• 제목/요약/키워드: Bottom electrode

검색결과 349건 처리시간 0.022초

Ru CMP Slurry의 개발 및 특성평가 (Development and Characterization of Ru CMP Slurry)

  • 김인권;권태영;박진구;박형순
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.57-58
    • /
    • 2006
  • In MIM (metal insulator metal) capacitor, Ru (ruthenium) has been suggested as new bottom electrode due to its excellent electrical performance, a low leakage of current and compatibility to the high dielectric constant materials. In this case of Ru bottom electrode, CMP (chemical mechanical planarization) process was needed m order to planarize and isolate the bottom electrode. In this study, the effect of chemical A on polishing and etching behavior was investigated as functions of chemical A concentration, abrasive particle and pressure. Chemical A was used as oxidant and etchant. The thickness of passivation layer on the treated Ru surface increased with the increase of chemical A concentration. The etch rate and removal rate of Ru were increased by the addition of chemical A. The removal rate was highest m slurry of pH 9 with the addition of 0.1 M chemical A and 2 wt% alumina at 4 psi. The maximum removal rate is about 80 nm/min.

  • PDF

Fabrication of a Bottom Electrode for a Nano-scale Beam Resonator Using Backside Exposure with a Self-aligned Metal Mask

  • Lee, Yong-Seok;Jang, Yun-Ho;Bang, Yong-Seung;Kim, Jung-Mu;Kim, Jong-Man;Kim, Yong-Kweon
    • Journal of Electrical Engineering and Technology
    • /
    • 제4권4호
    • /
    • pp.546-551
    • /
    • 2009
  • In this paper, we describe a self-aligned fabrication method for a nano-patterned bottom electrode using flood exposure from the backside. Misalignments between layers could cause the final devices to fail after the fabrication of the nano-scale bottom electrodes. A self-alignment was exploited to embed the bottom electrode inside the glass substrate. Aluminum patterns act as a dry etching mask to fabricate glass trenches as well as a self-aligned photomask during the flood exposure from the backside. The patterned photoresist (PR) has a negative sidewall slope using the flood exposure. The sidewall slopes of the glass trench and the patterned PR were $54.00^{\circ}$ and $63.47^{\circ}$, respectively. The negative sidewall enables an embedment of a gold layer inside $0.7{\mu}m$ wide glass trenches. Gold residues on the trench edges were removed by the additional flood exposure with wet etching. The sidewall slopes of the patterned PR are related to the slopes of the glass trenches. Nano-scale bottom electrodes inside the glass trenches will be used in beam resonators operating at high resonant frequencies.

$Sr_{0.8}Bi_{2.4}Ta_2O_9/Pt/Si$ 구조의 수소열처리에 의한 강유전특성 열화에 미치는 W-N/Pt 전극효과 (Effects of W-N/Pt Bottom Electrode on the Ferroelectric Degradation of $Sr_{0.8}Bi_{2.4}Ta_2O_9/Pt/Si$ Structure due to the Hydrogen Annealing)

  • 이창우
    • 마이크로전자및패키징학회지
    • /
    • 제11권4호
    • /
    • pp.87-91
    • /
    • 2004
  • [ $Sr_{0.8}Bi_{2.4}Ta_2O_9(SBT)/Pt$ ] 구조에서 $350^{\circ}C$ 온도로 수소열처리에 의한 강유전특성 열화를 방지하기 위한 W-N/Pt 하부전극의 효과를 살펴보았다. 그 결과 Pt와 SBT 박막사이에 증착된 W-N박막에 의해 수소의 확산을 차단할 수 있었다. Pt 표면에서 수소원자가 화학적인 흡착이 일어나지 않음으로써 흡착된 수소가 SBT 박막내의 산소와 결합하게 됨으로써 oxygen deficiency가 발생하는 것을 막을 수 있었다. W-N 박막이 양호한 확산방지막으로 작용하여 강유전특성의 열화현상을 방지 할 수 있었다.

