internal fit

검색결과 68건 처리시간 0.024초

코발트-크롬 합금으로 제작된 금속-도재관의 적합도 평가 (Evaluation of fitness of metal-ceramic crown fabricated by cobalt-chrome alloy)

  • 김재홍;김원수;김기백
    • 한국치위생학회지
    • /
    • 제13권2호
    • /
    • pp.361-368
    • /
    • 2013
  • Objectives : The purpose of this in vitro study was to evaluate the effect of firing cycles on the marginal and internal fit of metal ceramic crown. Methods : Ten same cases of stone models (abutment teeth 11) were manufactured. Ten cobalt-chrome cores were made per each models and the marginal and internal fit was evaluated through a silicone replica technique. The marginal and internal fit of specimens was measured twice. The first measurement was done after manufacturing cobalt-chrome alloy core and the second measurement was done after porcelain firing. T-test of paired sample for statistical analysis was executed with SPSS 12.0K for Windows (${\alpha}$=0.05). Results : Mean(SD) marginal and internal fit were 77.1(23.3) ${\mu}m$ for the cobalt-chrome alloy core group and 84.4(21.9) ${\mu}m$ for the metal-ceramic crown group. They were statistically significant differences between groups for marginal and internal fit (p<.05). Conclusions : All metal ceramic crowns showed marginal and internal fit ranged within the current clinical recommendations.

SLM 방식으로 제작한 도재관 금속하부구조물의 변연 및 내면 적합도 평가 (Evaluation of marginal and internal fit of metal copings fabricated by selective laser melting)

  • 배성령;이하빈;노미준;김지환
    • 대한치과기공학회지
    • /
    • 제45권1호
    • /
    • pp.1-7
    • /
    • 2023
  • Purpose: To evaluate the marginal and internal fit of metal coping fabricated by a metal three-dimensional (3D) printer that uses selective laser melting (SLM). Methods: An extraoral scanner was used to scan a die of the prepared maxillary right first molar, and the coping was designed using computer-aided design software and saved as an stereo lithography (STL) file. Ten specimens were printed with an SLM-type metal 3D printer (SLM group), and 10 more specimens were fabricated by casting the castable patterns output generated by a digital light processing-type resin 3D printer (casting the 3D printed resin patterns [CRP] group). The fit was measured using the silicon replica technique, and 8 points (A to H) were set per specimen to measure the marginal (points A, H) and internal (points B~G) gaps. The differences among the groups were compared using the Mann-Whitney U-test (α=0.05). Results: The mean of marginal fit in the SLM group was 69.67±18.04 ㎛, while in the CRP group was 117.10±41.95 ㎛. The internal fit of the SLM group was 95.18±41.20 ㎛, and that of the CRP group was 86.35±32 ㎛. As a result of statistical analysis, there was a significant difference in marginal fit between the SLM and CRP groups (p<0.05); however, there was no significant difference in internal fit between the SLM group and the CRP group (p>0.05). Conclusion: The marginal and internal fit of SLM is within the clinically acceptable range, and it seems to be applicable in terms of fit.

시멘트 공간이 적층 가공으로 제작한 지르코니아 하부구조물의 변연 및 내면 적합도에 미치는 영향 (Effect of cement space on marginal and internal fit of a zirconia core fabricated using by additive manufacturing)

  • 민지원;김세연;김재홍
    • 대한치과기공학회지
    • /
    • 제46권1호
    • /
    • pp.1-7
    • /
    • 2024
  • Purpose: The goal of this study was to determine the clinical acceptability of various cement space settings for the marginal and internal fit of a zirconia core manufactured using additive manufacturing. Methods: The maxillary right incisor served as the master model. After scanning the maxillary right incisor with a dental 3D (three-dimensional) scanner, the stereo lithography file was created using different cement space settings of 40, 120, and 200 ㎛ using computer-aided design software (Dental System 2018; 3Shape). The marginal and internal fit of the 3 groups were determined using the silicon replica technique. Measurement points were divided into the following three categories: margin, axial wall, and incisal. To ensure more accurate measurements, these three measurement points were divided into 8 points. The Shapiro-Wilk, one-way ANOVA, and Tukey's honestly significant difference test (for all tests α=0.05) were the statistical analyses that were included in the study. Results: The CS (cement space)-200 group had better marginal and internal fit than the CS-40 and CS-120 groups, and there were statistically significant differences at the marginal and incisal points, except for the axial wall points. CS-200 group, both marginal and internal fit were within 120 ㎛, which is the clinically acceptable value. Conclusion: This study suggests that a 200 ㎛ cement space setting is ideal for optimal marginal and internal fit of 3D-printed ceramic crowns.

