Silica is used in shell materials to minimize oxidation and aggregation of nanoparticles. Particularly, porous silica has gained attention because of its performance in adsorption, catalysis, and medical applications. In this study, to investigate the effect of the density of the silica coating layer on the color of the pigment, we arbitrarily change the structure of a silica layer using an etchant. We use NaOH or $NH_4OH$ to etch the silica coating layer. First, we synthesize ${\alpha}-FeOOH$ for a length of 400 nm and coat it with TEOS to fabricate particles with a 50 nm coating layer. The coating thickness is then adjusted to 30-40 nm by etching the silica layer for 5 h. Four different shapes of ${\alpha}-FeOOH$ with different colors are measured using UV-vis light. From the color changes of the four different shapes of ${\alpha}-FeOOH$ features during coating or etching, the $L^*$ value is observed to increase and brighten the overall color, and the $b^*$ value increases to impart a clear yellow color to the pigment. The brightest yellow color was that coated with silica; if the sample is etched with NaOH or $NH_4OH$, the $b^*$ value can be controlled to study the yellow colors.
This study was carried out to evaluate whether EVAc, acryl latex and biobinder could substitute the part of SB latex for pre-coating color formula or not. Different coating colors prepared through the substitution of 30% SB latex with EVAc, acryl latex, and biobinder were applied for pre-coating layer. 100% SB latex is used as a binder for top coating color. The optical properties, gloss, roughness, stiffness, dry- and wet-pick strength were measured. There were no significant differences in the brightness, whiteness, opacity, roughness, ink set-off and gloss of paper coated with 5 different coating colors. However the stiffness, dry- and wet-pick strength were somewhat lower than those of conventional coating color which 100% SB latex was used as a binder. Although the part of SB latex could be substituted with EVAc, acryl latex and biobinder without sacrificing the qualities of coated paper. Further researches on the improvement of stiffness, dry- and wet-pick strength, and the optimization of rheology of coating color in order to improve the qualities of coated paper are strongly recommended.
Natural water-soluble polymers such as starch, casein and carboxy methyl cellulose(CMC) have been limited in their uses. However, the proper water retention of coating colors can not be obtained without addition of these polymers. Furthermore, the coating runnability and the physical properties of coated paper were not also satisfied. Therefore, the objective of this study was to synthesize the water retention and flow modifiers which can improve the water retention and flow properties of coating colors. We have measured physical properties of flow modifiers and coating colors which included flow modifiers. The viscosity of flow modifiers was very low at acid pH, and rapidly increased at about pH 7, and gradually reached to equilibrium at alkali pH. Such an increase comes from the molecular weight of flow modifiers and the amount of acrylic and methacrylic acids. The viscosity of coating color containing the flow modifiers was lower than that containing CMC. However, both of them had little difference in water retention. The water-phase viscosity of synthetic modifier containing coating color was either higher or similar compared to that of CMC containing coating color. The high shear viscosity of coating colors was low. Therefore, it can be concluded that the synthetic flow modifiers are very useful for improvement of flow properties and water retentions.
This research was intended to evaluate the effect of carboxymethylcellulose(CMC) on the coating structure and surface strength of coated paper prepared with amphoteric latex based coating color. Printability and optical properties of coated papers were compared. The influence of the consolidation behavior of coating color on the coating structure and the surface strength of coated paper was investigated. Compared with the conventional anionic latex, amphoteric latex formed bulkyer, smoother and more porous coating layer, which in turn, restricted binder migration in the coating layers, and facilitated immobilization of coating colors. However, dry pick strength of coated paper was decreased. The addition of CMC to these systems had strongly influenced on. the consolidation behavior and porosity in the dry state, through forming the network structure of coating layers by the interaction with amphoteric latex particles. Thus, printability and optical properties of coated papers were improved. Results indicated that amphoteric latex could be practically applied to the paper coating to improve printability and optical properties of coated papers.
한국정보디스플레이학회 2009년도 9th International Meeting on Information Display
/
pp.1386-1388
/
2009
We report on a new method of fabricating color filters based on selective wetting of color inks. The reversible formation of a hydrophobic layer provides sequential generation and protection of successive color filter patterns through a simple coating process. The transmittance and geometrical properties of the fabricated color filter were described.
