• Title/Summary/Keyword: Cold Rolled Sheet

Search Result 152, Processing Time 0.025 seconds

Characterization of Electro-Polymerized Polyaniline Film on the Cold Rolled Sheet in the Oxalic acid and Sodium Molybdate Electrolyte (옥살산과 몰리브덴산나트륨 전해액에서 냉연강판에 전해중합된 폴리아닐린 피막의 특성)

  • Lim, Ki-Young;Yoon, Jeong-Mo;Ki, Joon-Seo;Jang, Yong-Seok
    • Korean Journal of Materials Research
    • /
    • v.16 no.6
    • /
    • pp.386-393
    • /
    • 2006
  • Increasing environmental concerns require to solve the problem produced due to the use of heavy metals in coating formulations. Therefore, it is necessary to develop new coating strategy employing inherently conducting polymers such as polyaniline. Polyaniline is a conductive polymer that is synthesized by oxidation polymerization, and the electrochemical and chemical polymerization are possible for the oxidation of aniline. Electrochemical oxidation polymerization produces a fine surface and although voltage control is more convenient, it require electrolytic cells, and elaborate thin film can be acquired with the polymerization. Polyaniline films were electro-polymerized on cold rolled sheets using the galvanostat mode in the oxalic acidaniline-sodium molybdate electrolyte. The structure and properties of polyaniline film were studied using Potentiostat/Galvanostat 263A, FE-SEM,, AFM, SST, Colorimetry. A high corrosion resistance of polyaniline film was observed with an increase of corrosion potential by $500{\sim}600$ mV for the substrate covered with polyaniline.

A Study on Fatigue Fracture Behavior of Laser Beam Welding and Steel with Different Materials ($CO_2$ 레이저 용접 이종재료강의 피로파괴거동에 관한 연구)

  • Han, M.S.;Suh, J.;Lee, J.H.;Kim, J.O.;Jeon, S.M.
    • Laser Solutions
    • /
    • v.9 no.2
    • /
    • pp.1-9
    • /
    • 2006
  • In this paper, we investigated the characteristics of fatigue fracture on TB(Tailored Blank) weldment by comparing the fatigue crack propagation characteristics of base metal with those of TB welded sheet used for vehicle body panels. We also investigated the influence of center crack on the fatigue characteristic of laser weld sheet of same thickness. We conducted an experiment on fatigue crack propagation on the base metal specimen of 1.2mm thickness of cold-rolled metal sheet(SPCSD) and 2.0mm thickness of hot-rolled metal sheet(SAPH440) and 1.2+2.0mm TB specimen. We also made an experiment on fatigue crack propagation on 2.0+2.0mm and 1.2+1.2mm thickness TB specimen which had center crack. The characteristics of fatigue crack growth on the base metal were different from those on 1.2+2.0mm thickness TB specimen. The fatigue crack growth rate of the TB welded specimens is slower in low stress intensity factor range $({\Delta}K)$ region and faster in high${\Delta}K$ region than that of the base metal specimens. The slant crack angle slightly influenced the crack propagation of the TB specimen of 2.0+2.0mm thinkness.

  • PDF

The Low Cycle Fatigue Behavior of Laser Welded Sheet Metal for Different Materials (이종재료 레이저 용접 판재의 저주기 피로 특성)

  • Kim Seog-Hwan;Kwak Dai-Soon;Kim Woong-Chan;Oh Taek-Yul
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2005.10a
    • /
    • pp.627-631
    • /
    • 2005
  • In this study, low fatigue behavior of laser welded sheet metal were investigated. Before welding, the cross section of butt joint was prepared only by fine shearing without milling process. Specimens were same sheet metal and welding condition that using automobile manufacturing company at present. Butt joint of cold rolled sheet metal was welded by $CO_2$ laser. It is used that welding condition such as laser welding speed was 5.5m/sec and laser output power was 5kW for 0.8mm and 1.2mm sheet metal. The laser weldments were machined same or different thickness and same or different material. In order to mechanical properties of around welding zone, hardness test was performed. Hardness of welding bead is about 2 times greater than base material. We performed the low cycle fatigue tests for obtaining fatigue properties about thickness and the weld line direction of specimen. The results of strain controlled low cycle fatigue test indicate that all specimens occur cyclic softening, as indicated by the decrease in stress to reach a prescribed strain.

