• Title/Summary/Keyword: Chalcopyrite structure

Search Result 70, Processing Time 0.034 seconds

Au-Ag Minerals and Geneses of Weolyu Gold-Silver Deposits, Chungcheongbukdo, Republic of Korea (월유광산산(月留鑛山産) 금(金)-은(銀)광물(鑛物)과 광상(鑛床)의 생성환경(生成環境))

  • Lee, Hyun Koo;Yoo, Bong-Cheal;Jeong, Kwang Young;Kim, Kee Hyun
    • Economic and Environmental Geology
    • /
    • v.27 no.6
    • /
    • pp.537-548
    • /
    • 1994
  • The Weolyu gold-silver deposits at Hwanggan, Chungcheongbukdo, is of a late Cretaceous $(74.24{\pm}1.63Ma)$ epithermal vein-type, and is hosted in the quartz porphyry of late Cretaceous age. Based on mineral paragenetic sequence interpreted from vein structure and mineral assemblages, three stages mineralization were distinguished. A variety of ore minerals occurs including pyrite, sphalerite, chalcopyrite, galena with small amount of electrum, native silver, argentite, pearceite, sb-pearceite, argyrotite. The gangue minerals are quartz, rutile, calcite, apatite, fluorite and rhodochrocite. Wall-rock alteration such as pyritization, chloritization, sericitization, silicification is observed near the quartz veins. Au-Ag minerals were crystallized at middle and late stage of the two mineralization sequences. Results from the analysis of fluid inclusion and thermodynamic calculation indicate that Au-Ag mineral deposits were formed primarily by cooling and dilution of hydrothermal fluids($165{\sim}313^{\circ}C$, 0.4~2.4wt.% equivalent NaCl) with some degree mixing of meteoric water.

  • PDF

Temperature dependence of photocurrent spectra for $AgInS_2$ epilayers grown by hot wall epitaxy

  • Baek, Seung-Nam;Hong, Kwang-Joon
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.06a
    • /
    • pp.123-124
    • /
    • 2007
  • A silver indium sulfide ($AgInS_2$) epilayer was grown by the hot wall epitaxy method, which has not been reported in the liteniture. The grown $AgInS_2$ epilayer has found to be a chalcopyrite structure and evaluated to be high quality crystal. From the photocurrent measurement in the temperature range from 30 K to 300 K, the two peaks of A and B were only observed, whereas the three peaks of A, B, and C were seen in the PC spectrum of 10 K. These peaks are ascribed to the band-to-band transition. The valence band splitting of $AgInS_2$ was investigated by means of the photocurrent measurement. The temperature dependence of the energy band gap of the $AgInS_2$ obtained from the photocurrent spectrum was well described by the Varshni's relation, $E_g(T)=\;E_g(0)\;eV-(7.78\;{\times}\;10^{-4}\;eV/K)T^2/(T\;+\;116\;K\;K)$. Also, Eg(0) is the energy band gap at 0 K, which is estimated to be 2.036 eV at the valence band state A and 2.186 eV at the valence band state B.

  • PDF

Opto-electric properties for the $AgInS_2$ epilayers grown by hot wall epitaxy (Hot wall epitaxy법에 의해 성장된 $AgInS_2$ 박막의 광전기적 특성)

  • Lee, K.G.;Hong, K.J.
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07a
    • /
    • pp.267-270
    • /
    • 2004
  • A silver indium sulfide($AgInS_2$) epilayer was grown by the hot wall epitaxy method, which has not been reported in the literature. The grown $AgInS_2$ epilayer has found to be a chalcopyrite structure and evaluated to be high qualify crystal. From the photocurrent measurement in the temperature range from 30 K to 300 K, the two peaks of A and B were only observed, whereas the three peaks of A, B, and C were seen in the PC spectrum of 10 K. These peaks. are ascribed to the band-to-band transition. The valence band splitting of $AgInS_2$ was investigated by means of the photocurrent measurement. The crystal field splitting, $\ddot{A}cr$, and the spin orbit splitting, $\ddot{A}so$, have been obtained to be 0.150 eV and 0.009 eV at 10 K, respectively. And, the energy band gap at room temperature has been determined to be 1.868 eV. Also, the temperature dependence of the energy band gap, $E_g(T)$, was determined.

