• 제목/요약/키워드: Copper Slag

검색결과 75건 처리시간 0.028초

동제련 슬래그를 활용한 R.P.C.(Reactive Powder Concerete)의 역학적 특성에 관한 연구 (A Study on Mechanical Properties of Reactive Powder Concrete Using copper slag)

  • 이용무;신상엽;김영수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 추계 학술논문 발표대회
    • /
    • pp.74-75
    • /
    • 2013
  • The paper study on the mechanical properties of reactive powder concrete using copper slag. A change in the replacement ratio s of copper slag was measured compressive strength and slump flow. As a results, slump flow using copper slag tend to increase slump flow with replacement ratio. As the concrete with a replacement ratio of copper slag up to 30% was found to have a compressive strength superior to that of plain.

  • PDF

동제련 슬래그 잔골재를 이용한 고강도 콘크리트의 물성에 관한 연구 (The Study on the Property of High Strength Concrete Used Copper Slag)

  • 박정우;김상미;강태경;백민수;임남기;정상진
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 가을 학술발표회 논문집
    • /
    • pp.99-104
    • /
    • 2001
  • Slag product has the possibility as alternative aggregate and sand under the circumstance of natural resource shortage. Copper slag is the by-product produced in process of copper industry. Recycling the slag in construction industry could give positive effects on the environmental preservation. This study presents that the fundamental properties of high strength concrete which used copper slag as alternative sand. Testing factors are concrete's slump, bleeding, air contents and compressive strength. The results of this study are as follows. (1) Mixing of W/C 30%, substitution rate 25% shows the best slump. As substitution rates are going up, concrete slump is uprising and air contents are downsizing. (2) The bleeding of concrete becomes more serious as substitution rates are going up. (3) The best compressive strength of copper slag concrete is achieved in mixing of W/C 30%, substitution rate 25%.

  • PDF

대형압밀시험기를 이용한 동슬래그 다짐말뚝의 배수 특성 (Drainage Characteristics of Copper Slag Compaction Pile Installed in Clay Based on the Laboratory Consolidation Model Test)

  • 천병식;정헌철;김경민;조한영
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2001년도 추계학술대회 논문집
    • /
    • pp.552-557
    • /
    • 2001
  • Copper slag is the by-producted material on the proceeding of refining the copper. To verify applications of copper slag to vertical drain material can substitute for the sands in ground improvement, laboratory soil tests and consolidation model tests were conducted. The results of consolidation model test was analyzed as the hyperbolic method. The hyperbolic method assumes that the settlement(s) versus time(t) behavior approaches a straight line describes a hyperbolic reaction. The inverse of the slope of the line would then yield the ultimate settlement. Through in this study, copper slag is compatible with vertical drain material as like sands. Copper slag compaction pile promote the consolidation settlement.

  • PDF

지반개량재로써 동제련슬래그의 활용에 관한 연구 (Applications of the Copper Slags as Ground Improvement Material)

  • 천병식;정헌철;조한영
    • 한국지반환경공학회 논문집
    • /
    • 제3권1호
    • /
    • pp.27-36
    • /
    • 2002
  • 본 연구는 동제련슬래그를 지반개량재로써 활용하기 위하여 배수에 대한 적용가능성을 평가한 것이다. 모래말뚝의 모래 대체재로써의 동제련슬래그 활용방안을 검토하였고, 동제련슬래그의 재료특성, 동제련슬래그말뚝이 설치된 복합지반에서의 압밀배수 특성, 배수 필터재로써의 특성 등을 파악하였다. 연구결과, 동제련슬래그는 일반적으로 쓰여지는 모래와 유사한 연직배수효과를 나타내었으므로, 모래말뚝의 모래 대체재로써의 적용은 충분히 가능할 것으로 판단된다. 더욱, 분사현상에 대한 안정성 및 입자 유실에 대한 내적안정성을 검토한 결과, 일반적인 사질토에 비해 한계동수경사가 크게 나타나고, 내적안정성이 우수하게 평가되었다. 따라서 동제련슬래그는 지반조건에 따라 배수 필터기능을 충분히 발휘할 수 있으며, 내적으로도 안정된 배수 필터재로써 사용이 가능한 것으로 판단된다.

