• Title/Summary/Keyword: Cyclic cooling

Search Result 66, Processing Time 0.03 seconds

Glass Forming Ability of Bulk Amorphous Alloy Scrap by Fluxing (플럭스처리에 의한 벌크비정질합금 스크랩의 비정질형성능)

  • Kang, Bok-Hyun;Kim, Ki-Young
    • Journal of Korea Foundry Society
    • /
    • v.30 no.3
    • /
    • pp.94-99
    • /
    • 2010
  • When the returned scrap of bulk amorphous alloy is remelted, impurities such as oxides and intermetallic compounds increase. Glass forming ability of its scrap is deteriorated remarkably. Melt fluxing technique is introduced to enhance the glass forming ability during melting and freezing of bulk amorphous alloys. Cu and Zr based alloys are chosen. Small pieces of these alloy scraps and $B_2O_3$ flux are put together in a quartz tube. Cyclic heating and cooling are done by induction heating and water quenching or air cooling. Melting fluxing was effective for both Cu-based and Zr-based alloy, and their glass forming abilities were improved with increasing the number of fluxing.

Numerical analysis of the vertical tube-in-tube ground coil heat exchanger (수직으로 매설된 이중관형 지중 열교환기에 대한 해석적인 연구)

  • 유지오;금성민;신현준
    • Korean Journal of Air-Conditioning and Refrigeration Engineering
    • /
    • v.11 no.3
    • /
    • pp.339-348
    • /
    • 1999
  • A computer model was developed in order to predict the temperature distribution and the performance of the vertical tube-in-tube ground coil heat exchanger. This model has been validated by experimental results conducted by ORNL. The heat exchanger performance with the variation of the length is calculated and compared. As results, the heat exchanger performance is proportional to the length but the performance per unit length decreases. The minimum performance of 70m - PVC heat exchanger during cyclic operation for a week is obtained 20,054kJ/h for cooling operation and 13,915kJ/h for heating operation. And minimum temperature difference is $4.64^{\circ}C$ for cooling operation and $2.64^{\circ}C$ for heating operation. In each case, it is noted that the temperature difference between the pipe and the far-field occurs within 0.8m from the heat exchanger.

  • PDF

The performance evaluation of Stirling cryocooler for thermal imaging system (III) : Thermal environmental test (열상장비용 스터링 극저온 냉동기 특성평가 (III) : 열환경시험)

  • 김양훈;박성제;홍용주;김효봉;고득용;이승홍;나종문
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2003.10a
    • /
    • pp.163-166
    • /
    • 2003
  • This paper presents the results of a series of performance tests for the Stilting cryocooler. Infrared sensor systems incorporating cryocoolers are required to be qualified to the appropriate environmental specification. Linear drive Stilting cryocooler have matured to the stage of undergoing formal qualification test program The thermal environmental test of the Stilting cryocooler is presented in this paper. We performed that low and high temperature keeping test from -4$0^{\circ}C$ to +6$0^{\circ}C$ and operating test at high and low temperature cyclic range with acceptance tests performed at scheduled intervals. Cooling capacity was determined as a function of cooler components temperatures at the compressor, hot end and cold tip. Tests performed on this cooler have been successful with a measured cooling performance of more than 0.8W@80K for 23$^{\circ}C$ ambient temperature with 40 $W_{ac}$ input power.

  • PDF

The Influences of the Refrigerant Adulteration by an Absorbent on the Cooling Capacity and COP of the Absorption Chiller (흡수식 냉동기에서 흡수액이 증발기로 혼입시 냉각용량과 성능계수에 미치는 영향)

  • Park, Chan-Woo
    • Korean Journal of Air-Conditioning and Refrigeration Engineering
    • /
    • v.18 no.9
    • /
    • pp.753-760
    • /
    • 2006
  • The purpose of the present work is to investigate the influence of the refrigerant adulteration by LiBr solution on the cooling capacity and COP for three different types of abso게tion chillers: a single-effect type, a series-flow double-effect type and a parallel-flow with double-effect type. A simulation program has been prepared for the cyclic analysis of absorption chillers. With some assumptions, the calculations have been performed by solving the mass balance equation, energy balance equation and the state equation simultaneously. The range of the LiBr concentration of refrigerant was 0% to 20% in the present study. For the single-effect absorption chiller, the maximum decrease in the cooling capacity was 10% at the 20% of LiBr concentration. For the double-effect chiller, the capacity was decreased by 11.1% for the parallel-flow type and the series-flow type. Also, the COP was reduced by 3.0% in single-effect, 2.8% in series-flow type (SR=0.4) and 2.3% in parallel-flow type.

