The maturity concept proposes that concrete of the same mix at the same maturity has the same strength, whatever combination of temperature and time makes up that maturity. Maturity is the integral of time and temperature of concrete above a datum temperature. Tests are conducted in order to determine a datum temperature and to measure compressive strengths and maturity of test specimens. This study also proposes some appropriate functions to represent the relationship between maturity and strength development.
The strength development of concrete is influenced by temperature and cement type which greatly affect hydration degree of cement. There is not pertinent concrete strength management methods for estimating the in-place strength of concrete. One such method is the maturity concept. The maturity concept is based on the fact that concrete gains strength with time as a result of the cement hydration and, thus the rate of hydration, as in any chemical reaction, depends primarily on the concrete temperature during hydration. Thus, the strength of concrete is function of its time-temperature history. This goals of the present study are to investigate a relationship between strength of high-fluidity concrete and maturity that is expressed as a function of an integral of the curing period and temperature, predict strength of concrete.
It is the "maturity rule" that concrete of the same mix, at the same maturity, has the same strength. In this study, the Nurse-Saul function which was proposed to account for the effects of temperature and time on strength development is used in computing maturity. After existing various functions to relate concrete strength to the maturity value are considered, new strenth-maturity function is proposed. Tests are conducted in order to compare prediction value with measured concrete strength. The constants in proposed prediction equation are determined by standard specimens(cylinders) test, and the equation is adopted to predict strength of slab. The slab was cast in the laboratory from the same batch of mole, and cores are cut from slab in order to estimate the actual strength. Tehese values are used to compare with proposed equation. equation.
성숙도는 콘크리트의 양생 온도이력에서 구해지는 것으로 초기강도 예측을 위한 하나의 유용한 지표가 될 수 있다. 즉 성숙도 이론은 배합이 동일할 때 성숙도 값이 같으면 강도값은 같다는 이론이다. 본 연구에서는 성숙도 법칙의 이론적 전개과정을 살펴보고 그 값을 계산하기 위하여 가장 널리 알려진 Nurse-Saul함수를 검토하였다. 또한 성숙도 함수와 기준온도(datum temperature) 설정을 위한 일련의 포괄적인 실험연구를 수행하였다. 성숙도를 강도값에 연관시키기 위한 여러 가지 성숙도-강도함수를 비교해보고 그 장단점을 분석해 보았으며 이를 통하여 유용한 강도예측함수를 제안하였다. 성숙도 이론의 적용에 있어서 고려해야 할 변수들을 도출하기 위하여 양생조건과 시멘트의 종류, 그리고 물-시멘트비등을 달리 하였으며 이 경우에는 습도나 초기양생온도 등이 변수로 채택되었다. 마지막으로 제안된 함수의 타당성과 정확성을 검증하기 위하여 콘크리트 슬래브를 타설하고 시간단계별로 콘크리트 코아를 채취하여 예측된 강도값과 비교하여 보았다. 본 논문은 실제 콘크리트 구조물의 초기강도 예측을 위해 매우 유용할 것으로 사료되며 현장품질관리에 효율적으로 활용할 수 있을 것으로 기대된다.
The strength development of concrete is influenced by temperature and cement type which greatly affect hydration degree of cement. There is not pertinent concrete strength management method in korea. There are several methods for estimating the in-place strength of concrete. One such method is the maturity concept. The maturity concept is based on the fact that concrete gains strength gradually as a result of chemical reactions between cement and water; and for a specific concrete mixture, strength at any age and at normal conditions is related to the degree of hydration. The rate of hydration and, therefore, strength development of a given concrete will be a function of its temperature. Thus, strength of concrete depends on its time-temperature history. The goals of the present study are to investigate a relationship between strength of high-strength concrete and maturity that is expressed as a function of an integral of the curing period and temperature and predict strength of concrete.
