Effect of M2O3 on the Sinterbility and Electrical Conductivity of ZrO2(Y2O3) System(III) : Ceramics of the ZrO2-Y2O3-Ln2O3 System (ZrO2(Y2O3)계 세라믹스의 소결성과 전기전도도에 대한 M2O3의 영향(III) : ZrO2-Y2O3-Ln2O3계 세라믹스)

  • 오영제;정형진;이희수
    • Journal of the Korean Ceramic Society
    • /
    • v.24 no.2
    • /
    • pp.123-132
    • /
    • 1987
  • Yttria-stabilized zirconia with erbia-lanthana were investigated with respect to the amount of Ln2O3 (Ln; Er, La) addition in the range of 0.5∼5 mol% to the base composition of 8 mol% yttriazirconia. Following analysis and measurement were adopted for the characterization of synthesizes of solid electrolyte; phase transformation, lattice parameter, crystallite size, relative density, chemical composition and SEM/EDS. Electrical conductivity by two-probe method versus temperature from 350$^{\circ}C$ to 800$^{\circ}C$ and frequency in the range of 5Hz∼13MHz by complex impedance method was also conducted together with the determination of oxygen ion transference number by EMF method for the evaluation of their electrical properties. The results were as followsing; Electrical conductivity were decreased with increase in Ln2O3 content, but their activation energies increased. In the case of La2O3 addition, espicially, its electrical conductivity was decreased owing to the segregation of second phases at the grain-boundary. Grain-boundary conductivity of the specimen contained 0.5 mol% Er2O3 exhibited a maximum conductivity among thecompositions experimented. However, their bulk conductivities decreased in both case. Oxygen ion transference number was also reduced with decrease in oxygen partial pressure. For example, in the case of Er2O3 addition it retained value in the range of 0.97∼0.94 abvove 4.74${\times}$10-2in oxygen partial pressure. With the increase in the quantities of the evaporation of additive components, the crystallite size of stabilized zirconia decreased, and their relative density also reduced owing to the formation of porosity in their matrices. In the case of La2O3 the sinterbility was improved in the limited amount of addition up to 0.5 mol%, in the same range of addition the strength of sintered bodies were improved perhaps owing to the precipitation of metastable tetragonal phase in the fully stabilized zirconia.

  • PDF

Hardening Characteristics of Aluminum Alloy Surface by PTA Overlaying with Metal Powders (I) (플라즈마분체 오버레이법에 의한 알루미늄합금 표면의 경화특성에 관한 연구(I) -후막 표면 합금화층의 형성조건과 그 조직-)

  • ;中田一博;;;松田福久
    • Journal of Welding and Joining
    • /
    • v.12 no.4
    • /
    • pp.85-101
    • /
    • 1994
  • Effect of Cr, Cu and Ni metal powders addition on the alloyed layer of aluminum alloy (AC2B) has been investigated with the plasma transferred arc (PTA) overlaying process. The overlaying conditions were 125-200A in plasma arc current, 150mm/min in process speed and 5-20g/min in powder feeding rate. Main results obtained are summarized as follows: 1) It was made clear that formation of thick surface alloyed layer on aluminum alloy is possible by PTA overlaying process. 2) The range of optimum alloying conditions were much wider in case of Cu and Ni powder additions than the case of Cr powder addition judging from the surface appearance and the bead macrostructure. 3) Alloyed layer with Cu showed almost the homogeneous microstructure through the whole layer by eutectic reaction. alloyed layers with Cr and Ni showed needle-like and agglomerated microstructures, the structure of which has compound layer in upper zone of bead by peritectic and eutectic-peritectic reactions, respectively. 4) Microconstituents of the alloyed layer were analyzed as A1+CrA $l_{7}$ eutectics, C $r_{2}$al sub 11/, CrA $l_{4}$, C $r_{4}$A $l_{9}$ and C $r_{5}$A $l_{*}$ 8/ for Cr addition, Al+CuA $l_{2}$(.theta.) eutectics and .theta. for Cu addition, and Al+NiA $l_{3}$ eutectics. NiA $l_{3}$, N $i_{2}$A $l_{3}$ and NiAl for Ni addition. 5) Concerning defect of the alloyed layer, many blow holes were seen in Cr and Ni additions although there was lesser in Cu addition. Residual gas contents in blow hole for Cu and Ni alloyed layer were confirmed as mainly $H_{2}$ and a littie of $N_{2}$ Cracking was observed in compound zone of the alloyed layer in case of Cr and Ni addition but not in Cu alloyed layer.r.r.