Performance and Reliability Characteristics of the Free Piston Free Displacer Stirling Cryocooler

  • Park, Seong-Je;Hong, Yong-Ju;Kim, Hyo-Bong;Koh, Deuk-Yong;Kim, Yang-Hoon
    • Progress in Superconductivity and Cryogenics
    • /
    • v.6 no.2
    • /
    • pp.46-51
    • /
    • 2004
  • This paper presents the results of a series of performance and reliability tests for the Stirling cryocooler. Infrared sensor systems incorporating cryocoolers are required to be qualified to the appropriate specification for the performance and reliability. FPFD Stirling cryocooler is currently under development for cooling infrared detector. Manufactured Stirling cryocooler delivers approximately 0.9W cooling at 80K for 30W∼40W of input power. It takes approximately 2 minutes to cool down to 80K at the ambient temperature of 23$^{\circ}C$. Performance characteristics for the vibration, acoustic noise, EMI and leak rate of the Stirling cryocooler are evaluated. We performed low and high temperature keeping test from -32$^{\circ}C$ to +52$^{\circ}C$ and operating test at high and low temperature cyclic range with acceptance tests performed at scheduled intervals. Cooling capacity is determined as a function of the temperatures at the compressor, hot end and cold tip at the expander. Finally, we describe the experimental facility for the MTTF evaluation and some typical results of the Stirling cryocooler.

Cyclic fatigue resistance, torsional resistance, and metallurgical characteristics of M3 Rotary and M3 Pro Gold NiTi files

  • Pedulla, Eugenio;Lo Savio, Fabio;La Rosa, Giusy Rita Maria;Miccoli, Gabriele;Bruno, Elena;Rapisarda, Silvia;Chang, Seok Woo;Rapisarda, Ernesto;La Rosa, Guido;Gambarini, Gianluca;Testarelli, Luca
    • Restorative Dentistry and Endodontics
    • /
    • v.43 no.2
    • /
    • pp.25.1-25.10
    • /
    • 2018
  • Objectives: To evaluate the mechanical properties and metallurgical characteristics of the M3 Rotary and M3 Pro Gold files (United Dental). Materials and Methods: One hundred and sixty new M3 Rotary and M3 Pro Gold files (sizes 20/0.04 and 25/0.04) were used. Torque and angle of rotation at failure (n = 20) were measured according to ISO 3630-1. Cyclic fatigue resistance was tested by measuring the number of cycles to failure in an artificial stainless steel canal ($60^{\circ}$ angle of curvature and a 5-mm radius). The metallurgical characteristics were investigated by differential scanning calorimetry. Data were analyzed using analysis of variance and the Student-Newman-Keuls test. Results: Comparing the same size of the 2 different instruments, cyclic fatigue resistance was significantly higher in the M3 Pro Gold files than in the M3 Rotary files (p < 0.001). No significant difference was observed between the files in the maximum torque load, while a significantly higher angular rotation to fracture was observed for M3 Pro Gold (p < 0.05). In the DSC analysis, the M3 Pro Gold files showed one prominent peak on the heating curve and 2 prominent peaks on the cooling curve. In contrast, the M3 Rotary files showed 1 small peak on the heating curve and 1 small peak on the cooling curve. Conclusions: The M3 Pro Gold files showed greater flexibility and angular rotation than the M3 Rotary files, without decrement of their torque resistance. The superior flexibility of M3 Pro Gold files can be attributed to their martensite phase.

Effect of Annealing Heat Treatment to Corrosion Resistance of a Copper (구리의 내식성에 미치는 어닐링 열처리의 영향)

  • Kim Jin-Kyung;Moon Kyung-Man;Lee Jin-Kyu
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.29 no.6
    • /
    • pp.654-661
    • /
    • 2005
  • Copper is a well known alloying element that is used to improve the resistance to general corrosion of stainless steel And also Cu cation have the anti-fouling effect to inhibit adhesion of the marine algae and shellfish to the surface of heat exchanger cooling pipe or outside wall of the ship, Therefore there are some anti-fouling methods such as anti-fouling Paint mixed with copper oxide or MGPS(Marine Growth Preventing System) by using Cu cation dissolved to the sea wather solution. Cu cation can be dissolved spontaneously by galvanic current due to Potential difference between Cu and cooling pipe of heat exchanger with Ti material, which may be one of the anti-fouling designs. In this study the effect of annealing heat treatment to galvanic current and Polarization behavior was investigated with a electrochemical points of view such as measurement of corrosion Potential, anodic polarization curve. cyclic voltammetric curve, galvanic current etc The grain size of the surface in annealed at $700^{\circ}C$ was the smallest than that of other annealing temperatures. and also the corrosion Potential showed more positive potential than other annealing temperatures. The galvanic current between Ti and Cu with annealed at $700^{\circ}C$ was the largest value in the case of static condition. However its value in the case of flow condition was the smallest than the other temperatures. Therefore in order to increase anti-fouling effect by Cu cation, the optimum annealing temperature in static condition of sea water is $700^{\circ}C$, however non- heat treated specimen in the case of flow condition may be desirable.