  • PDF

Influence of the Composition of Shell Layers on the Photoluminescence of Cu0.2InS2 Semiconductor Nanocrystals with a Core-shell Structure

  • Kim, Young-Kuk;Ahn, Si-Hyun;Cho, Young-Sang;Chung, Kookchae;Choi, Chul-Jin;Shin, Pyung-Woo
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.11
    • /
    • pp.900-904
    • /
    • 2011
  • We have synthesized core-shell structured nanocrystals based on chalcopyrite-type $Cu_{0.2}InS_2$. The photoluminescence of the nanocrystals shows a significant blueshift in the emission wavelength by shell capping with ZnS layers. This shift can be explained with the compressive stress to core nanocrystals applied by the formation of a ZnS shell layer with a large lattice mismatch with the core. In this study, the emission wavelength could be tuned by changing the composition of the shell layers. Nanocrystals with emission wavelength ranging from 575 nm through 630 nm were synthesized by varying the portion of cadmium compared with zinc in the shell layers.

Occurrence and Mineral Characteristics of Au-Ag-Cu-Bi Bearing Quartz Veins in the Estancia de la Virgen area, Guatemala (과테말라 Estancia de la Virgen 지역 금-은-동-비스무스 광화대의 산상과 광물특성)

  • Shin, Eui-Cheol;Kim, Soo-Young;Hong, Sei-Sun;Kim, In-Joon
    • Economic and Environmental Geology
    • /
    • v.31 no.6
    • /
    • pp.463-472
    • /
    • 1998
  • The survey was carried out in order to delineate the occurrence of ore deposits and the mineralized characteristics in the Estancia de la Virgen area through the 1:2,000 scaled geological mapping and topographic measuring surveys. Gold-silver mineralization is in the fault block developed between the San Agustin Fault and Cabanas Fault. It is associated with ore bearing quartz veins controlled by the fault structure. The contents of Au and Ag range from traces up to 72 g/t and 180 g/t respectively. According to traversing the outcrops, the quartz veins are traced by 0.5 Km trended to north and south. In those extended part, they continue for 1,000 m intermittently. Gold-silver mineralization could be divided into three stages. In the first stage, pyrite, galena, sphalerite, and chalcopyrite were formed with the primary silver and gold associated with galena and copper sulfides respectively. In the second stage, Cu-Bi-Au-Ag bearing sulfides such as chalcocite, covellite, and linarite are formed and usually deposited on the cataclastic fractures of galena and/or chalcopyrite. In the third stage, both the carbonation of galena and sphalerite and the sulphatization of galena, took place in the surface environment. And then primary silver was carried away off and was deposited on galena and/or copper sulfides during oxidation near the water table. Low partitionings of Fe in sphalerite assist that the minerals were formed at the relatively low temperature, which is coincided with previously reported homogenization temperature of fluid inclusions.

  • PDF

Synthesis and Characterization of Cu(In,Ga)Se2 Nanostructures by Top-down and Bottom-up Approach

  • Lee, Ji-Yeong;Seong, Won-Kyung;Moon, Myoung-Woon;Lee, Kwang-Ryeol;Yang, Cheol-Woong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.08a
    • /
    • pp.440-440
    • /
    • 2012
  • Nanomaterials have emerged as new building blocks to construct light energy harvesting assemblies. Size dependent properties provide the basis for developing new and effective systems with semiconductor nanoparticles, quantized charging effects in metal nanoparticle or their combinations in 2 and 3 dimensions for expanding the possibility of developing new strategies for photovoltaic system. As top-down approach, we developed a simple and effective method for the large scale formation of self-assembled Cu(In,Ga)$Se_2$ (CIGS) nanostructures by ion beam irradiation. The compositional changes and morphological evolution were observed as a function of the irradiation time. As the ion irradiation time increased, the nano-dots were transformed into a nano-ridge structure due to the difference in the sputtering yields and diffusion rates of each element and the competition between sputtering and diffusion processes during irradiation. As bottom-up approach, we developed the growth of CIGS nanowires using thermal-chemical vapor deposition (CVD) method. Vapor-phase synthesis is probably the most extensively explored approach to the formation of 1D nanostructures such as whiskers, nanorods, and nanowires. However, unlike binary or ternary chalcogenides, the synthesis of quaternary CIGS nanostructures is challenging because of the difficulty in controlling the stoichiometry and phase structure. We introduced a method for synthesis of the single crystalline CIGS nanowires in the form of chalcopyrite using thermal-CVD without catalyst. It was confirmed that the CIGS nanowires are epitaxially grown on a sapphire substrate, having a length ranged from 3 to 100 micrometers and a diameter from 30 to 500 nm.

