• Title/Summary/Keyword: Compressive Failure Strength

Search Result 698, Processing Time 0.03 seconds

Effect of ages and season temperatures on bi-surface shear behavior of HESUHPC-NSC composite

  • Yang Zhang;Yanping Zhu;Pengfei Ma;Shuilong He;Xudong Shao
    • Advances in concrete construction
    • /
    • v.15 no.6
    • /
    • pp.359-376
    • /
    • 2023
  • Ultra-high-performance concrete (UHPC) has become an attractive cast-in-place repairing material for existing engineering structures. The present study aims to investigate age-dependent high-early-strength UHPC (HESUHPC) material properties (i.e., compressive strength, elastic modulus, flexural strength, and tensile strength) as well as interfacial shear properties of HESUHPC-normal strength concrete (NSC) composites cured at different season temperatures (i.e., summer, autumn, and winter). The typical temperatures were kept for at least seven days in different seasons from weather forecasting to guarantee an approximately consistent curing and testing condition (i.e., temperature and relative humidity) for specimens at different ages. The HESUHPC material properties are tested through standardized testing methods, and the interfacial bond performance is tested through a bi-surface shear testing method. The test results quantify the positive development of HESUHPC material properties at the early age, and the increasing amplitude decreases from summer to winter. Three-day mechanical properties in winter (with the lowest curing temperature) still gain more than 60% of the 28-day mechanical properties, and the impact of season temperatures becomes small at the later age. The HESUHPC shrinkage mainly occurs at the early age, and the final shrinkage value is not significant. The HESUHPC-NSC interface exhibits sound shear performance, the interface in most specimens does not fail, and most interfacial shear strengths are higher than the NSC-NSC composite. The HESUHPC-NSC composites at the shear failure do not exhibit a large relative slip and present a significant brittleness at the failure. The typical failures are characterized by thin-layer NSC debonding near the interface, and NSC pure shear failure. Two load-slip development patterns, and two types of main crack location are identified for the HESUHPC-NSC composites tested in different ages and seasons. In addition, shear capacity of the HESUHPC-NSC composite develops rapidly at the early age, and the increasing amplitude decreases as the season temperature decreases. This study will promote the HESUHPC application in practical engineering as a cast-in-place repairing material subjected to different natural environments.

Experiments Study on Critical Strain Properties of Sedimentary Rocks based on Mohr-Coulomb Strength Criterion (Mohr-Coulomb의 파괴기준을 기본으로한 퇴적암의 한계변형률 특성에 관한 연구)

  • Kim, Young-Su;Lee, Jae-Ho;Jin, Guang-Ril;Shin, Shi-Un;Kwon, Tea-Soon;Han, Hee-Su
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2008.03a
    • /
    • pp.821-832
    • /
    • 2008
  • The hazard warning levels are necessary for the rational design and safety construction of underground space, as mountain and urban tunnel. Sakurai provided the hazard warning levels for assessing the stability of tunnels using the critical strain of rock mass, which is defined as a ratio between uni-axial compressive strength and the Young's modulus. The concept of critical strain guidelines is introduced in this study for the assessment of tunnel safety during excavation. Moreover, in this paper, the critical strain properties of sedimentary rock in Korea has investigated and analysed in detail by Lab. test, as the uniaxial and triaxial compression tests. Finally, critical strain properties of sedimentary rock on uniaxial and triaxial stress condition is discussed the relationship of failure strain values, uniaxial and triaxial compression strengths, confining pressure and Young's modulus.

  • PDF

Analysis of the UHP-SFRCC(Ultra High Performance Steel Fiber Reinforced Cementitious Composites) I section Prestressed beam. (초고강도 섬유보강 시멘트 복합체 I형 프리스트레스트 보의 거동 해석)

  • Han Sang Mook;Kim Sung Wook;Kang Su Tae;Kang Jun Hyung
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.11a
    • /
    • pp.57-60
    • /
    • 2005
  • The objective of this paper is to investigate and analyze the behaviour of prestressed I section structural members constructed with ultra high perfomance steel fiber reinforced cementitious concrete (SFR-UHPC). This material is known as reactive powder concrete (RPC) mixed with domestic materials and its compressive strength is over 150MP. The parameters of test specimens were span to depth ratio, prestressing force, prestressing wire placement and web width. Most influential parameter to determine the failure mode between shear and flexural action was proved to be shear span ratio. The characteristics of ultra high-strength concrete is basically brittle, but due to the steel fiber reinforcement behaviour of this structure member became ductile after the peak load. As a result of the test, the stress block of compressive zone should be redefined. The proposed analytical calculation of internal force capacity based by plastic analysis gave a good prediction for the shear and flexural strength of specimens. The numerical verification of the finite element model which constitutive law developed for Mode I fracture of fiber reinforced concrete correctly captured the overall behaviour of the specimens tested.