Curtain coating has been considered as the best coating technology because it is a coating technology that forms contour coating layer with better coverage. To increase the curtain stability surfactants are being used. In this study, the effect of a surfactant on the stability of curtain coating colors was examined by evaluating dynamic surface tension with a bubble surface tensiometer. Di-2-ethylhexyl sodium sulfosuccinate was used as a surfactant since it showed low dynamic surface tension at low surface age. And we evaluated the influence of surfactant on coating color properties including surface tension, viscosity and curtain stability. The surface tension of coating color was decreased when surfactant addition was increased up to 0.5 pph, but it was leveled off at 0.3 pph of surfactant addition. With the increase of surfactant addition rate, viscosity of coating color were increased. Micelles formed by surfactant contributed to the increase of the viscosity. Curtain stability was improved with the addition of surfactant until it reached up to 0.5 pph. Excessive addition of surfactant (> 0.5 pph) didn't improve curtain stability. This was attributed to Marangoni effect(self-healing) and decreasing of curtain thickness.
A piece of coating color or base paper picked during printing is called coating pick. Loosely bonded materials of coating color or broken piece of fiber could be adhered to the blanket or would be mixed with ink during printing. Because the coating pick can make troubles in printing press such as piling, hickey and collecting, the coating pick of a paper has been one of the most serious problems in printing. In this paper, two influential factors to the coating pick in the printing, those are latex content and ash content of the coating color, are studied. The surface resistance of coating paper is directly proportional to the latex content, otherwise inversely proportional to the ash content. We propose a different way to evaluate the picking and used a homemade pick test device.
The quantitative analysis of SB latex contents in coating color and coated paper was investigated with FT/Raman spectroscopy. From the measured FT/IR and FT/Ramon spectra, the peaks of coating color were compared with those of each compoents . Calibration curves were obtained by the area of latex peaks and PLS method of QuantIR program. The relation of predicted values in PLS method and actual values in coating mixtures and coating layer was examined. The components of coating layer in coated paper were investigated by EDS , X-mapping and SEM, The contents of latex in z-direction were calculated in the coating layer of unknown coated paper. The latex concentration measurements of Top layer and Pre layer in double coated paper show that each layer has different value. In single coated paper, it is clear that the latex concentration is highest at the surface and decreases with an increase of depth. From those results it is indicated that the latex migrates to the coated surface. The result of this study may be applied to the binder migration study and the quality control in paper mill.
A combined PC and TV monitor has been developed in several companies. The characteristics of physical user interface in this monitor are likely to vary from existing monitors. Therefore, two experiments to investigate the physical interface characteristics of this monitor were conducted. The first experiment was to investigate the characteristics of color perception with monitor coating (coating vs. non-coating) and screen brightness (30fL vs. 35fL) in the PC mode. The second experiment was to investigate the characteristics of luminance contrast with monitor coating and image movement (static vs. dynamic) in the TV mode. Twenty-three subjects (male 12, female 11) were participated in this experiment. In the first experiment, average color temperatures were obtained in all experimental conditions. There was a significant difference between coating and non-coating screen at 0.1 level. In the second experiment, average luminance contrasts were obtained in all experimental conditions. There was a significant difference between coating and non-coating screen at 0.05 level. In addition, there was a significant difference between static picture and dynamic picture at 0.1 level.
무설탕 원료로서 xylitol, maltitol, isomalt, erythritol 및 sorbitol을 껌의 코팅 재료로 사용하여 코팅 공정 중 제조특성과 외관을 비교하였고, 코팅 후 표면 균일성, 색택 변화, 코팅시간, 건조시간 등을 비교하였을 때 maltitol이 가장 우수하였으며, erythritol과 sorbitol은 코팅품질과 코팅시간이 길어지는 등의 생산성과 품질면에서 껌의 코팅 소재로는 부적합하였다. 이에 maltitol, xylitol 및 isomalt로 코팅한 껌을 고온 저장하면서 코팅층의 색택 변화를 분석한 결과, maltitol 코팅껌의 경우 $80^{\circ}C$, 1일간 저장시 ${\Delta}E$값은 2.88로 상온보관 시료와 비교하여 색상의 변화가 비교적 작았으나, xylitol과 isomalt 코팅껌은 색상의 변화가 크게 나타났다. 또한, maltitol 코팅껌을 polypropylene 포장재에 넣고 저장 중 색택의 변화를 관찰한 결과, $40^{\circ}C$이하에서는 색택의 변화가 적었으며, $60^{\circ}C$에서도 30일간 저장시 색차는 3 이하로 나타나 유통과정 상 품질의 변화가 적을 것으로 판단되었다. 그러나 본 실험은 색상변화로만 저장 중 변화를 평가하였던 바, 향후 당알코올류를 코팅제로 사용한 코팅껌의 저장 중 품질에 대한 추가적인 연구가 진행되어야 할 것이다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.