Effect of the Processing Parameters on the Densification and Strength of 2D SiC Fiber-SiC Matrix Composites Fabricated by Slurry Infiltration and Stacking Process

  • Lim, Kwang-Young;Jang, Doo-Hee;Kim, Young-Wook;Park, Ji-Yeon;Park, Dong-Soo
    • 한국세라믹학회지
    • /
    • 제44권7호
    • /
    • pp.349-353
    • /
    • 2007
  • 2D SiC fiber-SiC (SiC/SiC) composites were fabricated via slurry infiltration and a stacking process. The effects of the additive composition and content in SiC slurries and the effect of the sintering time on the sintered density and strength of SiC/SiC composites were investigated. A slurry containing $Al_2O_3-Y_2O_3-MgO$ (AYM) additives led to a higher strength compared to a slurry containing $Al_2O_3-Y_2O_3-CaO$ (AYC) additives. The sintered density increased as the sintering time increased and showed a maximum (>98%) at 4 h. In contrast, the flexural strength increased as the sintering time increased and showed a maximum (615 MPa) at 6 h. The relative density and flexural strength increased as the additive content increased.

탄소/탄소 복합재 매트릭스 전구체인 이방성 메조페이스 형성을 위한 콜타르 핏치의 열분해 조건 연구 (A study on the Condition of Pyrolysis of Coal Tar Pitch to Form the Mesophase as a Matrix Precursor of Carbon/Carbon Composites)

  • 정형진;정윤중;조동환;임연수;김기원
    • 한국세라믹학회지
    • /
    • 제34권9호
    • /
    • pp.963-968
    • /
    • 1997
  • Coal tar pitch was used to study the effect of the pyrolysis conditions to produce mesophase pitch used as a matrix precursor for carbon/carbon composites. The pyrolysis conditions were presented in all cases that the total pressure was 1 atm and the first stage temperature was changed from 25$0^{\circ}C$ to 34$0^{\circ}C$ to remove the low molecular weight compounds in the pitch, and then, heated to 40$0^{\circ}C$ to form anisotropic mesophase as the second stage temperature. The first stage temperature was very affected to form resulting anisotropic mesophase pitch. The resulting mesophase pitches show a significantly increased anisotropic contents upto 30$0^{\circ}C$. However, the contents of mesophase were decreased above 30$0^{\circ}C$. It was the reason that the first stage temperature had been control the number of free radicals to react the aromatic compounds in the pitch to form high molecular weight compound. Therefore, the two stage pyrolysis method could be very effectively used to control various contents of anisotropic polyaromatic mesophase compared to continuous to continuous heating method.

  • PDF

상압소결한 Al2O3-SiC계 소결체의 기계적 성질(2) : SiC Whisker의 분산효과 (Mechanical Properties of the Pressureless Sintered Al2O3-SiC Composites(2) : Dispersion Effects of SiC Whisker)

  • 김경수;이홍림
    • 한국세라믹학회지
    • /
    • 제25권6호
    • /
    • pp.704-712
    • /
    • 1988
  • In order to investigate the effect of the second phase on Al2O3 matrix, SiC whisker was dispersed in Al2O3 matrix as a second phase over the content range of 5vol% to 20vol%. To this mixture, Y2O3 or TiO2 powder was added as a sintering additive before isostatically pressing and pressureless sintering at 1800-190$0^{\circ}C$ for 90min in N2 atmosphere. With increasing SiC whisker content, relative densities of composites were decreased and the grain growth of Al2O3 was restricted. When Y2O3 was added as a sintering aid the sintering temperature was 180$0^{\circ}C$, the maximum values of flexural strength, hardness and fracture toughness were 537MPa, 12.1GPa, 3.7MPa.m1/2, respectively. However, when the sintering temperature was elevated to 190$0^{\circ}C$, maximum values of flexural strength, hardness and fracture toughness were 453MPa, 17.5GPa, 4.9MPa.m1/2, respectively. Improved mechanical properties are assumed to be attributed to the crack deflection by the second phase SiC whisker and whisker pullout mechanism.

