• Title/Summary/Keyword: Controlled low-strength materials (CLSM)

Search Result 51, Processing Time 0.024 seconds

Characteristics of Shear Waves in Controlled Low Strength Material with Curing Time (양생시간에 따른 유동성 채움재의 전단파 특성)

  • Han, Woojin;Lee, Jong-Sub;Byun, Yong-Hoon;Cho, Samdeok;Kim, Juhyong
    • Journal of the Korean GEO-environmental Society
    • /
    • v.17 no.3
    • /
    • pp.13-19
    • /
    • 2016
  • The ultrasonic waves for monitoring concrete materials have been used to investigate the setting and hardening process of concrete. This paper presents the application of bender elements for monitoring the hardening properties of Controlled Low Strength Material (CLSM) and the characterization of shear waves in CLSM according to curing time. To ensure the early age properties and flow, the CLSM consists of CSA cement, sand, silt, water, fly ash, and accelerator. In addition, three different type specimens according to fine contents are mixed. A couple of bender elements are installed at the wall of measurement cell and the CLSM specimen are prepared at the measurement cell for 28 days. Experimental results show that the resonant frequency and shear wave velocities increase with an increase in the curing time, regardless of the fine contents. Up to ten hours, the amplitudes of shear waves also increase, and the resonant frequency and shear wave velocities at the same time increase as the fine contents increase. The shear wave measurement technique using the bender elements may be effectively used to evaluate the hardening properties of CLSM along the curing time.

Engineering Properties of Flowable Fills with Various Waste Materials

  • Lee, Kwan-Ho;Lee, Byung-Sik;Cho, Kyung-Rae
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.8 no.2
    • /
    • pp.105-110
    • /
    • 2008
  • Flowable fill is generally a mixture of sand, fly ash, a small amount of cement and water. Sand is the major component of most flowable fill with waste materials. Various materials, including two waste foundry sands(WFS), an anti-corrosive waste foundry sand and natural soil, were used as a fine aggregate in this study. Natural sea sand was used for comparison. The flow behavior, hardening characteristics, and ultimate strength behavior of flowable fill were investigated. The unconfined compression test necessary to sustain walkability as the fresh flowable fill hardens was determined and the strength at 28-days appeared to correlate well with the water-to-cement ratio. The strength parameters, like cohesion and internal friction angle, were determined for the samples prepared by different curing times. The creep test for settlement potential was conducted. The data presented show that by-product foundry sand, an anti-corrosive WFS, and natural soil can be successfully used in controlled low strength materials(CLSM), and it provides similar or better properties to that of CLSM containing natural sea sand.

Optimal Mixture Contents of Accelerated Flowable Backfill Materials Using Surplus Soil for Underground Power Utilities (굴착잔토를 재활용한 지중전력구조물 급결성 유동화 뒷채움재의 최적배합비)

  • Cheon, Seon-Ho;Jeong, Sang-Seom;Lee, Dae-Soo;Cho, Hwa-Kyung
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2005.10a
    • /
    • pp.395-404
    • /
    • 2005
  • This study is to evaluate the physical and mechanical characteristics of flowable backfill and search for the optimal mixture contents of it used for constructing underground power utilities. flowable backfill is known as soil-cement slurry, void fill, and controlled low-strength material(CLSM). The benefits of CLSM include reduced equipment costs, faster construction, re-excavation in the future, and the ability to place material in confined spaces such as narrow parts nearly impossible for compaction or perimeter of underground power cables. The flowable slurry mixture made with 9 types of soil and 6 types of accelerated mixtures in the laboratory were evaluated for bleeding, flowability, heat resistance, and unconfined compressive strength to meet the aim values of this study.

