2상 스테인리스강과 크롬동합금의 브레이징부 생성상의 생성기구에 관한 연구 (A Study on the Formation Mechanism of Microconstituents in Brazed Joint of Duplex Stainless Steel and Cr-Cu Alloy)

  • 김대업
    • Journal of Welding and Joining
    • /
    • 제19권5호
    • /
    • pp.534-539
    • /
    • 2001
  • The formation mechanism of microconstituents in brazed joints of duplex stainless steel and Cr-Cu alloy which is an essential process of rocket engine manufacturing was investigated using Cu base insert metal. $SUS329J_3L$ and C18200 were used for base metal and AMS 4764 was used for insert metal. The brazing was carried out under various conditions. There were various phases in the joints, because of reaction between liquid insert metal and base metals. Since liquid insert metal reacts with duplex stainless steel, liquid Cu from insert metal infiltrated into the $\alpha/\beta$ interface of duplex stainless steel. Through the process of Cu infiltration, isolated stainless steel pieces come into the liquid insert metal. Since liquid insert metal reacts with Cr-Cu alloy. Cr precipitates from C18200 come into the liquid insert metal. With increment of bonding temperature and holding time, amounts and sizes of phases increased. but Cr-Mn compounds decreased at 1303k for 1.2ks and Mn-rich phases disappeared Fe-Cr compounds formed.

  • PDF

기계적 합금화방법으로 만들어진 Ag계 삽입금속의 젖음성과 미세조직 (Wettability and Microstructures of Ag System Insert Metals Manufactured by Mechanical Alloying Method:)

  • 김광수;노기식;황선효
    • 한국재료학회지
    • /
    • 제11권12호
    • /
    • pp.1020-1027
    • /
    • 2001
  • Powder type Ag system insert metals were manufactured by mechanical alloying method. Alloying method was the ball milling process using zirconia ball media, and all alloying variables were constant except the milling time. The milling times were selected 24, 48 and 72 hours. The insert metals made by milling method were observed using scanning electron microscope and x-ray analyses. And also, the evaluation of wettability and microstructures of the insert metals were conducted to investigate the characteristics of the brazed joint. The wettability of the insert metals made by milling of 48 hours, was the best condition. And the insert metals contained Cd shows good wettability, however, there was the oxides residue on the brazing test specimen. The microstructures of the manufactured and the commercial insert metals were almost same displaying the Cu- rich proeutectic and Ag-rich eutectic. Further, there were some porosities. The 48 hours alloyed insert metal was exhibited the most sound brazed joint without containing porosity due to the superior wettability and good alloying condition.

  • PDF

구속 링을 이용한 관 결합 공정의 응력해석 (Stress Analysis of Pipe Connection Process Using Clamping Ring)

  • 양영수;배강열
    • 한국기계가공학회지
    • /
    • 제16권2호
    • /
    • pp.81-87
    • /
    • 2017
  • The pipe connection process using a clamping ring is used for joining small pipes in the refrigerator and air-conditioner industries instead of the brazing process, which induces inevitable thermal deformation in the pipes. However, few studies have been carried out on the process to select optimal parameters in joining pipes, and studies on the relation between the process parameters of the connection and connecting force of the joint have not been conducted. In this study, the connection process of pipes with the clamping ring was modeled using the finite element method (FEM) and analyzed to obtain the contact stress distribution between the pipes with which the connecting force of the joint was estimated. Considering the characteristics of pipe connection, the process was modeled and simulated in a two-dimensional axisymmetric solution domain. With the numerical model, the effect of ring shape on the connection was studied by adding a projection to the end of a ring or changing the length of a ring. The results of the analyses revealed that the contact stress distribution could be predicted with the suggested model. The effect of the ring shape was also presented. The effect of any combination of process parameters could be easily estimated through the related analyses.

Al2O3/Cu 접합에서 Metallizing paste의 조성이 접합강도에 미치는 영향 (The Effect of the Composition of Metallizing Paste on the Bonding Strength in the Joining of Al2O3/Cu to Cu)

  • 윤종혁;박현균
    • Journal of Welding and Joining
    • /
    • 제31권6호
    • /
    • pp.65-70
    • /
    • 2013
  • In joining Alumina to copper plate by Mo-Mn metallizing process, the effects of the composition of metallizing paste on the bonding strength were investigated. The bonding strength increased with increasing Mn amount in the paste up to 20% but followed by the decrease with addition of Mn. The maximum bonding strength reached 50MPa at 20%Mn when heated to $1550^{\circ}C$ for 60minute. The addition of Si to the metallizing powder increased the bonding strength of the joint by enhancing the mechanical bonding between the Alumina and the metallizing layer due to the decrease of layer viscosity with the addition of $SiO_2$. It is thought that MnO reacted with $Al_2O_3$ to yield $MnAl_2O_4$ spinel, forming a joint.

