• Title/Summary/Keyword: Creep-Rupture Time

Search Result 112, Processing Time 0.027 seconds

Creep Properties of Superalloy Udimet 720 in relation to Exposed (초내열합금 U720의 노출시험에 따른 크리프 특성)

  • Kong, Y.S.;Oh, S.K.
    • Journal of Power System Engineering
    • /
    • v.5 no.2
    • /
    • pp.57-62
    • /
    • 2001
  • Gas turbine performance is highly dependent on the engine performance which is closely related to the engine materials since they are exposed to severe working environments, i.e, high temperature and high stresses. For this reason, advanced materials with improved properties are required for the engine. The purpose of this research is to develop key materials technologies for aircraft industry and to tester domestic production of related parts. In this paper, the real-time prediction of high temperature creep strength and creep life for nickel-based superalloy Udimet 720(high-temperature and high-pressure the gas turbine engine materials) was performed on round-bar type specimens under pure load at the temperatures of 538, 649 and $704^{\circ}C$.

  • PDF

Long-term Creep Strain-Time Curve Modeling of Alloy 617 for a VHTR Intermediate Heat Exchanger (초고온가스로 중간 열교환기용 Alloy 617의 장시간 크리프 변형률-시간 곡선 모델링)

  • Kim, Woo-Gon;Yin, Song-Nam;Kim, Yong-Wan
    • Korean Journal of Metals and Materials
    • /
    • v.47 no.10
    • /
    • pp.613-620
    • /
    • 2009
  • The Kachanov-Rabotnov (K-R) creep model was proposed to accurately model the long-term creep curves above $10^5$ hours of Alloy 617. To this end, a series of creep data was obtained from creep tests conducted under different stress levels at $950^{\circ}C$. Using these data, the creep constants used in the K-R model and the modified K-R model were determined by a nonlinear least square fitting (NLSF) method, respectively. The K-R model yielded poor correspondence with the experimental curves, but the modified K-R model provided good agreement with the curves. Log-log plots of ${\varepsilon}^{\ast}$-stress and ${\varepsilon}^{\ast}$-time to rupture showed good linear relationships. Constants in the modified K-R model were obtained as ${\lambda}$=2.78, and $k=1.24$, and they showed behavior close to stress independency. Using these constants, long-term creep curves above $10^5$ hours obtained from short-term creep data can be modeled by implementing the modified K-R model.

A Study on the Creep Deformation Characteristic of AZ31 Mg Alloy at High Temperature (AZ3l 마그네슘 합금의 고온 크리이프 변형특성에 관한 연구)

  • An Jungo;Kang Daemi;Koo Yang;Sim Sungbo
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.13 no.3
    • /
    • pp.186-192
    • /
    • 2005
  • The apparent activation energy Qc, the applied stress exponent n, and rupture life have been determined from creep test results of AZ31 Mg alloy over the temperature range of 200$^{\circ}C$ to 300$^{\circ}C$ and the stress range of 23.42 MPa to 93.59 MPa, respectively, in order to investigate the creep behavior. Constant load creep tests were carried out in the equipment including automatic temperature controller with data acquisition computer. At the temperature of $200^{\circ}C{\sim}220^{\circ}C$ and under the stress level of 62.43~93.59 MPa, and at around the temperature of $280^{\circ}C{\sim}300^{\circ}C$ and under the stress level of 23.42~39.00 MPa, the creep behavior obeyed a simple power-law relating steady state creep rate to applied stress and the activation energy fur the creep deformation was nearly equal to that of the self diffusion of Mg alloy including aluminum From the above results, at the temperature of $200^{\circ}C{\sim}220^{\circ}C$ the creep deformation for AZ31 Mg alloy seemed to be controlled by dislocation climb but controlled by dislocation glide at $280^{\circ}C{\sim}300^{\circ}C$ .And relationship beween rupture time and stress at around the temperature of $200^{\circ}C{\sim}220^{\circ}C$ and under the stress level of 62.43~93.59 MPa, and again at around the temperature of $280^{\circ}C{\sim}300^{\circ}C$ and under the stress level of 23.42~39.00 MPa, respectively, appeard as fullow; log$\sigma$=-0.18(T+460)(logtr+21)+5.92, log$\sigma$ = -0.25(T+460)(logtr+21)+8.02 Also relationship beween rupture time and steady state creep rate appears as follow; ln$\dot$ =-0.881ntr-2.45