  • PDF

하부전극 변화에 따른 PZT 박막 특성에 관한 연구 (The effects of PZT thin film capacitor with various bottom electrode)

  • 박영;정규원;임승혁;송준태
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 하계학술대회 논문집 D
    • /
    • pp.1986-1988
    • /
    • 1999
  • Ferroelectric lead zirconate titanate(PZT) thin films were prepared on various bottom electrodes by rf magnetron sputtering methode. The structural phase and surface morphology of the PZT thin films were largely affected by the bottom electrodes. P-E curves of PZT thin films deposited on Pt. $RuO_2$ and Ru/$RuO_2$ bottom electrode showed typical P-E hysteresis loop. The measure values of $P_r,\;E_c$ of the Ru/PZT/Ru/$RuO_2$ capacitor were $16.9{\mu}C/Cm^2$, 140kV/ cm, respectively. The Ru/PZT/Ru/$RuO_2$ capacitors were fatigue free uP to nearly $10^9$ switching cycle but Pt/PZT/Pt capacitor showed 34% degradation uP to $10^9$ switching cycle.

  • PDF

체적 탄성파 공진기의 하부 전극이 압전 박막의 배향성 및 공진기의 압전 특성에 미치는 영향 (Effects of bottom electrodes on the orientation of piezoelectric thin films and the frequency response of resonators in FBARs)

  • 이명호;정준필;이진복;박진석
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2002년도 하계학술대회 논문집 C
    • /
    • pp.1397-1399
    • /
    • 2002
  • Effects of bottom electrode materials (Al, Cu, Ti, and Mo), included in film bulk acoustic resonators (FBARs), on the orientation of piezoelectric AlN thin films and the frequency response characteristic of resonators were investigated. The texture coefficient (TC) for (002) orientation, crystallite size, full width half maximum (FWHM), and surface roughness of deposited AlN films were measured for the various bottom electrodes. The return tosses estimated from the frequency responses of fabricated resonators were also compared. Experimental results showed that the difference of lattice constant and thermal expansion coefficient between the bottom electrode and the AlN film were the most important factors for achieving a high performance resonator.

  • PDF

전극 구조에 따른 유기 트랜지스터 특성 (Organic Transistor Characteristics with Electrode Structures)

  • 이붕주
    • 한국전자통신학회논문지
    • /
    • 제8권1호
    • /
    • pp.93-98
    • /
    • 2013
  • 본 논문에서는 유기박막트랜지스터용 절연막에 활용코자 플라즈마 중합방법을 이용하여 PMMA 절연막을 제작하였다. 유기트랜지스터 성능향상을 위해 전극구조에 따른 특성을 파악하고자 트랜지스터의 이동도 및 출력특성을 본결과, 상부전극구조의 경우 최대 이동도는 $8{\times}10^{-3}[cm^2V^{-1}s^{-1}]$을 보이고 하부전극구조의 경우 $2{\times}10^{-4}[cm^2V^{-1}s^{-1}]$의 낮은 이동도 값을 얻었으며, 하부전극구조의 경우 off current값이 증가되는 특성을 볼 수 있다. 그러므로 유기트랜지스터의 전극구조는 상부전극 방식이 좋은 것 알 수 있었다.

폴리이미드 용량형 습도센서의 전극 패턴에 따른 감습 특성 (Humidity Sensitive Characterization by Electrode Pattern on the Capacitive Humidity Sensor Using Polyimide)

  • 박성백;신훈규;임준우;장상목;권영수
    • 한국전기전자재료학회논문지
    • /
    • 제27권9호
    • /
    • pp.566-570
    • /
    • 2014
  • Electrode pattern effects on the capacitive humidity sensor were investigated. The fabrication of the capacitive humidity sensor was formed with three steps. The bottom electrode was formed on the silicon substrate with Pt/Ti thin layer by using shadow mask and e-beam evaporator. The photo sensitive polyimide was formed on the bottom electrode by using photolithography process as a humidity sensitive thin film. The upper electrode was formed on the polyimide thin film with Pt/Ti thin layer by using e-beam evaporator and lift-off method. Three electrode patterns, such as circle, square, and triangle pattern, were used and changed the sizes to investigate the effects. The capacitances of the sensors were decreased 622 to 584 pF with the area decreament of patterns 250,000 to $196,250{\mu}m^2$. From these results, a capacitive humidity sensor with photo sensitive polyimide is expected to be applied to a high sensitive humidity sensor.

