Synthesis and Property Evaluation of Bio-adhesives Using Peach Gum(桃膠) (도교(桃膠)를 이용한 바이오 접착제의 합성 및 물성 평가)

  • Park, Min-Seon;Oh, Seung-Jun;Wi, Koang-Chul
    • Journal of Conservation Science
    • /
    • v.37 no.3
    • /
    • pp.282-288
    • /
    • 2021
  • This basic research was conducted to support the development of woodcraft bio-adhesives using peach gum, which is the resin produced by peach trees. The synthesis conditions of these adhesives were optimized by performing 144 experiments. The application potential of peach gum adhesives was explored by comparing their properties with those of three natural adhesives and four synthetic adhesives. The best adhesive strength was obtained by dissolving the resin in 80 mL of distilled water containing 1.5 g NaOH, 1.65 g H2O2 ( pH 8.0-9.0), 0.5 g NaClO, and 0.5 g H2BO2. The adhesive strength, which showed minimal changes and excellent reversibility, was 125.39 kgf/cm2. Ultraviolet radiation-mediated deterioration in strength in the absence of total aerobic bacteria was negligible (△E*ab = 2.75). These data confirm the potential value of peach gum-based bio-adhesives for woodcraft as well as their utility as alternatives for natural and synthetic adhesives used for the manufacture and restoration of handicrafts and preservation of cultural assets.

Adhesion Performances of Natural Adhesives Made by Rosin (로진을 이용한 천연접착제의 접착물성)

  • Choi, Jae-Hoon;Hwang, Hyeon-Deuk;Moon, Je-Ik;Kim, Hyun-Joong;Yeo, Hwanmyeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.35 no.4
    • /
    • pp.38-44
    • /
    • 2007
  • As environmental issues is important thing, our study aims to develop natural adhesives made by rosin instead of synthesis adhesive with the formaldehyde emission. Natural adhesives were formulated to enhance curing speed and adhesion performances with various drying agent contents. Adhesion performances were evaluated with tack values measured by texture analyzer and shear strengths determined by single lap shear test. The adhesion performances of nature adhesives developed in this study and compared with those of overseas natural adhesives made by AURO, BioFa, Livos. Optimum drying agent formulation was Co 0.7 part, Zr 1.0 part, Ca 0.5 part, and Activ8 0.1 part. Shear strength of the adhesives manufactured by the optimum drying agent formulation was $93.2{\pm}19.1N/cm^2$.

Synthesis and Characterization of Water-borne Pressure Sensitive Adhesives Polymerized using Styrenated Phenol Type Surfactants (스티렌페놀계 계면활성제 기반 친환경 수계 점착제 합성 및 특성 분석)

  • Song, Young Kyu;Lee, Sang-Ho;Park, Young Il;Kim, Jin Chul
    • Journal of Adhesion and Interface
    • /
    • v.21 no.4
    • /
    • pp.156-161
    • /
    • 2020
  • Waterborne pressure sensitive adhesives (PSA) has been received much attentions from both academia and industries as an environmental friendly-technology because it can significantly reduce use of hazardous organic volatile solvents. However, in the process of the mass production of waterborne PSAs, hazardous phenol type amphiphilic compounds have essentially been used as surfactants for the emulsion polymerization. For the reason, tremendous research efforts have been made to develop environment-friendly organic surfactant which can replace the phenol type surfactants. In this study, we verify the potential of a new class of surfactants based on the styrenated phenol derivatives as an alternative to the phenol type surfactants.

The Scattering Beam Measurement of the RBC and the Fabrication of the Micro Cell Biochip (적혈구의 산란빔 측정과 마이크로 세포 분석 바이오칩 제작)

  • Byun, In Soo;Kwon, Ki Jin;Lee, Joon Ha
    • Progress in Medical Physics
    • /
    • v.25 no.2
    • /
    • pp.116-121
    • /
    • 2014
  • Next future, The bio technology will be a rapidly developing. This paper is the scattering beam measurement of the red blood cell (RBC) and the fabrication of the micro cell biochip using the bio micro electro mechanical system (Bio-MEMS) process technology. The Major process method of Bio-MEMS technology was used the buffered oxide etchant (BOE), electro chemical discharge (ECD) and ultraviolet sensitive adhesives (UVSA). All experiments were the 10 times according to the process conditions. The experiment and research are required the ultraviolet expose, the micro fluid current, the cell control and the measurement of the output voltage Vpp (peak to peak) waveform by scattering angles. The transmitting and receiving of the laser beam was used the single mode optical fiber. The principles of the optical properties are as follows. The red blood cells were injected into the micro channel. The single mode optical fiber was inserting in the guide channel. The He-Ne laser beam was focusing in the single mode optical fiber. The transmission He-Ne laser beam is irradiating to the red blood cells. The manufactured guide channel consists of the four inputs and the four outputs. The red blood cell was allowed with the cylinder pump. The output voltage Vpp waveform of the scattering beam was measured with a photo detector. The receiving angle of the output optical fiber is $0^{\circ}$, $5^{\circ}$, $10^{\circ}$, $15^{\circ}$. The magnitude of the output voltage Vpp waveform was measured in the decrease according to increase of the reception angles. The difference of the output voltage Vpp waveform is due differences of the light transmittance of the red blood cells.

Comparison of Formaldehyde Emission of Wood-based Panels with Different Adhesive-hardener Combinations by Gas Chromatography and Standard Methods

  • Eom, Young Geun;Kim, Sumin;Baek, In-Chan;Kim, Hyun-Joong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.33 no.2 s.130
    • /
    • pp.29-39
    • /
    • 2005
  • Formaldehyde emissions from wood-based panels bonded with pine and wattle tannin-based adhesives, urea-formaldehyde resin (UF), melamine-formaldehyde resin (MF), and co-polycondensed resin of urea-melamine-formaldehyde (UMF) were measured by the Japanese standard method using a desiccator (JIS A 1460) and the EN 120 (European Committee For Standardization, 1991) method using the perforator value. In formaldehyde emission, all particleboards made using the wattle tannin-based adhesive with three different hardeners, paraformaldehyde, hexamethylenetetramine, and tris(hydroxyl)nitromethan (TN), satisfied the requirements of grade $E_1$. But only those made using the pine tannin-based adhesive with the hexamine as hardener met the grade $E_1$ requirements. Hexamine was effective in reducing formaldehyde emission in tannin-based adhesives when used as the hardener. While the UF resin showed a desiccator value of $7.1mg/{\ell}$ and a perforator value of 12.1 mg/100 g, the MF resin exhibited a desiccator value of $0.6mg/{\ell}$ and a perforator value of 2.9 mg/100 g. According to the Japanese Industrial Standard and the European Standard, the formaldehyde emission level of the MDF panels made with UF resin in this study came under grade $E_2$. The formaldehyde emission level was dramatically reduced by the addition of MF resin. The desiccator and perforator methods produced proportionally equivalent results. Gas chromatography, a more sensitive and advanced method, was also used. The samples for gas chromatography were gathered during the experiment involving the perforator method. The formaldehyde contents measured by gas chromatography were directly proportional to the perforator values.