  • PDF

Study of thin film transition liquid crystal display (TFT-LCD) optical waste glass applied in early-high-strength controlled low strength materials

  • Wang, Her-Yung;Chen, Jyun-Sheng
    • Computers and Concrete
    • /
    • v.5 no.5
    • /
    • pp.491-501
    • /
    • 2008
  • The present study verifies compressive strength, ultrasonic pulse velocity, electrical resistance,permeable ratio, and shrinkage from waste glass controlled low strength materials (WGCLSM) and early-high-strength WGCSLM specimens, by replacing the sand with waste glass percentages of 0%, 10%,20%, and 30%. This study reveals that increasing amounts of waste LCD glass incorporated into concrete increases WGCLSM fluidity and reduces the setting time, resulting in good working properties. By increasing the glass to sand replacement ratio, the compressive strength decreases to achieve low-strength effects. Furthermore, the electrical resistance also rises as a result of increasing the glass to sand replacement ratio. Early-high-strength WGCSLM aged 28 days has twice the electrical resistance compared to general WGCSLM. Early-high-strength WGCSLM aged 7 days has a higher ultrasonic pulse velocity similar to WGCSLM aged 28 days. The variation of length with age of different compositions is all within the tolerance range of 0.025%. This study demonstrates that the proper composition ratio of waste LCD glass to sand in early-high-strength WGCSLM can be determined by using different amounts of glass-sand. A mechanism for LCD optical waste glass usage can be established to achieve industrial waste minimization, resource recycling, and economic security.

Deformation Behavior Underground Pipe with CLSM (유동성 채움재를 이용한 지하 매설관의 변형특성 연구)

  • Park, Jae-Hun;Lee, Kwan-Ho;Jo, Jae-Yun;Sung, Sang-Kyu
    • International Journal of Highway Engineering
    • /
    • v.5 no.2 s.16
    • /
    • pp.25-35
    • /
    • 2003
  • During construction of circular lifeline pipe, the non-proper compaction along the pipe and the decrease of compaction efficiency are the main problems to induce the failure of underground pipe. The use of CLSM(controlled low strength materials) is one of the applications to overcome those problems. In this research, the numerical analysis by PENTAGON FEM program was carried out for 20 cases with the couple of combinations on bedding materials, backfill materials, and pipes. From the FEM analysis, the use of CLSM as backfill materials reduced the settlement of ground surface and the deformation of pipe employed. In case of the vertical deformation on the pipe, common soil backfill for flexible pipes showed 2 times for rigid pipes, but CLSM backfill case did less deformation than the soil backfill for rigid pipes. CLSM backfills for rigid pipes showed the similar results. Judging from the FEM analysis, the use of CLSM increases the structure capacity of the underground pipes.

  • PDF

A Study on the pH Reduction of Controlled Low Strength Material with Coal Ash (석탄회를 활용한 CLSM의 pH 저감에 관한 연구)

  • Kim, Youngil;Jee, Sunghyun;Chun, Byungsik
    • Journal of the Korean GEO-environmental Society
    • /
    • v.11 no.9
    • /
    • pp.39-45
    • /
    • 2010
  • Controlled low strength material(CLSM) is produced by mixing portland cement, fine aggregates, water and chemical admixtures. Sand is the most commonly used as the fine aggregates in the conventional CLSM. It is getting more and more difficult to obtain sand in Korea so it is required that the alternative materials be developed as the replacement of sand. Since the engineering characteristics of coal ash are similar to the sand, it becomes necessary to examine the application of the coal ash as the alternative material for CLSM and as the environment-friendly material. When the results meet the optimum pH level that plants can live, it can be expanded the scale of application of the study on the plant as the important field. This study was subjected to present the method to reduce the pH range of CLSM to a suitable condition that plants can survive. To verify this method, the care of neutralization was conducted by immersing the specimen to Ammonium monohydrogen phosphate. Before curing and neutralization, the maximum pH of developmental CLSM is approximately 11. However, the pH value of developmental CLSM has under 9.5 after peaceful curing and neutralization management.

