Synthesis, Characterization and Enhanced Selectivity in RP-HPLC of Polar Carbonyl Group Embedded Poly (Vinyl Octadecanoate) Grafted Stationary Phase by Simple Heterogeneous "Graft from" Technique

  • Rana, Ashequl A.;Karim, Mohammad Mainul;Takafuji, Makoto
    • Bulletin of the Korean Chemical Society
    • /
    • 제32권1호
    • /
    • pp.77-82
    • /
    • 2011
  • A new high performance liquid chromatograpgy (HPLC) stationary phase that possesses an internal carbonyl functional group is synthesized by heterogeneous "graft from" method. This new stationary phase, poly (vinyl octadecanoate) grafted silica (Sil-2) is then characterized by different physico-chemical methods such as diffuse reflectance infrared fourier transform, suspension state $^1H$ NMR, solid state $^{13}C$ CP/MAS NMR, $^{29}Si$ CP/MAS NMR, elemental analysis and thermogravimetric analysis. Chromatographic properties of Sil-2 were evaluated under reversed phase condition by separating polycyclic aromatic hydrocarbons (PAHs) and comparing the chromatographic results with those on polymeric as well as monomeric octadecylated silica stationary phases.

Solid-State $^1H$ and $^{29}Si$ NMR Studies of Silicate and Borosilicate Gel to Glass Conversion

  • 양경화;우애자
    • Bulletin of the Korean Chemical Society
    • /
    • 제17권8호
    • /
    • pp.696-699
    • /
    • 1996
  • Silicate and borosilicate gels were prepared by the sol-gel process and thermally treated in the 150-850 ℃ temperature range. Solid-state 1H MAS and 29Si CP/MAS NMR spectroscopy were used to investigate the effects of heat treatments on the silicate gel to glass conversion process. The 1H NMR isotropic chemical shifts and the relative intensities of hydrogen bonded and isolated silanol groups have been used to access the information concerning the dehydration process on the silicate gel surface. The 29Si NMR isotropic chemical shifts affected by the local silicon environment have been used to determine the degree of crosslinking, i.e. the number of siloxane bonds. These NMR results suggest that the silicate gel to glass conversion process is occurred by two stages which are dependent on the temperature; (1) the formation of particles up to 450 ℃ and (2) the formation of large particles by aggregation of each separated single particle above 450 ℃. In addition, the effects of B atom on the formation of borosiloxane bonds in borosilicates have been discussed.

Dynamics of Poly[oxy-1,4-phenyleneoxy-2-{6-(4-(4-butylphenylazo)phenoxy)hexyloxy}terephthaloyl] and Poly[oxy-1,4-phenyleneoxy-2-{10-(4-(4-butylphenylazo)phenoxy)decyloxy}terephthaloyl] Studied by $^{13}C$ CP-MAS NMR

  • 조경규;한옥희;진정일
    • Bulletin of the Korean Chemical Society
    • /
    • 제19권2호
    • /
    • pp.178-183
    • /
    • 1998
  • Carbon-13 CP-MAS NMR techniques were used to investigate dynamics of new combined type liquid crystalline polymers, poly[oxy-1,4-phenyleneoxy-2-{6-(4-(4-butylphenylazo)phenoxy)hexyloxy}terephthaloyl] and poly[oxy-1,4-phenyleneoxy-2-{10-(4-(4-butylphenylazo)phenoxy)decyloxy}terephthaloyl]. Noticeable mobility change of either aromatic groups or methylene groups is not detected between 25 ℃ and 82 ℃ from 13C spinlattice relaxation time in the rotating frame (T1ρ(C)) and contact time array experiments. However, line shape analysis shows the increase of mobility of methylene carbons in poly[oxy-1,4-phenyleneoxy-2-{6-(4-(4-butylphenylazo)phenoxy)hexyloxy}terephthaloyl] at higher temperature. The dynamics of side chanis does not seem to be affected in our experimental temperature range by the length of aliphatic chain which is connecting the side chain group to the main chain.

La0.8Ca0.2MnO3의 합성 및 특성연구 (Preparation and Characterization of La0.8Ca0.2MnO3)

