• 제목/요약/키워드: Bi-2223 Wire

검색결과 54건 처리시간 0.024초

1MW 고온초전도 동기모터의 개념설계 고찰 (Conceptual Design Considerations of 1MW Class HTS Synchronous Motor)

  • 백승규;손명환;이언용;권영길;문태선;박희주;김영춘
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제6권3호
    • /
    • pp.38-43
    • /
    • 2004
  • 1MW class superconducting synchronous motor is designed considering several conditions such as superconducting wire length, machine efficiency and size. As the machine is larger and larger, the superconducting machine shows the advantages more and more over the conventional machines. Although the advantages at 1MW rating are not so great, the design approach to get an appropriate result would be very helpful for larger superconducting synchronous machine design. Major design concerns are focused on reducing expensive Bi-2223 HTS(High Temperature Superconducting) wire which is used for superconducting field coil carrying the rating current around 30K(-243$^{\circ}C$) while the machine efficiency is higher than conventional motors or generators with the same rating. Furthermore, some iron cored structure is considered to reduce the HTS wire requirement without bad effect on machine performances such as sinusoidal armature voltage waveform, synchronous reactance and so on.

BSCCO 초전도 선재의 미세조직 및 임계전류밀도에 미치는 공정변수 효과 (Effect of Processing Variables on Microstructure and Critical Current Density of BSCCO Superconductors Tape)

  • 지봉기;김태우;주진호;김원주;이희균;홍계원
    • 한국전기전자재료학회논문지
    • /
    • 제11권11호
    • /
    • pp.1014-1021
    • /
    • 1998
  • We evaluated the effect of processing variables on microstructural evolution interface irregularity between Ag sheath and superconductor core and resultant critical current density(J$_{c}$) of (Bi,Pb)$_2$Sr$_2$Ca$_2$Cu$_3$O$_{x}$(2223) superconductor tape. The value of J$_{c}$ was significantly influenced by the interface irregularity, degree of texturing and relative 2223 content. The interface became more irregular(sausage effect), while the degree of texturing gradually improved as the dimension of tape decreased during forming process. As the dimension of wire/tape were changed from diameter of 3.25 mm to thickness of 0.20 mm, J$_{c}$ value was observed to be increased by 10 times. In addition, optimum sintering temperature for improved J$_{c}$ was observed to be 835$^{\circ}C$ in a ambient atmosphere probably due to combined effect of both improved texturing and high 2223 content. Microstructural investigation showed the degree of texturing was degraded by the existence of both second phases and interface irregularity. It was observed that larger grain size and better texturing was developed near relatively flat interface compared to those inside superconducting core.ting core.

  • PDF

고온초전도 PIT 장선재 제조 및 특성 평가 (Fabrication and evaluation of superconducting properties of HIS PIT long tapes)

  • 하홍수;이동훈;양주생;황선역;최정규;김상철;하동우;오상수;권영길
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.1
    • /
    • pp.597-600
    • /
    • 2003
  • Bi-2223/Ag HTS wires have been fabricated by the PIT(powder in tube)process. Intermediate annealing was carried out to increase the homogenization and uniformity of the superconducting filaments embedded in the silver matrix during the deformation process that is important to sustain the engineering critical current density in long superconducting wire. Intermediate annealing act to release the deformation hardening of the superconducting wires during drawing process. Rolling parameters were investigated to roll the superconducting tapes with uniform thickness, width and winding tensions. Critical current of 60 m long superconducting tapes was measured 54.3 A continuously after final sintering heat treatment. The phase analysis of Bi-2223/Ag superconducting tapes are examined by the XRD.

