• Title/Summary/Keyword: Cr-Mo steel

Search Result 548, Processing Time 0.034 seconds

Spherical Indentation Testing to Evaluate Mechanical Properties In 1Cr-1Mo-0.25V Steel (Spherical Indentation Testing에 의한 1Cr-1Mo-0.25V 강의 기계적 물성 평가)

  • Lee, J.M.;Nam, Y.H.;Nham, S.H.;Lee, S.S.;Lee, O.S.
    • Proceedings of the KSME Conference
    • /
    • 2001.11a
    • /
    • pp.266-271
    • /
    • 2001
  • Spherical indentation technique was developed to evaluate the flow properties of metallic materials in carbon steel, stainless steel and alloys, etc. Through the spherical indentation test, differently degraded 1Cr-1Mo-0.25V steel's mechanical properties were observed and compared with conventional standard test data. The flow properties of 1Cr-1Mo-0.25V steels were estimated by analyzing the indentation load-depth curve. To characterize the flow property, we used material yield slope and constraint factor index rather than strain-hardening exponent because the variation of strain-hardening exponent was very little and the data showed irregularly. And the constraint factor's effect was small when the material yield slope was taken into account.

  • PDF

Manufacturing 2.25Cr-1Mo Steel In Hot Rolling Strip Mill (2.25% Cr-1%Mo 합금계 열연강판 제조기술)

  • 노태훈
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1999.08a
    • /
    • pp.390-398
    • /
    • 1999
  • The thermomechanical control process(in hot rolling strip mill) was employed to produce 2.25Cr-1Mo steel, which is to be construction material for the steam generator for power plant. Although the Conventional processes has been the primary means of producing the 2.25Cr-1Mo steel, an alternative method was used to meet the specification of ASTM heat treatment for A387-22-Classl using autotempering after coiling in hot rolling strip mill. The microstructures, tensile properties at various temperatures, and creep-rupture properties have been investigated to compare the properties with those of materials produced by the conventional process and to certify the application of the thermomechanical control process to an actual process of manufacturing 2.25-Cr-1Mo steel, this in turn, will reduce the cost of the process. About 14 to 34% glanular bainite (remainder proetectoid ferrite) formed in a coil, and this variety of volume fraction stems from the different cooling rates, which varies with position of the coil after coiling. Tensile testing from room temperature to 700$^{\circ}C$ indicated that strength increases with test temperature showing peaks at around 600$^{\circ}C$. Creep-rupture properties have been being investigated at the temperature of 500$^{\circ}C$ with 27.5, 32kg/$\textrm{mm}^2$ loads and have showed no rupture for over 1000 hours.

  • PDF

Effect of Thermal History on Pitting Corrosion of High Nitrogen and Low Molybdenum Stainless Steels

  • Kim, Kwangsik;Chang, Hyunyoung;Kim, Youngsik
    • Corrosion Science and Technology
    • /
    • v.2 no.2
    • /
    • pp.75-81
    • /
    • 2003
  • Chromium, molybdenum. and nitrogen are very important alloying elements in stainless steels and its effect was approved in pitting resistance equivalent (PRE) equations and many experimental results. However, Cr can improve the corrosion resistance, but facilitate the formation of sigma phase. Also. Mo has the same effect in stainless steels. If Cr and Mo are added at high amount to increase the corrosion resistance of stainless steel, corrosion resistance in annealed alloys can be improved, but in case of welding or aging heat treatment. its resistance will be drastically decreased. In this work, increasing Cr and N contents but decreasing Mo than the commercial alloys made the experimental alloys. Typical alloys are 25Cr-4.5Mo-0.43N alloy, 27Cr-4.7Mo-0.4N alloy, 27Cr-5.3Mo-0.25N alloy, 32Cr-2.6Mo-0.36N alloy. After annealing and aging heat treatment, microstructures, anodic polarization test, and pitting corrosion test were performed. Annealed alloys showed $100^{\circ}C$ of CPT and aged alloys showed the different tendency depending upon Cr and Mo contents(SFI)