  • PDF

Theoretical explanation of rock splitting based on the micromechanical method

  • Huang, Houxu;Li, Jie;Hao, Yiqing;Dong, Xin
    • Geomechanics and Engineering
    • /
    • v.14 no.3
    • /
    • pp.225-231
    • /
    • 2018
  • In this paper, in order to explain the splitting of cylindrical rock specimen under uniaxial loading, cracks in cylindrical rock specimen are divided into two kinds, the longitudinal crack and the slanting crack. Mechanical behavior of the rock is described by elastic-brittle-plastic model and splitting is assumed to suddenly occur when the uniaxial compressive strength is reached. Expression of the stresses induced by the longitudinal crack in direction perpendicular to the major axis of the crack is deduced by using the Maxwell model. Results show that the induced stress is tensile and can be greater than the tensile strength even before the uniaxial compressive strength is reached. By using the Inglis's formula and simplifying the cracks as slender ellipse, the above conclusions that drawn by using the Maxwell model are confirmed. Compared to shearing fracture, energy consumption of splitting seems to be less, and splitting is most likely to occur when the uniaxial loading is great and quick. Besides, explaining the rock core disking occurred under the fast axial unloading by using the Maxwell model may be helpful for understanding that rock core disking is fundamentally a tensile failure phenomenon.

Performance of BMSC column with large eccentricity under natural exposure conditions

  • Ma, Haiyan;Zeng, Xiangchao;Yu, Hongfa;Yue, Peng;Zhu, Haiwei;Wu, Chengyou
    • Structural Engineering and Mechanics
    • /
    • v.76 no.4
    • /
    • pp.541-550
    • /
    • 2020
  • As a new type of concrete material, basic magnesium sulfate cement concrete (BMSC) has the advantages, such as early strength, high strength, good toughness and crack resistance. However, it is unclear about the degradation of the mechanical properties of BMSC columns, which is exposed to the natural environment for several years. In order to apply this new concrete to practical engineering, six large-eccentricity compressive columns of BMSC were studied. The mechanical properties such as the crack propagation, failure morphology, lateral displacement and bearing capacity of BMSC column were studied. The results show that the degradation rate of ultimate load of BMSC column is from 6% to 7%. The degradation rate of the stiffness of the column is from 6% to 13%. With the increase of compressive strength of BMSC, the axial displacement and lateral displacement are gradually reduced. The calculation model of bearing capacity of the BMSC column under the large eccentric compression is proposed. This paper provides a reference for the application of BMSC columns in the civil engineering.

A Study for the Adaptation of Simulation of Uniaxial Compressive Strength Test for Concrete in 3-Dimensional Particle Bonded Model (3차원 입자 결합 모델에서 콘크리트의 일축압축실험 모사 적용성 연구)

  • Lee, Hee-Kwang;Jeon, Seok-Won
    • Journal of the Korea Concrete Institute
    • /
    • v.20 no.2
    • /
    • pp.147-156
    • /
    • 2008
  • In an uniaxial compressive test of a concrete standard specimen (150$\times$300 mm) the crack initiation and extension with the stress increase are the major reason of the failure, which is similar to the breakage of the particle bonding in the simulation by using particle bonded model, especially particle flow code in 3 dimensions (PFC3D) developed by Itasca Consulting Group Inc. That is the main motive to study the possibility of an uniaxial compressive strength test simulation. It is important to investigate the relationship between the micro-parameters and the macro-properties because the 3-dimensional particle bonded model uses the spherical particles to analyze the physical phenomena. Contact bonded model used herein has eight micro-parameters and there are five macro-properties; Young's modulus, Poisson's ratio, uniaxial compressive strength and the crack initiation stress and the ratio concerning the crack propagation with the stress. To simulate the compressive test we made quantitative relationships between the micro-parameters and the macro-properties by using the fractional factorial design and various sensitivity analyses including regression analysis, which result in the good agreement with the previous studies. Also, the stress-stain curve and the crack distribution over the specimen given by PFC3D showed the mechanical behavior of the concrete standard specimen under the uniaxial compression. It is concluded that the particle bonded model can be a good tool for the analyzing the mechanical behavior of concrete under the uniaxial compressive load.

2D numerical study of the mechanical behaviour of non-persistent jointed rock masses under uniaxial and biaxial compression tests

  • Vaziri, Mojtaba Rabiei;Tavakoli, Hossein;Bahaaddini, Mojtaba
    • Geomechanics and Engineering
    • /
    • v.28 no.2
    • /
    • pp.117-133
    • /
    • 2022
  • Determination of the mechanical behaviour of jointed rock masses has been a challenge for rock engineers for decades. This problem is more pronounced for non-persistent jointed rock masses due to complicated interaction of rock bridges on the overall behaviour. This paper aims to study the effect of a non-persistent joint set configuration on the mechanical behaviour of rock materials under both uniaxial and biaxial compression tests using a discrete element code. The numerical simulation of biaxial compressive strength of rock masses has been challenging in the past due to shortcomings of bonded particle models in reproducing the failure envelope of rock materials. This problem was resolved in this study by employing the flat-joint contact model. The validity of the numerical model was investigated through a comprehensive comparative study against physical uniaxial and biaxial compression experiments. Good agreement was found between numerical and experimental tests in terms of the recorded peak strength and the failure mode in both loading conditions. Studies on the effect of joint orientation on the failure mode showed that four zones of intact, transition to block rotation, block rotation and transition to intact failure occurs when the joint dip angle varies from 0° to 90°. It was found that the applied confining stress can significantly alter the range of these zones. It was observed that the minimum strength occurs at the joint dip angle of around 45 degrees under different confining stresses. It was also found that the joint orientation can alter the post peak behaviour and the lowest brittleness was observed at the block rotation zone.

