치과용 복합레진으로 수리된 CAD-CAM hybrid 수복물의 전단결합강도 (Shear bond strength of dental CAD-CAM hybrid restorative materials repaired with composite resin)

  • 문윤희;이종혁;이명구
    • 대한치과보철학회지
    • /
    • 제54권3호
    • /
    • pp.193-202
    • /
    • 2016
  • 목적: 본 연구에서는 치과용 CAD-CAM (computer aided design-computer aided manufacturing) hybrid 수복재료인 LAVA Ultimate와 VITA ENAMIC을 광중합 복합레진을 사용하여 수리할 때 표면처리방법(grinding, air abrasion with aluminum oxide, HF acid)과 접착재료(Adper Single Bond 2, Single Bond Universal)의 종류가 두 재료 사이의 전단결합강도에 어떠한 영향을 미치는지 알아보고자 하였다. 재료 및 방법: LAVA Ultimate와 VITA ENAMIC 시편을 30일간 $37^{\circ}C$의 인공타액(Xerova solution)에 보관하여 시효처리를 실시한 후 각각 SiC paper grinding한 것, grinding 후 air abrasion처리를 추가한 것, grinding 후 HF 처리한 것으로 분류하고 각각 no bonding, Adper Single Bond 2, 또는, Single Bond Universal 도포로 세분하여 9개의 group, 총 18개의 subgroup으로 나누어 실험을 실시하였다(N=10). HF 처리group에서는 도재시편을 대조군으로 추가하였다(N=10). 표면 처리 후 광중합 복합레진(Filtek Z250)을 각각의 시편에 부착하고 이를 1주일간 실온의 물에 침적시켰고 이후 전단결합강도를 측정하고 파절양상 및 표면처리 효과를 SEM으로 확인하였다. One-way ANOVA를 이용하여 group 간의 유의성을 분석하였고 사후 분석으로 Scheffe test를 실시하였다(${\alpha}=.05$). 결과: 실험 결과 접착재료 처리를 한 group들이 접착재료 처리를 하지 않은 group에 비해 모든 표면처리에서 더 높은 전단결합력을 나타내었으며, 표면처리만 시행한 group에서는 aluminum oxide air abrasion이 전단결합력의 증가에 약간의 영향을 미치는 것으로 나타났으나 통계적 유의성은 보이지 않았다. 결론: LAVA Ultimate와 VITA ENAMIC의 두 재료를 광중합 복합레진을 이용하여 수리를 실시할 경우 각각의 재료에 적합한 표면처리방법과 접착재료의 선택에 대한 연구가 더 필요할 것으로 사료된다. 특히 LAVA Ultimate의 경우 접착재료의 사용은 추천된다고 사료되었다.

지르코니아 표면 처리와 시멘트 종류에 따른 치면과의 전단 결합 강도 비교 연구 (In Vitro Evaluation of Shear Bond Strengths of Zirconia Cerami with Various Types of Cement after Thermocycling on Bovine Dentin Surface)

  • 조수현;조인호;이종혁;남기영;김종배;황상희
    • 구강회복응용과학지
    • /
    • 제23권3호
    • /
    • pp.249-257
    • /
    • 2007
  • State of problem : The use of zirconium oxide all-ceramic material provides several advantages, including a high flexural strength(>1000MPa) and desirable optical properties, such as shading adaptation to the basic shades and a reduction in the layer thickness. Along with the strength of the materials, the cementation technique is also important to the clinical success of a restoration. Nevertheless, little information is available on the effect of different surface treatments on the bonding of zirconium high-crystalline ceramics and resin luting agents. Purpose : The aim of this study was to test the effects of surface treatments of zirconium on shear bond strengths between bovine teeth and a zirconia ceramic and evaluate differences among cements Material and methods : 54 sound bovine teeth extracted within a 1 months, were used. They were frozen in distilled water. These were rinsed by tap water to confirm that no granulation tissues have left. These were kept refrigerated at $4^{\circ}C$ until tested. Each tooth was placed horizontally at a plastic cylinder (diameter 20mm), and embedded in epoxy resin. Teeth were sectioned with diamond burs to expose dentin and grinded with #600 silicon carbide paper. To make sure there was no enamel left, each was observed under an optical microscope. 54 prefabricated zirconium oxide ceramic copings(Lava, 3M ESPE, USA) were assigned into 3 groups ; control, airborne-abraded with $110{\mu}m$ $Al_2O_3$ and scratched with diamond burs at 4 directions. They were cemented with a seating force of 10 ㎏ per tooth, using resin luting cement(Panavia $F^{(R)}$), resin cement(Superbond $C&B^{(R)}$), and resin modified GI cement(Rely X $Luting^{(R)}$). Those were thermocycled at $5^{\circ}C$ and $55^{\circ}C$ for 5000 cycles with a 30 second dwell time, and then shear bond strength was determined in a universal test machine(Model 4200, Instron Co., Canton, USA). The crosshead speed was 1 mm/min. The result was analyzed with one-way analysis of variance(ANOVA) and the Tukey test at a significance level of P<0.05. Results : Superbond $C&B^{(R)}$ at scratching with diamond burs showed the highest shear bond strength than others (p<.05). For Panavia $F^{(R)}$, groups of scratching and sandblasting showed significantly higher shear bond strength than control group(p<.05). For Rely X $Luting^{(R)}$, only between scratching & control group, significantly different shear bond strength was observed(p<.05). Conclusion : Within the limitation of this study, Superbond $C&B^{(R)}$ showed clinically acceptable shear bond between bovine teeth & zirconia ceramics regardless of surface treatments. For the surface treatment, scratching increased shear bond strength. Increase of shear bond strength by sandblasting with $110{\mu}m$ $Al_2O_3$ was not statistically different.

