• 제목/요약/키워드: Bi-2223/Ag superconducting tape

검색결과 69건 처리시간 0.025초

고온 초전도체 테이프의 상전도 영역 전파 특성 해석 (Analysis of normal Bone propagation characteristics in a high-temperature superconducting tape)

  • 정신근;설승윤
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제3권1호
    • /
    • pp.11-15
    • /
    • 2001
  • Stability of a Bi-2223/Ag tape was studied by using a numerical model considering the temperature distribution of cross-sectional area. The dynamic evolution of normal zone of a HTS tape can be shown by the developed two-dimensional Program using finite difference method. Two kinds of analyses are compared to quantify the critical disturbance energy for quenching HTS tapes. One is the length-thickness(x-r) side and the other is the length-width(x-z) side. For each case. the governing energy balance equations and corresponding boundary conditions are formulated. The results of analyses shows that the critical disturbance energies for each cases seem to be very close for considered Bi-2223/Ag tape .

  • PDF

Hard bending시 Bi-2223 초전도테이프의 임계전류 열화 거동 (The Ic degradation behavior in Bi-2223 superconducting tapes during hard bending)

  • 신형섭;최수용;고동균;하홍수;하동우;오상수
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2002년도 학술대회 논문집
    • /
    • pp.144-148
    • /
    • 2002
  • Influences of bending strain on the critical current (I$_{c}$) were investigated in Bi-2223 superconducting tapes at 77K. The effect of bending mode on the I$_{c}$ degradation behavior was discussed in viewpoints of test method, n-value and damage morphology. Especially, in this paper, we reported the I$_{c}$ behavior in Ag alloy/Bi-2223 multifilamentary super- conducting tapes under bending occurred within width x length plane of the tape which was called as a hard bending.nding.

  • PDF

Bi-2223산화물 복합 초전도 테이프의 기계적 특성 평가 (Evaluation of Mechanical Properties in Bi-2223 Composite Superconducting Tapes)

  • 신형섭;최수용
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제3권2호
    • /
    • pp.1-4
    • /
    • 2001
  • For the practical use of a superconducting wire to magnet application, it is important to assess the Young modulus and other mechanical properties of HTS tapes. In order to establish a test method of mechanical properties for oxide composite superconductors. tensile tests of Bi-2223 multi- filamentary tapes were carried out at room temperature, as an activity of the International round robin test proposed by the committee of VAMAS/TWA 16-Subrgroup. The tapes consisting of mutli-filamentary showed a three stage tensile behavior. At the initial stage of the stress-streain curve. The elastic deformation existed in a quite nattrow strain region. But the plastic deformation was observed in a wide strain region due to the platic flow of the Ag alloy matrix. The results of RRT were also reported and discussed.

  • PDF

PIT법에 의한 Bi-2223 고온 초전도 테이프의 임계전류밀도 향상에 관한 연구 (A study on the improvements of Critical Current Density of Bi2223 Superconducting Tapes in PIT process)

  • 장현만;오상수;하동우;류강식;김상현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1996년도 춘계학술대회 논문집
    • /
    • pp.198-201
    • /
    • 1996
  • In order to investigate control factors to critical current density, Ag sheathed Bi2223 superconducting tapes were fabricated using PIT process. Optimizing the reduction ratio of rolling, critical current density 7f rolled Bi2223 tape could be improved with the value of 15,000 A/$\textrm{cm}^2$(77 K, zero field). The correlation between J$\_$c/ and work inhomogeneity was revealed as a dependence of COV of measured oxide layer thickness.

  • PDF

굽힘상태의 외부보강한 Bi-2223 초전도테이프에서 임계전류 열화특성에 미치는 인장변형률의 영향 (Effect of Tensile Strain on $I_c$ Degradation Characteristics In Bent Externally Reinforced Bi-2223 Superconducting Tapes)

  • 신형섭;김기현;오상수;하동우
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제6권1호
    • /
    • pp.6-11
    • /
    • 2004
  • The influences of mixed strain mode of bending-tension on the critical current. Ic in externally reinforced Bi-2223 tapes and their interaction were investigated in this study. A test fixture which providing a mixed deformation mode of bending-tension to HTS tapes has been newly devised. When the total strain induced in the tape in the mixed strain mode was expressed by the superposition of the bending and tensile strains the irreversible strain for the critical current degradation of Bi-2223 tapes increased, as compared with the simple bending mode case. The $I_c$ degradation at the region exceeding the irreversible strain showed a medium between the simple bending case and the simple tension case. As the initial bending strain imparted increased , namely as the diameter of mandrel adopted decreased. the apparent irreversible strain in Bi-2223 tapes increased . but the increment became smaller As a result. it can be found that the tension to be applied to bent Bi-2223 tapes during cabling should be smaller. as the mandrel diameter becomes smaller.

트위스트 피치를 고려한 Bi-2223 선재 제작과 AC 손실 측정 및 분석 (Fabrication, AC Loss Measurement and Analysis of Bi-2223 Conductors with Respect to Various Twist Pitch)

  • 장미혜;추용;임준형;주진호;고태국
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제49권11호
    • /
    • pp.589-595
    • /
    • 2000
  • In this papre, AC losses of Bi-2223 tapes with different twist pitch of superconducting core were fabricated, measured and analyzed. These samples produced by a powder-in-tube method are multi-filamentary tape with Ag matrix. Also, it's produced by non-twist and different twist pitch(8, 10, 13, 30, 50, 70 mn). The critical current measurement was carried out under the environment in Liquid nitrogen and in zero field by 4-probe method. And the AC loss measurement was carried out under the environment of applied time-varying transport current by transport method. From experiment, the critical current is larger non-twist than twisted filament. And, the AC loss by Norris equation is higher non-twisted tape than 13mm twisted tape. Also, it is confirmed that of AC loss of tape having non-twist pitch larger than those having differnet twist pitch.

