This study aimed to evaluate the nutrient digestibility of growing rabbits fed diets with different levels of either Leucaena leucocephala (LLM) or Moringa oleifera (MOLM) leaf meals and also to compare total collection and $TiO_2$ marker methods for estimating digestibility. A total of 30 California growing rabbits ($1.81{\pm}0.19kg$ live weight on average) were randomly distributed into five experimental groups of six rabbits each and were housed in individual cages. The groups were control, 30% LLM, 40% LLM, 30% MOLM, and 40% MOLM. All groups received pelleted diets for two weeks; diets also contained 4 g/kg titanium dioxide as dietary marker. Daily feed intake was recorded during the whole experimental period and total feces were collected daily and weighed individually during four days. The results showed that there were no difference (p>0.05) in feed, dry matter (DM), organic matter (OM), crude protein (CP), digestible energy, and crude fiber (CF) intake between the control group and the other experimental groups. The apparent digestibility values of DM, OM, CP, CF, acid detergent fiber, and gross energy were the highest for control group (p = 0.001), meanwhile MOLM diets had generally higher nutrient digestibility coefficients than LLM diets. Increasing the inclusion level of leaf meal in the diet from 30% to 40% improved the digestibility of CF from 45.02% to 51.69% for LLM and from 48.11% to 55.89% for MOLM. Similar results for apparent nutrient digestibility coefficients were obtained when either total collection or indigestible marker method was used. In conclusion, the digestibility of MOLM containing diets were better than LLM diets, furthermore $TiO_2$ as an external marker could be used as a simple, practical and reliable method to estimate nutrients digestibility in rabbit diets.
산업의 고도화에 따른 구조물의 사용 환경이 열악해지고 최근 에너지저감과 환경문제 개선을 위한 경화의 요구에 따라 뛰어난 내식성 및 우수한 고비강도 특성을 갖고 있는 타이타늄 및 타이타늄합금의 활용에 대한 연구가 많은 주목을 받고 있다. 이에 따라 타이타늄 신합금의 개발뿐만 아니라 기존에 개발되어 비교적 보편적으로 적용되고 있는 타이타늄 부품의 제조 및 성형기술에 대한 수요도 급증하고 있다. 특히, 기기 및 부품 제조를 위한 용접/접합기술도 매우 중요한 요소기술로 자리메김하고 있다. 타이타늄은 산소, 수소 등의 침입형 원소와의 친화력이 강한 활성이 큰 금속으로 용접시 고온에 노출되면 급격히 산화 및 취화 등의 문제를 발생한다. 따라서 타이타늄의 용접시에는 $426^{\circ}C$이상의 온도에서는 대기로부터 용접부가 차단되도록 하는 쉴딩기술이 매우 중요하다. 타이타늄의 용접은 일반적으로 아크용접, 전자빔 용접, 레이저 용접 및 확산접합 등이 적용되고 있으나 용접입열 조정이 용이하고 아크 안정성이 높고 용접부의 기계적 특성이 우수한 GTA 용접이 작업성을 고려하여 가장 많이 적용되고 있다. 본 연구에서는 미국용접학회(AWS)의 타이타늄 용접가이드를 분석 및 소개하였고, 1t 이하의 박판 CP Ti를 대상으로 GTAW 용접부 미세조직 및 기계적 특성을 분석하였다. 이때, 용접 비드폭 제어 및 펄스 용접기술을 통하여 박판 타이타늄의 최적 GTAW 공정변수 제어기술을 분석하였다.
STATEMENT OF PROBLEM. When veneering composite resin-metal restoration is prepared, the fact that bond strength between Ti and composite resin is relatively weak should be considered. PURPOSE. The purpose of this study is to evaluate the shear bond strength between the veneering composite resin and commercial pure (CP) Ti / Ti-6Al-4V alloy according to the method of surface treatment. MATERIAL AND METHODS. The disks were cast by two types of metal. Their surfaces were treated by sandblasting, metal conditioner, TiN coating and silicoating respectively. After surface treatment, the disks were veneered by composite resin (Tescera$^{TM}$, Bisco, USA) which is 5 mm in diameter and 3 mm in thickness. The specimens were stored in water at $25^{\circ}C$ for 24 hours, and then evaluated for their shear bond strength by universal testing machine (STM-$5^{(R)}$, United Calibration, USA). These values were statistically analyzed. RESULTS. 1. All methods of surface treatment were used in this study satisfied the requirements of ISO 10477 which is the standard of polymer-based crown and bridge materials. 2. The metal conditioner treated group showed the highest value in shear bond strength of CP Ti, silicoated group, TiN coated group, sandblasted group, in following order. 3. The silicoated group showed the highest value in shear bond strength of Ti-6Al-4V alloy, metal conditioner treated group, sandblasted group, TiN coated group, in following order. CONCLUSION. Within the limitations of this study, all methods of surface treatment used in this study are clinically available.