CAD/CAM 세라믹 인레이에 대한 3종의 레진 시멘트의 전단결합강도에 관한 연구 (Shear bond strength of the three different kinds of resin cement on CAD/CAM ceramic inlay)

  • 백철우;박철우;박준섭;류재준
    • 대한치과보철학회지
    • /
    • 제51권1호
    • /
    • pp.20-26
    • /
    • 2013
  • 연구 목적: 본 연구는 최근 심미수복에 주로 사용되는 CAD/CAM 세라믹 인레이와 각종 레진 시멘트간의 결합강도를 알아보고자 하였다. 연구 재료 및 방법: 원기둥 모양의 세라믹 블록(높이: 5 mm, 직경: 3 mm)을 Cerec3로 제작하고, 총 90개의 우식이 없는 대구치의 상아질 표면에 세 종류의 레진 시멘트(Unicem$^{(R)}$, Biscem$^{(R)}$, Variolink II$^{(R)}$)를 사용하여 각각 제조업체의 지시에 따라 접착했다. 90개의 시편을 레진 시멘트의 종류에 따라 3개의 군으로 나누고, 각 군의 절반은 $5-55^{\circ}C$, 5,000 cycle 조건 하에서 thermocycling을 시행하였고, 다른 절반은 시행하지 않았다. 모든 시편은 결합강도를 측정하기 전에 $37^{\circ}C$ 생리 식염수에 24시간 동안 보관되었다. 전단결합강도는 만능시험기를 이용하여 0.5 mm/min의 cross head speed로 측정하였다. 결과 값은 t-test 및 one-way ANOVA를 사용하여 통계 분석하였다. 결과: Unicem$^{(R)}$ 군의 전단결합강도가 thermocycling 후에 약간 감소했으나 3 개의 군 중 가장 높은 결합 강도를 보였다. Unicem$^{(R)}$ 및 Valiolink II$^{(R)}$ 군의 전단결합강도가 thermocycling에 영향을 받았지만 Biscem$^{(R)}$은 영향을 받지 않았다(P<.05). Thermocyling 전에는 3개의 군 간의 결합강도에 유의한 차이가 없었지만, thermocyling 후에는 Unicem$^{(R)}$과 Valiolink II$^{(R)}$ 군 간에 유의한 차이가 있었다(P<.05). 결론:CAD/CAM 세라믹 인레이 수복물을 치아에 접착할 때, etch-and-rinse 레진 시멘트인 Valiolink II$^{(R)}$ 대신self-adhesive 레진 시멘트인 Unicem$^{(R)}$과 Biscem$^{(R)}$을 사용해도 임상적으로 유용하다.