  • PDF

Utilisation of glass powder in high strength copper slag concrete

  • Zaidi, Kaleem A.;Ram, Shobha;Gautam, Mukesh K.
    • Advances in concrete construction
    • /
    • 제5권1호
    • /
    • pp.65-74
    • /
    • 2017
  • This study was focused on the use of partial replacement of cement with glass powder in high strength concrete and also copper slag as a partial replacement of coarse sand in concrete. The high strength concrete was prepared with different mineral admixtures like silica fume, fly ash and rice ash husk in different proportions. An experimental investigation has been carried to study about the effect of glass powder on high strength copper slag concrete. The range of glass powder was 10%, 15% and 20% as a replacement of cement. The range of copper slag was 0%, 20%, 40% and 60% as a replacement of natural sand. In addition to the different percentage of fly ash, silica fume, and rice husk ash 5% and 10% was also studied in copper slag concrete. Thus, a total of 51 cubes were casted and compressive strength test was performed on them. The result of the study shows that the value of average compressive strength of concrete after addition of 10%, 15% and 20% of glass powder are 70.47, 72.01 and 73.31 respectively. The value of average compressive strength after addition of 20%, 40% and 60% copper slag as a replacement of sand are 72.18, 74.38 and 73.08 respectively. The value of average compressive strength after addition of 5% and 10% fly ash as a replacement of cement are 71.56 and 73.22. The value of average compressive strength after addition of 5% and 10% silica fume as a replacement of cement are 72.33 and 73.53. The value of average compressive strength after addition of 5% and 10% rice husk ash as a replacement of cement are 72.86 and 69.49. At the level of 20% replacement of cement by glass powder meets maximum strength as compared to that of controlled concrete and copper slag high strength concrete.

폐동(廢銅)슬래그를 활용(活用)한 폐전기전자(廢電氣電子) 스크랩으로부터 유가금속(有價金屬) 고온용융추출(高溫鎔融抽出) 공정(工程) 개발(開發) (A Novel Process for Extracting Valuable Metals from Waste Electric and Electronic Scrap Using Waste Copper Slag by a High temperature Melting Method)

  • 김병수;이재천;이광호
    • 자원리싸이클링
    • /
    • 제16권3호
    • /
    • pp.27-33
    • /
    • 2007
  • 구리, 주석 등의 유가금속을 다량 함유하고 있는 폐전기전자 스크랩으로부터 유가금속을 회수하는 것은 자원 재활용 측면에서 매우 중요하다. 본 연구에서는 폐동슬래그를 슬래그 형성제로 활용하여 폐전기전자 스크랩으로부터 유가금속을 추출하기 위한 새로운 공정이 제시되었다. 제안된 공정은 슬래그 형성제로 동 제련소에서 배출되는 폐동슬래그를 재활용한다는 장점이 있다. 각 실험에서는 일정한 비율로 혼합된 폐전기전자 스크랩과 폐동슬래그의 혼합시료를 보조 슬래그 형성제인 CaO와 함께 고온 용융되었다. 실험 결과 폐전기전자 스크랩에 함유된 구리와 주석이 Cu-Fe-Sn 합금상으로 각각 95% 이상, 85% 이상 추출되었다.

6~7C 부여 관북리 유적의 동 생산기법 연구 (A Study of Copper Production Techniques at the Archaeological Site in Gwanbukri, Buyeo in the 6th and 7th Centuries)