  • PDF

Textures Evolution of Rolled AA5182 Alloy Sheets after Annealing (알루미늄 5182 압연 판재의 어닐링 집합조직)

  • Kim Kee Joo;Shin Kwang Seon;Jeong Hyo-Tae;Paik Young-Nam
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.13 no.6
    • /
    • pp.128-134
    • /
    • 2005
  • In order to fabricate the aluminum alloys with good drawability, the textures evolution of the AA5182 sheets after rolling and annealing was studied. The measurement of the deformation textures was carried out for the sheets which were cold rolled with high reduction ratio by using the symmetric roll. In addition, the change of the recrystallization texture was investigated after heat-treatments of the rolled sheets with various heat treatment conditions. Rolling without lubrication and subsequent annealing led to the formation of favorable $rot-C_{ND}\;\{001\}<110>\;and\;{\gamma}-fiber ND//<111>$ textures in AA5182 sheets. From the results, the ${\gamma}$-fiber ND//<111> component well evolved during rolling at highest reduction ratio (over $90\%$, l/d parameter of 6.77). Among shear deformation textures, the ${\gamma}$-fiber ND//<111> was not rotated in holding time of $180\~7,200$ seconds at $350^{\circ}C$. The Monte-Carlo technique was used and could be representatively simulated these textures evolution during recrystallization.

Effect of Initial Structure on the Retained Austenite and Tensile Properties of Fe-Si-Mn-P Steel Sheet (Fe-Si-Mn-P강판의 초기조직변화가 잔류오스테나이트 형성 및 인장성질에 미치는 영향)

  • Moon, Won-Jin;Kang, Chang-Yong;Kim, Han-Goon;Kim, Ki-Don;Sung, Jang-Hyun
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.10 no.1
    • /
    • pp.10-19
    • /
    • 1997
  • This study has been conducted to investigate the effects of initial structure on the microstructure and tensile properties of high strength trip steel sheet. The initial structure before austempering remarkably influenced the second phase. The specimen with normalized initial structure showed mainly bainitic ferrite and retained austenite, while the as rolled specimen and spherodized specimen showed martensite plus retained austenite and martensite plus bainitic ferrite with small retained austenite, respectively. Two type of retained austenite, film type and granual type were observed in all specimens. The as rolled specimen appeared the highest contents of retained austenite owing to the compressive stress by cold rolling. The contents of retained austenite increased with increasing intercritical annealing temperature and austempering time. Tensile strength showed the highest in the as rolled specimen, while the highest elongation were obtained in the normalized specimen. The maximum T.S.${\times}$El. Value showed in normalized initial structure and increased with increasing intercritical annealing and austempering time. The highest Value of T.S.${\times}$El. obtained at austempering temperature of $400^{\circ}C$ and retained austenite of 12%.

  • PDF

Hot and Cold Rolling Characteristic with High-Nitrogen Steel of Austenitic Stainless (HNS) (오스테나이트계 고질소 스테인레스 강의 열간 및 냉간 압연특성)

  • Lee, J.W.;Kim, D.S.;Kim, B.K.;Kim, D.K.;Kim, Y.D.;Cha, D.J.;Lee, M.R.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.10a
    • /
    • pp.99-101
    • /
    • 2008
  • At 21st century, material development concepts were changed to fulfill the environmental friendly demands. This study is to study the effect of pressurized nitrogen gas and manganese in high nitrogen austenitic stainless steel(HNS) in which N and Mn elements substitute the nickel element. 100kg HNS ingots were made by Pressurized Vacuum Induction Melting(P-VIM) and were forged according to free forging process. As forged HNS were hot and cold rolled by pilot scale rolling machine. Depending on the rolling condition, the mechanical properties of HNS were changed. The roll thrust and sheet folding showed asymmetry condition between work and drive side during cold and hot rolling. The purpose of this study are to improve workability the hot and cold rolling machine and to set the conditions for establishing the rolling process.