Correlation Between Tensile Strength and Compressive Strength of Ultra High Strength Concrete Reinforced with Steel Fiber (초고강도 강섬유 보강 콘크리트의 인장강도와 압축강도 사이의 상관관계에 관한 연구)

  • Bae, Baek-Il;Choi, Hyun-Ki;Choi, Chang-Sik
    • Journal of the Korea Concrete Institute
    • /
    • v.27 no.3
    • /
    • pp.253-263
    • /
    • 2015
  • Ultra-high strength concrete which have 100 MPa compressive strength or higher can be developed applying RPC(Reactive Powder Concrete). Preventing brittle failure under compression and tension, ultra-high strength concrete usually use the steel fibers as reinforcements. For the effective use of steel fiber reinforced ultra-high strength concrete, estimation of tensile strength is very important. However, there are insufficient research results are available with no relation between them. Therefore, in this study, correlation between compressive strength and tensile strength of ultra-high strength concrete was investigated by test and statistical analysis. According to test results, increasing tendency of tensile strength was also shown in the range of ultra-high strength. Evaluation of test results of this study and collected test results were carried out. Using 284 splitting test specimens and 265 flexural test specimens, equations suggested by previous researchers cannot be applied to ultra-high strength concrete. Therefore, using database and test results, regression analysis was carried out and we suggested new equation for splitting and flexural tensile strength of steel fiber reinforced ultra-high strength concrete.

Strength and Permeability Characteristics of Soil-Bentonite Mixture (Soil-Bentonite 혼합토의 강도 및 투수 특성)

  • Jin, Guangri;Im, Eunsang;Kim, Kiyoung;Sin, Donghoon
    • Journal of the Korean GEO-environmental Society
    • /
    • v.11 no.4
    • /
    • pp.5-12
    • /
    • 2010
  • Soil mixture using bentonite as a cutoff material is used a lot for various structures such as landfills, banks and dams as cutoff materials. But seepage water is expected to seep since shear failure of filter layer occurs due to external load, embankment load when constructed. Generally, only coefficient of permeability of Soil Mixture is considered irrespective of the changes of intensity on amount of additives. This research is to study on how the changes of amount of bentonite affects permeability and strength of soil mixture. So successive experiments for measuring permeability and strength were conducted as the amount of bentonite changes from 0 to 4%, mixing with the bed material and then making specimens. Around construction site of B dam. As a result, 2.085E-07 cm/sec was shown when the amount of Soil Mixture was 4%. It is proved that unconfined compressive strength and tensile strength increase as the amount of bentonite increases, but saturation shear strength of bentonite soil mixture from the CD experiment is hardly influenced by the amount of bentonite.

COMPARATIVE STUDY ON THE FLUORIDE RELEASE AND COMPRESSIVE STRENGTH OF SEVERAL F-CONTAINING RESTORATIVE MATERIALS (수종의 불소 함유 수복재의 불소 유리 및 압축 강도에 관한 연구)

  • Park, Jee-Young;Kim, Jong-Soo;Kim, Seung-Oh
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.35 no.3
    • /
    • pp.469-476
    • /
    • 2008
  • This study was performed to compare the fluoride release pattern and compressive strength of recently developed resin-modified glass ionomers($Ketac^{TM}$ N 100 and Fuji Fil LC) with those of conventional glass ionomer restorative material(Fuji II LC). Fifteen sample discs(6 mm diameter and 1 mm height) were prepared for each tested material. The fluoride release was measured by pH/ISE meter(750P, Istek, Korea) for 31 days. For compressive strength experiment, fifteen cylindrical specimens were prepared for each tested material. Each specimen was submitted to compressive strength testing in an universal testing machine(Kyung-sung Testing Machine Co., Korea) at crosshead speed of 5.0mm/min until failure. The results can be summarized as follows; 1. Fuji Fil LC released the highest amount of fluoride, followed by Fuji II LC and $Ketac^{TM}$ N 100(p<0.05). 2. The compressive strength of Fuji Fil LC was the lowest(p<0.05). However, no significant difference was found from Fuji II LC and $Ketac^{TM}$ N 100(p>0.05). By considering the above results, careful case selection and accurate clinical application is recommended when using $Ketac^{TM}$ N 100 and Fuji Fil LC.

  • PDF