Yang Yong Suk;Chu Hye Yong;Lee Jeong-Ik;Park Sang-He;Hwang Chi Sun;Chung Sung Mook;Do Lee-Mi;Kim Gi Heon
Journal of the Korean Vacuum Society
/
v.15
no.1
/
pp.64-72
/
2006
We demonstrated organic light-emitting devices (OLEDs) based on the organic thin-film materials such as tris-(8-hydroxyquinoline) aluminum $(Alq_3)$. The structure of OLEDs was vacuum deposited upon transparent and thin glass substrates pre-coated with a transparent, conducting indium tin oxide thin film. The luminance characteristics, current, capacitance, and dispersion factor for degraded OLEDs, which were made by various bias currents $(0.5mA\;{\leq}\;I_{Bias}\;{\leq}9mA)$, are studied. The current dependences of lifetime were divided at approximately 2mA, and they represented nearly linear behaviors but had different slopes in a logarithmic plot of lifetime versus bias current. With lighting OLEDs, the anomaly of capacitance, as shown in the CV curve, occurred because of two factors, polarization in the bulk of organic materials and the interface between the metal and organic layers. In decayed OLEDs that had lower bias currents of less than 2mA, it was found that the degradation of luminance was related to both the decrease of polarization and to the lowering of the injection barrier.
To investigate the long-term corrosion resistance of an uncoated weathering steel, an important outdoor constructional steel material, skyward surfaces of the weathering steel and a control steel initially exposed to rural and industrial atmospheres for 9 years were electrochemically tested in neutral artificial rain in terms of electrochemical potentials, impedances, and anodic potentiodynamic polarization curves. Their results were then discussed. A quite passive and stable rust layer to the artificial rain was well formed on the skyward surface of the weathering steel exposed to the industrial and rural atmospheres, and its corrosion rate in the artificial rain was measured to be about a low $3{{\mu}m}/y$. Continuous immersion of all the weathered surfaces in the artificial rain revealed the gradual degradation of the weathered corrosion layers on the steel, resulting in a cathodically controlled corrosion of the substrate steel by the electrochemical measurements. Alloy components of the weathering steel were found to retard the degradation of the weathered corrosion layers on the steel in the artificial rain. For better corrosion evaluation of the weathering steel, more electrochemical measurements of surfaces that have been exposed for more than 9 years to more closely simulated atmospheric waters are needed. These measurements are almost non-destructive and can provide online and in situ information on the corrosion rate, the development of corrosion and the conditions of rust layers on any interested surface and at any exposure time of the steel, so they can be effectively applicable to the corrosion evaluation of steel structures such as bridges, towers, and architectures by forming an electrochemical cell on an interested structural surface and by using a portable electrochemical instrument.
The contamination effect of toluene in the airstream on PEM fuel cell performance was studied with various toluene concentration under different operation conditions. And the recovery of the cell performance by applying clean air and the removal of toluene in the air by adsorption of active carbon were investigated. The toluene concentration range used in the experiments was from 0.1 ppm to 5.0 ppm. The performance degradation and recovery were measured by constant-current discharging and electrochemical impedance spectroscopy(EIS). Toluene adsorption capacity of KOH impregnated active carbon was obtained from the adsorption isotherm curve. The severity of the contamination increased with increasing toluene concentration, current density and air stoichiometry, but decrease with increasing relative humidity. The cell performance was recovered by toluene oxidation with oxygen and water in humidified neat air. EIS showed that the increase of charge transfer resistance due to toluene adsorption on Pt surface mainly reduced the performance of PEMFC. Toluene adsorption capacity of active carbon decreased as KOH weight increased in KOH impregnated active carbon.