베릴륨이 함유되지 않은 니켈-크롬 합금 코어와 코발트-크롬 합금 코어의 적합도 비교평가 (Comparison of the marginal and internal fit of cores fabricated by Ni-Cr alloy(non-beryllium) and Co-Cr alloy)

  • 김기백;김재홍;김웅철;김지환
    • 대한치과기공학회지
    • /
    • 제34권4호
    • /
    • pp.353-359
    • /
    • 2012
  • Purpose: The aim of this study measured and compared the marginal and internal fit of metal cores with two base metal alloy (Ni-Cr alloy(non-beryllium), Co-Cr alloy). Methods: Maxillary right first molar abutment fabricated by titanium was prepared for this study. Impressions(10ea) were made from titanium model, and study models were poured with improved dental stone. Wax cores of twenty were prepared for burn-out and casting. Ten wax cores cast Ni-Cr alloy(non-Be), and finally ten cast Co-Cr alloy. Marginal and internal fit of cores was evaluated using silicone replica technique and digital microscope(x160). The data were statistically analyzed with the independent samples t-test (${\alpha}$ <.05). Results: Mean(standard deviation, SD) marginal and internal fit total size of Ni-Cr alloy(non-Be) group was $73.3(14.4){\mu}m$ and of Co-Cr alloy group $65.6(17.4){\mu}m$. The marginal and internal fit total size of Ni-Cr alloy group(non-Be) was statistically significantly greater than that of Co-Cr alloy group (P=.004). Conclusion: Co-Cr alloy cores in this study had a better marginal fit than Ni-Cr alloy(non-Be) cores.

금속 밀링과 직접 금속 레이저 소결 방식으로 제작한 3본 코발트-크롬 구조물의 변연 및 내부 적합도 비교 평가 (Comparative evaluation of marginal and internal fit of three-unit Co-Cr frameworks fabricated by metal milling and direct metal laser sintering methods)

  • 안재석;이정환
    • 대한치과기공학회지
    • /
    • 제42권2호
    • /
    • pp.81-89
    • /
    • 2020
  • Purpose: This in vitro study was conducted to evaluate the marginal and internal fit of three-unit Co-Cr frameworks fabricated by computer-aided metal milling and direct metal laser sintering(DMLS) systems in comparison to conventional casting method. Methods: Three-unit Co-Cr frameworks were fabricated by conventional wax up with casting(CWC), computer-aided metal milling(MM) and direct metal laser sintering(DMLS)(n=10 each). The marginal and internal fit of specimens were examined using a light-body silicone impression material. The thickness of light-body silicone was measured at eight reference points each, divided in the mesio distal and bucco lingual directions. All measurements were conducted by a stereomicroscope. Digital photos were taken at 150× magnification and then analyzed using a measurement software. The Kruskal-Wallis test and Bonferroni correction were used for analyzing the results. Results: The mean(SD) is ㎛ for fabrication methods, the mean marginal fit were recorded respectively, DMLS 39(27), followed by CWC 63(38), MM 220(128). and the mean internal fit CWC 95(47), DMLS 116(49), MM 210(152). In addition, the largest gap was found in the occlusal surface area among the internal measurement areas of all groups. Conclusion: As a result, the direct metal laser sintering method showed better marginal and internal fit than the metal milling method. The marginal and internal fit were statistically different according to the three fabrication methods(p<0.001). Except the MM group, the marginal fit of the CWC and DMLS groups was below the clinical standard of 120 ㎛. Based on the results of this study, it can be applied to clinical use in the future.

