  • Vacuum interrupters in order to be used in various switch-gear components such as circuit breakers, distribution switches, contactors, etc. spread the arc uniformly over the surface of the contacts. The electrodes of vacuum interrupters are made of sinter-forged Cu-Cr materials for good electrical and mechanical characteristics. Since the closing velocity is 1-2m/s and impact deformation of the electrode depends on the strain rate at that velocity, the dynamic behavior of the sinter-forged Cu-Cr is a key to investigate the impact characteristics of the electrodes. The dynamic response of the material at intermediate strain rate is obtained from the high speed tensile test machine test and at the high strain rate is obtained from the split Hopkinson pressure bar test. Experimental results from both quasi-static and dynamic compressive tests are interpolated to construct the Johnson-Cook model as the constitutive relation that should be applied to simulation of the dynamic behavior of the electrodes. The impact characteristics of a vacuum interrupter are investigated with computer simulations by changing the amount of chromium content.

  • PDF

로켓엔진용 구리크롬 합금의 저주기 피로수명 예측방법 비교 및 평가 (Comparison and Evaluation of Low-Cycle Fatigue Life Prediction Methods Using Cu-Cr Alloy Developed for Rocket Engines)

  • 박종찬;김재훈;이금오
    • 한국추진공학회지
    • /
    • 제26권5호
    • /
    • pp.1-10
    • /
    • 2022
  • 로켓엔진용으로 개발된 구리크롬 합금에 대해 저주기 피로시험을 수행하고 여러가지 피로수명 예측방법을 이용해 예측수명을 구하여 이를 시험수명과 비교하여 보았다. 피로수명 예측방법으로는 Coffin-Manson 관계식, 소성 및 전 변형률 에너지 밀도 관계식, Smith-Watson-Topper 관계식, Tomkins 관계식, Jahed-Varvani 관계식 등 총 6가지 방법을 이용하였다. 피로 예측수명을 계산한 결과 모든 방법에서 시험수명 대비 분산범위 2 이내를 만족하였다. 예측수명 편차의 정량적 확인을 통해 전 변형률 에너지 밀도 관계식이 가장 우수한 결과를 나타냈다.

Transformation Behavior of Ti-(45-x)Ni-5Cu-xCr (at%) (x = 0.5-2.0) Shape Memory Alloys

  • Im, Yeon-Min;Jeon, Young-Min;Kim, Min-Su;Lee, Yong-Hee;Kim, Min-Kyun;Nam, Tae-Hyun
    • Transactions on Electrical and Electronic Materials
    • /
    • 제12권1호
    • /
    • pp.28-31
    • /
    • 2011
  • Transformation behavior and shape memory characteristics of Ti-(45-x)Ni-5Cu-xCr (x=0.5-2.0) alloys have been investigated by means of electrical resistivity measurements, differential scanning calorimetry, X-ray diffraction and thermal cycling tests under constant load. Two-stage B2-B19-B19' transformation occurred in Ti-(45-x)Ni-5Cu-xCr alloys. The B2-B19 transformation was separated clearly from the B19-B19' transformation in Ti-44.0Ni-5Cu-1.0Cr and Ti-43.5Ni-5Cu-1.5Cr alloys. A temperature range where the B19 martensite exists was expanded with increasing Cr content because decreasing rate of Ms (85 K / % Cr) was larger than that of Ms' (17 K / % Cr). Ti-(45-x)Ni-5Cu-xCr alloys were deformed in plastic manner with a fracture strain of 68% ~ 43% depending on Cr content. Substitution of Cr for Ni improves the critical stress for slip deformation in a Ti-45Ni-5Cu alloy due to solid solution hardening.

플라즈마분체 오버레이법에 의한 알루미늄합금 표면의 경화특성에 관한 연구( II ) -후막 표면 합금화층의 경화특성과 내마모성- (Hardening Characteristics of Aluminum Alloy Surface by PTA Overlaying with Metal Powders (II) -Hardening charactersteristics and wear resistance of thicker surface alloyed layer-)

  • 이규천;;강원석;이영호
    • Journal of Welding and Joining
    • /
    • 제12권4호
    • /
    • pp.102-109
    • /
    • 1994
  • The thick and hard alloyed layer was formed on the surface of Aluminum Cast Alloy(AC2B) by PTA overlaying process with Cr, Cu and Ni metal powders under the condition of overlaying current 150A, overlaying speed 150mm/min and different powder feeding rate 5-20g/min. The characteristics of hardening and were resistance of alloyed layer have been investigated in relation to microstructure of alloyed layer. As a result, it was made clear that Cu powder was the most superier one in three metal powders used due to an uniform hardness distribution of Hv 250-350, good wear resistance and freedom from cracking in alloyed layer of which microstructure consisted of hypereutectic. On the contrary, irregular hardness distribution was usually obtained in Cr or Ni alloyed layers of which hardness was increased as Cr or Ni contents and reached to maximum hardness of about Hv 400-850 at about 60wt% Cr or 40wt% Ni in alloyed layer. However the cracking occurred in these alloyed layers with higher hardness than Hv 250-300 at more than 20-25wt% of Cr or Ni contents in alloyed layer. Wear rate of alloyed layer was decreased to 1/10 in Cu alloyed layer and 1/5 or 1/3 in Cr or Ni alloyed layer with same hardness of about Hv 300 in comparison with that of base metal at higher sliding speed.

