• Title/Summary/Keyword: Coating Sputtering

Search Result 366, Processing Time 0.027 seconds

Transparent Electrode Forming Technology using ESD Coating Methode (ESD 기법을 이용한 투명전도막 형성 기술)

  • Kim, Jung-Su;Kim, Dong-Soo
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2009.11a
    • /
    • pp.348-348
    • /
    • 2009
  • The conductive coating method is used for various industrial fields. For example, Sputtering process is used to coat ITO layer in LCD or OLED panel manufacture process and fabricate a base layer of substrate of an electric printing device. However, conventional coating processes (beam sputtering, spin coating etc.) has a problems in the industrial manufacturing process. These processes have a very high cost and critical manufacturing environment as a vacuum process. Recently, many researchers have proposed various printing process instead of conventional coating processes. In this paper, we propose an ESD printing process in ITO coating layer and apply to fabricate a conductive coating film. Furthermore, the effect of the nozzle and also the applied voltage on different configuration of the nozzle head was also studied for better understanding of the Electro Static deposition process.

  • PDF

A Comparative Study of Nanocrystalline TiAlN Coatings Fabricated by Direct Current and Inductively Coupled Plasma Assisted Magnetron Sputtering (DC 스퍼터법과 유도결합 플라즈마를 이용한 마그네트론 스퍼터링으로 제작된 나노결정질 TiAlN 코팅막의 물성 비교 연구)

  • Chun, Sung-Yong;Kim, Se-Chul
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.5
    • /
    • pp.375-379
    • /
    • 2014
  • Nanocrystalline TiAlN coatings were prepared by reactively sputtering TiAl metal target with $N_2$ gas. This was done using a magnetron sputtering system operated in DC and ICP (inductively coupled plasma) conditions at various power levels. The effect of ICP power (from 0 to 300 W) on the coating microstructure, corrosion and mechanical properties were systematically investigated using FE-SEM, AFM and nanoindentation. The results show that ICP power has a significant influence on coating microstructure and mechanical properties of TiAlN coatings. With increasing ICP power, the coating microstructure evolved from the columnar structure typical of DC sputtering processes to a highly dense one. Average grain size of TiAlN coatings decreased from 15.6 to 5.9 nm with increasing ICP power. The maximum nano-hardness (67.9 GPa) was obtained for the coatings deposited at 300 W of ICP power. The smoothest surface morphology (Ra roughness 5.1 nm) was obtained for the TiAlN coating sputtered at 300 W ICP power.

Coating System for High Quality Ferromagnetic Thin Films (고품위 자성체 박막 코팅 시스템)

  • Kim, Gi-Bum;Hwang, Yoon-Sik;Kim, Yeong-Shik;Park, Jang-Sick;Park, Jae-Bum
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.231-232
    • /
    • 2007
  • Nickel oxide thin films were deposited by the DC magnetron reactive sputtering process under the conditions such as various oxygen flow rates(0, 3, 6, 8, 10 sccm) with constant 33 sccm argon flow rate for the sputtering time of 40 second with the power of 0.3 kW. Sheet resistances were measured by the four point probes. In order to observe discharge voltage characteristics according to the oxygen flow rates, the sputtering processes were performed under the powers of 0.2kW and 0.3kW. The feasibility of the coating system for high quality ferromagnetic thin films was tested through the electromagnetic simulation and the thin film thickness measurement from the experiment. It was shown that a discharge voltage was decreased under the low power and low oxygen flow rate, since the oxygen was quickly saturated on nickel target surface. The sheet resistance was increased as oxygen flow rate increased. The film thickness deposited by the coating system for ferromagnetic target was improved approximately 10% in comparison with previous coating systems.

