Fatigue Life Evaluation of Butt-Welded Tubular Joints

  • Kim, Dong-Sup;Nho, In-Sik
    • International Journal of Ocean Engineering and Technology Speciallssue:Selected Papers
    • /
    • v.6 no.1
    • /
    • pp.69-74
    • /
    • 2003
  • Recent deepwater offshore structures in the Gulf of Mexico utilize butt welded tubular joints. Application of a welded tubular joint includes tendons, production risers, and steel catenary risers. Fatigue life assessment of these joints becomes more critical, as the structures to which they are attached are allowed to undergo cyclic and sometimes large displacements around an anchored position. Estimation of the fatigue behavior of these tubular members in the design stage is generally conducted by using S-N curves, as specified in the codes and standards. Applying the stress concentration factor of the welded structure to the S-N approach often results in a very conservative assessment, because the stress field acting on the tubular has a non-uniform distribution through the thickness. Fatigue life analysis using fracture mechanics has been applied in the design of the catenary risers. This technology enables the engineer to establish proper requirements on weld quality and inspection acceptance criteria to assure satisfactory structural integrity during its design life. It also provides guidance on proper design curves and a methodology for accounting for the effects of non-uniform stress distribution through the wall thickness. Still, there is inconsistency when designing tubular joints using a conventional S-N approach and when specifying weld flaw acceptance criteria using fracture mechanics approach. This study developed fatigue curves that are consistent with both the S-N approach and the fracture mechanics approach. Accounting for non-uniform stress distribution and threshold stress intensity factor were key parameters in relating both approaches. A series of S-N curves, generated from the fracture mechanics approach, were compared to the existing S-N curves. For flat plate butt joint, the S-N curve generated from fracture mechanics matches with the IIW class 100 curve when initial crack depth was 0.5 mm (0.02). The new curves for tubular joint agree very well with the experimental results. The comparison also indicated the degree of conservatism built into the API X design curve.

  • PDF

Butt Weldability for SS400 Using Laser-Arc Hybrid Welding (레이저-아크 하이브리드 용접을 이용한 SS400의 맞대기 용접 특성)

  • Kim, Jong Do;Myoung, Gi Hoon;Park, In Duck
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.40 no.7
    • /
    • pp.667-672
    • /
    • 2016
  • This study presents results of an experimental investigation of the laser-arc, hybrid, butt welding process of SS400 structural steel. Welding parameters including laser power, welding current and speed were varied in order to obtain one-pass, full-penetration welds without defects. The conditions that resulted in optimal beads were identified. After welding, hardness measurements and microstructure observations were carried out in order to study weld properties. The mechanical properties of both the base material and welded specimen were compared based on the results of tensile strength measurements. The yield and tensile strengths were found to be similar.

A Study of Weldability for Pure Titanium by Nd:YAG Laser(II) - Welding Properties of Butt Welding - (순티타늄판의 Nd:YAG 레이저 용접성에 관한 연구(II) - 맞대기 용접 특성 -)

  • Kim, Jong-Do;Kwak, Myung-Sub;Song, Moo-Keun;Park, Seung-Ha
    • Journal of Welding and Joining
    • /
    • v.27 no.6
    • /
    • pp.68-73
    • /
    • 2009
  • Recently, as titanium and titanium alloys are being increasingly used in wide areas, there are on-going researches to obtain high quality weld zone. In particular, growing interest is being drawn to laser welding, which involves low heat input and large aspect ratio in various welding processes and can facilitate shield in atmospheric condition compared with electron beam welding. The first report covered the analysis of embrittlement by the bead color of weld zone through quantitative analysis of oxygen and nitrogen and measurement of hardness as basic experiment to apply laser welding to titanium. Results indicated that the element that affect embrittlement the most was nitrogen, and as embrittlement and oxygenation go on, bead color changed to silver, gold, brown, blue and gray. This study performed butt welding of pure titanium and STS304 by using 1kW CW Nd:YAG laser, and to find out basic physical properties, evaluated welding performance by laser output, welding speed, root gap and misalignment etc, and examined mechanical properties through tensile stress and Erichsen test. The reason particles of pure titanium welded metal and HAZ are greater than STS304 is because they are pure metal and do not include many impure elements that work as nuclei in case of resolidification, thus becoming coarse columnar crystals eventually. In addition, the reason STS304 requires more energy during welding than pure titanium is because the particle size of base metal is smaller.

A study on surface fatigue crack behavior of SS400 welding Zone (SS400용접 부위의 표면 피로균열거동에 관한 연구)

  • 이용복;조남익;박강은
    • Proceedings of the KWS Conference
    • /
    • 1995.10a
    • /
    • pp.214-217
    • /
    • 1995
  • In order to investigate characteristics of surface fatigue crack propagation from a pit shaped surface defect which frequently exists near weld joints, SS400 steel with thickness of 12mm, which generally used for structure members, was submerged-arc welded with butt type and machined for both surface. The weld joints were devided into 5 regions, weld metal, boundary between heat affected zone (HAZ), HAZ, boundary between HAZ and base metal, and base metal. Specimens from each region were machined for a pit shaped initial surface defect with aspect ratio of 2. characteristics of surface fatigue crack por pagation from the defect under the same loading condition were compared and discussed.

