Hydrogenation and Electrochemical Characteristics of Amorphous-nanostructured Mg-based Alloys

  • Gebert, A.;Khorkounov, B.;Schultz, L.
    • Journal of Powder Materials
    • /
    • v.13 no.5 s.58
    • /
    • pp.327-335
    • /
    • 2006
  • In the development of new hydrogen absorbing materials for a next generation of metal hydride electrodes for rechargeable batteries, metastable Mg-Ni-based compounds find currently special attention. Amor phous-nanocrystalline $Mg_{63}Ni_{30}Y_7$ and $Mg_{50}Ni_{30}Y_{20}$ alloys were produced by mechanical alloying and melt-spinning and characterized by means of XRD, TEM and DSC. On basis of mechanically alloyed Mg-Ni-Y powders, complex hydride electrodes were fabricated and their electrochemical behaviour in 6M KOH (pH=14,8) was investigated. The electrodes made from $Mg_{63}Ni_{30}Y_7$ powders, which were prepared under use of a SPEX shaker mill, with a major fraction of nanocrystalline phase reveal a higher electrochemical activity far hydrogen reduction and a higher maximum discharge capacity (247 mAh/g) than the electrodes from alloy powder with predominantly amorphous microstructure (216 mAh/g) obtained when using a Retsch planetary ball mill at low temperatures. Those discharge capacities are higher that those fur nanocrystalline $Mg_2Ni$ electrodes. However, the cyclic stability of those alloy powder electrodes was low. Therefore, fundamental stability studies were performed on $Mg_{63}Ni_{30}Y_7$ and $Mg_{50}Ni_{30}Y_{20}$ ribbon samples in the as-quenched state and after cathodic hydrogen charging by means of anodic and cathodic polarisation measurements. Gradual oxidation and dissolution of nickel governs the anodic behaviour before a passive state is attained. A stabilizing effect of higher fractions of yttrium in the alloy on the passivation was detected. During the cathodic hydrogen charging process the alloys exhibit a change in the surface state chemistry, i.e. an enrichment of nickel-species, causing preferential oxidation and dissolution during subsequent anodization. The effect of chemical pre-treatments in 1% HF and in $10\;mg/l\;YCl_3/1%\;H_2O_2$ solution on the surface degradation processes was investigated. A HF treatment can improve their anodic passivation behavior by inhibiting a preferential nickel oxidation-dissolution at low polarisation, whereas a $YCl_3/H_2O_2$ treatment has the opposite effect. Both pre-treatment methods lead to an enhancement of cathodically induced surface degradation processes.

Variations of the Electrochemical Properties of LiMn2O4 with the Calcining Temperature

  • Song, Myoung-Youp;Shon, Mi-suk
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.6
    • /
    • pp.523-527
    • /
    • 2002
  • LiMn$_2$O$_4$ compounds were synthesized by calcining a mixture of LiOH and MnO$_2$(CMD) at 47$0^{\circ}C$ for 10 h and then calcining again at $650^{\circ}C$ to 90$0^{\circ}C$ fur 48 h in air with intermediate grinding. All the synthesized samples exhibited XRD patterns for the cubic spinel phase with a space group Fd3m. The lattice parameter increased gradually as the sintering temperature rose. The electrochemical cells were charged and discharged fur 20 cycles at a current density 300$\mu$A/$\textrm{cm}^2$ between 3.5 V and 4.3 V. The voltage vs. discharge capacity curves for all the samples showed two plateaus. The LiMn$_2$O$_4$ sample calcined at 90$0^{\circ}C$ had the largest first discharge capacity. This sample exhibited the best crystallinity, had relatively large lattice parameter and had relatively large particles with rectatively homogeneous size. All the samples showed good cycling performances. Among all the samples, the LiMn$_2$O$_4$ calcined at 85$0^{\circ}C$ had relatively large first discharge capacity and very good cycling performance. The addition of excess LiOH and the mixing in ethanol considered to help the formation of the more LiMn$_2$O$_4$ phase per unit weight sample and the more stable LiMn$_2$O$_4$phase. These led to the larger discharge capacities and the better cycling performances. The cyclic voltammograms fur the second cycle of the LiMn$_2$O$_4$ samples showed the oxidation and reduction peaks around 4.05 V and 4.18 V and around 4.08 V and 3.94 V, respectively. The larger first discharge capacity of the sample calcined at the higher temperature is related to the larger lattice parameter.

