• Title/Summary/Keyword: Conventional Dense-Graded

Search Result 11, Processing Time 0.028 seconds

An Evaluation of Mechanical Characteristics of Modified Asphalt Concrete Mixture (개질아스팔트 콘크리트 혼합물의 기계적 특성평가)

  • Kim, Nakseok;Bang, Sanyoung
    • Journal of the Society of Disaster Information
    • /
    • v.7 no.1
    • /
    • pp.32-42
    • /
    • 2011
  • Many researches have been conducted to evaluate the performance of modified asphalt concrete mixtures. The research was conducted to estimate the laboratory mechanical characteristics of Elvaloy-modified asphalt concrete mixture. To achieve its intended objective, indirect tensile test and resilient modulus test were performed. The rest results revealed that indirect tensile strengths and resilient moduli of the Elvaloy-modified asphalt concrete mixture were higher than those of the conventional dense-graded. As a result, within the limits of the tests conducted in this research, it is predicted that the performance and stability of the Elvaloy-modified asphalt concrete mixture are better than that of the conventional dense-graded one.

Remarks on the use of Electric Arc Furnace (EAF) Steel Slag in Asphalt Mixtures for Flexible Pavements (Electric Arc Furnace (EAF) Steel Slag의 아스팔트 포장 혼합물 내 대체 골재로서 적용 가능성에 대한 고찰)

  • Falchetto, Augusto Cannone;Moon, Ki Hoon
    • International Journal of Highway Engineering
    • /
    • v.17 no.1
    • /
    • pp.25-33
    • /
    • 2015
  • PURPOSES : This paper, presents the results of a laboratory study aimed to verify the suitability of a particular type of Electric Arc Furnace (EAF) steel slag to be recycled in the lithic skeleton of both dense graded and porous asphalt mixtures for flexible pavements. METHODS : Cyclic creep and stiffness modulus tests were performed to evaluate the mechanical performance of three different asphalt mixtures (dense graded, porous asphalt, and stone mastic) prepared with two types of EAF steel slag. For comparison purposes, the same three mixtures were also designed with conventional aggregates (basalt and limestone). RESULTS : All the asphalt mixtures prepared with EAF steel slag satisfied the current requirements of the European standards, which support EAF steel slag as a suitable material for flexible pavement construction. CONCLUSIONS : Based on the experimental work, the use of waste material obtained from steel production (e.g. EAF steel slag) as an alternative in the lithic skeleton of asphalt mixtures can be a satisfactory and reasonable choice that fulfills the "Zero Waste" objective that many iron and steel industries have pursued in the past decades.

Evaluation of Reflection Cracking Resistance of Grid-Reinforced Asphalt Pavement Using Overlay Tester (Overlay Tester를 이용한 그리드 보강 아스팔트 포장의 반사균열 저항성 평가)

  • Yoo, Byung Soo;Seo, Woo Jin;Kim, Jo Soon;Park, Dae Wook
    • International Journal of Highway Engineering
    • /
    • v.18 no.1
    • /
    • pp.57-62
    • /
    • 2016
  • PURPOSES : Reflection cracking has been one of the major causes of distress when asphalt pavement is laid on top of concrete pavement. This study evaluated the reflection cracking resistance of asphalt mixtures reinforced with asphalt embedded glass fiber and carbon fiber using a Texas Transportation Institute (TTI) overlay tester. METHODS : Different asphalt mixtures such as polymer-modified mastic asphalt (PSMA) and a dense graded asphalt mixture were reinforced with asphalt-embedded carbon fiber and glass fiber. For comparison purposes, two PSMA asphalt mixtures and one dense graded asphalt mixture were evaluated without fiber reinforcement. Two different overlay test modes, the repeated overlay test (R-OT) and monotonic overlay test (M-OT), were used to evaluate the reflection cracking resistance of asphalt mixtures at $0^{\circ}C$. In the R-OT test, the number of repeated load when the specimen failed was obtained. In the M-OT test, the tensile strength at the peak load and tensile strain were obtained. RESULTS : As expected, the fiber-reinforced asphalt mixture showed a higher reflection cracking resistance than the conventional nonreinforced asphalt mixtures based on the R-OT test and M-OT test. The dense graded asphalt mixture showed the least reflection cracking resistance and less resistance than the PSMA. CONCLUSIONS : The TTI overlay tester could be used to differentiate the reflection cracking resistance values of asphalt mixtures. Based on the R-OT and M-OT results, the carbon-fiber-reinforced asphalt mixture showed the highest reflection cracking resistance among the nonreinforced asphalt mixtures and glass-fiber-reinforced asphalt mixture.