Fatigue Characteristics of Laser Welded Zirconium Alloy Thin Sheet (레이저 용접된 박판 지르코늄 합금의 피로특성)

  • Jeong, Dong-Hee;Kim, Jae-Hoon;Yoon, Yong-Keun;Park, Joon-Kyoo;Jeon, Kyeong-Rak
    • Journal of Welding and Joining
    • /
    • v.30 no.1
    • /
    • pp.59-63
    • /
    • 2012
  • The spacer grid is one of the main structural components in a fuel assembly. It supports fuel rods, guides cooling water and maintains geometry from external impact load and cyclic stress by the vibration of nuclear fuel rod, it is necessary to have sufficient strength against dynamic external load and fatigue strength. In this study, the mechanical properties and fatigue characteristics of laser beam welded zircaloy thin sheet are examined. The material used in this study is a zirconium alloy with 0.66 mm of thickness. The fatigue strength under cyclic load was evaluated at stress ratio R=0.1. S-N curves are presented with statistical testing method recommend by JSME- S002 and compared with S-N curves at R.T. and $315^{\circ}C$. As a result of the experimental approach, the design guide of fatigue strength is proposed and the results obtained from this study are expected to be useful data for spacer gird design.

The Effect of Pre-strain on Cyclic Deformation Characteristic of Ti-Ni Alloy (Ti-Ni합금의 반복변형특성에 미치는 pre-strain의 효과)

  • 박영철;조용배;허선철
    • Journal of Ocean Engineering and Technology
    • /
    • v.9 no.1
    • /
    • pp.101-110
    • /
    • 1995
  • In SMA(Shape Memory Alloy), the degradation by fatigue is one of the most important problems to be overcome, when SMA is used for robot-actuator materials. The actuator is operated repetitively for long time and its repeating operation develops the fatigue degradation of SMA. The fatigue degradation changes the transformation temperature and deformation behavior and results in inaccurate operation and deformation which results form repeating operation is to be investigated in advance and the scheme to resolve those problems have to be made for the design of actuator. In this paper, for the improvement of the fatigue degradation by repetive movement and better control of the correct movement by the stability of martensite transformation in the development of Robots actuator, Pre-strain(0, 1.5, 5, 8%) are loaded in the specimens and fatigue testing were carried out by the method of heating and cooling in direct condition. From the results of these experiments, the effect on pre-strain which affect the transformation characteristic and fatigue degradation phenomena were correctly investigated.

  • PDF

Evaluation for Fatigue Life of Rubber Isolator for Vibration Characteristic on Automotive Cooling Module (진동 특성을 고려한 자동차 냉각모듈 방진고무의 내구성 평가)

  • Shim, Hee-Jin;Kim, Han-Chul;Kim, Jung-Kyu
    • Proceedings of the KSME Conference
    • /
    • 2008.11a
    • /
    • pp.350-355
    • /
    • 2008
  • A Rubber mount is widely used for mechanical parts or engineering materials. Especially, it plays an important role in reducing mechanical vibration due to cyclic loading. But, rubber mount is damaged due to the cyclic loading and resonance. Therefore, it is necessary to investigate evaluation of fatigue life considering vibration characteristics for rubber. In this study, a vibration fatigue analysis was performed and based on Power Spectral Density(PSD) and the stress-life curve and a result of frequency response analysis in the finite element method. The measured load history in experiment was transformed to PSD curve. The stress-life curve was obtained by nonlinear static analysis and fatigue test. In addition, frequency response analysis was conducted for mechanical part. In order to evaluate fatigue life of rubber mount, vibration fatigue test was conducted at the constant acceleration-level as well. Fatigue life was determined when the load capacity is reduced to 60% of its initial value. As a result, predicted fatigue life of rubber mount agreed fairly well with the experimental fatigue life.

  • PDF