Mechanical Properties and Resistance to Freezing and Thawing of the Recycled Aggregate Concrete with Metakaolin (메타카올린을 혼합한 재생골재 콘크리트의 역학적 특성 및 동결융해 저항성)

  • Moon, Han-Young;Kim, Yang-Bae;Moon, Dae-Joong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.9 no.4
    • /
    • pp.270-278
    • /
    • 2005
  • Recycled aggregate concrete has lower strength and durability compared to concrete with natural aggregate. Therefore, metakaolin is used to improve the properties of recycled aggregate concrete. Main components of metakaolin are $SiO_2$ and $Al_2O_3$. and specific surface area is 9 times larger than that of ordinary portland cement. Quality of demolished-recycled aggregate(DRA) satisfies the type 1 of KS F 2573, but quality of source-recycled aggregate(SRA) does not satisfy with the type 2 of KS F 2573. When metakaolin was replaced with 20% of cement, compressive strength of concrete with SRA and DRA develops about 40~64% of control concrete. Water absorption ratio was reduced about 2% by replacing 20% metakaolin and it represents low compared to the natural aggregate concrete without metakaolin. In addition, the resistance to freezing and thawing, of concrete with DRA is indicated to remarkably enhanced due to the contribution of metakaolin. However, when metakaolin is replaced with 20% of cement, relative dynamic modulus of elasticity of concrete with SRA was below 60% at 210 freezing and thawing cycles.

Freezing and Thawing Properties of Concrete Using Recycled Coarse Aggregate (재생굵은골재를 사용한 콘크리트의 동결융해 특성)

  • Sung, Chan-Yong;Youn, Joon-No;Kim, Young-Ik;Im, Sang-Hyuk;Jung, Duck-Hyun
    • Korean Journal of Agricultural Science
    • /
    • v.30 no.2
    • /
    • pp.154-163
    • /
    • 2003
  • This study was performed to examine the freezing and thawing properties of the high strength concrete using recycled coarse aggregate. The recycled coarse aggregate was replaced by 0%, 25%, 50%, 75% and 100% of natural crushed aggregate. The compressive strength of the concrete used recycled coarse aggregate was shown in more than $400kgf/cm^2$ at the curing age 28 days. The weight loss ratio by freezing and thawing was shown in less than 1% at all mix type. The pulse velocity and relative dynamic modulus were decreased with increasing the freezing and thawing cycles. Also, durability factor for the freezing and thawing were decreased with increasing the content of recycled coarse aggregate. But, recycled concrete replaced with recycled coarse aggregate 100% was shown in more than 60 by durability factor in freezing and thawing of 300cycles Accordingly, these recycled coarse aggregate can be used for high strength concrete.

  • PDF

Development of Surface Pavement Materials for Environment-Friendly Farm Road (환경친화형 경작로를 위한 표층포장재료의 개발)

  • Sung, Chan-Yong;Kim, Young-Ik
    • Korean Journal of Agricultural Science
    • /
    • v.31 no.2
    • /
    • pp.105-114
    • /
    • 2004
  • This study was performed to examine the physical and mechanical properties of eco-concrete using soil, natural coarse aggregate, soil compound and polypropylen fiber. The mass loss ratio was decreased with increasing the content of coarse aggregate and soil compound. The compressive strength, flexural strength, ultrasonic pulse velocity and dynamic modulus of elasticity were increased with increasing the content of coarse aggregate, soil compound and polypropylene fiber. The compressive and flexural strengths were showed in 8.07 MPa and 2.641 MPa at the curing age 28 days, respectively. The coefficient of permeability was decreased with increasing the content of coarse aggregate and soil compound, but it was increased with increasing the content of polypropylene fiber. The lowest coefficent of permeability was showed in $5.066{\times}10^{-9}cm/s$.

  • PDF

Applicability Evaluation of Tailing Admixture as Grout Material (그라우트 재료로서 광물찌꺼기 혼화재의 활용 가능성 평가)

  • Kim, Daehyeon;Noh, Jeongdu;Kang, Seong-Seung
    • Tunnel and Underground Space
    • /
    • v.26 no.2
    • /
    • pp.110-119
    • /
    • 2016
  • The purpose of this study is to evaluate the applicability of tailing in the ${\bigcirc}{\bigcirc}$ mine as a grout material. For the purpose, XRD analysis was performed for mineralogical properties of tailing. In addition, flow, velocity, and uniaxial compressive strength tests were carried out for physical and mechanical properties of a grout material with the mixing ratio of cement and tailing and curing periods. By the result of XRD analysis, tailing of the mine was found to mostly consist of quartz, galena, and pyrite. The flow observed by the flow test showed decreasing tendency with increasing the mixing ratio of tailing. The velocity was also lowered with increasing the mixing ratio of tailing regardless of curing periods. The uniaxial compressive strength as well as Young's modulus also show a tendency to decrease with increasing the mixing ratio of tailing independently on the curing periods. Considering only the physical and mechanical properties of a grout material with tailing, the results are considered to be sufficiently used as a grout material. However, since metallic minerals such as galena and pyrite in tailing contents and these are causing environmental contamination, countermeasures should be considered for this problem in future.