  • PDF

Structural and optical properties of $CuInS_2$ thin films fabricated by electron-beam evaporation (전자빔 증착으로 제조한 $CuInS_2$ 박막의 구조적 및 광학적 특성)

  • Park, Gye-Choon;Jeong, Woon-Jo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.193-196
    • /
    • 2001
  • Single phase $CuInS_2$ thin film with the highest diffraction peak (112) at diffraction angle $(2\theta)$ of $27.7^{\circ}$ and the second highest diffraction peak (220) at diffraction angle $(2\theta)$ of $46.25^{\circ}$ was well made with chalcopyrite structure at substrate temperature of $70^{\circ}C$, annealing temperature of $250^{\circ}C$, annealing time of 60 min. The $CuInS_2$ thin film had the greatest grain size of $1.2{\mu}m$ and Cu/In composition ratio of 1.03. Lattice constant of a and c of that $CuInS_2$ thin film was 5.60 A and 11.12 A respectively. Single phase $CuInS_2$ thin films were accepted from Cu/In composition ratio of 0.84 to 1.3. P-type $CuInS_2$ thin films were appeared at over Cu/In composition ratio of 0.99. Under Cu/In composition ratio of 0.96, conduction types of $CuInS_2$ thin films were n-type. Also, fundamental absorption wavelength, the absorption coefficient and optical energy band gap of p-type $CuInS_2$ thin film with Cu/In composition ratio of 1.3 was 837 nm, $3.0{\times}104cm^{-1}$ and 1.48 eV respectively. When Cu/In composition ratio was 0.84, fundamental absorption wavelength, the absorption coefficient and optical energy band gap of n-type $CuInS_2$ thin film was 821 nm, $6.0{\times}10^4cm^{-1}$ and 1.51 eV respectively.

  • PDF

Aerosol Jet Deposition of $CuInS_2$ Thin Films

  • Fan, Rong;Kong, Seon-Mi;Kim, Dong-Chan;Chung, Chee-Won
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.02a
    • /
    • pp.159-159
    • /
    • 2011
  • Among the semiconductor ternary compounds in the I-III-$VI_2$ series, $CulnS_2$ ($CulnSe_2$) are one of the promising materials for photovoltaic applications because of the suitability of their electrical and optical properties. The $CuInS_2$ thin film is one of I-III-$VI_2$ type semiconductors, which crystallizes in the chalcopyrite structure. Its direct band gap of 1.5 eV, high absorption coefficient and environmental viewpoint that $CuInS_2$ does not contain any toxic constituents make it suitable for terrestrial photovoltaic applications. A variety of techniques have been applied to deposit $CuInS_2$ thin films, such as single/double source evaporation, coevaporation, rf sputtering, chemical vapor deposition and chemical spray pyrolysis. This is the first report that $CuInS_2$ thin films have been prepared by Aerosol Jet Deposition (AJD) technique which is a novel and attractive method because thin films with high deposition rate can be grown at very low cost. In this study, $CuInS_2$ thin films have been prepared by Aerosol Jet Deposition (AJD) method which employs a nozzle expansion. The mixed fluid is expanded through the nozzle into the chamber evacuated in a lower pressure to deposit $CuInS_2$ films on Mo coated glass substrate. In this AJD system, the characteristics of $CuInS_2$ films are dependent on various deposition parameters, such as compositional ratio of precursor solution, flow rate of carrier gas, stagnation pressure, substrate temperature, nozzle shape, nozzle size and chamber pressure, etc. In this report, $CuInS_2$ thin films are deposited using the deposition parameters such as the compositional ratio of the precursor solution and the substrate temperature. The deposited $CuInS_2$ thin films will be analyzed in terms of deposition rate, crystal structure, and optical properties.

  • PDF

Stable Isotope and Fluid Inclusion Studies of the Daebong Gold-silver Deposit, Republic of Korea (대봉 금-은광상에 대한 유체포유물 및 안정동위원소 연구)