Creep Properties of Aircraft Gas Turbine Materials in relation to Heat Treatment (항공기용 가스터빈 재료의 열처리에 따른 크리프 특성)

  • Kong, Yu-Sik;Oh, Sae-Kyoo;Park, No-Kwang
    • Journal of Ocean Engineering and Technology
    • /
    • v.13 no.4 s.35
    • /
    • pp.112-117
    • /
    • 1999
  • In this paper, the creep properties and creep life prediction by Larson-Miller Parameter method for Udimet 720 to be used for aircraft gas turbine engines or other high temperature components were presented at the elevated temperatures of 538, 649 and $704^{\circ}C$. It was confirmed experimentally and quantitatively that a creep life predictive equation at such various high temperatures was well derived by LMP.

  • PDF

Standard Error Analysis of Creep-Life Prediction Parameters of Type 316LN Stainless Steels (Type 316LN 강의 크리프 수명예측 파라메타의 표준오차 분석)

  • Kim, Woo-Gon;Yoon, Song-Nam;Ryu, Woo-Seog
    • Proceedings of the KSME Conference
    • /
    • 2004.04a
    • /
    • pp.19-24
    • /
    • 2004
  • A number of creep data were collected and filed for type 316LN stainless steels through literature survey and experimental data produced in KAERI. Using these data, polynomial equations for predicting creep life were obtained for Larson Miller (L-M), Qrr-Sherby-Dorn (O-S-D) and Manson-Haferd (M-H) parametric methods. In order to find out the suitability for them, the relative standard error (RSE) and standard error of estimate (SEE) values were obtained by statistical process of creep data. The O-S-D parameter showed better fitting to creep-rupture data than the L-M or the M-H parameters, and the three parametric methods did not generate the large difference in the SEE and the RSE values.

  • PDF

Material Degradation of 2Cr and 12Cr Tube Steels for High Temperature and Long-Time Exposure (2Cr 및 12Cr 크롬강튜브의 고온 장시간 사용에 따른 열화현상)

  • Choe, Byung-Hak;Lee, Gil Jae;Kim, Sang-Ho;Hong, Key-Yong;Kim, Woo Sik;Baek, Un Bong;Nahm, Seung Hoon
    • Journal of the Korean Institute of Gas
    • /
    • v.16 no.5
    • /
    • pp.28-34
    • /
    • 2012
  • Material degradation of Cr steels in using for boiler tubes was studied in the relation of microstructural changes like carbide behavior and mechanical properties of hardness and creep-rupture life. The carbide dissolution was occurred in 2Cr steel of T22 during high temperature operation. And the grain refinement within martensite lath of 12Cr steel of X20 was derived by the high temperature-long time exposure. But the specific phenomena of material degradation which might be represented by hardness or creep-rupture time of the used tubes were not shown in all the tubes of T22 and X20 even in the fire-side using.

Creep Life Prediction and Error Analysis for Type 316LN Stainless Steel (Type 316LN 스테인리스강의 크리프 수명예측과 오차분석)

  • Yi W.;Yin S.N.;Kim W.G.;Ryu W.S.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2006.05a
    • /
    • pp.109-110
    • /
    • 2006
  • Various parametric methods, Larson-Miller (L-M), Orr-Sherby-Dorn (O-S-D), Manson-Haferd (M-H) parameters, and minimum commitment method (MCM), were used to predict longer rupture time from short-term creep data. A number of the creep data were collected through literature surveys and experimental data produced in KAERI for predicting the creep type of type 316LN SS. Polynomial equations for predicting the creep life were obtained by the time-temperature parameters (TTP) and the MCM. standard error (SE) and standard error or mean (SEM) values were compared for the each method with temperatures. The TTP methods were good in the creep-life prediction, but the MCM was much superior to the TTP ones at $700^{\circ}C\;and\;750^{\circ}C$. The MCM was found to be lower in the SE values compared to the TTP methods

  • PDF

Creep-Life Prediction and Standard Error Analysis of Type 316LN Stainless Steel by Time-Temperature Parametric Methods (시간-온도 파라미터 방법에 의한 Type 316LN 강의 크리프 수명 예측과 표준오차 분석)

  • Yoon Song Nam;Ryu Woo Seog;Yi Won;Kim Woo Gon
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.29 no.1 s.232
    • /
    • pp.74-80
    • /
    • 2005
  • A number of creep rupture data for type 316LN stainless steels were collected through literature survey or experimental data produced in KAERI. Using these data, polynomial equations for predicting creep life were obtained by Larson-Miller (L-M), Orr-Sherby-Dorn (O-S-D) and Manson-Haferd (M-H) parameters using time-temperature parametric (TTP) methods. Standard error of estimate (SEE) values for the each parameter was obtained with different temperatures through the statistical process of the creep data. The results of L-M, O-S-D and M-H methods showed good creep-life prediction, but M-H method showed better agreement than L-M and O-S-D methods. Especially, it was found that SEE values of M-H method at $700^{\circ}C$ were lower than that of L-M and O-S-D methods.