  • PDF

Crystallization of 90wt% Cordierite-10wt% Enstatite Melt by $TiO_2$ Addition (90wt% Cordierite-10wt% Enstatite 총체의 $TiO_2$ 첨가에 의한 결정화)

  • Rhee, Jhun;Han, Duck-Huyn;Jo, Dong-Soo;Jun, Jong-Pil
    • Journal of the Korean Ceramic Society
    • /
    • v.23 no.5
    • /
    • pp.9-16
    • /
    • 1986
  • The effect of $TiO_2$ addition to the 90wt% Cordierite-10wt% Enstatite base glass was investi-gated to understand the crystallization behavior of the glass. Glasses with addition of $TiO_2$ less than 7, 5wt% had a tendency of surface crystallization and were cracked when heat treated and in this case the crystalline phase formed was indialite. glasses with addition of $TiO_2$ more than 10wt% to 15wt% were crystallized in bulk when heat treated and were suitable for glass-ceramics. The highest microhardness 1640kg/$mm^2$ was obtained when the glass of 12.5wt% $TiO_2$ addition was heat treated at 762$^{\circ}C$ for 60 minutes for nucleation and at 1135$^{\circ}C$ for 20 minutes for crystal growth and in general higher microhardness was obtained when crystalline phase of magnesium aluminum titanate and $\mu$-cordierite were developed. Avrami equation for crystal growth kinetics was applicable in glasses of less than 7.5 wt% $TiO_2$ addition and in case of glasses of more than 10wt% $TiO_2$ addition it was not applicable because of too fast crystal growth.

  • PDF

Hydration of Active-Belite Cement with Gypsum and Slag (석고와 슬래그를 첨가한 Active-Belite Cement의 수화특성)

  • 이성호;박동철;김남호;최상흘
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.4
    • /
    • pp.330-330
    • /
    • 1998
  • Active belite cement clinkers were synthsized by using natural raw materials with borax and calcium phosphate ({{{{ {Ca }_{3 }( {PO}_{4}) }}2) In both case {{{{alpha ^、 {C }_{2 }S }} were formed but borax was more efficient. The cement syn-thesized with the addition of borax was hydrated with the addition of anhydrite(5 wt%) and slag(30wt%, 40wt% 50wt%) The addition of 50wt% slag with anhydrite was good for strength development in 7days and the compressive strength was developed to twice than no addition of slag at 28 days strength.

Studies of Cooking Quality with Various Functional Rice (특수미의 혼합취반 적성 검정)

  • Yoo, Kyung-A;Kang, Mi-Young
    • Journal of the Korean Society of Food Culture
    • /
    • v.20 no.3
    • /
    • pp.293-298
    • /
    • 2005
  • This study was investigated to examine the physicochemical properties of functional rice and the adaptable food processing of the added functional rice. The functional rice are Sanghwang rice, Agaricus rice(fermented with basidiomycota), Tochukaso rice, fermented with Monascus rubber rice. Fermented with Monascus rubber rice contains more crude protein, curde lipid, moisture, and total dietary fiber. The cross sectional shapes of the functional rice show polygon shapes, the starch granules of those rice are transformed. In sensory evaluation, fermented with Monascus rubber rice was showed the lowest values for glossness, color, flavor, sweetness, harshness, overall acceptability. The textural properties for those ratios were also affected by the period of storage. After 48 hours, the lowest hardness level was 30% Tochukaso rice addition, and the highest hardness level was 10% Sangwhang rice addition case. In 30% Sangwhang rice, and 30% tochukaso rice case gumminess values were decreased after 48 hours. But in 30% Sangwhang rice, and 30% Tochukaso rice case, the chewiness values decreased. This result suggest that the most suitable addition ratio for the rice cooking condition is 10% functional rice addition.

A Study on the Generating Efficiency and NOx Emissions of a 30kW Gas Engine Generator with Hydrogen Addition (수소 첨가에 따른 30kW급 가스엔진 발전기의 발전효율 및 질소산화물 배출량 특성 연구)

  • Cha, Hyo-Seok;Kim, Tae-Soo;Eom, Tae-Jun;Chun, Kwang-Min;Song, Soon-Ho
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.22 no.3
    • /
    • pp.313-318
    • /
    • 2011
  • This study is about characteristics of generating efficiency and $NO_x$ emissions of a 30 kW gas engine generator in case of using model biogas with hydrogen addition. In this case, both generating efficiency and $NO_x$ emissions are lower than the case of using urban gas (LNG). However, generating efficiency and $NO_x$ emissions are higher than the case of using model biogas only. It means that adding hydrogen which has a high flame propagation velocity has the possibility to improve the generating efficiency, but simultaneously it is also able to increase the $NO_x$ emissions of a gas engine generator.

