임상가를 위한 특집 1 - 치과심미수복용 세라믹의 최신 특성평가 (Recent characteristics of dental esthetic restorative ceramics)

  • 오승한
    • 대한치과의사협회지
    • /
    • 제51권1호
    • /
    • pp.6-11
    • /
    • 2013
  • Dental ceramics is well known to have excellent esthetics, biocompatibility as well as high compressive strength. However, the fragility of ceramics against tensile and shear loads leading to the delayed fracture of micro crack on ceramic surface and the backwardness of ceramic fabrication technique limit the usage of ceramic materials in dentistry. Among all ceramic materials, zirconia has been introduced to overcome the drawback of conventional dental ceramics in the field of dentistry due to the nature of zirconia featuring proper opalescence and high fracture toughness. Also, novel manufacturing techniques enable ceramic materials to prepare high esthetic anterior and posterior all ceramic system. In this paper, it is introduced and discussed that novel techniques characterizing the bond strength between zirconia core and veneering ceramics and analyzing the fluorescence of dental ceramics in order to overcome the gap between the results of basic research and the feasibility of the results in the field of dental clinics.

Influence of polishing systems on roughness and color change of two dental ceramics

  • Maciel, Lucas Campagnaro;Silva, Carlos Frederico Bettcher;de Jesus, Ricardo Huver;da Silva Concilio, Lais Regiane;Kano, Stefania Carvalho;Xible, Anuar Antonio
    • The Journal of Advanced Prosthodontics
    • /
    • 제11권4호
    • /
    • pp.215-222
    • /
    • 2019
  • PURPOSE. To evaluate the polishing effect on roughness and color change of pressed and layering ceramics after immersion in coffee solution. MATERIALS AND METHODS. 88 ceramic discs ($1.0mm{\times}10.0mm$) were manufactured - 44 nano-fluorapatite layering ceramics (IPS e.max Ceram. Group C) and 44 pressed lithium disilicate ceramic discs (IPS e. max Press - Group P). Each group was divided into 4 subgroups according to surface treatments: (G) Glaze, (S) Shofu polishing system (Shofu Inc.), (E) Edenta AG polishing System, (KG) $30-{\mu}m$ diamond granulation tip. Surface roughness (Ra) and color change (${\Delta}E$) measurings after the surface treatments were performed, before and 12 days after the immersion in coffee solution. A samples' qualitative analysis was conducted with a scanning electron microscopy (SEM). Data were statistically-treated with one-way-ANOVA and Duncan's tests, apart from paired t-test and Pearson's correlation test (${\alpha}=5%$). RESULTS. The decrescent order, both for surface roughness (Ra) and ${\Delta}E$ for both ceramics were: KG > E > S > G (P<.05). With exception for PG and CG subgroups, which did not present statistical difference between them, all other pressed ceramics subgroups presented smaller Ra values and greater ${\Delta}E$ values than the layering ceramics subgroups (P<.05). CONCLUSION. Although mechanical polishing systems presented intermediate Ra values, their colors were considered clinically acceptable. There is a strong correlation between the surface roughness and the color change of tested ceramics.

치관보철용 $CaO-MgO-SiO_{2}-P_{2}O_{5}-TiO_2$계 글라스 세라믹의 결정화와 기계적 물성에 미치는 열처리 조건의 영향 (Effects of Heat-treatment on Crystallization and Mechanical Properties of Glass ceramics for Dental crown prosthesis in the system $CaO-MgO-SiO_{2}-P_{2}O_{5}-TiO_2$)

  • 정인성;김부섭
    • 대한치과기공학회지
    • /
    • 제26권1호
    • /
    • pp.77-88
    • /
    • 2004
  • Glass ceramics for dental crown prosthesis were prepared by crystallization of CaO-MgO-SiO2-P2O5-TiO2 glasses. Their crystallization behaviors have been investigated as a function of heattreatment temperature and holding time in relation to mechanical properties. The results are as follows: Vickers hardness and bending strength of glass ceramics increased due to the precipitation of apatite, whitlockite, $\beta$-wollastonite, magnesium titanate, and diopside crystal phases within glass matrix. The final crystalline phase assemblages and the microstructures of the glass ceramics were found to be dependent on heat-treatment temperature and holding time. Vickers hardnes and bending strength of glass ceramics increased with increasing heat-treatment temperature and holding time.