Effects of Melatonin on the Meiotic Maturation of Mouse Oocytes in vitro (생쥐 난자의 체외 성숙에 미치는 Melatonin의 영향)

  • Ahn, Hee-Jin;Bae, In-Ha
    • Clinical and Experimental Reproductive Medicine
    • /
    • v.31 no.3
    • /
    • pp.155-168
    • /
    • 2004
  • Objective: Melatonin, which is secreted by pineal gland play an important role in the regulation of ovarian function via seasonal rhythm and sleep in most mammals. It also has a role in the protection of cells by removing toxic oxygen free radicals brought about by metabolism. In the present study, effects of melatonin on the mouse oocyte maturation were examined using two different culture conditions provided with 5% or 21% oxygen concentration. Material and Method: Immature mouse oocytes were obtained from the ovarian follicles of $3{\sim}4$ weeks old ICR strain mice intraperitoneally injected with 5 I.U. PMSG 44 hour before. Under stereomicroscope, morphologically healthy oocytes with distinct germinal vesicle (GV) were liberated from the graafian follicles and collected using mouth-controlled micropipette. They were then cultured for 17 hour at $37^{circ}C$, 5% $CO_2$ and 21% $O_2$ (95% air) or 5% $CO_2$, 5% $O_2$ and 90% $N_2$. New modified Hank's balanced salt solution (New MHBS) was used as a culture medium throughout the experiments. Effects of melatonin were examined at a concentration of $0.0001{\mu}M$, $0.01{\mu}M$ or $1.0{\mu}M$. For the prevention of spontaneous maturation of immature oocytes during culture, dibutyryl cyclic AMP (dbcAMP) and/or hypoxanthine were included in the medium. Results: Under 21% oxygen condition, oocytes cultured in the presence of $0.01{\mu}M$ melatonin showed a significantly higher maturation rates, in terms of germinal vesicle breakdown (95.0% vs 89.0%) and polar body formation (88.1% vs 75.4%), compared to those cultured with $0.0001{\mu}M$ or $1.0{\mu}M$ melatonin. However, no difference was observed in oocytes cultured under 5% oxygen whether they were treated with melatonin or not. In the presence of $0.01{\mu}M$ melatonin, oocytes either cultured under 21% or 5% oxygen exhibited no difference in the polar body formation (85.6% vs 86.7%). However, in the absence of melatonin, oocytes cultured under 21% oxygen exhibited lower polar body formation (74.7%). When oocytes were cultured in the presence of dbcAMP alone or with varying concentrations of melatonin, those treated with both compounds always showed better maturation, i.e., germinal vesicle breakdown and polar body formation, compared to those cultured with dbcAMP alone. At the same concentration of melatonin, however, oocytes exposed to 21% oxygen showed poor maturation than those to 5% oxygen. Similar results were obtained from the experiments using hypoxanthine instead of dbcAMP. Conclusion: Based upon these results, it is suggested that melatonin could enhance the meiotic maturation of mouse oocytes under 21% oxygen concentration, and release oocytes from the meiotic arrest by dbcAMP or hypoxanthine regardless of the concentration of oxygen, probably via the removal of oxygen free radicals.

Comparison of the Effects of Cyclodextrin-Naringin Inclusion Complex with Naringin on Lipid Metabolism in Mice Fed a High-Fat Diet (고지방식이를 섭취한 마우스에서 나린진과 나린진-사이클로텍스트린 포접화합물의 지질대사에 대한 영향 비교)

  • Jeon, Seon-Min;Choi, Myung-Sook
    • Journal of the East Asian Society of Dietary Life
    • /
    • v.20 no.1
    • /
    • pp.20-29
    • /
    • 2010
  • Naringin has antioxidant and antihyperlipidemic properties, however, phenolic compounds including naringin are unstable in the presence of light, heat and oxygen. Beta-cyclodextrin ($\beta$-CD) is a cyclic heptamer composed of seven glucose units that enhances the stability and solubility of molecules through the formation of inclusion complexes. This study was conducted out to compare the effects of CD-naringin (CD-N) inclusion complexes with naringin on lipid metabolism in high fat-fed animals. Male C57BL/6 mice were fed either CD-N (0.048%, w/w) or naringin (N, 0.02%, w/w) in a 20% high-fat (HFC, 15% lard, 5% corn oil, w/w) diet for 10 weeks. Orlistat (Xenical, 0.01%, w/w) was used as a positive control (PC). There were no differences in body weight, food intake, liver and heart weights, plasma triglyceride(TG), leptin, adiponectin, resistin, IL-$1{\beta}$ and IL-6 concentrations, and hepatic $\beta$-oxidation, carnitine palmitoyl transferase(CPT), glucose-6-phosphate dehydrogenase (G6PD) and malic enzyme activities between the HFC and CD-N groups or between the HFC and N groups. However, both CD-naringin and naringin supplementation les to a significant reduction in the epididymal and perirenal white adipose tissue weights, plasma free fatty acid, insulin and blood glucose concentrations, hepatic cholesterol and TG contents and hepatic fatty acid synthase (FAS), phosphatidate phosphohydrolase (PAP) and HMG-CoA reductase activities compared to the HFC group. The plasma HDL-cholesterol concentration was significantly higher in CD-N and N groups than in HF and PC groups. These results indicate that both CD-naringin and naringin supplementation effectively improved plasma and hepatic lipid metabolism without differences between CD-N and naringin groups.