  • PDF

Plastic Strain Ratios of Asymmetry Rolled Aluminum Sheets (비대칭 압연 알루미늄의 소성변형비)

  • Akramov, S.;Kim, I.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2007.05a
    • /
    • pp.425-426
    • /
    • 2007
  • The physical and mechanical properties of the sheets metals are closely related to the presence of preferred crystallographic orientations which were produced by the manufacturing process. To obtain the aluminum alloys sheets with good Al sheet formability, the plastic strain ratio (or r-value) of AA1050 Al sheets after asymmetric rolling and subsequent heat treatment was studied. The AA1050 aluminum alloy sheets after asymmetric rolling with high reduction ratio and following heat treatment had the higher plastic strain ratio.

  • PDF

Evolution of Strain States and Textures During Rolling with Various Conditions (압연조건에 따른 변형률 상태의 변화와 집합조직의 형성)

  • Kang, H.G;Huh, M.Y
    • Transactions of Materials Processing
    • /
    • v.15 no.7 s.88
    • /
    • pp.479-484
    • /
    • 2006
  • The evolution of strain states and textures during rolling with various conditions was investigated by finite element method (FEM) simulations and measurements of rolling textures. Symmetrical rolling with a high friction gives rise to a strong variation of shear strains in rolled sample leading to the formation of texture gradients throughout the thickness layers. A small variation of shear strains during rolling with a well lubrication condition leads to the formation of a fairly homogeneous rolling texture throughout the sheet thickness. During asymmetrical rolling, a proper control of rolling parameters provides the evolution of a fairly homogeneous shear texture throughout the whole sheet thickness.

Press Formabilities of Aluminum Sheets for Autobody Application (차체용 알루미늄 판재의 프레스 성형성)

  • Kim, Y.S.;Kim, K.S.;Kwon, N.C.
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.2 no.1
    • /
    • pp.73-83
    • /
    • 1994
  • Press formabilities of aluminum sheets for automobile body were investigated. Plane strain stretching test (called RIST-PSST), cupping test and U bending test were performed to assess the press formability of aluminum sheets respectively. The results showed that aluminum sheets are generally inferior to cold-rolled steel sheet of deep drawing quality (CSP3N) in press formability. The limiting punch height (LPH) and limiting plane strain (FLCo) of aluminum sheets are 50%-70% level compared to that of CSP3N. Moreover, the limiting drawing ratios(LDR) of aluminum sheets are ranged between 1.95 and 2.1. The poor press formability of aluminum sheets is responsible for low values of total elongation and plastic anisotropy parameter in tensile characteristic. The shape fixability of aluminum sheets evaluated in U bending test is very poor due to its low elastic modulus compared to CSP3N.

  • PDF

Study on the Friction Characteristics of Various Bead Materials in Drawbead Forming of Cold Rolled Steels for Automotive Parts (자동차용 냉간압연재의 드로우비드 성형시 비드 재질별 마찰특성에 관한 연구)

  • Lee D. H.;Kim W. T.;Moon Y. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.08a
    • /
    • pp.91-97
    • /
    • 2004
  • The drawbead is one of the most important factors in sheet metal forming for automotive parts. So clarifying the friction characteristics between sheets and drawbead is essential to improve the formability of sheet metal. Therefore in this study, drawbead friction test was performed at various bead materials(FC300, HC891, FCD550, HD700, HK600, HK700, SKD11) and surface treatment of beads(Base, induction hardening, Cr plating, ion nitriding, Toyoda diffusion process, TiCN, TiN, CrN). Circular shape bead has been used for the test. The results show that friction and drawing characteristics were mainly influenced by surface treatment.