• 제목/요약/키워드: Charpy absorbed energy

검색결과 47건 처리시간 0.028초

고장력강 용접부에 있어서 한계 COD값과 V charpy충격치와의 상관성에 관한 연구 (A study on the correlation between V charpy absorbed energy and critical COD value in the welded parts of high tensil strength steel under various welding methods)

  • 김영식;김충해
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제12권3호
    • /
    • pp.57-67
    • /
    • 1988
  • Although handicapped by the inability to bridge the size gap between small laboratory sample and large engineering component, the V charpy test sample method does possess certain advantages, such as each of preparation, simplicity of test method, speed, low cost in test machinery, and low cost per test. On the other hand, the COD test method does posses advantages, which reduce the size gap between the laboratory sample and actual engineering component. Consequently, the correlation between V charpy absorbed energy and the critical COD value is required for estimating critical COD value from the simple V charpy test results. In this paper, the high tensile strength steel AH36 plate specimens having a single edge cracked notch were investigated to find out the correlation between V charpy absorbed energy and critical COD value in the welded parts under such various welding methods as shielded metal arc welding, the submerged arc welding and the electro gas welding by means of V charpy impact test and static 3-point bending test. Main results obtained are as follow ; 1. The relationships between V charpy absorbed energy Wc' and critical COD value ($\delta_c$)show; $\delta_c$=0.0065 Wc'+0.1906. 2. Ductile- brittle transition behaviours can be estimated by means of fracture appearance and general yielding behaviours. 3. The V charpy absorbed energy of SMAW is higher than that of SAW, EGW and similar relationships are obtained in the COD tests.

  • PDF

베이나이트계 고강도강의 합금원소와 냉각조건이 미세조직, 인장성질, 충격성질에 미치는 영향 (Effects of Alloying Elements and the Cooling Condition on the Microstructure, Tensile Properties, and Charpy Impact Properties of High-Strength Bainitic Steels)

  • 성효경;신상용;황병철;이창길;김낙준;이성학
    • 대한금속재료학회지
    • /
    • 제48권9호
    • /
    • pp.798-806
    • /
    • 2010
  • The effects of alloying elements and the cooling condition on the microstructure, tensile properties, and Charpy impact properties of high-strength bainitic steel plates fabricated by a controlled rolling process were investigated in the present study. Eight kinds of steel plates were fabricated by varying C, Cr, and Nb additions under two different cooling rates, and their microstructures and tensile and Charpy impact properties were evaluated. The microstructures present in the steels increased in the order of granular bainite, acicular ferrite, bainitic ferrite, and martensite as the carbon equivalent or cooling rate increased, which resulted in a decrease in the ductility and Charpy absorbed energy. The steels containing a considerable amount of bainitic ferrite or martensite showed very high strengths, together with good ductility and Charpy absorbed energy. In order to achieve the best combination of strength, ductility, and Charpy absorbed energy, granular bainite and acicular ferrite were properly included in the high-strength bainitic steels by controlling the carbon equivalent and cooling rate, while about 50 vol.% of bainitic ferrite or martensite was maintained to maintain the high strength.

복합산화물이 형성된 API X80 라인파이프강의 용접열영향부 미세조직과 기계적 특성의 상관관계 연구 (Correlation Study of Microstructure and Mechanical Properties in Heat Affected Zones of API X80 Pipeline Steels containing Complex Oxides)

  • 신상용;오경식;이성학
    • 대한금속재료학회지
    • /
    • 제47권2호
    • /
    • pp.59-70
    • /
    • 2009
  • This study is concerned with the correlation between microstructure and mechanical properties in heat affected zones (HAZs) of API X80 pipeline steels containing complex oxides. Three kinds of specimens were fabricated by varying alloying elements of Ti, Al, and Mg to form complex oxides, and their microstructures, Vickers hardness, Charpy impact properties were investigated. The number of complex oxides increased as the excess amount of Ti, Al, and Mg was included in the steels. The simulated HAZs containing a number of oxides showed a high volume fraction of acicular ferrite region because oxides acted as nucleation sites for acicular ferrite. According to the correlation study between thermal input, volume fraction of acicular ferrite region, and Charpy impact properties, the ductile fracture occurred predominantly when the volume fraction of acicular ferrite region was 65% or higher, and the Charpy absorbed energy was excellent over 200 J. When the volume fraction of acicular ferrite region was 35% or lower, the Charpy absorbed energy was poor below 50 J as the brittle cleavage fracture occurred. These findings suggested that the active nucleation of acicular ferrite in the oxide-containing steel HAZs was associated with the great improvement of Charpy impact properties of the HAZs.

