• Title/Summary/Keyword: CaO-$ZrO_2$

Search Result 182, Processing Time 0.027 seconds

CaO Crucible Induction Melting and Investment Casting of TiAl Alloys (TiAl 합금의 CaO 도가니 유도용융 및 정밀주조)

  • Kim, Myoung-Gyun;Sung, Si-Young;Kim, Young-Jig
    • Journal of Korea Foundry Society
    • /
    • v.22 no.2
    • /
    • pp.75-81
    • /
    • 2002
  • The main objectives were to investigate the suitability of CaO crucible for melting TiAl alloys and to develop investment mold for investment casting of TiAl alloys. TiAl alloy specimen were prepared by plasma arc furnace under argon atmosphere. After melting of TiAl alloy using CaO crucible, the results showed that there is little contamination of oxygen in the TiAl bulk. Conventional vacuum induction furnaces can be readily adaptable to produce cast parts of TiAl without high skilled techniques. The determination of optical metallography and microhardness profiles in investment cast TiAl alloy rods has allowed the gradation of the relative thermal stability of the oxides examined. The molds used for the present study were $ZrO_2$, $Al_2O_3$, CaO stabilized $ZrO_2$ and $ZrSiO_4$. Even although high temperature of mold preheating, $Al_2O_3$ mold is a promising mold material for investment casting of TiAl alloys in terms of thermal stability, cost and handling strength. It is important to take thermal stability and preheating temperature of mold into consideration for investment casting of TiAl alloys.

Geochemical Dispersion and Enrichment of Fluvial Sediments Depending on the Particla Size Distribution (입도분포에 따른 하상퇴적물의 지구화학적 분산 및 부화)

  • 이현구
    • Economic and Environmental Geology
    • /
    • v.32 no.3
    • /
    • pp.247-260
    • /
    • 1999
  • Geochermical characteristics of the fluvial sediments deprnding on particle size distribution size were investigated in the respect of majir, minor and rare eath element chemisitry. Ratios of $Al_{2}O_{3}/Na_{2}O$ and $K_{2}O/Na_{2}O$ of the sediments show the homogeneous valus, and partly positive correlation with $SiO_{2}/Al_{2}O_{3}$, respecively. Characteristics of minor element ratios (V/Ni, Cr/V, Ni/Co and Zr/Hf)are within the lower and narrow range. Thesesuggested that sediment sources may be acidic to intermediate granitic rock, and may be explained by simple weathering and sedimentation. With increasing SiO2 contents, concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, CaO and MgO decreased, but those of $K_{2}O$ and $Na_{2}O$ increased, Concentrations of Ba, Be, Cs, Cu, Li, Ni, Sr, V and Zr show comparatively normal negative and some positive trends. Compared with the mean composition of granite, concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, MnO, CaO and MgO in the sediments of the study area were highly enriced. Among some minor and rare earth elements, concentrations of As, Cd, Cu, and V were enriched, but those of Be, Ce, Rb, Sc, Sr and Zn were depleted when compared with average composition of granite. By decreasing of particle size fractions, SiO2, Rb and Sr conterts decreased, but concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, CaO, MgO, $TiO_{2}$, MgO, $P_{2}O_{5}$, Be, Cu, Hf, Pb, V and Zr increased. From the correlations between particle size fractions and element concenreations, some elements of $Fe_{2}O_{3}$, CaO, MgO, $P_{2}O_{5}$, Cu, Ni, Zn and Zr showed typical trends in the secondary contramination sediments. These trends are typically shown under 100 mesh fractions. It indicates that the fraction of minus 100 mesh is the optimum size fraction for geochemical and environmental survey.

  • PDF

Synthesis of Spherical ZrO2 Powders by Thermal Hydrolysis and Hydrothermal Crystallization (열가수분해 및 수열결정화에 의한 구형 ZrO2 분말의 합성)

  • Cho, Churl-Hee;Jin, Ming-Ji;Choi, Jae-Young;Kim, Do-Kyung
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.4
    • /
    • pp.420-426
    • /
    • 2002
  • $ZrO_2$, $Y_2O_3$-doped $ZrO_2$ and CaO-doped $ZrO_2$ powders were prepared by hydrothermal crystallizing spherical $ZrO_2$ gel which had been synthesized by thermal hydrolysis reaction. After the hydrothermal crystallization process, the formed crystallized powders sustained its original spherical shape and had the mean particle size of $0.4{\mu}m$. The particles were composed of about 10nm sized primary particles. The agglomeration strength between the primary particles appears very weak considering that the spherical particles were broken into the primary particles during the pressing process. The particle shape, size, phase fraction and dopant content were analyzed and crystallization mechanism of spherical gel was discussed.

