• Title/Summary/Keyword: Ceramic Substrate

Search Result 950, Processing Time 0.025 seconds

Soldering characteristics of Ag-Pd electrodes in relationship to differing particle size of LTCC substrate (LTCC 기판의 Particle Size 에 따른 Ag-Pd 전극의 Soldering 특성 변화)

  • 조현민;유명재;박종철
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2002.05a
    • /
    • pp.130-133
    • /
    • 2002
  • Solder leaching resistance of the metal electrode is an important factor with regard to adhesion properties of ceramic substrate. In the Low Temperature Co-fired Ceramics (LTCC), Ag-Pd or Ag-Pt pastes are used instead of pure Ag paste to prevent leaching. Solder leaching behavior of the Ag-Pd paste in relation to LTCC raw material powder size was investigated. First fabrication of LTCC green tape with different particle size was done. LTCC substrates with Ag-Pd electrode were prepared using conventional multilayer ceramic process. Dipping test was performed to test solder leaching behavior of the electrode. Ag-Pd electrode on LTCC substrate with smaller particle size achieved higher solder leaching resistance.

  • PDF

Effect of self-assembled monolayer and aluminum oxide ALD film on a PMMA substrate

  • Shin, Sora;Park, Jongwan
    • Journal of Ceramic Processing Research
    • /
    • v.19 no.6
    • /
    • pp.525-529
    • /
    • 2018
  • The antireflective (AR) coated poly methyl methacrylate (PMMA) substrate was deposited by atomic layer deposition (ALD) on a self-assembled monolayer (SAM) to improve hydrophobicity and mechano-chemical properties of organic thin films. The water contact angles (WCA) were tested to characterize the surface wettability of SAM octadecyltrichlorosilane (OTS) films. Results showed that a contact angle of $105.9^{\circ}$ was obtained for the SAM films with an annealing process, and the highest WCA of $120^{\circ}$ was achieved for the films prepared by the SAM and ALD multi-process. The surface morphology of the SAM films with different assembly times and varying number of ALD cycles was obtained by atomic force microscopy (AFM). The maximum light transmittance for the SAM films on the PMMA substrate reached 99.9% at a wavelength of 450 nm. It was found that the SAM surfaces were not affected at all by the ALD process.

Effect of residual oxygen in a vacuum chamber on the deposition of cubic boron nitride thin film

  • Oh, Seung-Keun;Kang, Sang Do;Kim, Youngman;Park, Soon Sub
    • Journal of Ceramic Processing Research
    • /
    • v.17 no.7
    • /
    • pp.763-767
    • /
    • 2016
  • The structural characterization of cubic boron nitride (c-BN) thin films was performed using a B4C target in a radio-frequency magnetron sputtering system. The deposition processing conditions, including the substrate bias voltage, substrate temperature, and base pressure were varied. Fourier-transform infrared spectroscopy and X-ray photoelectron spectroscopy were used to analyze the crystal structures and chemical binding energy of the films. For the BN film deposited at room temperature, c-BN was formed in the substrate bias voltage range of -400 V to -600 V. Less c-BN fraction was observed as the deposition temperature increased, and more c-BN fraction was observed as the base pressure increased.

Investigation on Lead-Borosilicate Glass Based Dielectrics for LTCC (Lead-Borosilicate Glass계 LTCC용 유전체에 대한 고찰)

  • Yoon, Sang-Ok;Oh, Chang-Yong;Kim, Kwan-Soo;Jo, Tae-Hyun;Shim, Sang-Heung;Park, Jong-Guk
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.6 s.289
    • /
    • pp.338-343
    • /
    • 2006
  • The effects of lead-borosilicate glass frits on the sintering behavior and microwave dielectric properties of ceramic-glass composites were investigated as functions of glass composition of glass addition ($10{\sim}50vol%$), softening point (Ts) of the glass, and sintering temperature of the composites ($500{\sim}900^{\circ}C$ for 2 h). The addition of 50 vol% glass ensured successful sintering below $900^{\circ}C$. Sintering characteristics of the composites were well described in terms of Ts. PbO addition in to the glass enhanced the reaction with $Al_{2}O_3$ to form liquid phase and $PbAl_{2}Si_{2}O_8$, which was responsible to lower Ts. Dielectric constant(${\epsilon}_r$), $Q{\times}f_0$ and temperature coefficient of resonant frequency (${\tau}_f$) of the composite with 50 vol% glass contents ($B_{2}O_{3}:PbO:SiO_{2}:CaO:Al_{2}O_3$ = 5:40:45:5:5) demonstrated 8.5, 6,000 GHz, $-70\;ppm/^{\circ}C$, respectively, which is applicable to substrate requiring a low dielectric constant. When the same glass composition was applied sinter $MgTiO_3\;and\;TiO_2,\;at\;900^{\circ}C$ (50 vol% glass in total), the properties were 23.8, 4,000 GHz, $-65ppm/^{\circ}C$ and 31.1, 2,500 GHz, $+80ppm/^{\circ}C$ respectively, which is applicable to filter requiring an intermidiate dielectric constant.