A Study on Aggregate Gradation of 10 mm Dense-graded Asphalt Mixture using Slag Aggregate (슬래그 골재를 사용한 10 mm 밀입도 아스팔트 혼합물의 골재입도 기준 연구)

  • Jo, Shin Haeng;Kim, Kyungnam;Kim, Nakseok
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.35 no.6
    • /
    • pp.1367-1375
    • /
    • 2015
  • The purpose of this paper is to suggest 10 mm aggregate specification for thin layer asphalt pavement using steel slag. Aggregate gradations of conventional dense-graded asphalt mixtures were made by fuller's model, whereas 10 mm dense-graded asphalt mixture was obtained tender mix due to close to the maximum density line. The proposed aggregate gradation specification was made to have enough VMA and well-interlocking refer to foreign standards. The correlation between the proposed aggregate gradation and the properties of mixtures were analyzed using Gradation Ratio (GR) and Compacted Aggregate Density (CAD). The CAD index has a high $R^2$ of 0.86-0.99 because the CAD index is able to reflect various aggregate properties. As the results of evaluation by CAD index the proposed aggregate gradation provides more reliable stability and VMA. The percent passing (%) of aggregate size smaller than 0.3 mm was limited 10% or more for improving crack resistance. This limitation increased for 15% of the asphalt mixture's toughness.

An Evaluation of Skid Resistance Properties of Asphalt Concrete Pavement (아스팔트콘크리트 포장의 노면 미끄럼 저항성 평가)

  • Kim, Nakseok;Jeong, Haesoo
    • Journal of the Society of Disaster Information
    • /
    • v.7 no.2
    • /
    • pp.87-95
    • /
    • 2011
  • The skid resistant of pavement surface is an important parameter since it is directly related to the traffic safety under moving vehicular loads. In particular, it should be considered as a major factor in pavement performance evaluations to reduce the traffic accident from vehicular sliding. In this study, a portable and an automatic skid resistance tests were used to evaluate the skid resistances of the in-situ pavements. The test results showed that the skid resistance of the conventional dense graded pavement was more noticeable than the other pavement types such as the drainage pavement and the stone mastic asphalt(SMA) pavement as the service life of pavement was increased.

Factors Affecting Breast Cancer Detectability on Digital Breast Tomosynthesis and Two-Dimensional Digital Mammography in Patients with Dense Breasts

  • Soo Hyun Lee;Mi Jung Jang;Sun Mi Kim;Bo La Yun;Jiwon Rim;Jung Min Chang;Bohyoung Kim;Hye Young Choi
    • Korean Journal of Radiology
    • /
    • v.20 no.1
    • /
    • pp.58-68
    • /
    • 2019
  • Objective: To compare digital breast tomosynthesis (DBT) and conventional full-field digital mammography (FFDM) in the detectability of breast cancers in patients with dense breast tissue, and to determine the influencing factors in the detection of breast cancers using the two techniques. Materials and Methods: Three blinded radiologists independently graded cancer detectability of 300 breast cancers (288 women with dense breasts) on DBT and conventional FFDM images, retrospectively. Hormone status, histologic grade, T stage, and breast cancer subtype were recorded to identify factors affecting cancer detectability. The Wilcoxon signed-rank test was used to compare cancer detectability by DBT and conventional FFDM. Fisher's exact tests were used to determine differences in cancer characteristics between detectability groups. Kruskal-Wallis tests were used to determine whether the detectability score differed according to cancer characteristics. Results: Forty breast cancers (13.3%) were detectable only with DBT; 191 (63.7%) breast cancers were detected with both FFDM and DBT, and 69 (23%) were not detected with either. Cancer detectability scores were significantly higher for DBT than for conventional FFDM (median score, 6; range, 0-6; p < 0.001). The DBT-only cancer group had more invasive lobular-type breast cancers (22.5%) than the other two groups (i.e., cancer detected on both types of image [both-detected group], 5.2%; cancer not detected on either type of image [both-non-detected group], 7.3%), and less detectability of ductal carcinoma in situ (5% vs. 16.8% [both-detected group] vs. 27.5% [both-non-detected group]). Low-grade cancers were more often detected in the DBT-only group than in the both-detected group (22.5% vs. 10%, p = 0.026). Human epidermal growth factor receptor-2 (HER-2)-negative cancers were more often detected in the DBT-only group than in the both-detected group (92.3% vs. 70.5%, p = 0.004). Cancers surrounded by mostly glandular tissue were detected less often in the DBT only group than in the both-non-detected group (10% vs. 31.9%, p = 0.016). DBT cancer detectability scores were significantly associated with cancer type (p = 0.012), histologic grade (p = 0.013), T and N stage (p = 0.001, p = 0.024), proportion of glandular tissue surrounding lesions (p = 0.013), and lesion type (p < 0.001). Conclusion: Invasive lobular, low-grade, or HER-2-negative cancer is more detectable with DBT than with conventional FFDM in patients with dense breasts, but cancers surrounded by mostly glandular tissue might be missed with both techniques.