Sliding wear mechanism of the high-nitrogen austenitic 18Cr-18Mn02Mo-0.9N steel (고질소 Fe-18Cr-18Mn-2Mo-0.9N강의 미끄럼 마멸 기구)

  • Kim S. D.;Kim S. J.;Kim Y. S.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2005.10a
    • /
    • pp.105-108
    • /
    • 2005
  • Sliding wear mechanism of a high nitrogen austenitic 18Cr-18Mn-2Mo-0.9N steel has been investigated. Dry sliding wear tests of the steel were carried out at various loads of 1N-10N under a constant sliding speed condition of 0.15m/s against AISI 52100 bearing steel balls. Solution $(1050^{\circ}C)$ and isothermal aging $(900^{\circ}C)$ heat treatments were performed on the steel and the effect of the heat treatments on the wear were investigated. Wear rates of the solution-treated steel specimen remained low until 5N, and then increased abruptly at loads above 5N. The rates of isothermally aged specimens were low and increased gradually with the applied load. Worn surfaces, their cross sections, and wear debris of the steel specimens were examined with a scanning electron microscopy. Phases of the heat-treated specimen and the wear debris were identified using XRD. Phases transformed underneath the sliding track during the wear were investigated and analyzed using TEM. Effects of the phase transformation during the wear and $Cr_2N$ precipitates formed during the isothermal aging on the wear of the austenitic steel were discussed.

  • PDF

Reheat Cracking Susceptibility of CrMoV Steel (CrMoV강의 재열균열 민감도에 관한 연구)

  • 김광수
    • Proceedings of the KWS Conference
    • /
    • 2004.05a
    • /
    • pp.168-170
    • /
    • 2004
  • 터빈로터는 발전설비 중에서 가장 핵심 부분이며 동시에 심한 고온 응력을 받는 부분이다. 터빈로터 재료로는 Ni-Cr-Mo-V강과 CrMoV 강등이 사용된다. CrMoV 강은 발전 설비로 장시간 사용 중 열적피로나 크립손상, 고온 부식 등의 문제가 단독 혹은 복합적으로 발생하여 재료에 손상을 입히게 되고 결국에는 설비의 수명을 단축 시키곤 한다. (중략)

  • PDF

The Evaluation of Mechanical Property of X20CrMoV12.1 Boiler Tube Steels (X20CrMoV12.1강의 열화에 따른 기계적특성 평가)

  • Kim, B.S.;Lee, S.H.;Kim, D.S.;Jung, N.G.
    • Journal of Power System Engineering
    • /
    • v.8 no.3
    • /
    • pp.18-22
    • /
    • 2004
  • Boiler is one of the most important utilities providing steam to turbine in order to supply mechanical energy in thermal power plant. It is composed of thousands of tubes for high efficient heat transfer. The material for boiler tubes is used in such high temperature and pressure condition as $540^{\circ}C$, 22MPa. The boiler tube material is required to resist creep damage, fatigue cracking, and corrosion damages. 2.25%Cr-1Mo steel is used for conventional boiler tubes, and austenitenite stainless steel is used for higher temperature boiler tubes. But the temperature and pressure of steam in power plant became higher for high plant efficiency. So, the property of boiler tube material must be upgaded to fit the plant property. Several boiler tube material was developed to fit such conditions. X20CrMoV12.1 steel is also developed in 1980's and used for superheater and reheater tubes in supercritical boilers. The material has martensite microstructures which is difficult to evaluate the degradation. In this thesis, degrade the X20CrMoV12.1 steel at high temperatures in electric furnace, and evaluate hardness with Vickers hardness tester and strengths with Indentation tester.