Effects of the Surface Roughness of a Graphite Substrate on the Interlayer Surface Roughness of Deposited SiC Layer (SiC 증착층 계면의 표면조도에 미치는 흑연 기판의 표면조도 영향)

  • Park, Ji Yeon;Jeong, Myung Hoon;Kim, Daejong;Kim, Weon-Ju
    • Journal of the Korean Ceramic Society
    • /
    • v.50 no.2
    • /
    • pp.122-126
    • /
    • 2013
  • The surface roughness of the inner and outer surfaces of a tube is an important requirement for nuclear fuel cladding. When an inner SiC clad tube, which is considered as an advanced Pressurized Water Cooled Reactor (PWR) clad with a three-layered structure, is fabricated by Chemical Vapor Deposition (CVD), the surface roughness of the substrate, graphite, is an important process parameter. The surface character of the graphite substrate could directly affect the roughness of the inner surface of SiC deposits, which is in contact with a substrate. To evaluate the effects of the surface roughness changes of a substrate, SiC deposits were fabricated using different types of graphite substrates prepared by the following four polishing paths and heat-treatment for purification: (1) polishing with #220 abrasive paper (PP) without heat treatment (HT), (2) polishing with #220 PP with HT, (3) #2400 PP without HT, (4) polishing with #2400 PP with HT. The average surface roughnesses (Ra) of each deposited SiC layer are 4.273, 6.599, 3.069, and $6.401{\mu}m$, respectively. In the low pressure SiC CVD process with a graphite substrate, the removal of graphite particles on the graphite surface during the purification and the temperature increasing process for CVD seemed to affect the surface roughness of SiC deposits. For the lower surface roughness of the as-deposited interlayer of SiC on the graphite substrate, the fine controlled processing with the completed removal of rough scratches and cleaning at each polishing and heat treating step was important.

Phase Formation of $BaTiO_3$ Thin Films by Sputtering (Sputtering법에 의한 $BaTiO_3$ 박막의 상형성에 관한 연구)

  • 안재민;최덕균;김영호
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.8
    • /
    • pp.657-663
    • /
    • 1993
  • BaTiO3 sputtering targets of 3 inch diameter were prepared by sintering the CIP (Cold Isotatic Pressing) compacts at 136$0^{\circ}C$ for 3hrs. The apparent density and grain size were 97% and 30${\mu}{\textrm}{m}$, respectively. After BaTiO3 films were deposited on Si and Pt/Ti/SiO2/Si substrates using these targets, films were annealed at various conditions and the crystallization behavior, reaction with the substrate and the electrical properties were investigated. The films on both substrates required 5~20hrs furnace annealing for crystallization at the temperatures from $600^{\circ}C$ to 80$0^{\circ}C$. For the films on Si substrate, interaction between the film and the substrate was suppressed upt o $700^{\circ}C$ for 10 hrs and the relative dielectric constant was 30. As the annelaing temperature and time were increased, the relative dielectric constants of the films decreased due to the formation of silicate phases through the reaction with the substrate. For the BaTiO3 films on Pt/Ti/SiO2/Si substrate, the reaction with the substrate was further reduced when the annealing condition was identical to that for Si substrate, but the reaction between the layers in Pt electrode took place above $700^{\circ}C$. When the films were annealed at $600^{\circ}C$ where the stability of Pt electrode was sustained, relative dielectric constant was increased to 110 since the reaction with substrate was effectively reduced even for a longer annealing time and the crystallization was enhanced.

  • PDF