Synthesis of anhydrite in the mixtures of alunite and limestone by roasting (Alunite와 limestone의 혼합소성에서의 무수석고의 합성)

  • Kim, Hyung-Seok;Ahn, Ji-Whan;Kim, Hwan;Shin, Kang-Ho;Cho, Dong-Sung
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.11 no.5
    • /
    • pp.190-196
    • /
    • 2001
  • Alunite was dehydrated at 500~$580^{\circ}C$ and desulfurued at 580~$780^{\circ}C$ in air atmosphere. Therefore, this study was carried out to investigate the formation conditions of anhydrite ($CaCO_4$) when the mixtures of alunite TEX>$[K_2SO_4$.$Al_2(SO_4)_3$.$4Al(OH)_3$] and limestone ($CaCO_3$)were roasted. Alunite scarcely dected the partial pressures of $CO_2$(g), but limestone was bansformed into CaO at $650^{\circ}C$ in air and $900^{\circ}C$ in saturated $CO_2$(g), atmosphere, respectively. When the the mixtures of 1 mol of alunite and 6 rnol of limestone were roasted for 2 hours at lO00C in air and saturated $CO_2$(g), anhydrite was formed at $550^{\circ}C$ calciumlangbeinite, at $700^{\circ}C$and haiiyne, at 800~$950^{\circ}C$. The formation rate of anhydrite in air and saturated $CO_2$(g), was 99.0 % and 95.0 %, respectively. then the formation rate of anhydrite was not changed in air atmosphere but increased according to the decreasing of the particle size of limestone in saturated $CO_2$(g). Therefore, when the mixture of 1 mol of alunite and 6 rnol of limestone were roasted, the clinker composed of lmol of haiiync and 1 mol of calciumlangbeiilte can be manufactured

  • PDF