Characterization of Textures for Low Noise Concrete Pavement

  • Moon, Han-Young;Ha, Sang-Wook
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.11a
    • /
    • pp.461-464
    • /
    • 2003
  • Portland Cement Concrete (PCC) pavements have the advantage of durability and superior surface friction when compared to most dense-graded asphalt. However, data collected to date generally show PCC pavements to create more noise than asphaltic surfaces. As the results of research, surfaces of exposed aggregate, tining and grooving concrete pavements appear to provide better noise quality characteristics as well as good frictional characteristics and durability. In this paper, several methods of texturing were considered to reduce tire/pavement noise. As the results of this paper, PCC pavements with special texturing have superior surface friction as well as noise reductions when compared to conventional PCC pavement. Especially, Exposed Aggregate Concrete (EAC) surface appears to provide better noise quality characteristics. Conclusively, if overall noise and safety are considered simultaneously, EAC pavement that provides satisfactory friction as well as better noise reductions is suggested.

  • PDF

Evaluation of Laboratory Performance Characteristics of Fiber-Reinforced Asphalt Concrete (섬유활용 아스팔트 콘크리트의 실험적 공용특성평가)

  • Kim, Nak-Seok
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.2 no.2 s.5
    • /
    • pp.61-72
    • /
    • 2002
  • The optimum fiber and asphalt binder contents were decided on the base of the Mashall mix design method. To compare the mechanical characteristics between the conventional(dense-graded 20) and the fiber-reinforced mixtures, indirect tension tests were conducted under three temperatures(5, 20, 60$^{\circ}C$). In particular, the wheel tracking tests were performed to evaluate the rutting resistances of the mixtures. Test results showed that the indirect tensile strength of fiber-reinforced asphalt concrete was higher than that of conventional one. The toughness of fiber-reinforced mixture was 1.27 to 1.97 times higher than that of conventional one, depending upon the temperature. In addition, the results of wheel tracking tests and the retained indirect splitting tension tests conducted at $60^{\circ}C$ revealed that the resistance to permanent deformation of fiber-reinforced mixture was stronger than that of the conventional one.

Fatigue Resistance of Fiber-Reinforced Asphalt Concrete in Flexible Pavement (연성포장용 섬유보강 아스팔트 콘크리트의 피로저항성)

  • Kim, Nak-Seok;Choo, Sang-Hyuk;Lee, Suck-Hong
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.2 no.3 s.6
    • /
    • pp.79-88
    • /
    • 2002
  • The main purpose of this paper is to evaluate the possibility of improvement in fatigue resistance of asphalt concrete mixture using the industrial waste material of K fiber. In this research, as an experimental equipment, the MTS with Closed-Loop Servohydraulic System was used and it was designed according to the U.S. standard testing procedure of ASTM D 4123. According to the test results, the optimum content of fiber with the length of 8mm was about 0.2 percent of total mixture weight. The optimum asphalt content for the fiber-reinforced asphalt concrete was about 5.5 percent of total mixture weight. Fatigue resistance of fiber-reinforced asphalt concrete was noticeable compared to the conventional dense-graded 20 asphalt concrete. In addition, the resilient moduli of fiber-reinforced asphalt mixture were $1.15{\sim}1.18$ times higher than those of conventional asphalt concrete.

Laboratory Performance Characteristics of Cold-Mixed Reclaimed Asphalt Pavement(RAP) (상온재생공법활용 회수아스팔트 혼합물의 실험적 공용특성)

  • Kim, Nak-Seok;Jo, Myoung-Hwan;Im, Jung-Soon
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.3 no.1 s.8
    • /
    • pp.133-140
    • /
    • 2003
  • The research was performed to evaluate the cracking resistance characteristics of cold-mixed reclaimed asphalt pavement (RAP) using indirect tensile strength test and fatigue tests. Indirect tensile tests were conducted to estimate the indirect tensile strength at variable temperatures($10^{\circ}C\;and\;20^{\circ}C$). Fatigue tests were also carried out using 500kgf, 400kgf, and 300kgf of dynamic loads, and the fatigue life (Nf) for each mixture was measured. Indirect tensile strength of cold-mixed reclaimed asphalt pavement was about 90% of conventional 13mm dense-graded asphalt mixture. Fatigue life of cold-mixed reclaimed asphalt mixture was 70%, 55%, 30% (for 500kgf, 400kgf, 300kgf of load level, respectively) of the conventional one.