  • PDF

The Effect of High Power Sputtering Conditions on Surface Roughness of Carbon Mold for Glass Forming (유리성형용 카본금형의 표면조도에 미치는 고출력 스퍼터링 조건의 영향)

  • Sung-Hoo Ju;Jae-Woong Yang
    • Journal of the Korean Applied Science and Technology
    • /
    • v.41 no.1
    • /
    • pp.46-57
    • /
    • 2024
  • In this study, the various process conditions for high-power DC Magnetron Sputtering (DCMS) on the surface roughness of carbon thin films were investigated. The optimal conditions for Si/C coating were 40min for deposition time, which does not deviate from normal plasma, to obtain the maximum deposition rate, and the conditions for the best surface roughness were -16volt bias voltage and 400watt DC power with 1.3x10-3torr chamber pressure. Under these optimal conditions, an excellent carbon thin film with a surface roughness of 1.62nm and a thickness of 724nm was obtained. As a result of XPS analysis, it was confirmed that the GLC structure (sp2 bonding) was more dominant than the DLC structure (sp3 bonding) in the thin film structure of the carbon composite layer formed by DC sputtering. Except in infrequent cases of relatively plasma instability, the lower bias voltage and applied power induces smaller surface roughness value due to the cooling effect and particle densification. For the optimal conditions for Graphite/C composite layer coating, a roughness of 36.3 nm and a thickness of 711 nm was obtained under the same conditions of the optimal process conditions for Si/C coating. This layer showed a immensely low roughness value compared to the roughness of bare graphite of 242 nm which verifies that carbon coating using DC sputtering is highly effective in modifying the surface of graphite molds for glass forming.

Anti-Reflection Coating Application of SixOy-SixNy Stacked-Layer Fabricated by Reactive Sputtering (반응성 스퍼터링으로 제작된 SixOy-SixNy 적층구조의 반사방지 코팅 응용)

  • Gim, Tzang-Jo;Lee, Boong-Joo;Shina, Paik-Kyun
    • Journal of the Korean Vacuum Society
    • /
    • v.19 no.5
    • /
    • pp.341-346
    • /
    • 2010
  • In this paper, anti-reflection coating was investigated for decreasing the reflection in visible range of 400~650 [nm] through four staked layers of $Si_xO_y$ and $Si_xN_y$ thin films prepared by reactive sputtering method. Si single crystal of 6 [inch] diameter was used as a sputtering target. Ar and $O_2$ gases were used as sputtering gases for reactive sputtering for the $Si_xO_y$ thin film, and Ar and $N_2$ gases were used for reactive sputtering for the $Si_xN_y$ thin film. DC pulse power of 1900 [W] was used for the reactive sputtering. Refractive index and deposition rate were 1.50 and 2.3 [nm/sec] for the $Si_xO_y$, and 1.94 and 1.8 [nm/sec] for the $Si_xN_y$ thin film, respectively. Considering the simulation of the four layer anti-reflection coating structure with the above mentioned films, the $Si_xO_y-Si_xN_y$ stacked four-layer structure was prepared. The reflection measurement result for that structure showed that a "W" shaped anti-reflection was obtained successfully with a reflection of 1.7 [%] at 550 [nm] region and a reflection of 1 [%] at 400~650 [nm] range.

Surface Characteristics of Titanium/Hydroxyapatite Double Layered Coating on Orthopedic PEEK by Magnetron Sputtering System (마그네트론 스퍼터링 시스템을 이용한 정형외과용 PEEK의 타이타늄/하이드록시아파타이트 이중 코팅층의 표면 특성 분석)

  • Kang, Kwan-Su;Jung, Tae-Gon;Yang, Jae-Woong;Woo, Su-Heon;Park, Tea-Hyun;Jeong, Yong-Hoon
    • Journal of the Korean institute of surface engineering
    • /
    • v.51 no.3
    • /
    • pp.164-171
    • /
    • 2018
  • In this study, we have fabricated pure titanium (Ti)/hydroxyapatite (HA) double layer coating on medical grade PEEK from magnetron sputtering system, an investigation was performed whether the surface can be had more improve bio-active for orthopedi/dental applications than that of non-coated one. Pure Ti and HA coating layer were obtained by a radio-frequency and direct current power magnetron sputtering system. The microstructures surface, mechanical properties and wettability of the pure Ti/HA double layer deposited on the PEEK were analyzed by scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS), X-ray diffraction (XRD), nano-indentation, and contact angle test. According to the EDS and XRD results, the composition and crystal structure of pure Ti and HA coated surface were verified. The elastic modulus and hardness value were increased by pure Ti and HA coating, and the pure Ti/HA double layer coating surface has the highest value. The contact angle showed higher value for pure Ti/HA double layered coating specimens than that of non-coated (PEEK) surface.