터널형 2급와동 충전재의 탄성계수와 전단결합강도 및 수복치의 변연융선 파절강도에 관한 연구 (ELASTIC CONSTANTS, SHEAR BOND STRENGTH OF TUNNEL RESTORATIVE MATERIALS AND MARGINAL RIDGE STRENGTH OF RESTORED TEETH)

  • 이가연;박영준;양규호
    • 대한소아치과학회지
    • /
    • 제23권3호
    • /
    • pp.746-763
    • /
    • 1996
  • An alternative design to conventional class II cavity preparation for proximal carious lesions is the tunnel preparation. It preserves the marginal ridge intact, thus making it possible to maintain the natural contact relationship with the adjacent tooth and minimize tooth reduction. This in vitro study was purposed to evaluate the effect of the materials' elastic constants and shear-bond strength on the marginal ridge fracture resistance of teeth restored by the tunnel technique, and to find the materials of choice for tunnel restorations. $Resinomer^{(R)}$, $Ketac-silver^{(R)}$, $Miracle-Mix^{(R)}$, and Tytin were used as restorative material. The elastic constants of each restorative material were evaluated by ultrasonic pulse measurement. Young's modulus and bulk modulus of the restorative materials were evaluated in three specimens for each material type. The shear-bond strength of the restorative materials to the dentin surface was measured after thermocycling 400 times between 6 and $60^{\circ}C$, using ten specimens for each material type. For measuring marginal ridge strength, 60 sound extracted molar teeth were distributed into six groups by size. Sound molar teeth were used as a Control group and unfilled prepared teeth were grouped as Unrestored. Another four groups were named Resinomer group, Ketac-Silver group, Miracle Mix group, and Tytin group by type of restorative material. Tunnel cavity preparation was done with ' 1/2, 2, and 4 round burs in sequence. Initial access to proximal surface was made through an occlusal access preparation started at least 2mm from the marginal ridge, and the proximal opening was formed about 2.5mm below the marginal ridge. After restoration and thermocycling, marginal ridge strength was measured using a universal testing machine. The results were as follows: 1. The Young's modulus of $Tytin^{(R)}$ was 63.95 GPa, followed by $Ketac-Silver^{(R)}$ 27.60 GPa, $Miracle-mix^{(R)}$ 18.48 GPa, and $Resinomer^{(R)}$ 10.74 GPa showing significant differences between the groups(P<0.05). The bulk modulus of the materials showed the same order as Young's modulus. The value of $Tytin^{(R)}$ showed 59.57 GPa indicating that it will deform less than other materials under the same stress. It was followed by $Ketac-Silver^{(R)}$ 23.57 GPa, Miracle $Mix^{(R)}$ 12.50 GPa, and $Resinomer^{(R)}$ 11.60 GPa. 2. The Resinomer group had a shear-bond strength of 7.41 MPa which was significantly higher than those of the Ketac-Silver group (1.80 MPa) and the Miracle Mix group (2.84 MPa) (P<0.01). All the specimens of Tytin group detatched from the dentin surface during thermocycling. 3. The mean marginal ridge strength of the Unrestored group(46.14 kgf) was significantly lower than that of the Control group (84.24 kgf) (P<0.01). The marginal ridge strength of teeth restored by the tunnel technique was, in order, Ketac-Silver group 74.06 kgf, Miracle Mix group 73.36 kgf, Resinomer group 63.47 kgf, and Tytin group 58.76 kgf. The Ketac-Silver, Miracle Mix, and Resinomer groups showed no significant difference with the Control group (P>0.05), but the Tytin group showed significantly lower strength compared to the Control group(P<0.05). The results showed that the marginal ridge strength of the teeth restored by the tunnel technique was not significantly lower than that of sound teeth. They also demonstrated that the bonding strength of the restorative material to the tooth surface should be high and the modulus of elasticity should not be lower than that of the tooth in order to restore the marginal ridge strength to its natural condition.

  • PDF

Flowable 및 microfill 복합레진으로 충전된 제 5급와동에서 load cycling 전,후의 미세변연누출 비교 (MICROLEAKAGE OF MICROFILL AND FLOWABLE COMPOSITE RESINS IN CLASS V CAVITY AFTER LOAD CYCLING)