  • 이가영;조남철
    • 보존과학회지
    • /
    • 제36권3호
    • /
    • pp.162-177
    • /
    • 2020
  • 부여 관북리 유적에서 시행된 동 생산 및 제련과정을 살펴보기 위하여 '나'지구, '라'지구 출토동 생산 부산물(동 슬래그 및 동 도가니) 11점의 과학적 분석을 시행하였다. 분석방법은 파장분산형 X-선 형광 분석, X-선 회절 분석, 금속 현미경 관찰, 주사 전자현미경-에너지 분산형 X-선 분석기, 전계방출 전자탐침미량분석기, 라만 마이크로분광분석법을 사용하였다. 분석결과 관북리 동 슬래그에서는 주로 도가니 슬래그 및 정련 슬래그에서 전형적인 특징으로 나타나는 규산염 광물, Magnetite, Fayalite, Delafossite 등이 검출되었다. 또한 관북리 동 슬래그는 외형 및 미세조직의 양상의 특성에 따라 1. 유리질 바탕 기지 + Cu prill, 2. 유리질 바탕 기지 + Cu prill + Magnetite, 3. 규산염 광물 바탕 기지 + Cu prill, 4. 결정질(Delafossite, Magnetite)/유리질(비정질) 바탕 기지 + Cu prill, 5. Magnetite + Fayalite, 6. 청동합금 슬래그로 분류되었다. 미세조직 내에는 SiO2, Al2O3, CaO, SO4 P2O5, Ag2O, Sb2O3 등의 불순물이 잔재되어 있으며, 일부는 주석과 납이 합금되어 있는 것을 확인하였다. 이와 같은 결과를 통해 부여 관북리 유적에서는 동 생산과정 중 배소와 제련을 거친 동 중간생성물의 정련과 불순물이 함유된 동-주석, 또는 동-주석-납의 합금정련을 시행하였다고 판단된다.

동슬래그 및 플라이애쉬를 혼합하여 제작한 콘크리트의 성능 향상 연구 (A Study on the Improvement of Property of Concrete using Copper Slag and Fly ash)

  • 김춘호;이원구;김남욱
    • 자원리싸이클링
    • /
    • 제24권1호
    • /
    • pp.28-34
    • /
    • 2015
  • 일반적으로 동슬래그를 콘크리트에 혼입하여 사용하는 경우, 동슬래그의 높은 자중으로 인한 블리딩의 증가로 경화 콘크리트의 압축강도 및 내구성의 저하가 유발된다. 본 연구에서는 산업부산물인 동슬래그를 잔골재의 대체골재로 사용하고자 하였는데 이에 따른 단점의 해소 및 자원 재활용 측면에서 플라이애쉬와의 병용 사용을 실시하였다. 본 연구 결과, 플라이애쉬의 혼입은 동슬래그만 단독으로 사용한 경우보다, 블리딩은 50%, 건조수축은 5%, 중성화 저항성은 30% 감소 및 압축강도는 10% 정도 향상 효과가 나타났다.

잔골재로 사용한 동슬래그의 입도에 따른 모르타르의 기초적 특성 연구 (A Study on the Basic Property of Mortar as the Grading Distribution of Copper Slag Used as Fine Aggregate)

  • 이종찬;이문환;이세현
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.97-100
    • /
    • 2005
  • The purpose of this study is to research the basic property of mortar as the grading distribution of copper slag used as fine aggregate and the results are as follows. The compressive strength of mortar as the size of largest diameter of copper slag granule is the highest when the largest size is in 2.5-5mm, and flow of mortar is in proportion to the size. As the largest size of copper slag particle is under 2.5mm(Type 1) the compressive strength and flow is higher as the big granules is more included than small ones. As the largest size of copper slag granule is under 5mm(Type 2) the compressive strength and flow is similar to situation of Type 1, except compressive strength is higher as the percent of the size of granule in $2.5\~5mm$ is under 35$\%$. F.M.(Fine Modulus), compressive strength and flow is relative each other except the batch with 2.5$\∼$5mm granule size of copper slag.

  • PDF

동슬래그 혼합토의 기본 성질에 관한 연구 (A Study on the Fundamental Characteristics of a Copper Slag Mixed with Granite Soil)

  • 김영진;배정호;홍승서
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2000년도 가을 학술발표회 논문집
    • /
    • pp.447-454
    • /
    • 2000
  • This paper presents fundamental characteristics of a copper slag when used geotechnical materials. For this study, it was conducted laboratory tests such as compaction, large direct shear, hydraulic conductivity, leaching, TDR, frost heave test and so on. The results of laboratory tests shown gradually increase in draining capacity and shearing resistance more slag mixing. The unfrozen water in temperature changes and frost heave amounts in condition of -17 $^{\circ}C$ appeared to decrease. Also, toxicity tests based on the domestic solid waste regulations were satisfied with nonhazardous. By this research results, a copper slag mixed with granite soil may been used as granular base and embankment materials, fill etc.

  • PDF