  • PDF

Fatigue Properties of the Small Diameter Branch Welded Pipe Joint with variation of Welding Procedures and Welding Shapes. (용접공정 및 용접형상 변화에 따른 소구경 분기배관 용접부의 피로특성)

  • 백종현;김철만;김우식
    • Proceedings of the KWS Conference
    • /
    • 2003.11a
    • /
    • pp.191-193
    • /
    • 2003
  • S-N fatigue tests were conducted to investigate the fatigue strength of the small diameter socket and butt welded joints of carbon steels. Experimental parameters were pipe diameter, throat depth, shape of socket welds and welding procedure. Filler metals used in SMAW and GTAW procedure were E9016-G with diameter of 4.0 mm and ER70S-G with diameter of 2.4 m. API 5L Gr.B pipes were adopted as a small diameter branch pipes. All socket fittings were machined from ASTM A105 carbon steel. Fatigue strength in socket weld joints increased with increasing pipe diameter, area of weld metal and weld leg length of pipe side.

  • PDF

A Study on Fatigue Life of Weld Method for Excavator Bucket (굴삭기 버킷 용접부의 피로수명에 관한 연구)

  • Park, K.D.;Jung, J.W.
    • Journal of Power System Engineering
    • /
    • v.9 no.4
    • /
    • pp.102-109
    • /
    • 2005
  • An attachment part of the construction equipment frequently claimed from the crack occurrence that takes especially at the bucket. therefore we execute the fatigue examination and changes the welding method at the same materials. we executed a fatigue crack propagation experiment and got the conclusions at the normal temperature and Frequency 10Hz. We carried out butt welding for structure steel of SM490A and make three kinds of specimen of different weld method each. The fatigue limit of CASE 1 was determined to the low than CASE 2, CASE 3. the CASE 2 putting the interval of the 2mm creates back plate and make fatigue limit to high. Bead shapes and weld surfaces shape influence on fatigue life of materials. Specially, the crack growth becomes starting point that gap of back-plate and boundary surface of bead. It is confirmed by fracture showing on this study.

  • PDF

Laser weldability and mechanical behavior of hot rolled steels for hydroforming applications (하이드로포밍용 열연강재의 레이저 용접성 및 기계적 특성)

  • 이원범;이종봉
    • Proceedings of the KWS Conference
    • /
    • 2003.05a
    • /
    • pp.84-86
    • /
    • 2003
  • The laser welding and its analysis of thin-sheet carbon steels were carried out with high power CO$_2$1aser. Bead on plate welding of thin sheet was examined to investigate the effect of weld variables of laser welding, and to obtain optimum welding condition. Butt-welding was also carried out to show the effect of gap on the laser weldability of thin sheet. At high welding speed, the partial penetration was obtained by low heat input. Otherwise, porosity was formed in the bead at low weld speed because of too many heat input. The maximum gap tolerance on laser welding was observed to be about 0.2mm. This gap size has good relationship with beam size of laser spot(about 0.3mm). The formability of welded sheet was about 80% value of base metal and the gap size has not affected on the formability, although weld quality is dependent on the gap size.

  • PDF

Welding Residual Stress and Strength of Thick 9% Nickel Steel Plate (9% 니켈강 후판 용접부의 강도 및 잔류응력)

  • Kim, Young-Kyun;Kim, Young-Wann;Kim, Jae-Hoon
    • Journal of Power System Engineering
    • /
    • v.18 no.4
    • /
    • pp.85-90
    • /
    • 2014
  • In this paper, the transient thermal and residual stress analysis of the welding of 9% Ni steel plates using the FEA software ABAQUS are presented. The 9% Ni steel plates are welded manually with welding consumables of 70% Ni based Inconel type super-alloys (YAWATA WELD B (M)), producing a multi-pass/multi-layer butt weld. For these materials, temperature dependant mechanical and thermal material properties are used in the analysis. The back gouging is considered in welding process simulation. The FE thermal results are validated by comparing the real fusion profile and heat affected zone (HAZ). In addition, the continuous indentation test was conducted to measure the strength of base metal, HAZ and weld metal.

An Arc Sensor and Its Interface System for Welding Robots (용접로봇용 아크센서 및 인터페이스 시스템)

  • 오승준;김재웅
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.17 no.1
    • /
    • pp.76-82
    • /
    • 2000
  • An arc sensor system to compensate positional errors was developed on the foundation of sensor interface system to make use of the on-line shift function of industrial welding robot. Investigating the on-line shift function, we examine the quantitative relationship between the deviation from programmed path and the correction data transferred from personal computer to robot controller. The number of input parameters for weld seam tracking can be reduced by making the relationship between the deviation and the correction data during half weaving be the function of only cross time. With the results of weld seam tracking for the butt joint with V-groove and fillet joint of sheet metal, good performance was implemented. By developing the sensor interface system to compensate the positional errors, industrial welding robot can be expected to contribute to the promotion of welding automation.

  • PDF

Effect of Single Overload on the Fatigue Crack Growth Behavior of Laser Welded Sheet Metal (단일 과대하중에 의한 레이저 용접 판재의 피로균열 전파거동)

  • 곽대순;김석환;오택열
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.21 no.4
    • /
    • pp.161-169
    • /
    • 2004
  • In this study, we investigated fatigue crack growth behavior of laser welded sheet metal due to a single overload. Fatigue specimens were made using butt joint of cold rolled sheet metal that was welded by $CO_2$ laser. The fatigue crack propagation tests were performed in such a way that fatigue loading was parallel to the weld line while crack propagation was perpendicular to the weld line. Single overload was applied when fatigue crack tip was arrived near the weld line. The distances between the crack tip and the weld line at which a single overload was applied were 6, 4 and 2mm. The effect of specimen thickness and overload ratio on the fatigue behavior was determined. The plastic zone size of crack tip due to the single overload was determined from the finite element analysis. For investigating fatigue crack growth behavior, we used different thickness specimen 0.9mm and 2.0mm, and variable overload ratio applied fatigue crack propagation test. Also we used finite element analysis for investigating the plastic zone size of crack tip when single overload applied