A Comparative Study of HfN Coatings Deposited by DC and Pulsed DC Asymmetric Bipolar Magnetron Sputtering (DC 스퍼터법과 비대칭 바이폴라 펄스 DC 스퍼터법으로 증착된 HfN 코팅막의 물성 비교연구)

  • Jeon, Seong-Yong;Jeong, Pyeong-Geun
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.103.2-103.2
    • /
    • 2017
  • Nanocrystalline HfN coatings were prepared by reactively sputtering Hf metal target with N2 gas using a magnetron sputtering system operated in DC and ABPP (asymmetric bipolar pulsed plasma) condition with various duties and frequencies. The effects of duty and frequency, ranging from 75 to 100 % and 5 to 50 kHz, on the coating microstructure, crystallographic and mechanical properties were systematically investigated with FE-SEM, AFM, XRD and nanoindentation. The results show that pulsed plasma has a significant influence on coating microstructure and mechanical properties of HfN coatings. Coating microstructure evolves from the columnar structure to a highly dense one as duty decreases. Average grain size and nano hardness of HfN coatings were also investigated with various pulsed conditions.

  • PDF

A Comparative Study of Nanocrystalline HfN Coatings Fabricated by Direct Current and Inductively Coupled Plasma Assisted Magnetron Sputtering (DC 스퍼터법과 유도결합형 플라즈마 스퍼터법으로 증착된 HfN 코팅막의 물성 비교연구)

  • Jeon, Seong-Yong;Lee, So-Yeon
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.103.1-103.1
    • /
    • 2017
  • Nanocrystalline HfN coatings were prepared by reactively sputtering Hf metal target with N2 gas using a magnetron sputtering system operated in DC and ICP (inductively coupled plasma) condition with various powers. The effects of ICP power, ranging from 0 to 200 W, on the coating microstructure, corrosion and mechanical properties were systematically investigated with FE-SEM, AFM, potentiostat and nanoindentation. The results show that ICP power has a significant influence on coating microstructure and mechanical properties of HfN coatings. With the increasing of ICP power, coating microstructure evolves from the columnar structure of DC process to a highly dense one. Average grain size and nano hardness of HfN coatings were also investigated with increasing ICP powers.

  • PDF

Tendency of PVD coating technology on Metal cutting tools (금속 절삭공구에 대한 PVD 코팅기술의 동향)

  • Kim, Jong-Seong
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.18 no.8
    • /
    • pp.11-17
    • /
    • 2001
  • Industrial use of physical vapor deposition(PVD) has been widely expanded during last two decades, and in the mean time plasma assistance in PVD has become an essential tool in preparing compound films with dense microstructure. The principles of electron beam-based plating, balanced and unbalanced magnetron sputtering and cathodic arc deposition. consisting three basic configuration of plasma assisted PVD(PAPVD)process, were reviewed. Recent technical development in PVD coating process were discussed. This paper tries to show tendency for developing new coating film on cutting tools.

  • PDF

Sintering of Nd-Fe-B Magnets from Dy Coated Powder

  • Kim, Jin Woo;Kim, Young Do
    • Journal of Powder Materials
    • /
    • v.20 no.3
    • /
    • pp.169-173
    • /
    • 2013
  • High-coercive (Nd,Dy)-Fe-B magnets were fabricated via dysprosium coating on Nd-Fe-B powder. The sputtering coating process of Nd-Fe-B powder yielded samples with densities greater than 98%. $(Nd,Dy)_2Fe_{14}B$ phases may have effectively penetrated into the boundaries between neighboring $Nd_2Fe_{14}B$ grains during the sputtering coating process, thereby forming a $(Nd,Dy)_2Fe_{14}B$ phase at the grain boundary. The maximum thickness of the Dy shell was approximately 70 nm. The maximum coercivity of the Dy sputter coated samples(sintered samples) increased from 1162.42 to 2020.70 kA/m. The microstructures of the $(Nd,Dy)_2Fe_{14}B$ phases were effectively controlled, resulting in improved magnetic properties. The increase in coercivity of the Nd-Fe-B sintered magnet is discussed from a microstructural point of view.