Luminescence properties of a new $Tb^{3+}$ ion activated long persistent phosphor (새로운 $Tb^{3+}$ 이온 활성 축광성 형광체의 발광 특성)

  • Park, Byeong-Seok;Choi, Jong-Geon
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.19 no.3
    • /
    • pp.130-134
    • /
    • 2009
  • A new long persistent phosphors of $CaZrO_3$ was synthesized at high temperature with weak reduction atmosphere by a traditional solid state reaction method. Photoluminescence spectra analysis showed that the $CaZrO_3$ doped with $Tb^{3+}$ emitted green-yellow emission caused by the energy level transition from the $^5D_3$ and $^5D_4$ to $^7F_1{\sim}^7F_6$. The main emission spectra of 542 nm peak by the $^5D_4{\rightarrow}^7F_5$ transition was revealed through synthesizing at high temperature in $N_2$ gas atmosphere. The afterglow emission spectra of $CaZrO_3:Tb^{3+}$ long persistent phosphores arise at 546 nm peak of narrow range. After the 254 nm ultraviolet light excitation source was switched off, the green-yellow long persistent phosphor can be observed which could last for 8 h in the limit of light perception of dark-adapted human eyes ($0.32\;mcd/m^2$).

Sintered body characteristics of LAS by addition of CaCO3 and ZrO2 using a solid-state reaction (고상반응법을 이용한 LAS계의 CaCO3와 ZrO2 첨가에 따른 소결체 특성 연구)

  • Kim, Sang-Hun;Kang, Eun-Tae;Kim, Ung-Soo;Hwang, Kwang-Taek;Cho, Woo-Seok
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.21 no.5
    • /
    • pp.218-224
    • /
    • 2011
  • LAS ($Li_2O-Al_2O_3-SiO_2$) ceramics were sintered by a solid-state reaction. $CaCO_3$ and $ZrO_2$ were added to the ${\beta}$-spodumene ($Li_2O-Al_2O_3-4SiO_2$) composition of the LAS system for enhancement of sintering behavior and mechanical strength, respectively. We have investigated the sintering characteristics, microstructures, mechanical properties and thermal expansion characteristics according to the change of the amount of additive and sintering temperature of the ${\beta}$-spodumene. At 0.1 mol% $CaCO_3$, the densification of ${\beta}$-spodumene was significantly improved. At 0.04 mol% $ZrO_2$, the strength of ${\beta}$-spodumene was also improved. For all the selected all compositions, the thermal expansion coefficient was measured by a dilatometer, which revealed 1.2 to $1.7{\times}10^6/^{\circ}C$.

The Electric Properties of Multilayer Ceramic Capacitors with $(Ba,Ca)(TiZr)O_3$ Ceramics ($(Ba,Ca)(TiZr)O_3$ 세라믹을 적용한 적층 칩 커패시터의 전기적 특성)

  • Yoon Jung-Rag;Yeo Dong-Hun;Lee Heun-Young;Lee Suk Won
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.55 no.1
    • /
    • pp.1-5
    • /
    • 2006
  • The effect of A/B moi ratios and sintering temperatures on dielectric properties and microstructure of $(Ba_{0.93}Ca_{0.07})_m(Ti_{0.82}Zr_{0.18})O_3$ ceramics were investigated. The dielectric constant decreased with increasing the A/B mol ratio. However, the dielectric loss is improved. As the dielectric properties of A/B mol ratio with m = 1.009 at sintered temperature $1260^{\circ}C$, we obtained dielectric constant 12,800, dielectric loss $3.5\%$ and Y5V temperature characteristics. Highly reliable Ni-MLCCs, 1.6mm$(length){\time}0.8mm(width){\time}0.8mm$(height) with capacitance of 1.23 ${\mu}F$ and 야ssipation loss of $5.2\%$ were obtained employing dielectric material composed of $(Ba_{0.93}Ca_{0.07})_{1.009}(Ti_{0.82}Zr_{0.18})O_3$ - $MnO_2\;0.2wt\%-Y_2O_3\;0.18wt\%,\;-\;SO_2\;0.15wt\%-(Ba_{0.4}Ca_{0.6})SiO_3\;1wt\%$.

A Study on the Transparent Glass-Ceramics On Al2O3-SiO2 System (투명 결정화 유리에 관한 연구 - $Al_2O_3-SiO_2$계에 관하여)

  • 박용완;김용욱
    • Journal of the Korean Ceramic Society
    • /
    • v.29 no.3
    • /
    • pp.223-231
    • /
    • 1992
  • CaO and ZnO were added to Al2O3-SiO2 binary system respectively as flux, then ZrO2 and TiO2 were applied as nucleating agent to these CaO-Al2O3-SiO2 and ZnO-Al2O3-SiO2 ternary system glass. The transparency could not be kept in CaO-Al2O3-SiO2 system glass, whereas the transparent glass-ceramics were prepared in ZnO-Al2O3-SiO2 system glass containing ZrO2 as the nucleating agent. At this time the optimum heating temperatures for the nucleation and the crystal growth were 78$0^{\circ}C$ and 97$0^{\circ}C$. The sizes of the precipitated crystals in the transparent glass-ceramics were below 0.1 ${\mu}{\textrm}{m}$, and their light transmissibilities were more than 80%.