Fundamental Properties of Porous Concrete According to the Sizes of Aggregate (골재 크기에 따른 포러스콘크리트의 기초물성에 관한 실험적 연구)

  • 김무한;백용관;강석표;김용로;김재환
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.5
    • /
    • pp.438-446
    • /
    • 2001
  • Recently, porous concrete has been used for the purpose of decreasing the load of earth environment. It consists solely of cement, water and uniform-sized coarse aggregate. And its fundamental properties will be considerably affected by the physical properties of aggregate because the aggregate occupies for the most part in its mix proportion. For such a reason, this study was carried out to investigate the influence of the sizes and kinds of aggregate for the fundamental properties of porous concrete. It showed that the fundamental properties of porous concrete were the similar value in all sizes of aggregate except in the case of using the 2.5∼5㎜ aggregate and were varied according to the kinds of aggregate. In particular, compressive strength of porous concrete using 2.5∼5㎜ aggregate was more higher than that using other aggregate, and its void ratio and coefficient of permeability was lower. And the maintenance capacity of permeability of porous concrete was varied by the sizes and the kinds of aggregate. In particular, it was greatly decreased in case of using the 2.5∼5㎜ aggregate. And unlike dynamic modulus of elasticity of ordinary concrete, that of porous concrete was very high value in early ages and was slowly increased after that time.

A Study on the Determination of Setting Time of Concrete in the Determination of Slip-up Speed for Slip-Form System (슬립폼 시스템 상승속도 결정에 요구되는 콘크리트에서의 초기경화시간 결정을 위한 연구)

  • Kim, Heeseok;Kim, Young-Jin;Chin, Won-Jong
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.31 no.4A
    • /
    • pp.295-302
    • /
    • 2011
  • The setting time which is the important element for the determination of slip-up speed of Slip-Form system is the hardening time of early-age concrete when the in place concrete has minimum compressive strength before the concrete appears out of Slip-Form system. But it is very difficult to predict the setting time because it depends on not only the composition ratio of concrete but also various conditions of construction fields. Thus, the technique to estimate accurately and continuously the hardening time of early-age in place concrete during operating Slip-Form system is necessary to guarantee the safety of Slip-Form system and the maintenance of the shape of concrete. Ultrasonic wave-based nondestructive testing methods have the advantages which are accurate and continuous in estimating concrete compressive strength. Of such methods, the method using surface wave which propagates along the surface of material is effective for thick member such as a pylon. Thus, in this paper a study on the determination of slip-up speed for Slip-Form system using surface wave velocity is performed. The relation between the slip-up speed of Slip-Form system and the setting time is formulated, and the surface wave velocity is estimated from continuous wavelet transform of the numerical results for surface wave propagation. Finally, the accuracy of this method according to the distance between the wave source and receivers and the relation between the estimated surface wave velocity and the elastic modulus are investigated.

Shear stiffness of headed studs on structural behaviors of steel-concrete composite girders

  • He, Jun;Lin, Zhaofei;Liu, Yuqing;Xu, Xiaoqing;Xin, Haohui;Wang, Sihao
    • Steel and Composite Structures
    • /
    • v.36 no.5
    • /
    • pp.553-568
    • /
    • 2020
  • Steel-concrete composite structures have been extensively used in building, bridges, and other civil engineering infrastructure. Shear stud connectors between steel and concrete are essential in composite members to guarantee the effectiveness of their behavior in terms of strength and deformability. This study focuses on investigating the shear stiffness of headed studs embedded in several types of concrete with wide range of compressive strength, and their effects on the elastic behavior of steel-concrete composite girders were evaluated. Firstly, totally 206 monotonic push-out tests from the literature were reviewed to investigate the shear stiffness of headed studs embedded in various types of concrete (NC, HPC, UHPC etc.). Shear stiffness of studs is defined as the secant stiffness of the load-slip curve at 0.5Vu, and a formulation for predicting defined shear stiffness in elastic state was proposed, indicating that the stud diameter and the elastic modulus of steel and concrete are the main factors. And the shear stiffness predicted by the new formula agree well with test results for studs with a diameter ranging from 10 to 30 mm in the concrete with compressive strength ranging from 22.0 to 200.0MPa. Then, the effects of shear stiffness on the elastic behaviors of composite girders with different sizes and under different loading conditions were analyzed, the equations for calculating the stress and deformation of simply supported composite girders considering the influence of connection's shear stiffness were derived under different loading conditions using classical linear partial-interaction theory. As the increasing of shear stiffness, the stress and deflection at the most unfavorable section under partial connected condition tend to be those under full connected condition, but the approaching speed decreases gradually. Finally, the connector's shear stiffness was recommended for fully connection in composite girders with different dimensions under different loading conditions. The findings from present study may provide a reference for the prediction of shear stiffness for headed studs and the elastic design of steel-concrete composite girder.