The oxidation behaviors of Ti-10Ta-10Nb alloy and Ti-6Al-4V alloy were studied in dry air atmosphere. Specimens were melted in consumable vacuum arc furnace and homogenized at $1050^{\circ}C$ for 24 h. Hot rolling was performed at $1000^{\circ}C$. Specimens of the alloys were oxidized as the temperature range $400~650^{\circ}C$ for 30 min. The oxidation behavior of the alloys was analysed by optical microscope, SEM/EDX, XRD, XPS and TGA. Immersion test was performed in 1% Lactic acid. In the microscope observation, oxide layer of Ti-10Ta-10Nb alloy was denser and thinner than Ti-6Al-4V's. The weight gains during the oxidation rapidly increased at the temperature above $600^{\circ}C$ in Ti-6Al-4V's alloy and$ 700^{\circ}C$ in Ti-10Ta-10Nb alloy. According to XRD results, oxide layers were composed of mostly $TiO_2$(rutile) phase. It was analysed that the passive film of the Ti alloys consisted of $TiO_2$ through X-ray photoelectron spectroscopy(XPS) analysis.
In order to effectively utilize visible light in the photocatalytic reaction, nanaocomposite of Ni doped $TiO_2$ and $NiTiO_3$ powders were synthesized by mechanical alloying and heat treatment. About 5.4 wt% of $NiTiO_3$ with particle size less than 15nm was uniformly formed in the Ni-doped rutile $TiO_2$ matrix. The UV/VIS-DRS and PL investigation showed that the nanocompasite $TiO_2$ powders had a longer absorpt ion wavelength (600$\sim$650nm, 2.0$\sim$1.9eV) than that of Ni-doped $TiO_2$ or rutile $TiO_2$ powder. The carbon decomposition of 4-CP by the nanocompasite $TiO_2$ powders were higher than other $TiO_2$ (P-25).
In the present research, the simultaneous punching of ultra small size hole of $2\~10\;{\mu}m$ in diameter on flat rolled thin metal foils was conducted with elastic polymer punch. Workpiece used in the present investigation were the rolled pure copper of $3{\mu}m$ in thickness and CP titanium of 1.5fm in thickness. The metal foils were punched with the dies and arrays of circular and rectangular holes were made. The process set-up is similar to that of the flexible rubber pad farming or Guerin process. Arrays of holes were punched successfully in one step forming. The punched holes were examined in terms of their dimensions. The effects of the wafer die hole dimension and heat treatment of the workpiece on ultra small size hole formation of the thin foil were discussed. The process condition such as proper die shape, pressure, pressure rate and diameter-thickness ratio (d/t) were also discussed. The results in this paper show that the present method can be successfully applied to the fabrication of ultra small size hole away in a one step operation.
This study evaluated the mechanical properties of Ti-Cu alloys with the hope of developing an alloy for dental casting with better mechanical properties than unalloyed titanium. Ti-Cu alloys with four concentrations of Cu(2,5,10wt%) were made in an argon-arc melting furnace. The microstructure and micro-Vickers hardness were determined. X-ray diffraction pattern test was performed on the polished specimens. The microstructure of 2%Cu and 5%Cu alloys are shown acicular ${\alpha}Ti$ phase formed on the surfaces of previously formed $\beta$grains. The 10%Cu alloys has essentially a eutectoid structure; this structure includes lamella of ${\alpha}Ti$ and $Ti_2Cu$ phase that transformed from ${\alpha}Ti$ at the eutectoid temperature. The micro-Vickers hardness of CP Ti specimens was significantly(p<0.05) lower than that of any of the other alloys. Among the Ti-Cu alloys, the 10%Cu alloys exhibited a significantly(p<0.05) higher hardness value. but lower than that of Ti-6%Al-4%V alloy. From these results, it was concluded that new alloys for dental castings should be designed as Ti-Cu based alloys if other properties necessary for dental castings were obtained.