  • PDF

최근 치과용 지르코니아 CAD/CAM 수복물의 임상적 고찰 (A clinical consideration of current dental zirconia CAD/CAM restorations)

  • 이해형
    • 대한치과의사협회지
    • /
    • 제49권5호
    • /
    • pp.279-285
    • /
    • 2011
  • Currently there is no dental ceramic material can be used in all dental situations need to be restored. However, in view of recent clinical reports, the most viable alternative is zirconia ceramic. Clinical success of dental zirconia restorations strongly depends on proper selection of materials, accurate laboratory procedure and final cementation, which can be achievable with the correct understanding of zirconia. As dental materials, zirconia ceramics have a very bright future, because they are being used increasingly in the anterior region as implant fixtures, as well as crown and bridge restorations and implant abutments. Many dental ceramics showing poor clinical performance have been gone from the dental market. However, in terms of outstanding mechanical properties and esthetic nature, new dental materials can replace zirconia ceramics will not be available in the foreseeable future.

지르코니아 전장 세라믹의 파절강도에 관한 비교 연구 (Comparative Study in Fracture Strength of Zirconia Veneering Ceramics)

  • 이정환;안재석
    • 치위생과학회지
    • /
    • 제10권5호
    • /
    • pp.335-340
    • /
    • 2010
  • This study was performed to evaluate the fracture strength of the dental zirconia veneering ceramics for zirconia ceramic core. Six commercial zirconia veneering ceramics were used in this study, namely E-Max(Ivoclar vivadent, Inc, Liechtenstein), Creation ZI(KLEMA Dental produckte GmbH, Austria), Cercon ceram kiss(Degudent, GmbH, Hanau-Wolfgang, Germany), Triceram(Dentaurum, Ispringen, Germany), Zirkonzahn(Zirkonzahn GmbH, Italy), Zirmax(Alpadent, korea). All samples were prepared according to the relevant instructions of manufacture. Disc specimens were prepared to the final dimensions of 17 mm in diameter and 1.5 mm in thickness. The biaxial flexure strength test was conducted using a ball-on-three-ball method. All specimens were tested in a moisture-free environment. Average flexural strengths were analyzed with Weibull analysis and one-way analysis of variance(ANOVA). Significant differences were founded between the mean flexural strength values of five commercials zirconia veneering ceramics and the other. The flexural strengths and Weibull modulus were similar to those of five groups E-Max(EM), Creation ZI(CR), Cercon ceram kiss(CE), Triceram(TR), Zirkonzahn(ZI) with the exception of Zirmax(ZM). The biaxial flexural strength from Cercon ceram kiss(CE) was higher than those of other groups. Fracture analysis showed similar results for these five groups.

The effect of repeated firings on the color change and surface roughness of dental ceramics

  • Gonuldas, Fehmi;Yilmaz, Kerem;Ozturk, Caner
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권4호
    • /
    • pp.309-316
    • /
    • 2014
  • PURPOSE. The color of the ceramic restorations is affected by various factors such as brand, thickness of the layered the ceramic, condensation techniques, smoothness of surface, number of firings, firing temperature and thickness of dentin. The aim of this study was to evaluate the color change and surface roughness in dental porcelain with different thicknesses during repeated firings. MATERIALS AND METHODS. Disc-shaped (N=21) metal-ceramic samples (IPS Classic; Ivoclar Vivadent; Shaar, Liechtenstein) with different thickness were exposed to repeated firings. Color measurement of the samples was made using a colorimeter and profilometer was used to determine surface roughness. ANOVA and Tukey tests with repeated measurements were used for statistical analysis. RESULTS. The total thickness of the ceramics which is less than 2 mm significantly have detrimental effect on the surface properties and color of porcelains during firings (P<.05). CONCLUSION. Repeated firings have effects on the color change and surface roughness of the dental ceramics and should be avoided.

인공 치아용 결정화 유리의 제조(II) - 생체적합성 (Fabrication of Glass Ceramics for Dental Artificial Tooth(II) -Biocompatibility-)

  • 유기수;한복섭
    • 대한의용생체공학회:의공학회지
    • /
    • 제14권3호
    • /
    • pp.257-264
    • /
    • 1993
  • A study on the biocompatibility of two types of new glass-ceramics materials, metal disc and dental porcelain that were already made for dental artificial tooth in the previous study, have been attempted. The chemical behavior and the Victor's hardness change in she artificial saliva and Ringer's solution have been also investigated. From the experiment of Implantation of glass-ceramics Into dorsal subcutaneous tissue of Sprague-Dawley rats, glass-cerarmics did not show any particular system of rejection for histrocompatibility.

