• 제목/요약/키워드: Cable-in Conduit-Conductors

검색결과 16건 처리시간 0.028초

CIC 초전도 도체의 안정성 (Stability of the Cable-in-Conduit Conductors)

  • 류경우
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권9호
    • /
    • pp.895-900
    • /
    • 1997
  • A Quench in cable-in-conduit (CIC) conductors is often initiated by a disturbance such as strand motion that generates a highly localized normal zone in a strand or a few strands of the CIC conductors. The localized normal zone causes current and heat transfer between a disturbed strand and neighboring strands. Electrical and thermal contact characteristics between strands thus have an effect on the transient stability of the CIC conductors. In this paper the effect of contact characteristics between strands on the CIC conductor stability is presented based on the measured heat transfer characteristics of supercritical helium (SHe) for the local heating. The quench and recovery processes of the strands for the abrupt and highly localized disturbance are analyzed at the boundary between quench and recovery.

  • PDF

ITER TF 초전도 도체 개발과 특성 (Development of ITER TF Cable-in-Conduit Conductors and Their Characteristics)

  • 김형찬;오동근;박수현;김기만
    • Progress in Superconductivity
    • /
    • 제10권2호
    • /
    • pp.108-115
    • /
    • 2009
  • As a participant taking part in the ITER TF conductor R&D program, we developed two toroidal field conductors with variations of conduit thickness resulting in the different void fraction of the conductors. The estimated void fractions of the conductors are 31% and 33%. In this paper we present the details of the TF conductor development and performance test results of them carried out by the measurement of current sharing temperature under cyclic loading. Regarding the conductor development, the internal-Sn-processed $Nb_3Sn$ strand characteristics, strand cabling, twist pitch and characteristics of the conduit materials are presented. For the understanding of the conductor design and performance, the conductor test results are presented and the effect of the conductor design parameters such as void fraction and twist pitch is discussed based on the results.

  • PDF

$Nb_{3}$Sn 도관 케이블 도체의 굽힘변형 해석 (The analysis of bending processes in $Nb_{3}$Sn Cable-in-Conduit Conductors)

  • 남현일;이호진;박재학
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2002년도 학술대회 논문집
    • /
    • pp.259-262
    • /
    • 2002
  • Cable-in-Conduit Conductors (CICC) have been used for fabrication of nuclear fusion magnets. Bending process is included in fabrication of superconducting magnet such as termination of conductors. Because of plastic deformation by bending process, there can be a large residual stress and change of shape in bent conductors. Void volume fraction in conductors is also changed by bending process. In this study, Commercial code was used to analyze the bending process at various bending curvature radius. The calculated residual stress of conductors bent at less than about 40cm curvature radius exceeded the allowable stress.

  • PDF

Numerical Model for Thermal Hydraulic Analysis in Cable-in-Conduit-Conductors

  • Wang, Qiuliang;Kim, Kee-Man;Yoon, Cheon-Seog
    • Journal of Mechanical Science and Technology
    • /
    • 제14권9호
    • /
    • pp.985-996
    • /
    • 2000
  • The issue of quench is related to safety operation of large-scale superconducting magnet system fabricated by cable-in-conduit conductor. A numerical method is presented to simulate the thermal hydraulic quench characteristics in the superconducting Tokamak magnet system, One-dimensional fluid dynamic equations for supercritical helium and the equation of heat conduction for the conduit are used to describe the thermal hydraulic characteristics in the cable-in-conduit conductor. The high heat transfer approximation between supercritical helium and superconducting strands is taken into account due to strong heating induced flow of supercritical helium. The fully implicit time integration of upwind scheme for finite volume method is utilized to discretize the equations on the staggered mesh. The scheme of a new adaptive mesh is proposed for the moving boundary problem and the time term is discretized by the-implicit scheme. It remarkably reduces the CPU time by local linearization of coefficient and the compressible storage of the large sparse matrix of discretized equations. The discretized equations are solved by the IMSL. The numerical implement is discussed in detail. The validation of this method is demonstrated by comparison of the numerical results with those of the SARUMAN and the QUENCHER and experimental measurements.

