• Title/Summary/Keyword: DMDHEU

Search Result 32, Processing Time 0.019 seconds

Durable Press Performance and Water Repellency of Cotton/Polyester Fabrics Finished by BMDHEU/Fluorochemicals (DMDHEU/FC 일욕가공된 면/폴리에스테르 혼방직물의 DP성 및 발수성)

  • 권영아
    • Textile Coloration and Finishing
    • /
    • v.10 no.5
    • /
    • pp.24-31
    • /
    • 1998
  • The effects of DMDHEU alone and DMDHEU/Fluorochemical(FC) combined treatment on the physical properties of 75%/25% cotton/polyester(CP) blended fabrics were investigated. FC water repellent and DMDHEU durable press finishes were applied in combination to CP fabrics to provide good water repellency as well as great durable press(DP) performance. The physical properties of the fabrics were evaluated by wrinkle recovery angle(WRA), DP performance, contact angle, demand wettability, and water repellency. The durable press/water repellent finished(DP/WR) CP fabrics show considerably improved WRA and DP performance. The DP/WR finishes do not change the water contact angie of polyester fibers significantly, while the DP finishes increase it. Both DP and DP/WR finishes increase the contact angle of cotton fibers. The water uptake amount increases in the following order : DP/WR cotton, DP/WR CP<DP cotton, DP CP < Control CP, Control cotton. The water uptake amount increases in the following order DP/WR CP, DP/WR cotton <DP cotton <DP CP<Control CP, Control cotton. Considerable improvements for water repellency are imparted to the CP fabrics treated with DP/WR, and the level of improvement is not significantly different from that of the DP/WR cotton fabrics. These results lead to the conclusion that DP/YVR treatments a single pad bath on CP are effective finishes for improving both DP performance and water repellency.

  • PDF

Chemical Modifications of Regenerated Cellulose Fiber (셀룰로오스 재생 인조섬유의 화학개질에 관한 연구)

  • 이문철;이명선
    • Textile Coloration and Finishing
    • /
    • v.11 no.1
    • /
    • pp.48-60
    • /
    • 1999
  • In this paper, a new regenerated celluosic fiber, "Tencel" was treated with cellulase enzyme. Also Tencel fabrics were pretreated with NaOH and dyed with various reactive dyes, and subsequently finished with DMDHEU. $\Delta{E}^*_{ab}$ value was calculated by measuring color difference before and after wet abrasion test to rubbing. The fibrillation propensity was estimated on Tencel by means of weight loss, $\Delta{E}^*_{ab}$ value, and SEM observation. Weight loss of NaOH pretreated Tencel fabric is more lower than that of original fabric. The cellulase treatment decreased tensile strength but improved wet abrasion strength, wrinkle recovery, and bending properties. Tendency of fibrillation for Tencel fabric was reduced by NaOH-pretreatment, dyeing with multifunctional reactive dyes, and afterfinishing by DMDHEU.by DMDHEU.

  • PDF

BTCA/DMDHEU에 의한 면직물의 DP가공

  • 이주현;이의소
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 1998.10a
    • /
    • pp.133-136
    • /
    • 1998
  • DP가공은 면직물을 구성하고 있는 셀룰로오스 분자사이에 가교결합을 형성시켜 그 탄성한계를 높임으로써 구김을 방지할 목적으로 행해지는 가공이다. 현재 공업적으로 가장 많이 사용하고 있는 가교제는 셀룰로오스의 히드록시기와 ether형 가교를 형성하는 DMDHEU(dimethyloldihydroxyethylene urea) [1]이며 이와같은 ether형 가교제는 내가수 분해성이 높고 여러번의 세탁에도 견딜 수 있는 우수한 내구성을 지니고 있는 장점이 있으나 인체에 유해한 포름알데히드가 발생되는 단점이 있다. (중략)

  • PDF

Improvement of Wrinkle Recovery and Functional Properties in Linen Fabrics (아마직물의 방추성과 복합기능성 향상을 위한 연구)

  • Kang, Mi-Jung;Kwon, Young-Ah
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.34 no.11
    • /
    • pp.1859-1869
    • /
    • 2010
  • This study provides improved wrinkle recovery and UV protection capabilities as well as an antibacterial and deodorizing function to linen fabrics for summer shirts. The results obtained from this study are as follows. By setting catalyst concentration to 1.2% and DMDHEU concentration to 6% respectively and applying a heat treatment to them at $160^{\circ}C$ for 5 minutes, the decrease of fabric strength could be minimized and the crease resistance of linen fabrics improved. Compared to the treatment with DMDHEU only, the crease resistance of linen fabrics could be maintained and degradation of their properties could be more effectively prevented by applying the mixture of the UV absorber and the nano silver to the DMDHEU resin. The UV protection of fabrics could be improved by adding the UV absorber. Although the separate treatment of resin or the nano silver had no effect on the improvement of the UV protection properties for treated fabrics, they could increase the UV protection capability when they were combined with the UV absorber. Linen fabrics could possess an antibiosis and deodorizing capability by applying the mixture of the UV absorber, the nano silver, and the resin. The UV protection, crease resistance and flexibility of finished fabrics were maintained even after laundering. Washed treated fabrics maintained excellent antibiosis and odor free capabilities compared to untreated fabrics.