  • PDF

250 m 급 Bi-2223/Ag 고온 초전도선재 제조 (Fabrication of 250 m class Bi-2223/Ag HTS Tapes)

  • 하홍수;오상수;하동우;장현만;김상철;송규정;박찬;권영길;류강식
    • Progress in Superconductivity
    • /
    • 제3권1호
    • /
    • pp.130-133
    • /
    • 2001
  • A multifilamentary Bi-2223 HTS tape for superconducting power applications was studied through the fabrication of 250-meter long tapes by the PIT(powder in tube) process. To fabricate continuous long wire, a drawing machine, a two-drum bull block and a rolled tape winding machine were developed. Especially, 250-meter long tapes were heat treated in the shape of pancake coil to reduce the heat affect zone and to achieve the high critical current. Engineering critical current density was improved through both the enhancements of critical current density by control of thermal process and the increase of filling factor by using thin Ag alloy sheath tubes less than 1.5 mm in thickness. We have made successfully 250-meter long 37 filamentary tapes with high filling factor up to 31 % employing the modified drawing and rolling technique. The critical current of 250-meter long tapes with pancake coil type was measured by transport method at self-field up to 250 gauss of center field. The measured values, based on the transport critical current at self-field, $I_{c}$ -B characteristics and magnetic field analysis, are 34 A of I$_{c}$ and 4.0 $kA/\textrm{cm}^2$ of $J_{e}$ at 250 m, 77 K, and 0 T. We also have achieved the 56 A of I$_{c}$ and 7.0 $0 kA/\textrm{cm}^2$ of$ J_{e}$ in short tapes at 77K, self-field, and 1$mutextrm{V}$/cm.

  • PDF

고온 초전도 tape의 임계전류 저하에 따른 교류손실 특성 (AC loss Characteristics under Critical Current Degradation of HTS Tapes)

  • 김해준;조전욱;김재호;심기덕;곽동순;배준한;김해종;성기철
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제7권3호
    • /
    • pp.29-33
    • /
    • 2005
  • Critical current$(I_c)$ degradation of High $T_c$ Superconducting(HTS) tapes and AC loss under mechanical load is one of the hottest issues in HTS development and application. Mechanical load reduces the critical current of superconducting wire, and the $I_c$ degradation affects the AC loss of the wire. We measured the $I_c$ degradation and AC loss under tension and bending of Bi-2223 tapes made by 'Powder-in-Tube' technique at 77K with self-field. Also, we have studied the frequency characteristics on self-field AC loss in multi-filamentary Bi-2223/Ag tape at 77K. The measurement results and discussions on the relationship between $I_c$ degradation and AC loss are presented.

고온 초전도체의 임계전류 저하에 따른 교류 손실 특성 (Ac Loss Characteristics under Critical Current Degradation of HTS Tapes)

  • 김해준;김재호;심기덕;조전욱;곽동순;김해종;성기철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.286-287
    • /
    • 2005
  • Critical current(Ic) degradation of HTS tapes and AC loss under mechanical load is one of the hottest issues in HTS development and application. Mechanical load reduces the critical current of superconducting wire, and the Ie degradation affects the AC loss of the wire. We measured the Ie degradation and AC loss under tension and bending of Bi-2223 tapes processed by "Powder-in-Tube" technique at 17K with self-field. And we have studied the frequency dependence of self-field AC loss in multi-filamentary Bi-2223/Ag tape at 77K. The measurement results and discussions on the relationship between Ic degradation and AC loss are presented.

  • PDF

초전도 선재에서 초기 충진압력과 테이프화를 위한 가압이 임계특성에 미치는 영향 (The effects of initial packing pressure and repressure for tape type on critical properties of superconducting wire)