  • 정미원;이지윤;김현정
    • 한국세라믹학회지
    • /
    • 제40권5호
    • /
    • pp.434-440
    • /
    • 2003
  • 초거대 자기 저항 물질인 페로브스카이트 L $a_{0.8}$C $a_{0.2}$Mn $O_3$의 분말을 졸-겔방법으로 제조하였다. Lanthanum(III), Calcium(II) 그리고 Manganese(III) 2,4-Pentanedionate를 Propionic acid와 methane떠 혼합용매를 사용하고 PEG (l5 wt%) 용액을 첨가 하여 안정한 졸용액을 합성하였고 FT-IR spectroscopy로 반응의 진행 정도를 관찰하였다. L $a_{0.8}$C $a_{0.2}$Mn $O_3$ 겔 분말에 대해 온도를 변화시키면서 열처리하여 FT-IR, CP/MAS $^{13}$C solid state NMR spectroscopy와 XRD등을 이용해 구조변화를 관찰하였다. 열분석은 TG/DTA로 측정하였으며, FE-SEM을 통해 입자크기와 균일도를 관찰하였고, 양이온 조성 비율을 알아보기 위해 ICP-AES를 측정하였다. 자성 특성을 규명하기 위해 VSM을 이용하여 자기 모멘트를 측정하였으며, 상자기성 에서 강자기성으로 전이되는 큐리온도( $T_{c}$)를 관찰하였다.

티탄산바륨 분말과 박막의 제조 및 특성 연구 (Preparation and Characterization of BaTiO3 Powders and Thin films)

  • 정미원;손현진;이지윤;김현정
    • 분석과학
    • /
    • 제17권2호
    • /
    • pp.173-179
    • /
    • 2004
  • Ethylene glycol의 polymerization-complex route를 통한 졸-겔 합성법으로 안정하고 균일한 barium titanate 분말 및 박막을 제조하였다. 출발 용액으로 킬레이팅 리간드인 acetylacetone을 barium과 titanium 용액에 치환시켜 합성한 복합 산화물 졸 용액을 사용했을 때 박막을 만들 수 있었다. 졸 용액의 입자 분포도는 안정한 gaussian 분포를 보였으며, $1100^{\circ}C$에서 열처리한 겔 분말의 입자 크기는 40~77 nm이었다. 열분석 및 FT-IR, $^{13}C$ CP/MAS NMR 스펙트라와 XRD 결과로부터 (Ba-Ti)-oxycarbonate 중간상을 거쳐 $BaTiO_3$ 분말이 형성됨을 알 수 있었다. Quartz에 스핀 코팅으로 제조한 박막은 치밀하고 균열 없는 미세 조직을 보였다. $1100^{\circ}C$에서 열처리한 박막 표면의 입자 크기는 220 nm였으며 치밀한 입자 성장을 관찰할 수 있었다.

Solid-state NMR Study on Membrane Protein Structure in Biological Condition

  • Kang, Su-Jin;Lee, Bong-Jin
    • 한국자기공명학회논문지
    • /
    • 제16권2호
    • /
    • pp.103-110
    • /
    • 2012
  • Membrane proteins play a essential role in the biological systems and it is not easy to handle a membrane protein for its structural study. Solid-state NMR (ssNMR) can be a good tool to investigate the structures and dynamics of membrane proteins. In ssNMR, Magic Angle Spinning (MAS) and Cross Polarization (CP) can be utilized to reduce the line-broadening, leading to high resolution and sensitivity in the spectrum. ssNMR, if combined with other spectroscopic methods, can provide us a enough knowledge on structures and dynamics of membrane proteins in biological condition.

2차 아미노기를 갖는 실리카 나노입자와 (메타)아크릴레이트 단량체와의 마이클 부가반응에 대한 분광학적 분석 (Spectroscopic Analysis on the Michael Addition Reaction between Secondary Amino Group Containing Silica Nanoparticles with (Meth)acrylate Monomers)

  • 전하나;하기룡
    • 폴리머
    • /
    • 제36권5호
    • /
    • pp.668-676
    • /
    • 2012
  • 본 연구에서는 실리카 나노입자를 bis[3-(trimethoxysilyl)propyl]amine(BTMA) 실란 커플링제로 표면 개질한 후, 실리카에 도입되는 2차 아미노기인 -NH기와 Michael 부가반응이 가능한 acrylate기를 가지는 trimethylolpropane ethoxylate triacrylate(TMPET)와 3-(acryloyloxy)-2-hydroxypropyl methacrylate(AHM)로 표면 처리를 하여 반응성(meth)acrylate기를 가지는 brush를 도입하는 연구를 수행하였다. 1분자에 Michael 부가반응성이 있는 acrylate기를 3개 갖는 TMPET와 1분자에 반응성이 있는 acrylate기와 반응성이 없는 methacrylate기를 각각 1개씩 갖는 AHM을 사용하여, 처리 몰(mol)수의 변화가 실리카 표면에 도입되는 (meth)acrylate기에 미치는 영향을 Fourier transform infrared spectroscopy(FTIR), elemental analysis(EA) 및 고체 상태 cross-polarization magic angle spinning(CP/MAS) nuclear magnetic resonance spectroscopy(NMR)법을 사용하여 분석하였다. BTMA로 개질된 실리카를 TMPET로 처리하면, 액체상태의 순수 TMPET와 순수 BTMA의 반응과는 달리 TMPET 1분자당 3개씩 결합있는 acrylate기 대부분이 BTMA의 -NH기와 Michael 부가반응이 일어나는 것을 확인하였다. 따라서 BTMA로 처리한 실리카에 Michael 부가반응으로 반응성 (meth)acrylate기를 도입하기 위하여서는 AHM과 같이 Michael 부가반응성이 있는 acrylate기와 Michael 부가반응성이 없는 methacrylate기를 각각 1개씩 가지는 AHM을 사용하는 것이 필요함을 확인하였다.