  • PDF

치과용 열가압 글라스 세라믹스의 기계적 성질과 미세구조 (Mechanical Properties and Microstructure of Dental Heat-Pressable Glass-Ceramics)

  • 이해형;이병택
    • 한국세라믹학회지
    • /
    • 제41권2호
    • /
    • pp.143-150
    • /
    • 2004
  • 본 연구에서는 치아 수복에 사용되는 상용 글라스 세라믹들을 디스크 모양으로 열가압 성형하여 ball-on-3-bal에 의한 이축강도와 압입시험에 의한 파괴인성을 측정하였다. 시편들로부터 XRD, SEM, TEM을 이용하여 결정상과 미세구조를 분석하였다. 글라스 세라믹내의 결정들은 균열의 진행에 대하여 효과적인 저지를 하지 못하였으나 높은 결정화도가 기계적 성질의 향상에 기여하는 것으로 판단된다. Lithium disilicate결정의 글라스 세라믹은 상대적으로 결정함량이 낮은 leucite 세라믹에 비하여 유의하게 높은 이축강도와 파괴인성을 나타내어 치과용 글라스 세라믹으로서 높은 신뢰성이 기대된다.

The radioactivity levels and beta dose rate assessment from dental ceramic materials in Egypt

  • Mohamed Hasabelnaby;Mohamed Y. Hanfi;Hany El-Gamal;Ahmed H. El Gindy;Mayeen Uddin Khandakerf;Ghada Salaheldin
    • Nuclear Engineering and Technology
    • /
    • 제56권9호
    • /
    • pp.3898-3903
    • /
    • 2024
  • There is a lack of available data on the radioactivity levels of these materials, despite the potential risks they may pose to patients, dental technicians, and dentists. A total of forty samples were collected from different dental markets in Egypt. Using an NaI(Tl) detector, the gamma-ray spectrometer measured the activity levels of uranium-238, radium-226, thorium-232, and potassium-40. The findings revealed that the mean concentration of 238U (below the minimum detectable activity, MDA), 226Ra (135 ± 5 and 132 ± 5 Bq/kg), 232Th (187 ± 4 and 243 ± 8 Bq/kg), and 40K (1560 ± 52 and 2501 ± 89 Bq/kg) in feldspar and zirconia (ZrO2) dental ceramic samples, respectively, were all within the limits established by the International Organization for Standardization (ISO) and the European Commission (EC). The use of feldspar and zirconia dental ceramics to restore all teeth would result in an estimated maximum beta dose of 1.5 mGy/year to the oral tissue. The results suggest that there is no cause for concern regarding any additional beta dose to the oral cavity from the use of feldspar and zirconia dental ceramics.

The effect of repeated firings on the color change of dental ceramics using different glazing methods

  • Yilmaz, Kerem;Gonuldas, Fehmi;Ozturk, Caner
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권6호
    • /
    • pp.427-433
    • /
    • 2014
  • PURPOSE. Surface color is one of the main criteria to obtain an ideal esthetic. Many factors such as the type of the material, surface specifications, number of firings, firing temperature and thickness of the porcelain are all important to provide an unchanged surface color in dental ceramics. The aim of this study was to evaluate the color changes in dental ceramics according to the material type and glazing methods, during the multiple firings. MATERIALS AND METHODS. Three different types of dental ceramics (IPS Classical metal ceramic, Empress Esthetic and Empress 2 ceramics) were used in the study. Porcelains were evaluated under five main groups according to glaze and natural glaze methods. Color changes (${\Delta}E$) and changes in color parameters (${\Delta}L$, ${\Delta}a$, ${\Delta}b$) were determined using colorimeter during the control, the first, third, fifth, and seventh firings. The statistical analysis of the results was performed using ANOVA and Tukey test. RESULTS. The color changes which occurred upon material-method-firing interaction were statistically significant (P<.05). ${\Delta}E$, ${\Delta}L$, ${\Delta}a$ and ${\Delta}b$ values also demonstrated a negative trend. The MC-G group was less affected in terms of color changes compared to other groups. In all-ceramic specimens, the surface color was significantly affected by multiple firings. CONCLUSION. Firing detrimentally affected the structure of the porcelain surface and hence caused fading of the color and prominence of yellow and red characters. Compressible all-ceramics were remarkably affected by repeated firings due to their crystalline structure.