  • 유봉철;이현구;김상중
    • Economic and Environmental Geology
    • /
    • v.36 no.6
    • /
    • pp.391-405
    • /
    • 2003
  • The Daebong gold-silver deposit consists of mesothermal massive quartz veins thar are filling the fractures along fault shear (NE, NW) Bones within banded or granitic gneiss of Precambrian Gyeonggi massif. Based on vein mineralogy, ore textures and paragenesis, ore mineralization of this deposits is composed of massive white quartz vein(stage I) which was formed in the same stage by multiple episodes of fracturing and healing, and transparent quartz vein(stage II) which is separated by a major faulting event. Stage I is divided into the 3 substages. Ore minerals of each substages are as follows: 1) early stage I=magnetite, pyrrhotite, arsenopyrite, pyrite, sphalerite, chalcopyrite, 2) middle stage I=pyrrhotite, arsenopyrite, pyrite, marcasite, sphalerite, chalcopyrite, galena, electrum and 3) late stage I=pyrite, sphalerite, chalcopyrite, galena, electrum, argentite, respectively. Ore minerals of the stage II are composed of pyrite, sphalerite, chalcopyrite, galena and electrum. Systematic studies (petrography and microthermometry) of fluid inclusions in stage I and II quartz veins show fluids from contrasting physical-chemical conditions: 1) $H_2O-CO_2-CH_4-NaCl{\pm}N-2$ fluid(early stage I=homogenization temperature: 203∼3$88^{\circ}C$, pressure: 1082∼2092 bar, salinity: 0.6∼13.4 wt.%, middle stage I=homogenization temperature: 215∼28$0^{\circ}C$, salinity: 0.2∼2.8 wt.%) related to the stage I sulfide deposition, 2) $H_2O-NaCl{\pm}CO_2$ fluid (late stage I=homogenization temperature: 205∼2$88^{\circ}C$, pressure: 670 bar, salinity: 4.5∼6.7 wt.%, stage II=homogenization temperature: 201-3$58^{\circ}C$, salinity: 0.4-4.2 wt.%) related to the late stage I and II sulfide deposition. $H_2O-CO_2-CH_4-NaCl{\pm}N_2$ fluid of early stage I is evolved to $H_2O-NaCl{\pm}CO_2$ fluid represented by the $CO_2$ unmixing due to decrease in fluid pressure and is diluted and cooled by the mixing of deep circulated meteoric waters ($H_2O$-NaCl fluid) possibly related to uplift and unloading of the mineralizing suites. $H_2O-NaCl{\pm}CO_2$ fluid of stage II was hotter than that of late stage I and occurred partly unmixing, mainly dilution and cooling for sulfide deposition. Calculated sulfur isotope compositions ({\gamma}^{34}S_{H2S}$) of hydrothermal fluids (3.5∼7.9%o) indicate that ore sulfur was derived from mainly an igneous source and partly sulfur of host rock. Measured and calculated oxygen and hydrogen isotope compositions ({\gamma}^{18}O_{H_2O}$, {\gamma}$D) of ore fluids (stage I: 1.1∼9.0$\textperthousand$, -92∼-86{\textperthansand}$, stage II: 0.3{\textperthansand}$, -93{\textperthansand}$) and ribbon-banded structure (graphitic lamination) indicate that mesothermal auriferous fluids of Daebong deposit were two different origin and their evolution. 1) Fluids of this deposit were likely mixtures of $H_2O$-rich, isotopically less evolved meteoric water and magmatic fluids and 2) were likely mixtures of $H_2O$-rich. isotopically heavier $\delta$D meteoric water and magmaticmetamorphic fluids.

SEL 법으로 제조된 $CuInS_2$ 화합물 반도체 박막의 전기적 특성

  • Park, Gye-Choon;Jeong, Woon-Jo;Kim, Jong-Uk
    • Proceedings of the KIEE Conference
    • /
    • 2004.07c
    • /
    • pp.1605-1608
    • /
    • 2004
  • Single phase $CuInS_2$ thin film with a highest diffraction peak (112) at a diffraction angle ($2{\theta}$) of 27.7$^{\circ}$ was well made by SEL method at annealing temperature of 250 $^{\circ}C$ and annealing hour of 60 min in vacuum of $10^{-3}$ Torr or in S ambience for an hour. And the peak of diffraction intensity at miller index (112) of $CuInS_2$ thin film annealed in S ambience was shown a little higher about 11 % than in only vacuum. Single phase $CuInS_2$ thin films were appeared from 0.85 to 1.26 of Cu/In composition ratio and sulfur composition ratios of $CuInS_2$ thin films fabricated in S ambience were all over 50 atom%. Also when Cu/In composition ratio was 1.03, $CuInS_2$ thin film with chalcopyrite structure had the highest XRD peak (112). And lattice constant a and grain size of the thin film in S ambience were appeared a little larger than those in only vacuum. The largest lattice constant of a and grain size of $CuInS_2$ thin film in S ambience was 5.63 ${\AA}$ and 1.2 ${\mu}$m respectively. And the films in S ambience were all p-conduction type with resistivities of around $10^{-1}{\Omega}cm$.

  • PDF