Journal of Korean Society for Geospatial Information Science
/
v.23
no.4
/
pp.43-48
/
2015
We studied on pseudo-range correction(PRC) modeling in order to improve differential GNSS(DGNSS) accuracy. The PRC is the range correction information that provides improved location accuracy using DGNSS technique. The digital correction signal is typically broadcast over ground-based transmitters. Sometimes the degradation of the positioning accuracy caused by the loss of PRC signals, radio interference, etc. To prevent the degradation, in this paper, we have designed a PRC model through polynomial curve fitting and evaluated this model. We compared two quantities, estimations of PRC using model parameters and observations from the reference station. In the case of GPS, the average is 0.1m and RMSE is 1.3m. Most of GPS satellites have a bias error of less than ${\pm}1.0m$ and a RMSE within 3.0m. In the case of GLONASS, the average and the RMSE are 0.2m and 2.6m, respectively. Most of satellites have less than ${\pm}2.0m$ for a bias error and less than 3.0m for RMSE. These results show that the estimated value calculated by the model can be used effectively to maintain the accuracy of the user's location. However;it is needed for further work relating to the big difference between the two values at low elevation.
The reliability degradation phenomena in the SiGe hetero-junction bipolar transistor (HBT) are investigated in this review. In the case of the SiGe HBT the decrease of the current gain, the degradation of the AC characteristics, and the offset voltage are frequently observed, which are attributed to the emitter-base reverse bias voltage stress, the transient enhanced diffusion, and the deterioration of the base-collector junction due to the fluctuation in fabrication process, respectively. The reverse-bias stress on the emitter-base junction causes the recombination current to rise, increasing the base current and degrading the current gain, because hot carriers formed by the high electric field at the junction periphery generate charged traps at the silicon-oxide interface and within the oxide region. Because of the enhanced diffusion of the dopants in the intrinsic base induced by the extrinsic base implantation, the shorter distance between the emitter-base junction and the extrinsic base than a critical measure leads to the reduction of the cut-off frequency ($f_t$) of the device. If the energy of the extrinsic base implantation is insufficient, the turn-on voltage of the collector-base junction becomes low, in the result, the offset voltage appears on the current-voltage curve.
In this study, it was found that determined the photocatalytic degradation of antibiotics (lincomycin, LM) with various catalyst composite of titanium dioxide ($TiO_2$), hydroxyapatite (HAP) and germanium (Ge) under UV-A irradiation. At first, various type of complex catalysts were investigated to compare the enhanced photocatalytic potential. It was observed that in order to obtain the removal efficiencies were $TiO_2/HAP/Ge$ > $TiO_2/Ge$ > $TiO_2/HAP$. The composition of $TiO_2/HAP/Ge$ using a statistical approach based on mixture analysis design, one of response surface method was investigated. The independent variables of $TiO_2$ ($X_1$), HAP ($X_2$) and Ge ($X_3$) which consisted of 6 condition in each variables was set up to determine the effects on LM ($Y_1$) and TOC ($Y_2$) degradation. Regression analysis on analysis of variance (ANOVA) showed significant p-value (p < 0.05) and high coefficients for determination value ($R^2$ of $Y_1=99.28%$ and $R^2$ of $Y_2=98.91%$). Contour plot and response curve showed that the effects of $TiO_2/HAP/Ge$ composition for LM degradation under UV-A irradiation. And the estimated optimal composition for TOC removal ($Y_2$) were $X_1=0.6913$, $X_2=0.2313$ and $X_3=0.0756$ by coded value. By comparison with actual applications, the experimental results were found to be in good agreement with the model's predictions, with mean results for LM and TOC removal of 99.2% and 49.3%, respectively.
A fundamental study of drilled shafts subjected to lateral cyclic loading in weathered soil was carried out based on field tests and numerical analysis. The emphasis was given on quantifying the cyclic p-y curve function from lateral cyclic loading tests and three-dimensional finite element analysis. Lateral cyclic loading tests and three-dimensional finite element analysis were carried out to investigate the behavior of drilled shafts according to the direction of cyclic loading. Based on the field tests and numerical analysis, a modified lateral load transfer relationship and design chart with degradation factors were proposed by considering the characteristics of cyclic loading. It was found that the prediction by the proposed p-y curve function is in good agreement with the general trends observed by in-situ measurements, and it represents a practical improvement in the prediction of lateral displacement and bending moment distribution of drilled shafts subjected to cyclic loading.
