• 제목/요약/키워드: Bi superconductor

검색결과 241건 처리시간 0.018초

플라즈마 용사 BSCCO(Bismuth Strontium Calcium Copper Oxide) 초전도 피막의 접합 특성 (Joining Characteristics of Plasma Sprayed BSCCO Superconducting Coatings)

  • 박정식;조창은;고영봉;박광순;박경채
    • 한국표면공학회지
    • /
    • 제46권5호
    • /
    • pp.181-186
    • /
    • 2013
  • We performed plasma spraying for 2001 (Bi:Cu = 2:1), 0212 (Sr:Ca:Cu = 2:1:2) oxide powders. $Bi_2Sr_2CaCu_2Ox$ (2212) superconductor has been prepared by PMP-AT (partial melting process-annealing treatment). The 2212 phase is synthesized between Sr-Ca-Cu oxide coating layer (0212) and Bi-Cu oxide coating layer (2001) by movement of partial melted Bi on 2001 layer and the diffusion reaction (Cu, Sr, Ca) after PMP-AT. There are two different coating layers on joining process. The one is ABAB coating layers and the other is BAAB coating layers by arrangement of 2001 (A), 0212 (B) layers. We performed heat treatment these two different coating layers processes under same PMP-AT conditions. We obtained Bi-2212 superconducting layers at each experimental condition, and the result of MPMS, the critical temperature was showed about 78 K. But the microstructure images and result of EDS as each experimental variable were showed about the qualitatively different Bi-2212 superconducting phases. We also deduced the generation mechanism of Bi-2212 superconducting layer as a result of these experimental data, microstruc ture images, EDS data and phase diagram.

Phase Stability of Bi2212 and Bi2223 Thin Films Fabricated by Ion Beam Sputtering

  • Lee, Hee-Kab;Park, Yong-Pil;Kim, Jeong-Ho
    • 한국항해항만학회:학술대회논문집
    • /
    • 한국항해항만학회 2000년도 추계학술대회논문집
    • /
    • pp.108-111
    • /
    • 2000
  • Bi2212 and Bi2223 thin films are fabricated by ion beam sputtering method. Three phases of Bi2201, Bi2212 and Bi2223 appear as stable ones in spite of the condition for thin film fabrication of Bi2212 and bi2223 compositions, depending on substrate temperature(T$\sub$sub/) and ozone pressure (PO$_3$). It is found out that these phases show similar T$\sub$sub/ and PO$_3$dependence, and that the stable regions of these phases are limited within very narrow temperature.

  • PDF

Phase Stability of Bi2212 and Bi2223 Thin Films Fabricated by ion Beam Sputtering

  • Lee, Hee-Kab;Park, Yong-Pil;Kim, Jeong-Ho
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 추계학술대회 논문집
    • /
    • pp.108-111
    • /
    • 2000
  • Bi2212 and Bi2223 thin films are fabricated by ion beam sputtering method. Three phases of Bi2201, Bi2212 and Bi2223 appear as stable ones in spite of the condition for thin film fabrication of Bi2212 and bi2223 compositions, depending on substrate temperature(T$\sub$sub/) and ozone pressure (PO$_3$). It is found out that these phases show similar T$\sub$sub/ and PO$_3$ dependence, and that the stable regions of these phases are limited within very narrow temperature.

  • PDF

BSCCO 선재에서 초전도심의 깊이에 따른 집합조직 연구 (A study of texture through the depth of superconductor core)

  • 지봉기;임준형;이동욱;장석헌;주진호;나완수
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2001년도 학술대회 논문집
    • /
    • pp.6-8
    • /
    • 2001
  • We evaluated the degree of texture through depth of the superconductor core of Bi-Sr-Ca-Cu-O(BSCCO) superconductor tape. The degree of texture was characterized by pole figure analysis, indicating that the degree of texture varied significantly with depth of the superconductor core. It was observed that the degree of texture was higher near the interface than inside the superconducting core. Based on the result of degree of texture, the region near the interface is thought to carry significant current compared to that inside the core.

  • PDF

BSCCO 선재에서 극점도를 통한 초전도심의 깊이에 따른 집합조직 연구 (A Study of Texture Through the Depth of Core for BSCCO Superconductor Tape with Pole Figure Analysis)

  • 지봉기;주진호;나완수;류경우;박노진
    • 한국전기전자재료학회논문지
    • /
    • 제14권6호
    • /
    • pp.499-504
    • /
    • 2001
  • We evaluated the degree of texture through depth of the superconductor core of Bi-Sr-Ca-Cu-O(BSCCO) superconductor tape. The degree of texture was characterized by pole figure analysis indicating that the degree of texture varied significantly with depth of the superconductor core. It was observed that the degree of texture was higher near the interface than inside the superconductor core. Specifically, as getting near to the center from the sheath/core interface, the orientation of BSCCO became dispersed from normal direction(ND) which, in turn, resulted in the degradation of <001>-fiber texture. In addition, the <001> texture was non-uniform an, better texture was developed along rolling direction(RD), compared to transverse direction(TD). Microstructural investigation showed that grain alignment was locally degraded by the existence of second phases. I was observed that larger grain size and better texturing were developed near the relatively straight interface compared to those inside the superconducting core. Based on our study, the region near the interface is thought to carry significant current compared to that inside the core.