  • 강석호;김오영;오명환;조병훈;엄정문;권혁춘;손호현
    • Restorative Dentistry and Endodontics
    • /
    • 제27권2호
    • /
    • pp.142-149
    • /
    • 2002
  • Low-viscosity composite resins may produce better sealed margins than stiffer compositions (KempScholte and Davidson, 1988: Crim, 1989). Plowable composites have been recommended for use in Class V cavities but it is also controversial because of its high rates of shrinkage. On the other hand, in the study comparing elastic moduli and leakage, the microfill had the least leakage (Rundle et at. 1997) Furthermore, in the 1996 survey of the Reality Editorial Team, microfills were the clear choice for abfraction lesions. The purpose of this study was to evaluate the microleakage of 6 compostite resins (2 hybrids, 2 microfills, and 2 flowable composites) with and without load cycling. Notch-shaped Class V cavities were prepared on buccal surface of 180 extracted human upper premolars on cementum margin. The teeth were randomly divided into non-load cycling group (group 1) and load cycling group (group 2) of 90 teeth each. The experimental teeth of each group were randomly divided into 6 subgroups of 15 samples. All preparations were etched, and Single bond was applied. Preparations were restored with the following materials (n=15) : hybrid composite resin [Z250(3M Dental Products Inc. St. Paul, USA), Denfil(Vericom, Ahnyang, Korea)], microfill [Heliomolar RO(Vivadent, Schaan, Liechtenstein), Micronew(Bisco Inc. Schaumburg, IL, USA)], and flowable composite[AeliteFlo(Bisco Inc. Schaumburg, IL, USA), Revolution(Kerr Corp. Orange, CA, USA)]. Teeth of group 2 were subjected to occlusal load (100N for 50,000 cycles) using chewing simulator(MTS 858 Mini Bionix II system, MTS Systems Corp. Minn. USA). All samples were coated with nail polish 1mm short of the restoration, placed in 2% methylene blue for 24 hours, and sectioned with a diamond wheel. Enamel and dentin/cementum margins were analyzed for microleakage on a sclale of 0 (no leakage) to 3 (3/3 of wall). Results were statistically analyzed by Kruscal-Wallis One way analysis, Mann-Whitney U-test, and Student-Newmann-Keuls method. (p = 0.05) Results : 1. There was significantly less microleage in enamel margins than dentinal margins of all groups (p<0.05) 2. There was no significant between six composite resin in enamel margin of group 1. 3. In dentin margin of group 1, flowable composite had more microleakage than others but not of significant differences. 4. there was no significant difference between six composite resin in enamel margin of group 2. 5. In dentin margin of group 2, the microleakage were R>A =H=M>D>Z. But there was no significant differences. 6. In enamel margins, load cycling did not affect the marginal microleakage in significant degree. 7. In enamel margins, load cycling did affect the marginal microleakage only in Revolution. (p<0.05).

국내에서 제작된 고정성 보철물의 수명과 실패 요인 및 양상 (LONGEVITY AND FAILURE ANALYSIS OF FIXED RESTORATIONS SERVICED IN KOREA)

  • 신우진;전영식;이근우;이호용;한동후
    • 대한치과보철학회지
    • /
    • 제43권2호
    • /
    • pp.158-175
    • /
    • 2005
  • Statement of problem. Every effort has been continually made to obtain objectivity in measuring the longevity of fixed restorations, such as by establishing unified judgement standard for deciding success and adopting statistical method that analyzes the data of successful and failed cases at the same time. In Korea, however desired level of development has not to be made in this field yet. Purpose. This study, adopting California Dental Association (CDA) quality evaluation system, established objective standard for deciding success, and inferred the longevity of fixed restorations and their failure analysis through adopting Kaplan-Meier survival analysis. Material and method. In order to assess the longevity of flxed restorations serviced in Korea and causes of failure, a total of 1109 individuals (aged 15-74, 716 women and 393 men loaded with 2551 unit fixed restorations, and 1934 abutments) who lived in Kyung-In Province were examined and the findings were as follows : Results. 1. Length of service of fixed restorations serviced in Korea was 6.86$\pm$0.15 yr (mean), 5.5 yr (median), and the rate of success was 65.82% in 5 year survival, and 21.15% in 10 year survival. 2. When there was patient's need for replacing old prosthetics, longevity of fixed restorations was 7.51$\pm$0.27 yr (mean), 7 yr (median), and the rate of success was 61.08% in 5 year survival, and 17.57% in 10 year survival. 3. Longevity of fixed restorations was longest in the over-sixty age group(9.21$\pm$0.66) and that of the teen age group(3.39$\pm$0.28) was shortest (p<0.05). 4. Longevity of fixed restorations of women (7.38$\pm$0.18 years) was longer than that of men (6.00$\pm$0.26) (p<0.05). 5. As for the provider factor (such as unlicensed performers, university hospitals, and private clinic), there was no statistically significant difference in longevity of fixed restorations. 6. Defective margin (34.78%). periodontal disease (12.15%), periapical involvement (11.73%), was the most frequent causes of failure and poor esthetics group showed the longest life above all (p<0.05). Actual frequent causes of failure after removing old prosthetics were defective margin, periapical involvement, periodontal disease and uncemented restoration. In 75.67% of the cases, abutment state after removing old prosthetics was good enough for loading another prosthetics. 7. There was found to have statistically significant influence between longevity of single crown (6.35$\pm$0.20 yr) and that of 3 unit fixed restorations (7.60$\pm$0.30 y) (p<0.05). In each case the most frequent cause of failure was defective margin. 8. The number of cantilever pontic, pontic/abutment ratio, oral hygiene status were found to have no statistically significant influence on longevity of fixed restorations in all groups (p>0.05). 9. Longevity of fixed restorations made of non precious metal was longest (9.60$\pm$0.40 yr) semi precious and precious trailing behind(p<0.05). 10. Group function group (37.04%) and partial group function group (44.62%) were predominant in frequency but showed no correlation between them and among different types of occlusal plane and different types of occlusal surface (p>0.05). 11. Longevity of fixed restorations was longest in the centric interference group(9.35$\pm$0.62) (p<0.05) among different types of occlusal interference. Conclusion. We found that longevity of fixed restorations serviced in Korea is affected by age, gender and type of material, and that most frequent cause of failure is defective margin. In order to assess the accurate longevity of axed restorations, unified research design. overcoming inter-observer difference and establishing the objective research items are needed. Furthermore, it is thought that prospective approach through thorough study and regular follow-ups is needed just from the start of research. Nationwide detailed studies on length of service of fixed restorations manufactured in Korea are hoped to be conducted hereafter.