  • PDF

Variation of Residual Welding Stresses in Incoloy 908 Conduit during the Jacketing of Superconducting Cables

  • Lee, Ho-Jin;Kim, Ki-Baik;Nam, Hyun-Il
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제5권1호
    • /
    • pp.71-75
    • /
    • 2003
  • The conduit fer superconducting cable is welded and plastically deformed during the jacketing process to make the CICC (Cable-in-Conduit-Conductors) fer a fusion magnet. The jacketing process of KSTAR (Korea Superconducting Tokamak Advanced Research) conductors is composed of several sequential steps such as rounding, welding, sizing, and square-rolling. Since the welded zone in Incoloy 908 conduit is brittle and easy to have flaws, there may be a possibility of stress corrosion cracking during the heat treatment of coil when both the induced tensile residual stress and the concentration of oxygen in the furnace are sufficiently high. The steps of the jacketing process were simulated using the finite element method of the commercial ABAQUS code, and the stress distribution in the conduit in each step was calculated, respectively. Furthermore, the variations of residual welding stresses through the steps of the jacketing process were calculated and analyzed to anticipate the possibility of the stress corrosion cracking in the conduit. The concentrated high tensile residual welding stresses along the welding bead decrease by the plastic deformation of the following sizing step. The distribution in residual stresses in the conductor for magnet coil is mainly governed by the last step of square-rolling.

CICC manufacturing technology as a factor affecting on their performance during full-size testing

  • Kaverin, D.
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제22권4호
    • /
    • pp.24-30
    • /
    • 2020
  • The test results of the ITER toroidal field conductors demonstrated a decrease of the current sharing temperature (Tcs) with an increase in the number of electromagnetic cycles in general. This is associating with several factors. One of them is the superconducting Nb3Sn filaments cracking and another one is the redistribution of the relative deformation of the Nb3Sn strands under Lorentz forces. Despite these factors, some conductors have shown the absence or significantly less degradation of Tcs during electromagnetic cycling. This article considers another possible reason for a more stable conductors Tcs behavior, namely, the local compression of Nb3Sn wires in the cross section of a conductor. In this article presents the results of a quantitative analysis Nb3Sn superconducting filaments cracking of strands extracted from a conductor that has passed electromagnetic cycling and the model of a conductor compaction, as well as calculation results based on this model are presented also.

Moving Mesh Application for Thermal-Hydraulic Analysis in Cable-In-Conduit-Conductors of KSTAR Superconducting Magnet

  • Yoon, Cheon-Seog;Qiuliang Wang;Kim, Keeman;Jinliang He
    • Journal of Mechanical Science and Technology
    • /
    • 제16권4호
    • /
    • pp.522-531
    • /
    • 2002
  • In order to study the thermal-hydraulic behavior of the cable-in-conduit-conductor (CICC), a numerical model has been developed. In the model, the high heat transfer approximation between superconducting strands and supercritical helium is adopted. The strong coupling of heat transfer at the front of normal zone generates a contact discontinuity in temperature and density. In order to obtain the converged numerical solutions, a moving mesh method is used to capture the contact discontinuity in the short front region of the normal zone. The coupled equation is solved using the finite element method with the artificial viscosity term. Details of the numerical implementation are discussed and the validation of the code is performed for comparison of the results with thse of GANDALF and QSAIT.

Study on the unidirectional compaction of terminal cables in the CICC joint

  • 남현일;이호진;박재학;홍계원
    • Progress in Superconductivity
    • /
    • 제3권2호
    • /
    • pp.218-223
    • /
    • 2002
  • The void volume fraction of cables is one of the effective parameters to characterize the joints of superconducting magnet. Because electrical resistance and cooling stability in the CICC (Cable-in-Conduit Conductors) joint are governed by the void volume fraction, it should be controlled constantly in the termination of cable. The change of cross-section shape in the cable was fecund during the unidirectional compaction of terminal sleeve. The non-uniform thickness of the sleeve after compaction is expected because the loading is not taxi-symmetric, and the plastic flow is also not axi-symmetric. The CICC was compacted from 45% void volume fraction to 15% by using two-piece compaction jig, which could be pressed mini-directionally. Commercial code, ABAQUS, was used to analyze the plastic flow in the sleeve during the unidirectional compaction. The increment of radius of curvature of compaction jig could minimize the change of the deformed shape of cables. The calculated results were agreed with the experimental observations.

  • PDF

NbTi 관내 3연선 도체의 안정성 (Stability of Triplet NbTi Cable-In-Conduit Conductor)

  • 장현만;오상수;하동우;하홍수;배준한;김상철;류강식;왕추량
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 하계학술대회 논문집 A
    • /
    • pp.82-84
    • /
    • 1998
  • The normal zone propagation velocity and minimum quench energy (MQE) of cable-in-conduit conductors (CICC) has been investigated at the different background magnetic fields and supercritical helium pressures. The sample CICC of 2 m in length was fabricated with triplet NbTi/Cu strands inserting into a round stainless-steel tube. The heat pulse disturbance with duration time about 400 ms was acted on the center region of the CICC to quench the strands. The normal zone propagation velocity increased with operating current of the CICC. The measured velocity with respect to operation current could be fitted with numerical results.

  • PDF