  • PDF

BPSCCO 자기 효과 (Magnetic Characteristics of BiPbSrCaCuO Oxide Superconductor)

  • 이상헌;이성갑;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 추계학술대회 논문집 Vol.16
    • /
    • pp.252-254
    • /
    • 2003
  • A magnetic field sensor is fabricated with superconducting ceramics system. The sensor at liquid nitrogen temperature shows the increase in electrical resistance by applying magnetic field. Actually, the voltage drop across the sensor is changed from zero to a value more than $100{\mu}V$ by the applied magnetic field. The change in electrical resistance depends on magnetic field. The sensitivity of this sensor is 2.9 ohm/T. The increase in electrical resistance by the magnetic field is ascribed to a modification of the Josephson junctions due to the penetrating magnetic flux into the superconducting material.

  • PDF

AC loss comparison of Bi-2223 and coated conductor HTS tapes under bending

  • Kim, Hae-Joon;Cho, Jeon-Wook;Sim, Ki-Deok;Kim, Jae-Ho;Kim, Seok-Ho;Jang, Hyun-Man;Lee, Soo-Gil
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제9권4호
    • /
    • pp.41-45
    • /
    • 2007
  • Superconductor is developed for applications in high-power devices such as power-transmission cables, transformers, motor and generators. In such applications, HTS tapes are subjected to various kinds of stress or strain. AC loss is also important consideration for many large-scale superconducting devices. In the fabrication of the devices, the critical current $(I_c)$ of the high temperature superconductor degrades due to many reasons including the tension applied by bending and thermal contraction. These bending or tension reduces the $I_c$ of superconducting wire and the $I_c$ degradation affects the AC loss of the wire. The $I_c$ degradation and AC loss (self field loss) of Bi-2223 HTS and Coated conductor were measured under tension and bending conditions at 77K and self-field.

고온 초전도체 팬케이크 코일의 퀜치 해석 (Quench Analysis in HTS Pancake Coil)

  • 박차식;안태길;박경우;김도형;차귀수;서정식
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제11권3호
    • /
    • pp.6-9
    • /
    • 2009
  • The thermal characteristics of quench propagation is a crucial problem for the stability of the superconductor. The objective of this study is to simulate the quench propagation with the variation of disturbance energy in Bi-2223/Ag HTS pancake coil. In this analysis, the temperature-time trace of a point away from heater was calculated under conditions of different quench energy. The critical disturbance energy between quench propagation and quench recovering was calculated, In addition, the minimum quench energy with different transport currents was obtained through the present simulation. These results are significant to the application of HTS.

고온 초전도 케이블용 Bi-2223 선재의 기계적 특성 (Mechanical Characteristics of Bi-2223 Wire for High-Tc Superconducting Cable)

  • 백승명;김영석;정순용;김상현
    • 한국전기전자재료학회논문지
    • /
    • 제11권11호
    • /
    • pp.1028-1034
    • /
    • 1998
  • Bi-2223 superconductor is known as one of the candidates for practical superconducting wires. Ag-sheathed Bi-2223 superconducting wires were fabricated using the powder-in-tube(PIT) method. When the 19-filaments wire was immersed in liquid nitrogen(77K), maximum critical current density Jc of 62 A/$mm_2$ at 0T was achieved. The critical current density has been shown to depend on the mechanical properties such as tensile stress and bending strain in Ag-sheathed Bi-2223 superconducting wires. The tensile strain for Jc degradation onset was in the range of 0.12~0.3%. In the case of 19-filaments wire, the bending strain is estimated to be smaller than 0.3% for the reasonable Jc value. The observed degradation of the critical current density due to strain effect is inevitable and can be attributed to the formation of microcracks within the superconducting core.

  • PDF

Bi-2223 고온초전도 선의 상용화 공정 연구 (Study on commercialization process of Bi-B223 HTS tape)

  • 하동우;김상철;오상수;하홍수;이동훈;양주생;황선역
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제6권1호
    • /
    • pp.1-5
    • /
    • 2004
  • Long length of Bi-2223/Ag superconducting wives were fabricated by stacking and drawing process with advanced heat-treatment schedules. Intermediate annealing was carried out to increase the homogeneity and uniformity of the superconducting filaments embedded in the silver matrix. Phase modification from tetragonal to orthorhombic Bi-2212 by pre heat treatment(PHT) was executed to improve the texture and phase transformation of Bi-2223. Drawing stress was measured to predict the sausaging and stress limit. Rolling Parameters such as thickness. width and winding tension were investigated to roll the tape with uniformity. 1 km length of Bi-2223/Ag superconducting wires were fabricated without any breakage. Critical current (Je) of 270 m length of superconducting tapes was measured over than $70 A/cm^2$ continuously after final sintering.