치과 CAD/CAM 가공방식에 따른 임시보철물의 내면 적합도 : 3차원 중첩 분석 (Internal evaluation of provisional restorations according to the dental CAD/CAM manufacturing method : Three-dimensional superimpositional analysis)

  • 김재홍;김기백
    • 대한치과기공학회지
    • /
    • 제41권2호
    • /
    • pp.81-86
    • /
    • 2019
  • Purpose: The purpose of the present study was to compare the internal fit of two different temporary restorations fabricated by dental CAD/CAM system and to evaluate clinical effectiveness. Methods: Composite resin tooth of the maxillary first molar was prepared as occlusal reduction(2.0mm), axial reduction(1mm offset), vertical angle(6 degree) and chamfer margin for a temporary crown and duplicated epoxy die was fabricated. The epoxy dies were used to fabricate provisional restorations by CAD/CAM milling technique or 3D-printing technique. The inner data from all crowns were superimposed on the master die file in the 'best-fit alignment' method using 3D analysis software. Statistical analysis was performed using a Wilcoxon's rank sum test for differences between groups. Results: It showed that the internal RMS(Root Mean Square) values of the additive group were significantly larger than those of other group. No significant differences in internal discrepancies were observed in the temporary crowns among the 2 groups with different manufacturing method. Conclusion: All the groups had the internal fit within the clinical acceptable range (< $50{\mu}m$). The continuous research in the future to be applied clinically for the adaptation of additive manufacturing technique are needed.

광간섭단층영상기를 이용한 치과용 지르코니아 코어의 적합도 분석 (Analysis of the Marginal and Internal Fit of Dental Zirconia Core Using Optical Coherence Tomography(OCT))

  • 김재홍;김기백
    • 한국콘텐츠학회논문지
    • /
    • 제12권8호
    • /
    • pp.240-247
    • /
    • 2012
  • 보철물이 구강 내 제 기능을 하기 위해 가장 중요한 요소 중 하나는 적합도이다. 본 연구의 목적은 그 동안 시도되지 않았던 광간섭단층영상기를 이용하여 비파괴적인 방법으로 적합도를 측정해보고, 측정된 값을 기존의 방법으로 측정된 값과 비교하여 보고자 한다. 실험을 위해 상악 우측 중절치가 지대치인 석고모형 10개를 제작하고 치과용 캐드캠으로 각각의 모형에 해당하는 지르코니아 코어를 10개 제작하였다. 시편 당 5부위 씩 광간섭단층영상기로 적합도를 측정하고, 같은 부위를 기존의 방법인 실리 복제본 기술로 측정하였다. 두 집단 간의 평균 값에 유의한 차이가 있는지 알아보기 위해 독립표본 t-검정을 실시하였다(${\alpha}$=0.05). 그 결과 측정된 두 집단 간의 평균 값에는 유의한 차이를 보이지 않았고(P>0.05), 이러한 결과로 미루어 볼 때 앞으로 광간섭단층영상기를 이용한 보철물의 적합도 측정이 가능할 것으로 사료된다.

왁스 밀링 방법 및 디지털 광 프로젝션 방법으로 제작된 3본 금속 구조물의 적합도 비교 (Comparison the fit of three-unit metal framework fabricated by wax milling method and digital light projection method)