Commercially pure titanium (Cp-Ti) and Ti alloys (typically Ti-6Al-4V) display excellent corrosion resistance and biocompatibility. Although the chemical composition and topography are considered important, the mechanical properties of the material and the loading conditions in the host have, conventionally. Ti and its alloys are not bioactive. Therefore, they do not chemically bond to the bone, whereas they physically bond with bone tissue. The electrochemical deposition process provides an effective surface for biocompatibility because large surface area can be served to cell proliferation. Plasma electrolyte oxidation (PEO) enables control in the chemical composition, porous structure, and thickness of the TiO2 layer on Ti surface. Silicon (Si) in particular has been found to be essential for normal bone and cartilage growth and development. Zinc (Zn) plays very important roles in bone formation and immune system regulation, and is also the most abundant trace element in bone. The objective of this work was to study on electrochemical behaviors of PEO-treated Ti-6Al-4V Alloy in solution containing Zn and Si ions. The morphology, the chemical composition, and the microstructure analysis of the sample were examined using FE-SEM, EDS, and XRD. The potentiodynamic polarization and AC impedance tests for corrosion behaviors were carried out in 0.9% NaCl solution at similar body temperature using a potentiostat. The promising results successfully demonstrated the immense potential of Si/Zn-TiO2 coatings in dental and biomaterials applications.
티타늄과 티타늄 합금은 재료적 특이성 때문에 심장 혈관 임플란트에서 일반적으로 사용되어 왔다. 일찍이 적용된 예로는 인공심장판막, 심박조율기의 보호케이스, 혈액 순환 장치 등이 있다. 하지만 물질유도혈전증(Material-induced thrombosis)은 혈전폐색에 의해 기인한 기능 손실로 심장혈관 임플란트 장치의 주된 합병증으로 존재하고 있으며, 심장혈관 임플란트의 혈전유전자는 심장혈관장치의 발달에 주된 난관 중 하나로 남아있다. 그리고 텍스처 혈액 접합 물질(Textured blood-contacting material)은 1960년대 초반 이후부터 혈액순환 보조 장치의 임상실험에 사용되고 있다. 접합 물질에 내장된 텍스처 섬유조직 표면은 형성, 성장, 안정적 부착, 생물학적 내벽(neointimal layer) 등 유도 혈액(entrapping blood) 성분에 의해 형성된다. 공동(cavity) 형상의 용해 가능한 미립자를 사용하는 SCPL법(Solvent casting/particulate leaching method)은 티타늄 기질 이전에 형성된 폴리우레탄 위에 텍스처(texture)를 생성하기 위해 사용되었다. 또한 콜라겐의 부동화(不動化)에 의한 공동(cavity)은 혈액 접합면에 잔존하기 위한 내피세포를 고정할 수 있는 효과가 있다. cpTi로 층화된 PU 기소공성(microporous)은 구조적 특성과 혈전증 감소를 위한 생물학적 내벽 사용의 잠재성을 평가하기 위한 세포 공동체 실험을 통해서 평가되었다.
This paper presents a method by which multiple holes of ultra small size can be punched simultaneously. Silicon wafers were used to fabricate punching die. Workpiece used in the present investigation were the rolled pure copper of $3{\mu}m$ in thickness and CP titanium of $1.5{\mu}m$ in thickness. The metal foils were punched with the dies and arrays of circular and rectangular holes were made. The diameter of holes ranges from $2-10{\mu}m$. The process set-up is similar to that of the flexible rubber pad forming or Guerin process. Arrays of holes were punched successfully in one step forming. The punched holes were examined in terms of their dimensions, surface qualities, and potential defect. The effects of the die hole dimension on ultra small size hole formation of the thin foil were discussed. The optimum process condition such as proper die shape and diameter-thickness ratio (d/t) were also discussed. The results in this paper show that the present method can be successfully applied to the fabrication of ultra small size hole array in a one step operation.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.