Reference Electrode for Monitoring Cathodic Protection Potential

  • Panossian, Z.;Abud, S.E.
    • Corrosion Science and Technology
    • /
    • 제16권5호
    • /
    • pp.227-234
    • /
    • 2017
  • Reference electrodes are generally implemented for the purpose of monitoring the cathodic protection potentials of buried or immersed metallic structures. In the market, many types of reference electrodes are available for this purpose, such as saturated calomel, silver/silver chloride and copper/copper sulfate. These electrodes contain a porous ceramic junction plate situated in the cylindrical body bottom to permit ionic flux between the internal electrolyte (of the reference electrode) and the external electrolyte. In this work, the copper/copper sulfate reference electrode was modified by replacing the porous ceramic junction plate for a metallic platinum wire. The main purpose of this modification was to avoid the ion copper transport from coming from the inner reference electrode solution into the surrounding electrolyte, and to mitigate the copper plating on the coupon surfaces. Lab tests were performed in order to compare the performance of the two mentioned reference electrodes. We verified that the experimental errors associated with the measurements conducted with developed reference electrode would be negligible, as the platinum surface area exposed to the surrounding electrolyte and/or to the reference electrolyte are maintained as small as possible.

상부전극에 따른 상변화 메모리의 발열 특성 (Thermal characteristic of PRAM with top electrode)

  • 최홍규;장낙원;김홍승;이성환;마석범
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.97-98
    • /
    • 2007
  • In this paper, we analyzed the reset current variation of PRAM device with top electrode using the 3-D finite element analysis tool. As thickness of phase change material thin film decreased, reset current caused by phase transition highly increased. Joule's heat which was generated at the contact surface of phase change material and bottom electrode of PRAM was given off through top electrode to which was transferred phase change material. As thermal conductivity of top electrode decreased, heating temperate was increased.

  • PDF

Increased Sensitivity of Carbon Nanotube Sensors by Forming Rigid CNT/metal Electrode

  • 박대현;전동렬
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제41회 하계 정기 학술대회 초록집
    • /
    • pp.348-348
    • /
    • 2011
  • Carbon nanotube (CNT) field effect transistors and sensors use CNT as a current channel, of which the resistance varies with the gate voltage or upon molecule adsorption. Since the performance of CNT devices depends very much on the CNT/metal contact resistance, the CNT/electrode contact must be stable and the contact resistance must be small. Depending on the geometry of CNT/electrode contact, it can be categorized into the end-contact, embedded-contact (top-contact), and side-contact (bottom-contact). Because of difficulties in the sample preparation, the end-contact CNT device is seldom practiced. The embedded-contact in which CNT is embedded inside the electrode is desirable due to its rigidness and the low contact resistance. Fabrication of this structure is complicated, however, because each CNT has to be located under a high-resolution microscope and then the electrode is patterned by electron beam lithography. The side-contact is done by depositing CNT electrophoretically or by precipitating on the patterned electrode. Although this contact is fragile and the contact resistance is relatively high, the side-contact by far has been widely practiced because of its simple fabrication process. Here we introduce a simple method to embed CNT inside the electrode while taking advantage of the bottom-contact process. The idea is to utilize a eutectic material as an electrode, which melts at low temperature so that CNT is not damaged while annealing to melt the electrode to embed CNT. The lowering of CNT/Au contact resistance upon annealing at mild temperature has been reported, but the electrode in these studies did not melt and CNT laid on the surface of electrode even after annealing. In our experiment, we used a eutectic Au/Al film that melts at 250$^{\circ}C$. After depositing CNT on the electrode made of an Au/Al thin film, we annealed the sample at 250$^{\circ}C$ in air to induce eutectic melting. As a result, Au-Al alloy grains formed, under which the CNT was embedded to produce a rigid and low resistance contact. The embedded CNT contact was as strong as to tolerate the ultrasonic agitation for 90 s and the current-voltage measurement indicated that the contact resistance was lowered by a factor of 4. By performing standard fabrication process on this CNT-deposited substrate to add another pair of electrodes bridged by CNT in perpendicular direction, we could fabricate a CNT cross junction. Finally, we could conclude that the eutectic alloy electrode is valid for CNT sensors by examine the detection of Au ion which is spontaneously reduced to CNT surface. The device sustatined strong washing process and maintained its detection ability.

  • PDF