  • 이정환;안재석
    • 대한치과기공학회지
    • /
    • 제41권1호
    • /
    • pp.9-19
    • /
    • 2019
  • Purpose: This study was conducted to comparative evaluate the marginal and internal gap of three-unit metal frameworks(Co-Cr) fabricated by wax milling method and digital light projection method of CAD/CAM systems. Methods: All the specimens were fabricated by three different fabrication methods: conventional wax up with casting(CWC), milled wax block with casting(MWC), digital light projection with casting(DLPC) (n=10 each). The marginal and internal fits of specimens were examined using a replica technique. The light-body silicone thickness was measured at 8 reference points(each abutment: 16 measurements). All measurements were conducted by a stereomicroscope. Digital photo were taken at $150{\times}$ magnification and then analyzed using a measurement software. The Mann-Whitney test was used for analyzing the results. Results: Statistically significant differences were found between the fabrication methods(p<0.001). The mean(SD) is ${\mu}m$ for fabrication methods, the mean marginal fit were recorded respectively, CWC 63(38), MWC group 50(33), DLPC 103(54) and the mean internal fit CWC 96(47), MWC group 116(41), DLPC 138(66). Conclusion : The marginal and internal fit were statistically different according to the fabrication methods(p<0.001). In all fabrication methods, the greatest misfit was found the occlusal area of all specimens.

시멘트 공간이 캐드캠 시스템으로 제작한 지르코니아 수복물의 변연과 내부 적합도에 미치는 효과 (Effect of cement space on the marginal and internal fit of zirconia restorations fabricated by CAD/CAM system)

  • 이정환;안재석
    • 대한치과기공학회지
    • /
    • 제39권4호
    • /
    • pp.235-242
    • /
    • 2017
  • Purpose: The aim of this study was to evaluate the marginal and internal gap of zirconia copings fabricated by CAD/CAM system and to research the effect of cement space on the fit of zirconia prosthesis. Methods: Zirconia copings were designed using 3shape software and then milled from presintered zirconia blocks by Kavo dental milling machine. The cement space was set at $0{\mu}m$ around the margins for all groups, and additional cement space appling 1 mm above the finish lines of tooth. The samples were classified into 4 groups according to the cement space setting(Cs-0, Cs-40, Cs-80, Cs-120). Replica technique used to investigate marginal and internal gap. The silicone film thickness was recorded using a optical microscope with image software analysis system at 75${\times}$magnification. The assessment performed on the six points in bucco-lingual and mesio-distal sections(4 groups, 10 copings per group, 12 measuring points per coping). The data were statistically analyzed with one-way ANOVA followed by pair-wise Tukey's post hoc tests(${\alpha}$<0.05). Results: Better marginal and internal fit values were exhibited by $80{\mu}m$ cement space. The results showed that different cement space values had statistically significant effect on the marginal and internal gap of zirconia copings(p<0.001). The gap of margin and axial wall area was smaller than that the gap of occlusal area in all groups(p<0.001). Conclusion : Effect of different cement spaces on the marginal and internal gap of zirconia copings.

고정성 보철물의 적합도 측정 시 사용하는 실리콘 복제본 기술의 정확도 평가 (An Evaluation Validity of the Silicone Replica Technique at Measurement on Fit of Fixed Dental Prostheses)

  • 김재홍;김기백
    • 치위생과학회지
    • /
    • 제12권6호
    • /
    • pp.566-571
    • /
    • 2012
  • 제한된 조건 하에서 수행된 본 연구에서는 다음과 같은 결론을 얻었다. 1. 치형과 고정성 보철물을 근 원심 방향의 단면에 8지점을 선정한 후 서로 다른 두 가지 방식으로 적합도를 측정하여 비교한 결과 8지점 모두에서 유의한 차이를 보이지 않았다(p<0.05). 2. 8지점을 변연부, 경사부, 축벽부, 교합면으로 분류하여 비교한 결과에서도 역시 두 측정 방법 간에 유의한 차이를 보이지 않았다(p<0.05). 이와 같은 결과를 바탕으로 실리콘 복제본 기술을 이용하여 적합도를 측정하는 것이 치형과 고정성 보철물을 직접 절단하여 단면을 측정하는 것만큼 정확하다는 결론을 얻었다. 따라서 고정성 보철물의 적합도 측정 시 비 파괴적인 방법인 실리콘 복제본 기술을 이용한다면 치형과 고정성 보철물 모두 파괴하지 않고 측정이 가능할 것으로 사료된다.