  • In order to evaluate the fitness and the degree of rounding of porcelain margins in collarless metal cermic restorations, collarless metal ceramic restorations were fabricated with shoulder margins of 90 and 120 degress, each consisting of ten specimens, on master dies through the direct lift technique. And ten metal ceramic restorations with a shoulder 90 degrees were fabricated. All specimens were embedded in resin and sectioned longitudinally. The sections were observed under a stereomicroscope and photographed(${\times}$200). The labial marginal gap between the die and the porcelain margin were measured with a scale. The space between the porcelain margin and the die, that is formed from marginal rounding and cementation were calculated with a computer coordinating area curvimeter. The following results were obtained. 1. There was no statistical difference between the fitness of porcelain margin of collarless metal ceramic restorations and marginal fitness of metal ceramic restoration. 2. There was no statistical difference between a shoulder of 90 and 120 degrees in the fitness of porcelain margin of collarless metal ceramic resorations. 3. Collarless metal ceramic restorations with a shoulder of 90 degrees and 120 degrees showed significantly more labial marginal rounding than metal ceramic restorations. 4. There was no statistical difference between a shoulder of 90 and 120 degrees in rounding of porcelain margin of collarless metal ceramic restorations. According to the results, rounding of porcelain margins can be observed in collarless metal ceramic restorations. Thus, there is a need for improvement in dental materials and techniques to minimize this problem, Furthermore, care should be exercised during the clinical procedure.

  • PDF

구 보철물 치경부 변색의 심미 재수복 (- Esthetic Retreatment of Old Restorations with Cervical Discolorations -)

  • 김학수;김욱중;조문상;이종엽
    • 대한심미치과학회지
    • /
    • 제11권2호
    • /
    • pp.33-36
    • /
    • 2002
  • As patients have concerned the esthetics of dental restorations, the porcelain fused to metal restorations have gain their popularity due to their strength and esthetic appearance for many years. However, metal collar in subgingival level of porcelain fused to metal restoration often causes black shadows. Inadequately positioned metal collar causes plaque depositions, gingival inflammations, black shadows, and discolorations of margin area. Those problems can be avoided by a clear finishing line, well-fabricated provisional restorations with precise margin and fine polishing, collarless porcelain fused to metal restoration, and all ceramic restoration. In this case report, collarless porcelain fused to metal restoration was used to treat cervical discoloration from old restorations.

  • PDF

금속코핑 설계에 따른 Collarless Metal Ceramic Crown의 파절강도에 관한 연구 (A STUDY ON FRACTURE STRENGTH OF COLLARLESS METAL CERAMIC CROWN WITH DIFFERENT METAL COPING DESIGN)

  • 윤종욱;양재호;장익태;이선형;정헌영
    • 대한치과보철학회지
    • /
    • 제37권4호
    • /
    • pp.454-464
    • /
    • 1999
  • The metal ceramic crown is currently the most popular complete veneer restoration in dentistry, but in many cases, the metal cervical collar at the facial margin is unesthetic and unacceptable. Facial porcelain margin has been used in place of it. But this dose not solve the problems, such as dark gingival discoloration and cervical opaque reflection of porcelain veneer. Recently, metal copings which were designed to terminate its labio-cervical end on the axial walls coronal to the shoulder have been clinically used to solve the esthetic problem of metal ceramic crown. But in this design, porcelain veneer of labio-cervical area which is not supported by metal may not be able to resist the stress during cementation and mastication. The purpose of this study was to evaluate fracture strength and fractured appearance of crowns according to different coping designs. A resin maxillary left central incisor analogue was prepared for a metal ceramic crown, and metal dies were made with duplication mold. Metal copings were made and assigned to one of four groups based on facial framework designs: group 1, coping with 0.5mm metal collar; group 2, metal extended to the shoulder; group 3, metal extended to 1mm coronal tn the shoulder: group 4, metal extended to 2mm coronal to the shoulder. Copings and crowns were adjusted to be same size and thickness, and cemented to metal dies with zinc phosphate cement by finger pressure. Fracture strength was measured with Instron Universal Testing Machine. Metal dies were anchored in Three-way-vice at 3mm below finish line and at $130^{\circ}$ inclined to the long axis of the crown. Load was directed lingually at 2mm below midincisal edge. Load value at initial crack and at catastrophic fracture was recorded. The results obtained were as follows : 1. Fracture strength values at initial crack were higher in groups 1, 2 than in groups 3, 4 but this difference was not statistically significant(P<0.05). 2. Conventional metal collared crown had greater catastrophic fracture strength than any other collarless crowns. 3. The greater the labial metal coping reduction, the lower the catastrophic fracture strength of crowns but when more than 1mm of labial metal reduction was done, the difference in strengths was not statistically significant(p<0.05). 4. The strongest collarless coping design was group 2.

  • PDF

Alternate metal framework designs for the metal ceramic prosthesis to enhance the esthetics

  • Vernekar, Naina Vilas;Jagadish, Prithviraj Kallahalla;Diwakar, Dr Srinivasan;Nadgir, Ramesh;Krishnarao, Manjunatha Revankar
    • The Journal of Advanced Prosthodontics
    • /
    • 제3권3호
    • /
    • pp.113-118
    • /
    • 2011
  • PURPOSE. The objective of the present study was to evaluate the effect of five different metal framework designs on the fracture resistance of the metal-ceramic restorations. MATERIALS AND METHODS. For the purpose of this study, the central incisor tooth was prepared, and the metal analogue of it and a master die were fabricated. The counter die with the 0.5 mm clearance was used for fabricating the wax patterns for the metal copings. The metal copings with five different metal framework designs were designed from Group 1 to 5. Group 1 with the metal collar, Group 2, 3, 4 and 5 with 0 mm, 0.5 mm, 1 mm and 1.5 mm cervical metal reduction respectively were fabricated. Total of fifty metal ceramic crown samples were fabricated. The fracture resistance was evaluated with the Universal Testing Machine (Instron model No 1011, UK). The basic data was subjected to statistical analysis by ANOVA and Student's t-test. RESULTS. Results revealed that the fracture resistance ranged from 651.2 to 993.6 N/$m^2$. Group 1 showed the maximum and Group 5 showed the least value. CONCLUSION. The maximum load required to fracture the test specimens even in the groups without the metal collar was found to be exceeding the occlusal forces. Therefore, the metal frameworks with 0.5 mm and 1 mm short of the finish line are recommended for anterior metal ceramic restoration having adequate fracture resistance.