임시 시멘트 제거방법이 시멘트 유지형 임플란트 보철물의 유지력에 미치는 영향 (The Effect of Temporary Cement Cleaning Methods on the Retentive Strength of Cementation Type Implant Prostheses)

  • 신황규;송영균;신수연
    • 구강회복응용과학지
    • /
    • 제27권2호
    • /
    • pp.125-140
    • /
    • 2011
  • 보철물을 기능적으로 평가하기 위해 임시 시멘트로 임시 합착을 한 경우 보철물 내면의 잔여 임시 시멘트는 레진 시멘트를 이용한 최종 합착에 있어서 부정적인 영향을 미칠 수 있다. 이에 본 연구는 다양한 임시 시멘트 제거 방법과 임시 시멘트의 잔여 성분이 임플란트 전용 레진 시멘트와 보철물의 유지력에 어떠한 영향을 미치는지를 알아보고자 하였다. 임플란트 지대주는 일반적인 시멘트 유지형 보철물 제작에 사용되는 높이 5.5 mm, 직경 4.5mm, 6도의 축면 경사도와 chamfer 변연을 갖는 기성품(Solid abutment, GSRAS4621, Osstem Implant Co., Busan, Korea)을 사용하였다. 40개의 주조시편을 제작하여 합착 전 70 psi하에 공기입자 분사법을 시행하였고, 10개의 시편을 임시 시멘트의 합착과정 없이 바로 최종 시멘트로 합착하여 대조군으로 설정하였으며 나머지 시편을 각 10개씩 임시 시멘트 제거를 위하여 오렌지 솔벤트를 이용한 군, 초음파 세척을 이용한 군, 공기입자 분사법을 이용한 군으로 나누었다. 임시 시멘트의 합착과 분리 후 제거과정을 거쳐 최종 시멘트로 임플란트 전용 시멘트($Premier^{(R)}$ Implant $Cement^{TM}$, Premier Co., PA, U.S.A.)를 사용하여 최종 합착을 실시하였다. 각 시편은 10분간 5 kg의 하중 하에 합착하였으며 열순환을 거쳐 만능시험기에서 분당 0.5 mm의 속도로 인장접착강도를 측정하였다. 측정이 끝난 뒤 모든 시편을 초음파 세척과 공기입자 분사법, 증기 세척의 과정을 통해 내면의 잔여 성분을 제거하였다. 완전 건조 후 비유지놀계 임시 시멘트를 사용하여 다시 임시 합착, 분리를 거친 후 동일한 실험 과정을 반복하였고 인장접착강도를 측정하여 다음의 결과를 얻었다. 오렌지 솔벤트를 사용한 군이 가장 작은 유지력을 나타냈으며 초음파 세척법을 사용한 군과 공기 입자 분사법을 사용한 군과 비교시 통계적으로 유의한 차이가 있었다(p<0.05). 초음파 세척법을 사용한 군과 공기 입자 분사법을 사용한 군 간의 비교시 통계적으로 유의한 차이가 없었다. 오렌지 솔벤트를 사용한 군은 대조군과 비교시 통계적으로 유의한 차이가 있었으며(p<0.05), 초음파 세척법을 사용한 군과 공기 입자 분사법을 사용한 군은 대조군과 비교시 통계적으로 유의한 차이가 없었다. 임시 시멘트의 유지놀 성분의 유무에 따른 비교시 통계적으로 유의한 차이가 없었다. 이상의 결과로부터 임시 시멘트 제거를 위해 오렌지 솔벤트만을 사용하는 것은 임플란트 전용 시멘트를 사용한 최종 합착시 유지력 감소의 원인이 될 수 있음을 알 수 있었으며, 임플란트 보철물 내면의 임시 시멘트를 효과적으로 제거하기 위한 방법으로 초음파 세척법, 공기 입자 분사법, 또는 이들의 복합적인 사용이 필요함을 알 수 있었다.