  • 최효상;한태희;박성진;한병성
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제6권5호
    • /
    • pp.446-453
    • /
    • 1993
  • 초기충진압력이 서로 다른 시편에 가한 가압횟수와 열처리시간의 혼합공정이 임계전류밀도 특성에 미치는 영향을 관찰하기 위하여 power-in-tube방법으로 초전도 선재를 제조하였다. 일정 초기충진압력에서 테이프화를 위한 열처리 및 가압이 혼합공정횟수가 증가할수록 임계전류밀도가 증가하였다. 초기충진압력이 1000kg/$cm^{2}$에서 Bi-2223 고온상 체적비가 가장 높게 나타났고 결정립이 판상으로 성장되었을 뿐만 아니라 C축과 직각방향으로 잘 배양되어 있음을 관찰할 수 있었다. 특히 초기충진압력 1000kg/$cm^{2}$의 시편을 두께를 줄이기 위하여 3회 가압하고 450시간 열처리하였을때 임계전류밀도가 5800A/$cm^{2}$를 나타내었으며 이를 중심으로 500, 2500kg/$cm^{2}$이 양측단으로 가우시안분포를 보였다. 결론적으로 시편의 임계특성은 적정 초기충진압력, Bi-2223 고온상 체적비, 테이프화를 위한 가압횟수, 결정의 일방향배열, 결정립의 성장등에 강하게 의존함을 알 수 있었다.

  • PDF

Billet 장입 방식을 이용 제조한 Bi(Pb)-Sr-Ca-Cu-O 초전도 선재의 특성 (Characteristics of Bi(Pb)-Sr-Ca-Cu-O Superconductor Wire Fabricated using the Billet Insertion Method)

  • 장건익;유재근;홍계원
    • 한국세라믹학회지
    • /
    • 제33권4호
    • /
    • pp.471-477
    • /
    • 1996
  • During Bi(Pb)-Sr-Ca-Cu-O superconductor wire fabrication the effect of the initial packing density on the final characteristics of superconductor wire was systematically studied. To increase the powder packing density with uniform distribution of superconducting core a billet insertion method processed by CIP was applied instead of the commonly used vibration and ramming method of powder insertion into silver sheath. Compared with the vibration and ramming method the billent insertion technique processed by CIP cause the 30% incre-specimen with 130${\mu}{\textrm}{m}$(core thickness : 45 ${\mu}{\textrm}{m}$)and 5.24 mm width processed at 84$0^{\circ}C$for 200hrs. shows specimen with 130${\mu}{\textrm}{m}$ (core thickness ; 45${\mu}{\textrm}{m}$)and 5.24 mm width processed at 84$0^{\circ}C$ for 200 hrs. shows maximum 34A for Ic and 16, 700 A/cm2 for Ic measured at 77K and 0T. Also the sample rolled 3 times shows maximum 7, 2A for Ic and 11, 000 A/cm2 for 77K and 0T. Based on X-ray experimental results the formation of Bi-2223 and texture were significantly well developed at the interface between the superconducting core and silver sheath as compared with those of the interior area of superconducting core.

  • PDF

Ag-sheath Bi-2223 고온 초전도 선재 AC 손실 해석에 따른 설계 및 제작 (The Design and Manufature by Analysis of AC Loss of high temperature supercondutor wire of Ag-sheath Bi-2223)

  • 장미혜;추용;이준영;고태국
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 하계학술대회 논문집 A
    • /
    • pp.349-352
    • /
    • 1998
  • In future superconducting electrical machines and device. AC loss in the superconducting windings are one of the most impotent design paramenters. This paper descriptions a series of Characteristic of a high-Tc superconducting Bi-Pb-Sr-Ca-Cu-O Ag-sheathed filament. In the case simulation and design to reduce ac loss is considered the filament number, twitch pith number and diameter of filament. A filament sample with Tc of 78K is made by $835^{\circ}C$ sintering for 50h and $0.33^{\circ}C$/min heating rate in an atmosphere. The experiment observations are compared with self-field loss and AC losses of Bi-Pb-Sr-Ca-Cu-O filament at 77K in following environments ; (i)AC external parallel magnetic field in different frequencies. And an analytical expression of the loss the derivation of transposition from an optimum condition was derived for the external AC magnetic field, theoretical predictions were found to coincide with the experimental observations.

  • PDF