Ti합금 접합용 Ti-Cu-Ni-Si계 삽입금속의 개발에 관한 연구 (A study on the development of Ti-Cu-Ni-Si insert metal for Ti alloys)

  • 김경미;우인수;강정윤;이상래
    • Journal of Welding and Joining
    • /
    • 제14권1호
    • /
    • pp.47-56
    • /
    • 1996
  • The purpose of this study is to develope an insert metal which can be brazed at lower temperature than the conventionally used insert metal and provide higher strength joint than base metal. In the review of binary phase diagram concerning Ti, Cu and Ni resulted in the discovery of Si having eutectic composition with them. The microstructure and the distribution of elements in reaction zone between CP Ti and insert metal were investigated by Optical Microscopy, SEM/EDX, EPMA, X-RAY. The newly developed insert metal is Ti-15wt%Cu-18wt%Ni-2wt%Si, which can yield the lower brazing temperature(1183K) compared with the conventional Ti-Cu-Ni system insert metal. The joints with this insert metal had tensile strength of 385MPa in the bonding temperature range of 1183K to 1243K.

  • PDF

금속 표면 코팅된 $ZrO_2$와 Ti-6Al-4V의 접합 (Brazing of metal-coated $ZrO_2$ and Ti-6Al-4V)

  • 노명훈;정재필;김원중;김인호
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2011년도 춘계학술대회 및 Fine pattern PCB 표면 처리 기술 워크샵
    • /
    • pp.187-187
    • /
    • 2011
  • 지르코니아 ($ZrO_2$) 표면에 금속 (Au)으로 표면 코팅한 후 Ti-6Al-4V와 진공 브레이징 접합을 행하였다. 표면에 코팅한 Au 층의 영향을 비교 분석하기 위하여 Au를 코팅하지 않은 지르코니아도 모재로 사용하였다. 접합소재로는 Ag-Cu-Ti계 active filler를 사용하였다. $ZrO_2$/Ti-6Al-4V 브레이징 결과, active filler는 양측 모재 표면에 wetting 되었으며, Ti-6Al-4V 내부로 filler 확산으로 인하여 두 모재의 direct joint가 관찰되었다. 접합 계면 사이에 접합부 결함은 관찰되지 않았다.

  • PDF

은계(BAg) 삽입금속으로 접합된 초경합금 입자와 탄소강 브레이징부의 특성 (Characteristics of the Brazed Joint between Superhard Alloy Particles and Carbon Steel Using BAg System Insert Metals.)

  • 김광수;김상덕
    • 한국산학기술학회논문지
    • /
    • 제9권2호
    • /
    • pp.298-302
    • /
    • 2008
  • 초경합금입자와 탄소강사이의 브레이징 접합부 특성을 평가하였다 선택된 두 종류의 삽입금속은 기계적 합금 공정으로 만들어졌다. 한 가지는 Cu, Zn, Ag (MIM-1) 그리고 다른 한 가지는 Cu, Zn, Ag과 Cd(MIM-2)로 구성하였다. 삽입금속들의 화학조성은 AWS BAg-20계와 BAg-2a계의 성분과 유사하였다. 그리고 상용삽입금속들(CIM-1, CIM-2) 역시 비교 평가하였다. 삽입금속들의 특성은 젖음성 시험, 전단강도 시험, 그리고 미세조직 관찰로서 나타내었다. 젖음성 시험에서 MIM-1과 CIM-1 삽입금속의 젖음각이 MIM-2와 CIM-2보다 크게 나타났고, MIM-1의 젖음각이 CIM-1보다 더 큰 값을 나타났지만 모든 경우 젖음각이 $25^{\circ}$보다 작았다. 삽입금속, MIM-1이 가장 높은 전단강도를 나타냈고, 그 값은 $2.29{\times}10^2MPa$로 측정되었다. 이 값은 상용 삽입금속의 값과 같거나 높은 것으로 나타났다. 삽입금속의 미세조직은 Cu-rich 초정영역과 Ag-rich 공정영역으로 구성되었다. MIM-1계로 만들어진 초경합금과 탄소강의 접합부는 일부 접합부 계면에 기공을 포함하지만 초정을 기지로 하는 안정적인 미세조직을 나타냈다.