레진전색제의 마모저항성에 대한 평가 (EVALUATION ON THE ABRASION RESISTANCE OF A SURFACE SEALANT)

  • 김수미;한세희;조영곤
    • Restorative Dentistry and Endodontics
    • /
    • 제32권3호
    • /
    • pp.180-190
    • /
    • 2007
  • 이 연구는 강화형 미세입자 복합레진인 Micronew에 Biscover 레진전색제를 적용한 후 칫솔마모시험을 시행하여 복합레진 표면의 조도와 현미경적 변화를 비교함으로써 레진전색제를 복합레진 표면에 재적용할 시기를 알아보고자 하였다. 분리 가능한 알루미늄 판과 복합레진을 이용하여 $8\times3\times2mm$ 크기의 복합레진 시편 200개를 제작하였다. 복합레진 시편의 양쪽표면을 Sof-Lex disc로 거친 입자에서 중간 입자까지 마무리한 후 실온의 증류수에 24시간 동안 보관하였다. 시편은 disc로 마무리만 시행한 F군 (n = 10)과 마무리 후 레진전색제인 Biscover를 적용한 B군 (n = 190)으로 분류하였다. B군은 다시 칫솔질을 가하지 않은 B-IM군 (n = 10)과 칫솔질을 가한 군 (n = 180, B-1군에서 B-18 군)으로 분류하였다. 칫솔질을 가한 군은 칫솔마모검사기의 수조에 페리오 치약과 증류수를 무게 비 50 : 50으로 혼합하여 부은 다음, 홈이 파진 알루미늄 블록에 각 군의 시편을 위치시키고 칫솔을 고정장치에 부착하여 전, 후 왕복운동을 가하여 칫솔질을 가하였다. 칫솔질은 B-1 군에서 B-18군 까지 각각 900회씩 증가시켜 16,200회 까지 시행하였다 표면조도측정기를 사용하여 각 군의 복합레진 표면의 평균 표면조도 값 (Ra)을 산출한 후 통계적으로 분석하였고, 주사전자현미경하에서 각 군의 대표적인 시편 1개를 관찰하여 다음과 같은 결과를 얻었다. 1. F군의 Ra는 $0.898{\pm}0.145{\mu}m$, B-IM군의 Ra는 $0.289{\pm}0.142{\mu}m$를 나타냈으며, B-1 군에서 B-18 군까지의 Ra는 점차적으로 증가하여 B-1 군에서 $0.299{\pm}0.48{\mu}m$, B-18 군에서 $0.642{\pm}0.313{\mu}m$까지 나타났다. 2. Ra 최종 군집중심은 군집 1 $(B-IM\simB-7)$에서 $0.361{\mu}m$, 군집 2 $(B-8\simB-14)$에서 $0.511{\mu}m$, 군집 3 $(B-15\simB-18)$에서 $0.624{\mu}m$를 나타내어 각 군집의 Ra 최종 군집중심 간에 통계학적으로 유의한 차이를 나타내었다. (F = 49.705, p = 0.000) 3. B-IM군의 Ra 증감율은 F 군에 비해 210.72%감소되었으며, B-8 군과 B-15군의 Ra 증감율은 B-IM군에 비해 각각 35.49%와 51.35% 증가되었다. 4. FE-SEM 관찰에서 B-IM 군은 매우 평활한 복합레진 표면을 나타내었고, B-8 군은 전체적으로 평활한 복합레진 표면을 보였지만 표면에 수직으로 아주 얕은 흠집을 나타내었다. B-15 군은 복합레진 표면의 중앙에서 B-8군보다 더 넓고 불규칙한 수직의 흠집을 나타내었고, B-18군은 복합레진 표면 전체에 넓은 흠집을 나타내었다.