Reliability Prediction of Long-term Creep Strength of Gr. 91 Steel for Next Generation Reactor Structure Materials (미래형 원자로 구조 재료용 Gr. 91 강의 장시간 크리프 강도의 신뢰성 예측)

  • Kim, Woo-Gon;Park, Jae-Young;Yin, Song-Nan;Kim, Dae-Whan;Park, Ji-Yeon;Kim, Seon-Jin
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.4
    • /
    • pp.275-280
    • /
    • 2011
  • This paper focuses on reliability prediction of long-term creep strength for Modified 9Cr-1Mo steel (Gr. 91) which is considered as one of the structural materials of next generation reactor systems. A "Z-parameter" method was introduced to describe the magnitude of standard deviation of creep rupture data to the master curve which can be plotted by log stress vs. The larson-Miller parameter (LMP). Statistical analysis showed that the scattering of the Z-parameter for the Gr. 91 steel well followed normal distribution. Using this normal distribution of the Z-parameter, the various reliability curves for creep strength design, such as stress-time temperature parameter reliability curves (${\sigma}$-TTP-R curves), stress-rupture time-reliability curves (${\sigma}-t_{r}-R$ curves), and allowable stress-temperature- reliability curves ([${\sigma}$]-T-R curves) were reasonably drawn, and their results are discussed.

A study on the Creep fracture life prediction of Al7075 alloy under high temperature (고온상태에서 Al 7075 합금의 크리이프 파단수명 예측에 대한 연구)

  • Kang, Dae-Min;Koo, Yang;Baek, Nam-Ju
    • Journal of the Korean Society of Safety
    • /
    • v.3 no.2
    • /
    • pp.35-48
    • /
    • 1988
  • Modern technological progress demands the use of materials at high temperature and high pressure. One of the most critical factors in considering such applications - perhaps the most critical one - is creep behavior. In this study the stress exponents n were determined during creep over the temperature range of $90^{\circ}C\;to\;500^{\circ}C$ (0.4 - 0.85 Tm) and stress range of 0.64 kgt/$mm^2$ in order to investigate the creep hehavior. The stress dependence of rapture time (n') were determined over the temperature range of $200^{\circ}C\;to\;240^{\circ}C$ and stress range of 8.13 kgt/$mm^2$ to 9.55 kgt/$mm^2$ in order to investigate to creep rupture property. And the stress transient dip tests were also carried out for the internal stress ${\sigma}i$ over the temperature range of $90^{\circ}C\;to\;500^{\circ}C$ and stress range of 0.64kgt/$mm^2$ to 17.2 kgt/$mm^2$. The creep tests for constant temperature and stress transient dip tests were conducted in air with Al 7075 alloy under constant tensile load. At around the temperature range $200^[\circ}C\;-\;230^{\circ}C$ and the stress level 8.13 - 9.55 (kgt/$mm^2$), the temperature range $280^{\circ}C\;-\;310^{\circ}C$ and the stress level 1.85 - 2.55 (kgt/$mm^2$), the temperature range $380^{\circ}C\;-\;410^{\circ}C$ and the stress 1.53 - 0.91 (kgt/$mm^2$), the stress exponent in had the value of 6.2 - 6.65 but at around the temperature range $90^{\circ}C\;-\;120^{\circ}C$ and the stress level 10 - 17.2(kgt/$mm^2$), the value of 1.3, and at around the temperature range $470^{\circ}C\;-\;500^{\circ}C$, the stress level 0.62 - 1.02 (kgt/$mm^2$) the value of 1-1. Besides these results, at around the temperature $200^{\circ}C\;-\;240^{\circ}C$ the stress dependence of rupture time (n') had the value of 6.3. Finally, it was found that the value n calculated by considering the applied stress dependence of the internal stress were in good agreement with those obtained for the creep test. Then, it was concluded that the change in n was mainly attributed to the difference of the applied stress dependence of the internal stress and the ratio of the internal stress to the applied stress, and the creep rupture life may be represented as.

  • PDF