  • PDF

크롬동합금의 시효석출거동에 미치는 Cr 첨가량의 영향 (Effect of Cr Contents on Precipitation Process of Cu-Cr Alloys)

  • 구본흔;전검배;이찬규;김창주
    • 열처리공학회지
    • /
    • 제18권5호
    • /
    • pp.305-311
    • /
    • 2005
  • Effect of Cr contents(Cr: 0.27, 0.45 and 0.65wt.%) on precipitation process has been studied by electrical resistivity measurements, hardness and scanning electron microscope. The first stage of the process consists of the formation of Cr-rich particles, the second stage consists of the competitive growth of these particles. The kinetics of precipitation could be described by Johnson-Mehl-Avrami equation, $f(t)=1-\exp(-kt^n)$. The values of n were found to be in the range from 0.17 to 0.39 at the first stage and from 1.0 to 1.5 at the second stage. The activation energies of Cu-Cr alloys were determined by Cross-Cut method and were 90~136 kJ/mol. The maximum hardness value of $H_RB$ 84 was obtained in Cu-0.65wt.%Cr alloy.

DEVELOPMENT OF TITANIUM-BASED BRAZING FILLER METALS WITH LOW-MELTING-POING

  • Onzawa, Tadao;Tiyama, Takashi
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.539-544
    • /
    • 2002
  • Titanium and titanium alloy are excellent in corrosion resistance and specific intensity, and also in the biocompatibility. On the other hand, the brazing is bonding method of which productivity and reliability are high, when the complicated and precise structure of the thin plate is constructed. However, though conventional titanium-based brazing filler metal was excellent in bond strength and corrosion resistance, it was disadvantageous that metal structure and mechanical property of the base metal deteriorated, since the brazing temperature (about 1000 C) is considerably high. Authors developed new brazing filler metal which added Zr to Ti-Cu (-Ni) alloy which can be brazed at 900 C or less about 15 years ago. In this paper, the development of more low-melting-point brazing filler metal was tried by the addition of the fourth elements such as Ni, Co, Cr for the Ti-Zr-Cu alloy. As a method for finding the low-melting-point composition, eutectic composition exploration method was used in order to reduce the experiment point. As the result, several kinds of new brazing filler metal such as 37.5Ti-37.5-Zr-25Cu alloy (melting point 825 C) and 30Ti-43Zr-25Cu-2Cr alloy (melting point: 825 C) was developed. Then, the brazing joint showed the characteristics which were almost equal to the base metal from the result of obtaining metallic structure and strength of joint of brazing joint. However, the brazing filler metal composition of the melting point of 820 C or less could not be found. Consequentially, it was clarified that the brazing filler metal developed in this study could be practically sufficiently used from results such as metal structure of brazing joint and tensile test of the joint.

  • PDF

Development of Titanium-based Brazing Filler Metals with Low-melting-point

  • Onzawa, T.;Iiyama, T.
    • International Journal of Korean Welding Society
    • /
    • 제2권2호
    • /
    • pp.14-18
    • /
    • 2002
  • Titanium and titanium alloy are excellent in corrosion resistance and specific intensity, and also in the biocompatibility. On the other hand, the brazing is bonding method of which productivity and reliability are high, when the complicated and precise structure of the thin plate is constructed. However, though conventional titanium-based brazing filler metal was excellent in bond strength and corrosion resistance, it was disadvantageous that metal structure and mechanical property of the base metal deteriorated, since the brazing temperature ( about $1000^{\circ}C$ ) is considerably high. Authors developed new brazing filler metal which added Zr to Ti-Cu (-Ni) alloy which can be brazed at $900^{\circ}C$ or less about 15 years ago. In this paper, the development of more low-melting-point brazing filler metal was tried by the addition of the fourth elements such as Ni, Co, Cr for the Ti-Zr-Cu alloy. As a method for finding the low-melting-point composition, eutectic composition exploration method was used in order to reduce the experiment point. As the result, several kinds of new brazing filler metal such as 37.5Ti-37.5-Zr-25Cu alloy (melting point: $825^{\circ}C$) and 30Ti-43Zr-25Cu-2Cr alloy (melting point: $825^{\circ}C$) was developed. Then, the brazing joint showed the characteristics which were almost equal to the base metal from the result of obtaining metallic structure and strength of joint of brazing joint. However, the brazing filler metal composition of the melting point of $820^{\circ}C$ or less could not be found. Consequentially, it was clarified that the brazing filler metal developed in this study could be practically sufficiently used from results such as metal structure of brazing joint and tensile test of the joint.

  • PDF

공정변수에 의한 Ni/Cr/Al/Cu계 박막의 전기적 특성 (The effect of the process parameters on the electrical properties of Ni/Cr/Al/Cu alloy thin film)

  • 이붕주;박상무;박구범;박종관;이덕출
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.725-728
    • /
    • 2001
  • We have fabricated thin films using the DC/RF magnetron sputtering of 74wt%Ni-l8wt%Cr-4wt%Al-4wt%Cu alloy target and studied the effect of the process parameters on the electrical properties for low TCR(Temperature Coefficient of Resistance) films. In sputtering process, pressure, power and substrate temperature, are varied as controllable parameter. The films are annealed to 400$^{\circ}C$ in air and nitrogen atmosphere. The sheet resistance, TCR of the films increases with increasing annealing temperature. It abruptly increased as annealing temperature increased over 300$^{\circ}C$ in air atmosphere. From XRD, it is found that these results are due to the existence of NiO on film surface formed by annealing. As a results of them, TCR can be controlled by variation of sputter process parameter and annealing of thin film.