Anaerobic Treatment of Wastewater containing Nitrate by Upflow Process (질산염을 함유한 폐수의 상향류식 공법에 의한 혐기성 처리)

  • 이원식;은종극
    • Journal of environmental and Sanitary engineering
    • /
    • v.13 no.2
    • /
    • pp.95-105
    • /
    • 1998
  • This research was investigated which denitrification of wastewater containing nitrate, using upflow anaerobic sludge blanket process. The upflow anaerobic sludge blanket process is also used for both artifical and industrial wastewater. Main ingredients investigated in the artifical and industrial wastewater experiment were the determination of optimum organism/nitrate ratios, nitrate removal efficiency by various hydrogen donor addition and characteristics of granular sludge and gas production in case of various hydrogen donor addition. From the experimental results the following conclusions were made: In case of adding methanol, ethanol and sodium acetate as hydrogen donor granular sludge was formed 50 days after seeding. Average diameter of granular sludge was 4.0 mm and settling velocity was 37 cm/min. Production rate of gas 3.3 L/d in case of adding methanol as hydrogen donor in wastewater containing 150mg/L nitrate. However adding ethanol and sodium acetate as hydrogen donor, gas production rate were 2.2-2.7L/d respectively. In case of adding methanol as hydrogen donor treatability of artifical wastewater contained 150mg/L as nitrate was about 93%. But in addition of sodium acetate in wastewater contained 40mg.L as nitrate, nitrate removal efficiency was 80%.

  • PDF

Flavonoid Components in Plants of the Genus Scutellaria

  • YunChoi, Hye-Sook
    • Korean Journal of Pharmacognosy
    • /
    • v.23 no.4
    • /
    • pp.201-210
    • /
    • 1992
  • Scutellariae plants contain a large number of flavonoids and in addition, many of them are with unusual A- and/or B-ring substitutions. The total number of flavonoids reported up to the middle of 1991 are 137 including 89 of flavones, flavonols and their glycosides including 3 C-glycosides$(1{\sim}89)$, 39 of flavanones, dihydroflavonols and their glycosides $(90{\sim}128)$, 8 of chalcones $(129{\sim}136)$ and one biflavonoid, 8, 8'-bibaicalein(137). More than half of the flavonoids are with either unusual 5-metboxy(2'-methoxy in case of chalcones) in A-ring and/or 2'-oxygenation(2-oxygenation in case of chalcones) in B-ring substitutions. Four flavones, four flavanones and two chalcones are with methylation at 5-OH(2'-OH in case of chalcones) and six of them also have 2'-oxygenations(2- in case of chalcones). Sixtyeight out of total 137 flavonoids have oxygenated substitution at 2'-(2- in case of chalcones) position of B-ring and in addition, 27 of them have another oxygen function at 6'-(6- in case of chalcones) and 18 of them have additional oxygen substitutions either at 3'-, 5'-,3',6'-or 3', 4', 5'-(3, 4, 5- in case of chalcones) positions. The distribution and isolation of flavonoid components of Scutellariae plants are tabulated with references.

  • PDF

A Study on Fatigue Behavior according to Effective Case Depth in Induction Case Hardened SM45C Steel (고주파표면경화한 SM45C 강에서 유교경화층깊이가 피로거동에 미치는 영향)

  • 오세욱;호정원;박원조
    • Journal of Ocean Engineering and Technology
    • /
    • v.5 no.1
    • /
    • pp.71-80
    • /
    • 1991
  • This paper reveals the effect of the effective case depth(ECD) on the fatigue behavior of a high-frequency induction hardened SM45C in rotated bending fatigue test. In addition, the effects of fracture modes(surface origin type, inner origin type) on it are discussed. The fatigue limit of the induction hardened steel is remarkably increased compared with that of base metal. In addition, the fatigue limit is linearly increased as the effective casedepth grows deep in the region of this experiment (ECD/R;0.23-0.49). The S-N curve and fracture mode in the induction case hardened steel are classified into two kinds, as a result : N$_{f}$<10$^{5}$ ;surface origin type fracture(at high stress), N$_{f}$>10$^{5}$ ; in ner origin type fracture(at low stress). In case of inner origin type fracture; as the effective case depth(ECD) gets deep, the fatigue limit is increased by the reason that the fracture origin moves toward center; in reverse, is decreased by reason that the compressive residual stress gets low. As a result, the increasing effect of the former is much bigger than the decreasing effect of the latter, and the fatigue limit is increased as the ECD gets deep.eep.

  • PDF

Effect of MnO2 Addition on Sintering and PTCR Properties in Y2O3 doped BaTiO3 Semiconducting Ceramics (MnO2첨가가 Y2O3 doped BaTiO3 반도체 세라믹스의 소결 및 PTCR특성에 미치는 영향)

  • 이준형;박금덕;김정주;조상희
    • Journal of the Korean Ceramic Society
    • /
    • v.27 no.1
    • /
    • pp.7-12
    • /
    • 1990
  • The influence of MnO2 on the sintering property and PTCR behavior of(Ba0.8Sr0.2)TiO2 has been investigated. And the densities, grain sizes and electrical resitivities of specimens were measured as a function of doping with Mn ion of varying concentration. The density and grain size of the sintered specimens were almost the same regardless of MnO2 addition up to 0.2mol% MnO2. But in the case of 0.25mol% MnO2 addition, abnormal grain growth was appeared. So the grain size distribution was wide and density decreased greatly. The room-temperature resistivity increased as Mn content increased and the temperature coefficient of resistivity was highest in the case of 0.15mol% MnO2 addition.

  • PDF