  • PDF

Determination of Ni, Cr, Mo in Low Alloy Steel Reference Materials by Isotope Dilution Inductively Coupled Plasma Mass Spectrometry (동위원소희석 유도결합플라스마질량분석법에 의한 저 합금강 표준시료중의 Ni, Cr, Mo의 분석)

  • Suh, Jungkee;Woo, Jinchoon;Min, Hyungsik;Yim, Myeongcheul
    • Analytical Science and Technology
    • /
    • v.16 no.1
    • /
    • pp.82-89
    • /
    • 2003
  • Isotope dilution mass spectrometry (IDMS) was applied to the determination of Ni, Cr, Mo in low alloy steel reference materials. The Mo isotope ratio measurement was performed by dynamic reaction cell inductively coupled plasma mass spectrometry (DRC-ICP/MS) using ammonia as a reaction cell gas. In the case of Ni and Cr measurement, all data were obtained at medium resolution mode (m/${\Delta}m=3000$) of double focusing sector field high resolution inductively coupled plasma mass spectrometry (HR-ICP/MS). For the method validation of the technique was assessed using the certified reference materials such as NIST SRM 361, NIST SRM 362, NIST SRM 363, NIST SRM 364, NIST SRM 36b. This method was applied to the determination of Ni, Cr and Mo in low alloy steel sample (CCQM-P25) provided by NMIJ for international comparison study.

Development of Assessment Methodology on Creep-Fatigue Crack Behavior for a Grade 91 Steel Structure (Mod.9Cr-1Mo 강 구조의 크리프-피로 균열 거동 평가법 개발)

  • Lee, Hyeong-Yeon;Lee, Jae-Han
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.34 no.1
    • /
    • pp.103-110
    • /
    • 2010
  • In this study, an assessment method on creep-fatigue crack initiation and crack growth for a Mod.9Cr-1Mo steel (ASME Grade 91) structure has been developed with an extension of the French RCC-MR A16 procedure. The current A16 guide provides defect assessment procedure for a creep-fatigue crack initiation and crack growth for an austenitic stainless steel, but no guideline is available yet for a Mod.9Cr-1Mo steel which is now widely being adopted for structural materials of future nuclear reactor system as well as ultra super critical (USC) thermal plant. In the present study an assessment method on creep-fatigue crack initiation and crack growth is provided for the FMS (Ferritic-Martensitic Steel) and assessment on the creep-fatigue crack behavior for a structure has been carried out. The assessment results were compared with the observed images from a structural test.

Overview of Research Trends and Problems on Cr-Mo Low Alloy Steels for Pressure Vessel (압력용기용 Cr-Mo 계 저합금 강의 개발동향 및 재료적 문제점)

  • Chi, Byung-Ha;Kim, Jeong-Tae
    • Proceedings of the KSME Conference
    • /
    • 2000.11b
    • /
    • pp.67-76
    • /
    • 2000
  • Cr-Mo low alloy steels have been used for a long time for pressure vessel due to its excellent corrosion resistance, high temperature strength and toughness. The paper reviewed the latest trends on material development and some problems on Cr-Mo low alloy steel for pressure vessel, such as elevated temperature strength, hardenability, synergetic effect between temper and hydrogen embrittlement, hydrogen attack and hydrogen induced disbonding of overlay weld-cladding.

  • PDF

Overview of Research Trends and Problems on Cr-Mo Low Alloy Steels for Pressure Vessel (압력용기용 Cr-Mo 계 저합금 강의 개발동향 및 재료적 문제점)

  • Chi, Byung-Ha;Kim, Jeong-Tae
    • Proceedings of the KSME Conference
    • /
    • 2000.11a
    • /
    • pp.67-76
    • /
    • 2000
  • Cr-Mo low alloy steels have been used for a long time for pressure vessel due to its excellent corrosion resistance, high temperature strength and toughness. The paper reviewed the latest trends on material development and some problems on Cr-Mo low alloy steel for pressure vessel, such as elevated temperature strength, hardenability, synergetic effect between temper and hydrogen embrittlement, hydrogen attack and hydrogen induced disbonding of overlay weld-cladding.