압력용기강재 SA508 class 3 용착금속의 조사거동 (Irradiation Behavior of Reactor Pressure Vessel SA508 class 3 Steel Weld Metals)

  • 고진현;박형근;김수성;황용화;서윤석
    • Journal of Welding and Joining
    • /
    • 제28권5호
    • /
    • pp.69-74
    • /
    • 2010
  • Irradiation behavior of the reactor pressure vessel SA508 class 3 steel weld metals was examined by Charpy V Notch impact specimens. The specimens were exposed to a fluence of $2.8{\times}1019$ neutrons(n)/$cm^2$(E>1 MeV) at $288^{\circ}C$. The irradiation damage of weld metal was evaluated by comparison between unirradiated and irradiated specimens in terms of absorbed energy and lateral expansion. The specimens for neutron irradiation were welded by submerged arc welding process at a heat input of 3.2 kJ/mm which showed good toughness in terms of weld microstructure, absorbed energy and lateral expansion. The post-irradiation Charpy V notch 41J and 68J transition temperature elevation were $65^{\circ}C$ and $70^{\circ}C$, respectively. This elevation was accompanied by a 20% reduction in Charpy V notch upper shelf energy level. The lateral expansion at 0.9mm irradiated Charpy specimens showed temperature elevation of $65^{\circ}C$ and was greatly decreased due to radiation damage.

HSLA 강의 미세조직과 저온 샤르피 충격 특성에 미치는 탄소와 니켈의 영향 (Effect of Carbon and Nickel on Microstructure and Low Temperature Charpy Impact Properties of HSLA Steels)

  • 엄해원;조성규;조영욱;신건철;권용재;이정구;신상용
    • 한국재료학회지
    • /
    • 제30권4호
    • /
    • pp.184-196
    • /
    • 2020
  • In this study, effects of carbon and nickel on microstructure and low temperature Charpy impact properties of HSLA (high strength low alloy) steels are investigated. To understand the complex phase transformation behavior of HSLA steels with high strength and toughness before and after welding processes, three kinds of HSLA steels are fabricated by varying the carbon and nickel content. Microstructure analysis, low temperature Charpy impact test, and Vickers hardness test are performed for the base metals and CGHAZ (coarse-grain heat affected zone) specimens. The specimens with the lowest carbon and nickel content have the highest volume fraction of AF, the lowest volume fraction of GB, and the smallest GB packet size. So, the low temperature Charpy absorbed energy of the CGHAZ specimen is the highest. The specimens with increased carbon and nickel content have the lowest volume fraction of AF, the highest volume fraction of GB, and the largest GB packet size. So, the low temperature Charpy absorbed energy of the CGHAZ specimen is the lowest.

해양 구조물용 강재 FCAW 용접부의 파괴인성 특성에 관한 연구 (A Study on the Fracture Toughness Characteristics of FCAW Weldment of Steel for Offshore Structures)

  • 강성원;김명현;김용빈;신용택;이해우
    • Journal of Welding and Joining
    • /
    • 제22권6호
    • /
    • pp.57-63
    • /
    • 2004
  • Fracture toughness is an important parameter in designing offshore structures to ensure resistance to fracture at various temperatures. In this study, a series of experiments is carried out to obtain fracture toughness values (CTOD) of API 2W Gr.50B, welded using FCAW(Flux Cored Arc Weld). In particular, a comparison of absorbed impact energy and CTOD values are made with respect to two different welding groove shapes; double-V-groove and double-bevel-groove. Charpy impact tests are performed for specimens sampled near the root gap, and CTOD tests are carried out for three point bending specimens having the notch at weld zone. While Charpy impact test result is determined to be a good qualitative measure of fracture toughness, no quantitative correspondence between impact absorbed energy and CTOD values was found. Based on the experiment, it is observed that double-V-groove welds give lower transition temperature than those of double-bevel-groove.

FRACTURE TOUGHNESS CHARACTERISTICS IN HIGH ENERGY DENSITY BEAM WELDED JOINT OF HIGH TENSILE STEELS

  • Ro, Chan-Seung;Yamada, Tomoaki;Mochizuki, Masahito;Ishikawa, Nobuyuki;Bang, Han-Sur;Toyoda, Masao
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.583-588
    • /
    • 2002
  • The purpose of the study is to evaluate fracture toughness on the Laser and the electron beam welded joints of high tensile steels (HT500, HT550, HT650) by using 3-point bend CTOD and Charpy impact test. WM (weld metal) CTOD tests have been carried out using two kinds of CTOD specimen, the Laser beam welding (108mm length, and 24mm width, and 12mm thickness) and the electron beam welding (l71mm length, and 38mm width, and 19mm thickness). WM Charpy impact specimen is a standard V-notch type, and the temperature of the experiment is changed from -45 to 20 degree of centigrade. FE-analysis is also performed in order to investigate the effect of stress-strain fields on fracture characteristics. Results of the standard V-notch Charpy test are influenced by strength mis-match effect and the absorbed energy vE depends on crack path, and The transition temperature of Laser beam welded joints is more higher than that of electron beam welded joints. Results of the 3-point bend test give low critical CTOD and the crack path is in the weld metal of al specimens. These results indicate fracture toughness characteristics of the welded joints and transition temperature of HT500 are similar both a Laser beam welded joint and an electron beam welded joint. But the fracture toughness and the transition temperature of the electron beam welded joints of HT550 and HT650 are higher than those o the Laser beam welded joints.