응력특이성계수에 의한 이종 접합재료의 강도평가 (Strength Evaluation of Bonded Dissimilar Materials by Using Stress Singularity Factor)

  • 정남용;오봉택
    • 대한기계학회논문집A
    • /
    • 제20권7호
    • /
    • pp.2087-2096
    • /
    • 1996
  • Recentrly advantages in composite and light weight material techniques have led to the increased use of bonded dissimilar materials such as ceramics/metal bonded joints, IC package, brazing, coating and soldering in the various industries. It is required to analyze the evaluation method of fracture strength and design methodology of bonded joints in dissimilar materials. Stress singularity according to changes of scarf angles for bonded scarf joints in dissimilar materials was investigated by the boundary element method and static experiments. In this paper, effect of the stress singularity factors at the interface edges of scarf joints on various dissmilar materials combinations were investigated by analysis of its stress and stress singularity index using 2-dimensional elastic program of boundary element method. And the variations of stress singularity index by changes for Young's modulus ratios of materials and scarf angles were investigated. Also, it is found that stress singularities at bonded interface edges are disappeared for certain combination of scarf angle in a pair of bonded dissimilar materials. As the results, it is proposed that the strength evaluation by using stress singularity factors, $\Gamma$, considering stress singularity at the interface edges of bonded dissimilar materials, is very useful.

분말 혼합 공정으로 만들어진 은계 삽입금속의 특성 (Characterisrics of the Ag System Insert Metal Produced by Powder Mixing Process)

  • 김광수;김상덕
    • 한국산학기술학회논문지
    • /
    • 제9권2호
    • /
    • pp.311-316
    • /
    • 2008
  • Ag계 분말 삽입금속을 볼 밀링법으로 제조하였다. 밀링공정의 변수들은 밀링시간을 제외하고는 일정하게 하였고 밀링 시간은 24, 48, 72시간들로 정하였다. 밀링에 의해 제조된 삽입금속들은 SEM관찰, DSC분석, 퍼짐성, 젖음성 시험을 통해 평가하였다. 삽입금속들의 브레이징부 특성은 상용금속에 비하여 우수하였다. 48시간 동안 밀링한 삽입금속이 퍼짐성과 젖음 특성이 가장 우수한 조건임을 나타냈다. 또한 브레이징부는 작은 양의 기공을 포함하고 있지만 안정적인 미세조직을 보였고 미세경도는 138VHN으로 나타났다.

AlN 세라믹스와 금속간 계면접합에 관한 연구 : I. AlN/Cu 및 AlN/W 활성금속브레이징 접합체의 잔류응력 해석 (A Study on the Interfacial Bonding in AlN Ceramics/Metals Joints: I. Residual Stress Analysis of AlN/Cu and AlN/W Joints Produced by Active-Metal Brazing)

  • 박성계;이승해;김지순;유희;염영진
    • 한국재료학회지
    • /
    • 제9권10호
    • /
    • pp.962-969
    • /
    • 1999
  • Ag-Cu-Ti 삽입금속을 이용하여 제조된 AlN/Cu와 AlN/W 활성금속브레이징 접합체의 잔류응력을 유한요소법으로 탄성 및 탄소성 해석을 행하여 그 결과를 접합강도 측정 결과와 파단 거동 관찰 결과와 비교, 분석하였다. 최대 잔류 주응력의 크기는 AlN/W 접합체보다 모재간 열팽창계수 차이가 큰 AlN/Cu 접합체에서 더 크게 나타났으며, 접합계면에 인접한 AlN 세라믹스 자유표면에 인장 성분의 응력집중이 확인되었다. 모재와 삽입금속의 탄소성 변형을 모두 고려할 경우, AlN/Cu 접합체의 경우 연질의 삽입금속에 의해 최대 잔류 주응력이 감소하여 소성변형에 의한 응력완화 효과가 있음을 확인하였으나, 100$\mu\textrm{m}$ 이상으로 삽입금속 두께를 증가시키더라도 잔류 주응력의 크기는 더 이상 크게 감소하지 않았다. 측정된 최대 접합강도는 AlN/Cu와 AlN/W 접합체에서 각각 52 MPa와 108 MPa이었으며, 파단 형태는 AlN/Cu 접합체는 AlN 자유표면으로부터 AlN 내부로 큰 각도를 이루면 진행되는 돔형의 파단이, AlN/W 접합체에서는 접합계면의 삽입금속층을 따라 AlN 측에서 파단이 일어나는 형태를 보였다.

  • PDF