  • PDF

Influence of External Reinforcement on Strain Characteristics of Critical Current in BSCCO Superconducting Tapes

  • Shin, Hyung-Seop;Kazumune Katagiri
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제5권3호
    • /
    • pp.15-19
    • /
    • 2003
  • For the purpose of standardization of the critical current measurement, it is meaningful to describe how $I_{c}$ will behave as the stress/strain level changes. In this study, strain dependencies of the critical current $I_{c}$ in Ag-alloy sheathed multifilamentary Bi(2212) and Bi(2223) superconducting tapes were evaluated at 77K, 0T. The external reinforcement was accomplished by soldering AgMgNi alloy tapes onto single or both sides of the sample. With the external reinforcement to the Bi(2212) tape, the strength of the tapes increased but the critical current at the strain free state, $I_{c0}$ decreased in some cases. The strain for onset of the $I_{c}$ degradation, $\varepsilon$$_{\irr}$, increased with an increase of the reinforcing volume and then saturated to a certain value. The effect of external reinforcement on the degradation of $I_{c}$ due to the bending strain in the Bi(2223) tape was also examined. Contrary to the expectation, it showed a significant $I_{c}$ degradation even at a small strain of 0.4 %. The observations of damage morphologies gave a good explanation to the $I_{c}$ behavior.c/ behavior.r.

BSCCO 초전도 선재의 미세조직 및 임계전류밀도에 미치는 공정변수 효과 (Effect of Processing Variables on Microstructure and Critical Current Density of BSCCO Superconductors Tape)

  • 지봉기;김태우;주진호;김원주;이희균;홍계원
    • 한국전기전자재료학회논문지
    • /
    • 제11권11호
    • /
    • pp.1014-1021
    • /
    • 1998
  • We evaluated the effect of processing variables on microstructural evolution interface irregularity between Ag sheath and superconductor core and resultant critical current density(J$_{c}$) of (Bi,Pb)$_2$Sr$_2$Ca$_2$Cu$_3$O$_{x}$(2223) superconductor tape. The value of J$_{c}$ was significantly influenced by the interface irregularity, degree of texturing and relative 2223 content. The interface became more irregular(sausage effect), while the degree of texturing gradually improved as the dimension of tape decreased during forming process. As the dimension of wire/tape were changed from diameter of 3.25 mm to thickness of 0.20 mm, J$_{c}$ value was observed to be increased by 10 times. In addition, optimum sintering temperature for improved J$_{c}$ was observed to be 835$^{\circ}C$ in a ambient atmosphere probably due to combined effect of both improved texturing and high 2223 content. Microstructural investigation showed the degree of texturing was degraded by the existence of both second phases and interface irregularity. It was observed that larger grain size and better texturing was developed near relatively flat interface compared to those inside superconducting core.ting core.

  • PDF

Correlation of the 2223 percentage before the first intermediate pressing and the transport property of the fully processed Bi-2223/Ag tapes

  • Jiang, C.H.;Yoo, J.M.;Ko, J.W.;Kim, Y.K.;Chung, H.S.
    • Progress in Superconductivity
    • /
    • 제4권1호
    • /
    • pp.94-98
    • /
    • 2002
  • Two kinds of multifilament Bi-2223/Ag tapes, which are different in the precursor calcination temperatures, were heat treated for different time (12, 20, 30, 50, 70, or 100 h) firstly to obtain varied B2223 contents, and then followed by the same pressing and sintering cycles. The relation of the 2223 phase contents after the first sintering and the transport property of the fully processed tapes was studied. The results show that 75-80% 2223 phase formed in tapes before the first cold pressing is beneficial to get a high $I_{c}$ in the final tapes. Compensating the total heat treatment time of the tapes first sintered for 20 h to the same length as that first sintered for 50 h in the subsequent sintering stages, different $I_{c}$ enhancements were observed in these two tapes. No improvement on $I_{c}$ was found in the tape made from the powder calcined at higher temperature, whereas for the tape prepared with the lower temperature calcined powder, the $I_{c}$ was increased to the same level as that first sintered for 50 h. The 2223 contents before the intermediate mechanical work is related to the residual reactants, especially to the liquid phase, which is of vital importance to the phase conversion and healing microcracks, meanwhile, to the size and distribution of the non-superconducting secondary phases. The lower temperature calcined powder resulted in slow formation of 2223 phase, but also provided more reactants and liquid phase for the further phase conversion, as a consequence, for the Improvement of $I_{c}$. c/.

  • PDF

고온초전도 BSCCO 2223 선재간의 초전도 접합부 제조연구 (Fabrication of superconducting Joints Between PIT Processed BSCCO 2223 Tapes by Single and Multiple Press & reaction Annealing)

  • 유재무;고재웅;정형식
    • 연구논문집
    • /
    • 통권27호
    • /
    • pp.175-181
    • /
    • 1997
  • Superconducting joints between Bi-2223/Ag tapes are fabricated by a press & reaction anneal and a multiple press & anneal. The silver sheath was mechanically or chemically removed from one side of each tape without altering the superconducting core. The exposed superconducting core of the two tapes were brought into contact and pressed so as to form a lap joint. The joined tapes were then subjected to a series of different thermomechanical treatments to achieve optimum heat treatment condition. The result from transport measurements shows that critical current ($I_c$) transmitting through joined area reaches 9A, approximately 60% of the current capacity of the tapes themselves. The critical current through joined area was improved by repeated press and reaction annealing. Measurements of the current-voltage relationship were made with several configuration of the voltage probes to characterize the critical current variation and I-V curve along the joint. Also discussed are microstructural aspects of the superconducting joint.

  • PDF