China still has more than 30,000 patients of advanced schistosomiasis while new cases being reported consistently. D-dimer is a fibrin degradation product. As ascites being the dominating symptom in advanced schistosomiasis, the present study aimed to explore a prediction model of ascites with D-dimer and other clinical easy-achievable indicators. A case-control study nested in a prospective cohort was conducted in schistosomiasis-endemic area of southern China. A total of 291 patients of advanced schistosomiasis were first investigated in 2013 and further followed in 2014. Information on clinical history, physical examination, and abdominal ultrasonography, including the symptom of ascites was repeatedly collected. Result showed 44 patients having ascites. Most of the patients' ascites were confined in the kidney area with median area of $20mm^2$. The level of plasma D-dimer and pertinent liver function indicators were measured at the initial investigation in 2013. Compared with those without ascites, cases with ascites had significantly higher levels of D-dimer ($0.71{\pm}2.44{\mu}g/L$ vs $0.48{\pm}2.12{\mu}g/L$, P=0.005), as well ALB (44.5 vs 46.2, g/L) and Type IV collagen (50.04 vs $44.50{\mu}g/L$). Receiver operating characteristic curve analyses indicated a moderate predictive value of D-dimer by its own area under curve (AUC) of 0.64 (95% CI: 0.54-0.73) and the cutoff value as $0.81{\mu}g/L$. Dichotomized by the cutoff level, D-dimer along with other categorical variables generated a prediction model with AUC of 0.76 (95% CI: 0.68-0.89). Risks of patients with specific characteristics in the prediction model were summarized. Our study suggests that the plasma D-dimer level is a reliable predictor for incident ascites in advanced schistosomiasis japonica patients.
In order to investigate the impact properties of structural materials for LNG tank, instrumented Charpy impact tests were carried out at cryogenic temperatures. $9\%$ Ni steel showed a superior fracture resistance because of less degradation in toughness until 77 K. From the load-deflection curve obtained by an instrumented methods it was found that with the decrease of temperature from 173 K to 77 K, the peak load in the curve increased, but the total absorbed energy decreased. In addition, the energy absorbed during the crack growth was larger than one absorbed in the process of crack initiation. In SUS304L material, the energy absorbed in the process of the crack initiation was relatively large, but the energy absorbed in the process of crack growth was small, the behavior of absorbed energy was well agreed with the observations of the fracture surface which showed a relatively smooth fracture surface. The absorbed Charpy impact energy in the case of A5083 alloy was lower as compared with other steels, and some cracks were observed along the crack propagation direction at the fracture surface of 77 K.
Performances of retroreflectivity vary place to place, according to traffic volumes and time lengths after striping, depending on pavement marking materials and colors. The present paper uses the nation wide data of retroreflectivity, which has been collected from freeways and then tries to develop the regression curve setting traffic volume and service life as independent variables and retroreflectivities as dependent variables. The DB system includes two year's measurement in $2005{\sim}2006$ over Korean freeway pavement marking at an interval of three months for the period. The mobile measurement system, a laserlux, was employed for the purpose. The DB has provided a lot of information about materials and performance of the specific pavement marking such as geometric features, traffic volumes, material characteristics and the installation date. This study provides the comparison of pavement marking performances under diversified conditions. Based on accumulated pavement marking performances, this study provides performance curves based on the diversified factors. The goal of the retroreflectivity modeling is to develop equations that can be used to estimate an average retroreflectivity of pavement markings as a function time since application and traffic volume. After representing the variation of retroreflectivities and estimating regression curves by linear, exponential, logarithmic and power function, the regression curve which had the highest coefficient of determination and the value similar to the last field measurement was regarded as the retroreflectivity decay model. As a result of verification, the decay model showed the signification within the 90% confidence level and especially showed the clear relation with field data according to increase of cumulative vehicle exposure. Accordingly, these models can be used to determine service lives, retroreflectivity degradation rates, and retroreflectivity of new markings.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.