Bi-2223/Ag 고온초전도 선재의 기계적 특성 평가 (Evaluation of mechanical properties of Bi-2223/Ag HTS tapes)

  • 하홍수;이동훈;양주생;최정규;윤진국;하동우;오상수;권영길;김상철
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제4권1호
    • /
    • pp.45-59
    • /
    • 2002
  • Evaluation of the mechanical properties of Bi-2223/Ag HTS tapes was carried out by the tension and bending tests. Most of the Bi-2223/Ag tapes retained critical current up to 10 kgf/mm$_2$ axial tension stress, and 0.2% tension strain at room temperature. Applied tension strain exceeding 0.3% in superconducting tapes at 77 K leaded to rapid degradation of the critical current. It was observed that the more filaments, the better axial tension property at 77 K, self-field The influence of bending strain on critical current degradation was revealed to be less sensitive for Bi-2223/Ag HTS tapes with a more number of filaments and higher silver ratio.

HTS 케이블용 은시스 Bi-2223 테이프 및 원통형 적층 도체의 상전도 영역전파 특성 (Normal Zone Propagation Properties of Ag Sheathed Bi-2223 Tape for HTS Cable and Cylindrical Stacked Conductor)

  • 이병성;김영석;장현만;백승명;김상현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 추계학술대회 논문집
    • /
    • pp.448-451
    • /
    • 2000
  • Normal zone propagation(NZP) characteristics were investigated on Ag sheathed Bi-2223 tape and cylindrical stacked conductor. Normal zone propagation(N2P) experiments with tape were conducted with refrigerator in temperature from 45 K to 77 K, 0 T. Cylindrical stacked conductor was molding with epoxy and experiments were conducted with adiabatic condition in $LN_2$. NZP velocities of tape with two condition of DC and AC were almost same at each temperature. NZP velocities of cylindrical stacked conductor were 1.9-2.4 cdsec in $LN_2$. Numerical analysis was carried out by a one-dimensional heat balance equation. As a result, simulated results of NZP velocity with Bi-2223 tape were similar to experimental results in DC.

  • PDF

적층형 Bi-2223 고온초전도 선재 제작에 관한 연구 (A Study on fabrication of stacking type Bi-2223 HTS tapes)

  • 임성우;두호익;한병성
    • 한국전기전자재료학회논문지
    • /
    • 제13권8호
    • /
    • pp.718-723
    • /
    • 2000
  • The critical characteristics of Bi-2223 HTS tapes made by PIT method are influenced by the heat treatment and the mechanical processing. In this study firstly we investigated the influence o rolling reduction rate in mechanical process for improving Jc of HTS tapes. As a result the optimized rolling reduction rate that we obtained was 10%-50% and 30%-30% (1st-2nd). And then we fabricated the stacking type HTS tapes that made of the multi-filamentary tapes with various length(3, 5, 10cm) and with various number of stacking (1, 5, 10 layer). Measuring the critical current and observing the structure of grain we concluded that the stacking type tapes will be able to operate more stably by adding the number of stacking tapes. And we could expect that by minimizing the gap between Ag-sheath of tapes mechanical strength of stacking HTS tapes is enhanced and current in tapes will flow more stably.

  • PDF

Improvement of Critical Current In Bi-2223/Ag HTS Tapes by the Bubbling Control

  • 하홍수;오상수;하동우;이남진;김상철
    • Progress in Superconductivity
    • /
    • 제3권2호
    • /
    • pp.247-251
    • /
    • 2002
  • In general, the bubbling, generated during the fabrication of the tapes, breaks the superconducting filament, and critical current of the tapes will be decreased. Heat-treatment schemes of Bi-2223/Ag HTS tapes were modified, such as pre-annealing of multi-stacked billet, 2-step main sintering and ramp rate etc. The generation of bubbling was drastically decreased from 20 bubbles/m to 0 ~ 1 bubble/m by the modified heat-treatment. Therefore, the value of critical current of the tapes without bubbling was increased almost twice higher than that of already existing tapes. Critical current up to 42 A in 40 m length Bi-22231Ag tapes have been measured at 77K, self-field, 1$mutextrm{V}$/cm criterion. It could be confirmed that elimination of bubbling is effective to maintain the superconducting property along the tape length.