  • PDF

알콕사이드로부터 Mullite 분말의 합성 및 Mullite-Zirconia 복합체의 특성 (Synthesis of Mullite Powder from Alkoxides and the Properties of the Mullite-Zircocnia Composites)

  • 함종근;이홍림
    • 한국세라믹학회지
    • /
    • 제27권2호
    • /
    • pp.201-210
    • /
    • 1990
  • The mullite-15v/o ZrO2 composites were prepared by dispersing ZrO2-3m/o Y2O3 powders into the mullite matrix in order to improve the mechanical properties of the mullite. The densification and retention of t-ZrO2 in the matrix of synthetic mullite were also investigated. From IR spectroscopic analysis, the obtained amorphous SiO2-Al2O3 powder was observed to have Si-O-Al chemical bond in its structure which might result in the homogeneous mullite composition. The lattice parameter of the mullite powder calcined above 130$0^{\circ}C$ (a0=7.5468$\AA$) is nearly close to the value of stoichiometric mullite (71.8wt% Al2O3, a0=7.5456$\AA$). The sintering behavior, microstructure, flexural strength and fracture toughness of the mullite and mullite-15v/o ZrO2 composites have been studied. The mullite-15v/o ZrO2(+3m/o Y2O3) ceramics with relative densities of 96% were obtained when sintered at 1$600^{\circ}C$. The flexural strength and fractrue toughness of the composites sintered at 1$600^{\circ}C$(calcination temperature of mullite powders ; 125$0^{\circ}C$) had maximum values of 307MPa and 2.50MPa.m1/2, respectively. The fracture toughness improvement in the mullite-ZrO2 cmoposite is assumed to be resulted from the combined effect of the stress-induced phase transformation of tetragonal ZrO2 and the crack deflection due to microcracking by the monoclinic ZrO2 formation.

  • PDF

Effect of Formaldehyde on the Water Resistance of MDF Cement Composites

  • Nho, Jun-Seok;Park, Choon-Keun;Park, Sang-Heul
    • The Korean Journal of Ceramics
    • /
    • 제5권3호
    • /
    • pp.278-283
    • /
    • 1999
  • Formaldehyde has widely been used for the cross-linking of polyvinyl alcohol polyvinyl alcohol polymer. The effects of formaldehyde on the water resistance of MDF cement composites were investigated as a function of types of catalyst, base or acid, and the amount of formaldehyde. The acetalization, reaction of OH group of PVA with aldehyde, was ended incompletely under base atmosphere. However, by addition of citric acid, the cross-linking of PVA polymer could be acheved through acetalization of PVA and formaldehyde. The effects of these different patterne according to the types of catalyst on the water resistance of MDF cement were studied by the preparation of PVA films and MDF composites. Thanks to the cross-linking reaction of PVA polymer chains by formaldehyde, the modified PVA films and MDF composites showed a good water-resistant propety. The modified MDF cement composite to which 3 wt% formaldehyde and 1 wt% cirtic acid were added showed 80% of initial flexural strength and good interfacial state between cement grain and polymer matrix. However, 4 wt% formaldehyde deteriorted the processing conditions, microstructures and eventually the flexural strength, causing sharp increase in the viscosity of sample dough during the mixing process. To study the relatins of flexural strength and interface of cement grain and polymer matrix, SEM and MIP measurement were performed.

  • PDF

액상소결 $SiC_f$/SiC 복합재료의 미세조직 및 강도특성 (Microstructure and Strength Property of Liquid Phase Sintered $SiC_f$/SiC Composites)

  • 이문희;조경서;이상필;이진경
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2008년도 추계학술대회A
    • /
    • pp.234-238
    • /
    • 2008
  • The efficiency of fiber reinforced CMC(ceramic matrix composite) on the SiC materials have been investigated, in conjunction with the fabrication process by liquid phase sintering and the characterization. LPS-$SiC_f$/SiC composites was studied with the detailed analysis such as the microstructure, sintered density, flexural strength and fracture behavior. The applicability of carbon interfacial layer has been also investigated in the LPS process. Submicron SiC powder with the constant total amount and composition ratio of $Al_2O_3,\;Y_2O_3$ as sintering additives was used in order to promote the performance of the SiC matrix material. LPS-$SiC_f$/SiC composites were fabricated with hot press under the sintering temperature and applied pressure of $1820^{\circ}C$ and 20MPa for 1hr. The typical property of monolithic LPS-SiC materials was compared with LPS-$SiC_f$/SiC composites.