  • PDF

극저온용 오스테나이트계 고망간강의 인장 및 충격 특성에 미치는 C, Mn, Al 첨가의 영향 (Effect of C, Mn and Al Additions on Tensile and Charpy Impact Properties of Austenitic High-manganese Steels for Cryogenic Applications)

  • 이승완;황병철
    • 한국재료학회지
    • /
    • 제29권3호
    • /
    • pp.189-195
    • /
    • 2019
  • The effect of C, Mn, and Al additions on the tensile and Charpy impact properties of austenitic high-manganese steels for cryogenic applications is investigated in terms of the deformation mechanism dependent on stacking fault energy and austenite stability. The addition of the alloying elements usually increases the stacking fault energy, which is calculated using a modified thermodynamic model. Although the yield strength of austenitic high-manganese steels is increased by the addition of the alloying elements, the tensile strength is significantly affected by the deformation mechanism associated with stacking fault energy because of grain size refinement caused by deformation twinning and mobile dislocations generated during deformation-induced martensite transformation. None of the austenitic high-manganese steels exhibit clear ductile-brittle transition behavior, but their absorbed energy gradually decreases with lowering test temperature, regardless of the alloying elements. However, the combined addition of Mn and Al to the austenitic high-manganese steels suppresses the decrease in absorbed energy with a decreasing temperature by enhancing austenite stability.

해양플랜트용 500 MPa급 후판강의 모재 및 HAZ의 미세조직과 기계적 특성의 상관관계 (Correlation between Microstructure and Mechanical Properties of Base Metal and HAZ of 500 MPa Steel Plates for Offshore Platforms)

  • 박지원;조성규;조영욱;신건철;권용재;이정구;신상용
    • 한국재료학회지
    • /
    • 제30권3호
    • /
    • pp.123-130
    • /
    • 2020
  • In this study, two types of thick steel plates are prepared by controlling carbon equivalent and nickel content, and their microstructures are analyzed. Tensile tests, Vickers hardness tests, and Charpy impact tests are conducted to investigate the correlation between microstructure and mechanical properties of the steels. The H steel, which has high carbon equivalent and nickel content, has lower volume fraction of granular bainite (GB) and smaller GB packet size than those of L steel, which has low carbon equivalent and nickel content. However, the volume fraction of secondary phases is higher in the H steel than in the L steel. As a result, the strength of the L steel is higher than that of the H steel, while the Charpy absorbed energy at -40 ℃ is higher than that of the L steel. The heat affected zone (HAZ) simulated H-H specimen has higher volume fraction of acicular ferrite (AF) and lower volume fraction of GB than the HAZ simulated L-H specimen. In addition, the grain size of AF and the packet sizes of GB and BF are smaller in the H-H specimen than in the L-H specimen. For this reason, the Charpy absorbed energy at -20 ℃ is higher for the H-H specimen than for the L-H specimen.

유한요소법을 이용한 용접열영향부의 균열진전 및 샤르피 흡수에너지 연구 (Study of Crack Propagation and Absorbed Energy in Heat Affected Zone Using a Finite Element Method)

  • 장윤찬;이영석
    • 한국전산구조공학회논문집
    • /
    • 제22권6호
    • /
    • pp.541-548
    • /
    • 2009
  • 본 논문은 샤르피 충격실험과 유한요소법를 이용하여 노치위치에 따른 파괴거동과 흡수에너지의 영향을 평가하였다. 본 연구자는 쉴드메탈아크 용접방법으로 두께가 25mm인 압력용기용강(SA-516 Gr. 70)을 용접하였고, 이 용접된 평판으로 샤르피 시편을 제작하였다. 샤르피 충격실험에서는 용접열영향부(HAZ)에서 노치위치가 다른 시편이 사용되었다. 그리고 본 연구자는 유한요소법을 이용하여 샤르피 충격실험에서의 균열진전을 모사하였다. 용접열영향부(HAZ)의 기계적 물성을 유한요소해석에 적용하기 위해 HAZ를 2개 영역, 3개 영역 그리고 4개 영역으로 나누었다. 본 연구결과에서는 샤르피 충격실험의 흡수에너지가 노치위치에 의존적이라는 것을 보여주었다. 또한 샤르피 용접시편에서 신뢰성 있는 유한요소해석 결과를 얻기 위해서는 용접열영향부를 적어도 3개 이상의 영역으로 나누어야 한다는 결과를 얻었다.