A Study on the Durable Press Finish by Wet-Fixation Processes for Rayon Fabrics (I) - One Bath and Two Bath Processes - (레이온 직물의 Wet-Fixation에 의한 DP가공에 관한 연구(I) - 일욕법과 이욕법의 비교 -)

  • Hu Yoon Sook;Kim Eun Ae
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.13 no.3 s.31
    • /
    • pp.242-251
    • /
    • 1989
  • The purpose of this study was to investigate the changes in easy-care and strength properties of the wet fixation processed viscose rayon fabrics. Rayon fabrics were treated with mixed resins of melamine formaldehyde (MF) and DMDHEU by one bath and two bath wet fixation processes. The MF/DMDHEU mixed resin concentrations were 50/100, 50/150, 100/100, 100/150 and 150/100(g/1). Magnasium chloride was used as a catalyst. Treated fabrics were evaluated by nitrogen content, DP rating, wrinkle recovery angle, breaking strength, tearing strength and abrasion resistance. The properties were compared to the fabrics treated by conventional Pad-Dry-Cure (PDC) method. Wet fixation processed fabrics showed DP ratings of higher than 3 and higher than 275 degrees of wrinkle recovery angles in all the mixed resin concentrations. Wet fixation processed fabrics showed increase in breaking strength and tearing strength but decrease in abrasion resistance. However, the decrease in abrasion resistance was much less than the conventional PDC treated fabrics. The one bath wet fixation processed fabrics showed better physical properties than the two bath processed fabrics in general. The optimum treatment condition was the mixed resin concentration of MF/DMDHEU, 100/100 g/l in one bath wet fixation process.

  • PDF

Effect of DP Finishing Conditions on the Mechanical Properties and Hand of Cotton Fabrics (DP 가공조건이 면직물의 역학적 성질과 태에 미치는 영향)

  • 신윤숙
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.24 no.3
    • /
    • pp.440-447
    • /
    • 2000
  • The effects of DP finishing conditions including process technique and finishing agent on the mechanical properties and hand of cotton fabrics were investigated. 100% cotton fabrics were treated with NMA/DMDHEU and NMA/YF using wet-fixation and steam-fixation process. For comparison, conventional pad-dry-cure process was used with DMDHEU. After DP finishing, tensile and compressional resilience increased and bending hysteresis decreased, resulting in the improvement of dimensional stability of cotton fabric. WF and SF process rendered fabrics better shear properties, tensile energy, and compressional linearity and energy than PDC process. However, SF process produced fabrics with higher geometrical roughness than WF process. After DP finishing, primary hand values except Koshi increased, resulting in the increase of total hand value of cotton fabric.

  • PDF

A Study on the Physical Properties of Durable Press Finished Rayon Fabrics (Durable Press 가공된 레이온직물의 물성변화에 관한 연구)

  • Kim Hee Sook;Kim Eun Ae
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.11 no.3 s.25
    • /
    • pp.57-65
    • /
    • 1987
  • The purpose of this study was to investigate the optimum treatment [condition for the Durable press finish of viscose rayon fabrics. Three types of commercial N-methylol crosslinking agents were applied to the fabric utilizing the pad-dry-cure technique. Changes in physical properties were evaluated for the various resin and catalyst concentrations. For DMU, the effect of different catalysts, $MgCl_2$ and $NH_4Cl$, were also compared. DMU treated fabrics showed in crease recovery angle, tensile strength and tearing strength but drastic decrease in abrasion resistance. DMDHEU and MDMDHEU treated fabrics were similar in most physical properties. However, DMDHEU treated fabrics were better in crease recovery angle and stiffness, and MDMDHEU treated fabrics were better in tensile strength, tearing strength and abrasion resistance. For a given resin system, crease recovery angle, tensile strength and stiffness increased with a increase in resin concentration. Tearing strength showed very little change, while abrasion resistance was decreased significantly as the crease recovery angle was increased. For the treatment of DMU, $MgCl_2$ catalyst was much better than $NH_4Cl$ in all physical properties. When $NH_4Cl$ catalyst was used, strength reduction and discoloration were observed. As the catalyst concentration increased, crease recovery angle, stiffness were increased. Tensile strength and tearing strength were increcased than control but at high catalyst concentration, the strength were decreased and abrasion resistance was significantly lowered. DMDHEU and MDMDHEU were more sensitive to catalyst concentrations than DMU.

  • PDF

Glyoxal에 의한 면직물의 DP가공

  • 김승일;이의소
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 1998.10a
    • /
    • pp.129-132
    • /
    • 1998
  • 지금까지 면직물의 DP가공에 가장 많이 쓰여온 가교제로는 셀룰로오스의 히드록시기와 ether결합을 형성하는 DMDHEU(dimethyloldihydroxyethylene urea) [1] 이나, 인체에 암을 유발시킬 수 있는 포름알데히드를 발생하기 때문에 그 사용이 제한되고 있으며 현재는 셀룰로오스의 히드록시기와 ester형의 가교를 형성하는 polycarboxylic acid와 같이 포름알데히드를 발생하지 않는 가교제에 대한 연구가 활발히 진행되고 있다. (중략)

  • PDF