  • PDF

근역장 통신용 0-3형 고분자 자성 복합소재의 복소투자율 변화 (Complex Permeability of 0-3 Polymer Magnetic Composites for Near-Field Communication)

  • 남중희;임충혁;윤지선;정영훈;조정호;백종후;김효태;김종희
    • 한국자기학회지
    • /
    • 제22권6호
    • /
    • pp.216-220
    • /
    • 2012
  • 이 연구에서는 근역장 통신(NFC)용 소재로 응용하기 위해, MnZn 페라이트와 FeSi 합금 분말을 filler로 사용하여 제조한 0-3형 자성복합소재의 복소투자율 변화(1 MHz~1 GHz)를 측정하였으며, RFID 주파수(13.56 MHz)에서의 복소투자율 값을 검토한 결과, filler 함량에 따라 투자율 실수항은 증가하고 허수항은 감소하는 결과를 얻었다. 즉, 시트형 자성복합소재의 응용을 위한 연구 결과로서, 고투자율을 나타내면서 손실항인 허수항을 상대적으로 낮출 수 있는 소재 제조공정 기술을 확보할 수 있었으며, 복소투자율 변화는 자성분말 filler의 성분과 입자 형태, 그리고 polymer 종류에 의존함을 알 수 있었다.

Silicon Nitride Composites with Different Nanocarbon Additives

  • Balazsi, Csaba
    • 한국세라믹학회지
    • /
    • 제49권4호
    • /
    • pp.352-362
    • /
    • 2012
  • This paper explores the use of a variety of carbon nanoparticles to impart electrical, thermal conductivity, good frictional properties to silicon nitride matrices. We used the highly promising types of carbon as carbon nanotubes, exfoliated graphene and carbon black nanograins. A high-efficiency attritor mill has also been used for proper dispersion of second phases in the matrix. The sintered silicon nitride composites retained the mechanical robustness of the original systems. Bending strength as high as 700 MPa was maintained and an electrical conductivity of 10 S/m was achieved in the case of 3 wt% multiwall carbon nanotube addition. Electrically conductive silicon nitride ceramics were realized by using carbon nanophases. Examples of these systems, methods of fabrication, electrical percolation, mechanical, thermal and tribological properties are discussed.

Carbide Ceramics from Active-Filler-Controlled Pyrolysis in $CH_4$ Atmosphere

  • Kang, Keon-Taek;Kim, Deug-Joong;Annette Kaindl;Peter Greil
    • 한국분말재료학회지
    • /
    • 제6권4호
    • /
    • pp.320-324
    • /
    • 1999
  • The formation, microstructure and properties of novel ceramic composite materials manufactured by active-filler-controlled polymer pyrolysis were investigated. In the presence of active filler particles such as transition metals, bulk components of various geometry could be fabricated from siliconorganic polymer. Molybdenum- and tungsten-filled polymer suspensions were prepared and their conversion to ceramic composites by annealing in $CH_4$ atmosphere were studied. Dimensional change. porosity and phase distribution (filler network) were analyzed and correlated to the resulting hardness values. Molybdenum and tungsten as active filler were carburized completely to $Mo_2C$, $W_2C$ and WC in $CH_4$ atmosphere. Consequently, microcrystalline composites with the filler reaction products embedded in a silicon oxycarbide glass matrix were formed. Hardness was increased with increasing carburization and reached 8.6-9.5 GPa in the specimen pyrolyzed in $CH_4$ atmosphere.

  • PDF

Compressive Behavior of 7xxx Series Al Composites Reinforced with $Al_2O_3$

  • Seo, Young-Ik;Min, Kyung-Ho;Lee, Kyu-Hwan;Kim, Young-Do
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1063-1064
    • /
    • 2006
  • Mechanical properties of 7xxx series Al metal matrix composite (MMC) powders containing different amounts of ceramic were investigated. The ceramic contents of the starting powders were 5 wt.% or 10 wt.%. The powders were uniaxially cold compacted using a cylindrical die with a compacting pressure of 250 MPa and were sintered at $620^{\circ}C$ in a dry $N_2$ atmosphere for 60 min. For the heat treatment, sintered parts were solution treated at $475^{\circ}C$ and aged at $175^{\circ}C$. Compression tests were conducted to reveal the effect of $Al_2O_3$ particle content on the mechanical properties of the composites. Fractography was examined using a scanning electron microscope.