비파괴적으로 콘크리트 강도를 간편하게 구할 수 있는 방법으로 적산온도(Maturity) 개념을 통한 콘크리트 강도 추정방법이 많은 연구자를 통하여 검증되고 있다. 본 연구에서는 적산온도 개념을 도입하여 콘크리트 강도를 평가하고자 하는데, 11편 논문의 실험결과에서 W/B=18~70%의 범위에서 일정한 온도(5, 10, 20, 30, 40, 50℃)와 다양한 재령(0.5~182일)에 따른 843개의 실험값을 가지고 가장 간편한 적산온도 모델을 사용하고, 강도별로 보통강도 콘크리트(40Mpa이하), 고강도콘크리트(40~70MPa), 초고강도 콘크리트(70MPa 이상)로 구분하여 현장에서 쉽게 적용할 수 있는 적산온도와 콘크리트 강도관계를 도출하고, 적산온도에 따른 최저 보증 콘크리트 압축강도 추정식을 제시하였다.
연구목적: 적산온도를 이용하여 시멘트 종류별로 고강도 콘크리트(70MPa)의 초기 강도를 정확히 예측하여 콘크리트 품질의 신뢰성 확보, 거푸집 탈형 시기, PS 콘크리트의 텐셔닝 타임, 도로 보수 후 교통의 진입 시기 등을 정확히 도출하여 경제적이고 안전한 건설공사에 도움을 주고자 한다. 연구방법:시멘트 종류별 수화열을 재령마다 측정하여 적산온도를 계산하고, 재령별 콘크리트의 강도를 측정하여 임의의 적산온도에 상응하는 강도를 예측한다. 연구결과: 도로보수에서 교통개방에 필요한 시간을 추정하는데 있어서, ASTM C1074에서는 고강도 콘크리트의 경우에는 이론적으로 16.4시간으로 예측하였으나, 본 연구에서는 OPC인 경우의 적산온도 307, 14.4 시간, LHPC인 경우의 적산온도 2700, 34시간, ESPC인 경우의 적산온도 200, 8시간 정도로 계산되었다. 결론:고강도 콘크리트를 사용한 구조물의 거푸집 탈형시기 및 도로보수의 교통개방 시기는, ACI Committee 347을 적용한 설계기준강도 40MPa이하의 보통콘크리트의 경우보다 월등히 빨라질 수 있다.
Prediction of the early-stage strength of concrete is useful for modernized concrete construction. An experiment was attempted on the high-strength of concrete produced by ordinary portland cement under the curing temperatures of 30, 20, $10^{\cire}C$ and the various mixing proportions such as water-binder ratio of 0.30, 0.35 and silica fume content of 10% by weight of cement. It is the aim of this study to investigare and compare the development of concrete strength with maturity and analyze the application of Maturity as a parameter to correlation estimate test results of concrete. They are statistically analyzed to infer the correlation coefficient between the Maturity and the compressive strength of high-strength concrete.
The aim of this study is to compare the development of compressive strength of high-Flowing concrete with maturity and to investigate the applicability of strength prediction models of concrete. An experiment was attempted on the high-flowing concrete mixes using Ordinary portland cement, High belite cement, Blast furance slage cement and replaced Fly-ash of 30% by weight of Ordinary portland cement, the water-binder ratios of mixes being 0.35 and the curing temperatures being 30, 20, 10, 5$^{\circ}C$. Test results of mixes are statistically analyzed to infer the correlation coefficient between the maturity and the compressive strength of high-flowing concrete.
The objective of this study is to develop the predicting method of concrete strength when remove concrete form-work without making cement test piece at construction site. For this purpose, this study catches the Maturity Method by using RFID, the usability of which is now being emphasized at site, accumulates and record the strength data, which can be gained with the results of existing Maturity Method method that is accompanied with strength estimation study, in database, and finally proposes the system structure which can check the estimated strength by Maturity Method. The merits of this method by using of Maturity Method are as follows; More objective, precise, and rapid decision can be made to the concrete strength and about the maintaining period of concrete form and form support. More efficient control of integrated material management system can be possible. Architectural field example using RFID can be suggested more concretely. RFID applicability can be extended by using DB of material integration management system.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.