Sampling Methods for Quantification of Solid-state Phases in Powder Samples with Solid-state NMR Spectroscopy

  • Han, Oc-Hee;Kim, Sun-Ha;Ko, Tae-Jung
    • Bulletin of the Korean Chemical Society
    • /
    • 제30권5호
    • /
    • pp.1077-1079
    • /
    • 2009
  • To minimize the variance in the quantification of solid-state phases in powder samples, gently placing polycrystalline samples one next to another directly in a sample holder is better than trying to mix them homogeneously prior to transferring to a sample holder. However, the solid-state cross polarization-magic angle spinning (CP-MAS) nuclear magnetic resonance (NMR) spectroscopy results demonstrated that it is essential in this sampling method to place all the samples in the location of consistent signal sensitivity. The same sampling method may be employed in other spectroscopic quantification techniques of solid-state phases if the method to limit the sample to the location with uniform signal sensitivity in the sample holder is adapted to each technique.

생체적합성과 생분해성을 갖는 키틴유도체의 합성 및 물성 III -에스테르 키틴 유도체의 합성과 용해 특성- (Synthesis and Physical Properties of Biocompatible and Biodegradable Chitin Derivatives III. -Synthesis and Solubility of Ester Chitin Derivatives-)

  • 김선정;이영무;성용길;강인규;박영훈
    • 공업화학
    • /
    • 제4권4호
    • /
    • pp.785-790
    • /
    • 1993
  • 키틴의 글루코오스 단위에 메탄술폰산 존재하에서 아세트산 무수물, 프로피온산 무수물과 n-부틸산 무수물을 반응시켜 아세틸 키틴(AC), 프로피오닐 키틴(PC) 그리고 n-부티릴 키틴(BC) 등의 에스테르 형태를 갖는 개질화 키틴을 합성하였고 이들의 구조를 FT-IR과 solid state CP/MAS $^{13}C-NMR$ spectra로 확인하였다. 에스테르 형태의 키틴유도체는 대체로 키틴의 글루코오스 단위의 6번 탄소위치에 치환되었다. 유도체를 유기용매와 수용성 약산 유기용매에서 용해성을 검토하여 포름산에서 세 가지 유도체 모두 좋은 용해성을 나타냈고, 수용성 약산에서는 대부분의 유도체는 팽윤되는 것을 고찰할 수 있었다.

  • PDF

에폭시 수지와 층상광물로부터 나노복합재료의 합성 (Nanocomposites from Epoxy Resin and Layered Minerals)

  • 강재현;유성구;서길수
    • 폴리머
    • /
    • 제24권4호
    • /
    • pp.571-577
    • /
    • 2000
  • 본 연구에서는 새로운 형태의 에폭시 -광물 라노복합재료를 합성하기 위한 충전재를 층상 화합물인 나트륨-montmorillonite (Na-MMT)와 octadecyltrimethylammonium bromide와의 이온교환 반응으로부터 얻었다. 이렇게 합성된 octadecyltrimethylammonium-MMT에 3-aminopropyl triethoxysilane (APS)를 반응시켜 층상물질의 내부에 aminopropyl기가 삽입된 $C_{18}$ H$_{37}$ N($CH_3$)$_3$-APS-MMT를 합성하였다. 개질된 MMT의 층간저리와 구조를 X-선 회절 (XRD), IR 그리고 고상 $^{29}$ Si CP/MAS NMR을 이용하여 확인하였다. 이어서 $C_{18}$ H$_{37}$ N($CH_3$)$_3$-APS-MMT 존재하에 diglycidyl ether of bisphenol A (DGEBA)를 중합시켜 광물-고분자 나노복합재료를 합성하였다. 그리고 얻어진 나노복합재료의 구조를 XRD, 투과전자현미경 (TEM) 그리고 주사전자현미경 (SEM)으로 확인하였다. 확인 결과 합성된 유기몬모릴로나이트는 에폭시 고분자 내에서 실리케이트 층이 완전히 박리되어 있으며 단일층으로 고분자 매트릭스 내에 잘 분산되어 있음을 알았다.