  • PDF

Reaction between Calcium-doped Lanthanum Chromite and Yttria Stabilized Zirconia (칼슘이 첨가된 란탄-아크롬산 염과 이트리아 안정화 지르코니아 계면간의 반응)

  • Choe, Jin-Sam
    • Korean Journal of Materials Research
    • /
    • v.11 no.6
    • /
    • pp.460-464
    • /
    • 2001
  • The ceramic diffusion coupling with the green body of calcium-doped lanthanum chromite(La$_{0.8}$Ca$_{0.2}$CrO$_3$CLC- G) and sintered calcium-doped lanthanum chromite(La$_{0.8}$Ca$_{0.2}$CrO$_3$ CLC) by Pechini's method on yttria stabilized zirconia(YSZ) plate has been investigated. The X-ray diffraction pattern of CLC sides at the reacted CLC-G/ CLC and CLC/YSZ interface were identified as La$_{1-x}$ Ca$_{x}$CrO$_3$ and the unreacted YSZ side was cubic-ZrO$_2$ at the treated condition, 1300~1500 C for 10 hr in air, respectively. The order of migration components between CLC/YSZ interface was Zr>La>>Cr>>>Ca and these changes were not dependent upon the treated conditions. The grain shape and size at the interface of CLC-G/CLC was appeared to have a uniform distribution with increasing temperature. The bonding reaction of YSZ/CLC was occurred without a large amount change of the compositions in SEM photos.os.otos.os.

  • PDF

Fabrication of high purified zirconium dioxide (ZrO2) and stabilized zirconia (TZP: tetragonal zirconia polycrystal) powders (고순도 산화지르코늄(ZrO2) 및 안정화 지르코니아 (TZP: tetragonal zirconia polycrystal) 분말제조)

  • 최의석
    • Proceedings of the Korea Association of Crystal Growth Conference
    • /
    • 1996.06b
    • /
    • pp.55-85
    • /
    • 1996
  • 지르코니아 분말은 ZrO2 결정상이 온도변화에 따라 부피변화를 수반하는 상전이변태를 나타낸다. 단사정 ZrO2가 110$0^{\circ}C$에서는 정방정으로, 2$700^{\circ}C$ 내외에서는 입방정으로 결정구조가 가역적으로 변한다. 이 ZrO2에 금속산화물을 고용시키면 형석 (CaF2:Florite)형의 입방정 결정구조가 실온에서도 안정하게 존재하게 된다. 안정화제 산화물은 caO, MgO등 2가 산화물외에 3가 또는 4가의 금속산화물로서 Sc2O3, Y2O3, Sm2O3, Nd2O3, Gd2O3, Y2O3, CeO2 등이며 이들은 금속이온의 원자가가 변하기 쉬운 희토류 산화물이다. 안정화 지르코니아는 형석형 결정구조이며 결정화학적으로 보면 금속양이온이 산소이온에 대해서 정육면체형의 8배위를 하고 있다. 이때 이온반경비(양이온/음이온)에 따라 Zr+4자리와 O-2자리의 격자위치와 모양이 형성되므로 비틀어진 정육면체구조이건 이상적인 정육면체 형석구조를 이룬다. 이는 지르코니아의 결정상의 2상-3상인 부분안정화 지르코니아다결정체(PSZ : partially stabilized zirconia)이거나 단일상-2상인 정방정 지르코니아다결정체(TZP : tetragonal zirconia polycrystal)의 결정구조를 가지는데 기인한다. PSZ는 주로 MgO, CaO를 안정화제로 고용시켜 입방정 영역에서 소결하고 이를 다시 입방정과 정방정의 상 영역에서 열처리하여 입방정 입자내부에 정방정을 석출 형성시킨 것이며 TZP는 Y2O3 및 CeO2를 고용시켜 PSZ와 다르게 일반적인 상압소결한 정방정 결정상의 미립자이다. 산화지르코늄 분말은 지르콘사에서 열분해시킨 지르코늄소결.융해괴(caustic fusion clinker)를 산처리하여얻어진 지르코늄산용액(zirconyl acid solution : cloride, sulfide, nitride 등)으로부터 제조된다. 고순도 산화지르코늄은 용액 결정석출법에 의해 ZrOCl2.8H2O, 5ZrO2.3SO3.15H2O, ZrO(NO3)2.xH2O 등의 지르코늄 수화물만을 재결정화시킨 것으로부터 얻을 수 있으며 이 지르코늄염 수용액으로부터 입자미세구조를 효과적으로 제어하여 산화지르코늄 및 안정화 지르코니아 분말제조가 가능하다. 안정화 지르코니아 분말은 ZrO2와 안정화산화물의 고용을위하여 가열처리를 필요로 하며 일정온도에서 최적상태로 숙성하므로서 2가지 상(phase) 이상의 고용체를 가지게 된다. 안정화 지르코니아 분말은 고용처리온도를 낮추고 효과적으로 생성시키기 위해서는 지르코늄 및 안정화제염을 혼합하고 습식 직접합성하여 저온에서 고용체의 합해진상 영역을 생성시키는 것이다. 이는 지르코니아 원료분말의 미세구조를 제어하므로서 가능하며 이때 화학성분조성과 크기형태가 균일하게 분포된 입자분말을 얻을 수 있다.

  • PDF