  • PDF

Bi-2223/Ag 고온초전도 선재의 bubbling 제어에 관한 연구 (A Study on Bubbling Control of Bi-2223/Ag HTS tapes)

  • 하홍수;오상수;하동우;송규정;김상철;권영길;류강식
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2001년도 학술대회 논문집
    • /
    • pp.145-148
    • /
    • 2001
  • Bi-2223/Ag HTS tapes fabricated by PIT process are used to make the power transmission cable, motor, fault current limiter, transformer etc. But some problems are still remained as like bubbling, sausaging to got the high Jc. In this study. we carried out the experiment to prevent bubbling in the HTS tape. The bubbling mainly occurred when HTS tape was heat-treating. Therefore, additional vacuum annealing at 400 ~ $600^{\circ}C$and slowly ramp-up sintering method were used to decrease the bubbling. slowly ramp-up sintering was more effective to decrease the bubbling than the vacuum annealing, but Jc was also decreased after heat treatment. Optimum ramp-up sintering schedule was searched to get the high critical current and prevent bubbling at same time.

  • PDF

고온초전도 선재 제작에 관한 연구 (A Study on fabrication of Bi-2223 HTSC Tapes)

  • 홍세은;두호익;김병숙;임성우;이종배;한병성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 하계학술대회 논문집
    • /
    • pp.235-238
    • /
    • 2000
  • There have been a lot of studies to improve the characteristic of Bi-2223 tape by PIT method which is considered as one of the best way for applying superconductor. These improved characteristic of Bi-2223 tape is able to be acqured by control of mechanical deformation and heat treatment. In this work, we studied HTS tapes with the sheath(Ag and Ag-alloy)of tapes that affect mechenical strength and critical current, with each two kind of purity(99.9% and 99.999%) and with two kind of tapes(single and double concentric). These charateristics affect Jc of tapes seriously that is the most important factor of superconductor tapes.

  • PDF

Bi-2223 고온초전도 선의 상용화 공정 연구 (Study on commercialization process of Bi-B223 HTS tape)

  • 하동우;김상철;오상수;하홍수;이동훈;양주생;황선역
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제6권1호
    • /
    • pp.1-5
    • /
    • 2004
  • Long length of Bi-2223/Ag superconducting wives were fabricated by stacking and drawing process with advanced heat-treatment schedules. Intermediate annealing was carried out to increase the homogeneity and uniformity of the superconducting filaments embedded in the silver matrix. Phase modification from tetragonal to orthorhombic Bi-2212 by pre heat treatment(PHT) was executed to improve the texture and phase transformation of Bi-2223. Drawing stress was measured to predict the sausaging and stress limit. Rolling Parameters such as thickness. width and winding tension were investigated to roll the tape with uniformity. 1 km length of Bi-2223/Ag superconducting wires were fabricated without any breakage. Critical current (Je) of 270 m length of superconducting tapes was measured over than $70 A/cm^2$ continuously after final sintering.

초전도 한류기를 이용한 Bi-2223/Ag 선재의 퀜치 보호를 위한 기초 연구 (Preliminary study on the quench protection of Bi-22231 Ag tape using superconducting fault current limiter)

  • 두호익;임성우;현옥배;황시돌;조철용;박충렬;한영성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.243-244
    • /
    • 2006
  • As an preliminary study for the quench protection of high temperature superconducting (HTS) cable using superconducting fault current limiter (SFCL), experimental research was carried out. The test circuit was composed of Bi-2223/Ag HTS tape and a SFCL made of YBCO thin films. In the normal state, the applied current of 56 A, which was critical current of HTS tape, could be flown through the circuit without resistive loss. Increasing the currents, the quench development of both materials was investigated from the voltage signal acquired from the resistance of the quenched superconductor. Up to around 10 times of the critical current was applied to the HTS tape and the current limiting characteristics of SFCL were investigated. In addition, for the finding out the optimal operating condition of SFCL such as the numbers of elements, a shunt resistor was applied to the SFCL and quench characteristics were analyzed as well.

  • PDF

Bi-2223 초전도 테이프의 접촉식 Ic 측정을 위한 단자 형상 및 압력 조사 (Study on terminal shape and pressure for contact type Ic measurement of long Bi-2223 tape)

  • 하동우;양주생;하홍수;오상수;권영길;류강식
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 초전도 자성체
    • /
    • pp.25-28
    • /
    • 2002
  • Contact type Ic measurement system is needed to measure Ic continuously for long Bi-2223 tapes. Voltage and current terminals were designed several shapes for 4-probe method Ic measurement. Voltage terminals were made with brass and current terminals were made with Cu. We used 2 kinds of Bi-2223 tapes with different strength. When we measured Ic of Bi-2223 tape with Ag-Mg sheath, The proper weight was 0.3 kg and sharp pin type was better. according to voltage terminal shape and load. In case of Bi-2223 tape with Ag-Mn sheath, the proper terminal weight was 4 kg and sharp pin type was bad. It was possible to make continuous contact type Ic measurement system because We could get proper data - terminal shapes and loads - through these experiments.

  • PDF