Mechanical Properties of Strain Hardening Cement-Based Composite (SHCC) with Recycled Materials (자원순환형 재료를 사용한 변형경화형 시멘트 복합체(SHCC)의 역학적 특성)

  • Kim, Sun-Woo;Cha, Jun-Ho;Kim, Yun-Yong;Yun, Hyun-Do
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.5
    • /
    • pp.727-736
    • /
    • 2010
  • This paper describes results of an preliminary study to produce strain hardening cement-based composites (SHCCs)with consideration of sustainability for infrastructure applications. The aims of this study are to evaluate the influence of recycled materials on the mechanical characteristics of SHCCs, such as compressive, four-point bending, and direct tensile behaviors, and to give basic data for constitutive model for analyzing and designing infra structures with SHCCs. In this study, silica sand, cement, and PVA fibers, were partially replaced with recycled sand, fly-ash, and FET fibers in the mixture of SHCCs, respectively. Test results indicated that fly-ash could improve both bending and direct tensile performance of SHCCs due to increasing chemical bond strength at the interface between PVA fibers and cement matrices. However, SHCCs replaced with PET fibers showed much lower performance in bending and direct tensile tests due to originally low mechanical properties of own fibers, although compressive behavior is similar to PVA2.0 specimen. Also, it was noted that the recycled sand would increase elastic modulus of SHCCs due to larger grain size compared to silica sand. Based on pre-set target value to maintain the performance of SHCCs, it was concluded that the replacement ratio below 20% of fly-ash or below 50% of recycled sands would be desirable for creating sustainable SHCCs.

Development of the Structural Condition Evaluation Technique for Asphalt Pavements Using Falling Weight Deflectometer Deflections (Falling Weight Deflectometer 처짐값을 이욤한 아스팔트 포장체의 구조적 상태 평가기법 개발)

  • Son, Jong-Chul;Rhee, Suk-Keun;An, Deok-Soon;Park, Hee-Mun
    • International Journal of Highway Engineering
    • /
    • v.8 no.4 s.30
    • /
    • pp.115-124
    • /
    • 2006
  • The objectives of this paper are to develop the structural condition evaluation technique using Falling Weight Deflectometer deflections and propose the structural condition criteria for asphalt pavements. To figure out correlation between surface deflections and critical pavement responses, the synthetic database has been established using the finite element pavement structural analysis program. A regression approach was adopted to develop the pavement response model that can be used to compute the stresses and strains within pavement structure using the FWD deflections. Based on the pavement response model, the procedure for assessing the structural condition of pavement layers was proposed in this study. To validate the condition evaluation procedure for asphalt pavements, the FWD test, dynamic cone penetrometer test, and repeated triaxial compression test were conducted on 11 sections of national highway and 8 sections of local road. Test results indicate that the tensile strain at the bottom of AC layer and AC elastic modulus were good indicators for estimating the stiffness characteristics of AC layer. For subbase layer, the BDI value and compressive strain on top of the subbase layer were appropriate to predict the structural capacity of subbase layer. The BCI value and compressive strain on top of the subgrade were found to be good indicators for evaluating the structural condition of the subgrade. The evaluation criteria for structural condition in asphalt pavements was also proposed in this paper.

  • PDF

Engineering Characteristics of Mudeungsan Tuff and Ipseok-dae Columnar Joints (무등산응회암과 입석대 주상절리대의 공학적 특성)

  • Noh, Jeongdu;Jang, Heewon;Lim, Chaehun;Hwang, Namhyun;Kang, Seong-Seung
    • The Journal of Engineering Geology
    • /
    • v.30 no.2
    • /
    • pp.161-173
    • /
    • 2020
  • This study is to examine the engineering characteristics of colunmar joints in Mudeugsan National Park, a global geopark. For these purposes, physical and mechanical properties of Mudeungsan Tuff, evaluation for the weathering degree of columnar joints, and crack behavior monitoring in columnar joints were conducted. The physical properties of Mudeungsan tuff were 1.02% for the average porosity, 0.38% for the average absorption, 2.69 g/㎤ for the average specific gravity, and 4,948 m/s for the average elastic wave velocity. Its mechanical properties were 337 MPa for the average uniaxial compressive strength, 68 GPa for the average elastic modulus, 0.29 for the average Poisson's ratio, 41.3 MPa for the average cohesion strength, and 62.8° for the average friction angle. the average rebound Q-value of the silver Schmidt hammer for the three columnar joint blocks at the Ipseok-dae was shown as 49.3. when this value is converted into uniaxial compressive strength, it becomes 70.5 MPa, which is about 21% of the uniaxial compression strength of Mudeungsan tuff. In addition, according to the results of crack monitoring measurements for the three columnar joint blocks at the Ipseok-dae, the crack behavior is less than 1 mm, so it is believed that its behavior in Ipseak-dae columnar joints has hardly occured to date.