Thermal Resistant Characteristics of Flowable Backfill Materials Using Surplus Soil for Underground Power Utilities (굴착잔토를 재활용한 지중 전력케이블 유동성 뒤채움재의 열저항 특성)

  • Oh, Gidae;Kim, Daehong
    • Journal of the Korean GEO-environmental Society
    • /
    • v.11 no.10
    • /
    • pp.15-24
    • /
    • 2010
  • In the case of underground power utilities pipe such as circular pipe, the most difficult problem is low compaction efficiency of the bottom of pipe inducing the failure of utilities. To overcome this problem, various studies have been performed and one of these is CLSM(Controlled Low Strength Materials) accelerated flow ability. But underground power utilities pipe backfill materials is also needed to have good thermal property that can dissipate the heat as rapidly as it is generated. So, in this study, we performed thermal resistancy test for various materials such as sand, weathered soil, clay and mixed soil to analyze the thermal characteristics of CLSM(Controlled Low Strength Materials) with accelerated flow ability for various conditions(water content, unit weight, void ratio, curing time) and to evaluate the applicability for backfill material of underground power utilities pipe. The test results of 16 specimens for thermal resistancy test showed good thermal property that maintained below $85^{\circ}C\;cm/W$.

Assessment of Controlled Low Strength Material using Pond Ash for Pipe Backfill Materials (매립석탄재 활용 CLSM의 관 뒤채움재 적용성 평가)

  • Young-Wook Kim;Young-Cheol Lim;Doo-Bong Yeon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.11 no.1
    • /
    • pp.32-38
    • /
    • 2023
  • In this study, as part of the practical development of technology for CLSM using pond ash, the characteristics such as flowability, bleeding rate, and strength of the CLSM according to physical properties such as particle size distribution and particulate content of the pond ash were reviewed. As a result of analyzing the properties of the collected pond ash, it was found that the characteristics of density and particle size distribution were different. As a result of evaluating the characteristics of the CLSM for three types of pond ash, it was found that the blending conditions to satisfy the quality stipulated in ACI 229R were different, and mainly affected the particle size distribution characteristics and particulate content of the pond ash. In case of coarse-grained pond ash (PA-3), mixing conditions that satisfy the performance requirements stipulated in ACI 229R were not derived. But it is considered that further review is necessary according to particle size adjustment.

Mechanical Characteristics of Accelerated Flowable Backfill Materials Using Surplus Soil for Underground Power Utilities (굴착 잔토를 재활용한 지중전력구조물 뒷채움재의 역학적 특성)

  • Cheon, SeonHo;Jeong, Sangseom;Lee, DaeSoo;Kim, DaeHong
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.26 no.5C
    • /
    • pp.303-312
    • /
    • 2006
  • This study is to evaluate the mechanical characteristics of flowable backfill and offer a guide line of mixture proportion based on soil types for constructing underground power utilities. Flowable backfill is known as soil-cement slurry, void fill, and controlled low-strength material(CLSM). The benefits of CLSM are reduced equipment costs, faster construction, re-excavation in the future, and the ability to place materials in confined spaces, which are narrow parts or perimeters of underground power cables nearly impossible for compaction. The flowable slurry mixed with 17 soils and 6 accelerated mixtures in the laboratory were evaluated for flowability and unconfined compressive strength to meet the target values of this study.

A Study on the Suitability of CLSM Mixing Ratio Considering Dry Shrinkage (건조수축을 고려한 유동성 채움재 배합비 적합성에 관한 연구)

  • Jeon, Byeong-Won;Kim, Byeong-Jun
    • Journal of the Korean Geotechnical Society
    • /
    • v.38 no.12
    • /
    • pp.7-17
    • /
    • 2022
  • The ratios of water and controlled low-strength materials (CLSM) were selected as 1:0.4, 1:0.6, 1:0.8, 1:1.0, and 1:1.2 to minimize the construction and long-term decrease in uniaxial compressive strength due to dry shrinkage through the combination of water, CLSM, and expansion agent. Approximately 2% and 5% of the expansion agent were added for each blending condition. As a result, it was found that the compressive strength decreased and the expandability increased as the specific gravity of the water increased. In addition, it was confirmed that the compressive strength increased rapidly up to 15 days of age compared to the CLSM used in the field. However, the compressive strength decreased compared to the 15 days of the age as of the 28 days of the age. It showed engineering characteristics similar to CLSM generally used in the field. Therefore, the water and the CLSM were mixed at a ratio of 1:0.8, and the field test was performed by adding 5% of an expansion agent. As a result, 28 days after age, the cavity waveform was observed using the handy GPR exploration system, and it was found that cavity waveform was relaxed or disappeared.